Volumn 265, Issue 3-4, 2008, Pages 468-476

Research on oxidation wear mechanism of the cast steels

Author keywords

Cast steel; Mechanism; Microstructure; Oxidation wear; Oxide film

Indexed keywords

MICROSTRUCTURE; OXIDE FILMS; THERMAL EFFECTS; X RAY DIFFRACTION ANALYSIS;

EID: 42749092923     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.wear.2007.11.015     Document Type: Article
Times cited : (96)

References (26)
  • 1
    • 0020767596 scopus 로고
    • Mild wear of a low alloy steel at temperatures up to 500 °C
    • Sullivan J.L., and Athwal S.S. Mild wear of a low alloy steel at temperatures up to 500 °C. Tribol. Int. 16 3 (1983) 123-131
    • (1983) Tribol. Int. , vol.16 , Issue.3 , pp. 123-131
    • Sullivan, J.L.1    Athwal, S.S.2
  • 2
    • 0019292476 scopus 로고
    • The sliding wear mechanisms of metals, mainly steels
    • Childs T.H.C. The sliding wear mechanisms of metals, mainly steels. Tribol. Int. 13 12 (1980) 285-293
    • (1980) Tribol. Int. , vol.13 , Issue.12 , pp. 285-293
    • Childs, T.H.C.1
  • 3
    • 0011651040 scopus 로고
    • Wear oxidation-a new component of wear
    • Fink M. Wear oxidation-a new component of wear. Trans. Am. Soc. Steel Treat. 18 (1930) 1026-1034
    • (1930) Trans. Am. Soc. Steel Treat. , vol.18 , pp. 1026-1034
    • Fink, M.1
  • 4
    • 0000199962 scopus 로고
    • The wear of metals under unlubricated conditions
    • Archard J.F., and Hirst W. The wear of metals under unlubricated conditions. Proc. R. Soc. A236 (1956) 394-410
    • (1956) Proc. R. Soc. , vol.A236 , pp. 394-410
    • Archard, J.F.1    Hirst, W.2
  • 5
    • 0017905196 scopus 로고
    • The division of heat and surface temperatures at sliding steel interfaces and their relation to oxidational wear
    • Quinn T.F.J. The division of heat and surface temperatures at sliding steel interfaces and their relation to oxidational wear. Trans. ASLE 21 (1978) 78-86
    • (1978) Trans. ASLE , vol.21 , pp. 78-86
    • Quinn, T.F.J.1
  • 6
    • 0019050535 scopus 로고
    • Developments in the oxidational theory of mild wear
    • Quinn T.F.J., Sullivan J.L., and Rowson D.M. Developments in the oxidational theory of mild wear. Tribol. Int. 13 4 (1980) 153-158
    • (1980) Tribol. Int. , vol.13 , Issue.4 , pp. 153-158
    • Quinn, T.F.J.1    Sullivan, J.L.2    Rowson, D.M.3
  • 7
    • 0032052403 scopus 로고    scopus 로고
    • Oxidational wear modelling Part 3. The effects of speed and elevated temperatures
    • Quinn T.F.J. Oxidational wear modelling Part 3. The effects of speed and elevated temperatures. Wear 216 (1998) 262-275
    • (1998) Wear , vol.216 , pp. 262-275
    • Quinn, T.F.J.1
  • 9
    • 0018983938 scopus 로고
    • The development of wear protective oxides and their influence on sliding friction
    • Wilson J.E., Stott F.H., and Wood G.C. The development of wear protective oxides and their influence on sliding friction. Proc. R. Soc. A369 (1980) 557-574
    • (1980) Proc. R. Soc. , vol.A369 , pp. 557-574
    • Wilson, J.E.1    Stott, F.H.2    Wood, G.C.3
  • 10
    • 0037532343 scopus 로고    scopus 로고
    • Microscopy of glazed layers formed during high temperature sliding wear at 750 °C
    • Inman I.A., Datta S., and Du H.L. Microscopy of glazed layers formed during high temperature sliding wear at 750 °C. Wear 254 (2003) 461-467
    • (2003) Wear , vol.254 , pp. 461-467
    • Inman, I.A.1    Datta, S.2    Du, H.L.3
  • 11
    • 0029294350 scopus 로고
    • Mechanism of oxidational wear
    • So H. Mechanism of oxidational wear. Wear 184 (1995) 161-167
    • (1995) Wear , vol.184 , pp. 161-167
    • So, H.1
  • 12
    • 0036852941 scopus 로고    scopus 로고
    • Formation and wear mechanism of tribo-oxides and the regime of oxidational wear of steel
    • So H., Yu D.S., and Chuang C.Y. Formation and wear mechanism of tribo-oxides and the regime of oxidational wear of steel. Wear 253 (2002) 1004-1015
    • (2002) Wear , vol.253 , pp. 1004-1015
    • So, H.1    Yu, D.S.2    Chuang, C.Y.3
  • 13
    • 0030172723 scopus 로고    scopus 로고
    • Wear behavior of steel 1080 with different microstructures during dry sliding
    • Wang Y., and Lei T. Wear behavior of steel 1080 with different microstructures during dry sliding. Wear 194 (1996) 44-53
    • (1996) Wear , vol.194 , pp. 44-53
    • Wang, Y.1    Lei, T.2
  • 14
    • 0042602594 scopus 로고
    • The influence of surface oxidation on the wear resistance of cast iron
    • Liu Y.C., Schissler J.M., and Mathia T.G. The influence of surface oxidation on the wear resistance of cast iron. Tribol. Int. 28 7 (1995) 433-438
    • (1995) Tribol. Int. , vol.28 , Issue.7 , pp. 433-438
    • Liu, Y.C.1    Schissler, J.M.2    Mathia, T.G.3
  • 15
    • 0031127416 scopus 로고    scopus 로고
    • Research on the wear characteristics of hypereutectoid steel
    • Marui E., Hasegawa N., Endo H., Tanaka K., and Hattori T. Research on the wear characteristics of hypereutectoid steel. Wear 205 (1997) 186-199
    • (1997) Wear , vol.205 , pp. 186-199
    • Marui, E.1    Hasegawa, N.2    Endo, H.3    Tanaka, K.4    Hattori, T.5
  • 16
    • 0028419739 scopus 로고
    • The role of hard second phases in the mild oxidational wear mechanism of high-speed steel-based materials
    • Vardavoulias M. The role of hard second phases in the mild oxidational wear mechanism of high-speed steel-based materials. Wear 173 (1994) 105-114
    • (1994) Wear , vol.173 , pp. 105-114
    • Vardavoulias, M.1
  • 17
    • 42749084143 scopus 로고    scopus 로고
    • X.H. Cui, High-temperature wear of a new-developed hot-forging cast die steel, PhD Thesis of Jilin University, 2006.
    • X.H. Cui, High-temperature wear of a new-developed hot-forging cast die steel, PhD Thesis of Jilin University, 2006.
  • 18
    • 21444449602 scopus 로고    scopus 로고
    • On the oxidation behaviour of 5CrNiMo steel under the high temperature wear condition
    • Jie X.H., and Mao Z.Y. On the oxidation behaviour of 5CrNiMo steel under the high temperature wear condition. J. Zhejiang Univ. 32 6 (1998) 769-774
    • (1998) J. Zhejiang Univ. , vol.32 , Issue.6 , pp. 769-774
    • Jie, X.H.1    Mao, Z.Y.2
  • 19
    • 0021412773 scopus 로고
    • Reciprocating sliding wear of 9% Cr steel in carbon dioxide at elevated temperatures
    • Sullivan J.L., and Granville N.W. Reciprocating sliding wear of 9% Cr steel in carbon dioxide at elevated temperatures. Tribol. Int. 17 2 (1984) 63-71
    • (1984) Tribol. Int. , vol.17 , Issue.2 , pp. 63-71
    • Sullivan, J.L.1    Granville, N.W.2
  • 20
    • 33748714857 scopus 로고
    • Alloying of Cr-Mo(W)-V type hot-working die steel
    • Ma M.Y., and Shong W. Alloying of Cr-Mo(W)-V type hot-working die steel. Hot Working Technol. 166 (1990) 40-45
    • (1990) Hot Working Technol. , vol.166 , pp. 40-45
    • Ma, M.Y.1    Shong, W.2
  • 21
    • 33746638733 scopus 로고
    • Metallurgy Industry Press of China, Beijing
    • Chen G.L. High Temperature Alloys (1988), Metallurgy Industry Press of China, Beijing
    • (1988) High Temperature Alloys
    • Chen, G.L.1
  • 22
    • 0024107496 scopus 로고
    • The temperature of rubbing bodies: Part 2. The distribution of temperatures
    • Archard J.F., and Rowntre R.A. The temperature of rubbing bodies: Part 2. The distribution of temperatures. Wear 128 (1988) 1-17
    • (1988) Wear , vol.128 , pp. 1-17
    • Archard, J.F.1    Rowntre, R.A.2
  • 23
    • 17544404503 scopus 로고
    • The delamination theory of wear
    • Suh N.P. The delamination theory of wear. Wear 25 (1973) 111-124
    • (1973) Wear , vol.25 , pp. 111-124
    • Suh, N.P.1
  • 24
    • 0000929676 scopus 로고
    • The determination of the elastic field of an ellipsoidal inclusion and related problems
    • Eshelby J.D. The determination of the elastic field of an ellipsoidal inclusion and related problems. Proc. R. Soc. Lond. Ser. A 24 (1957) 376-396
    • (1957) Proc. R. Soc. Lond. Ser. A , vol.24 , pp. 376-396
    • Eshelby, J.D.1
  • 25
    • 0017522719 scopus 로고
    • Mechanics of crack propagation in delamination wear
    • Fleming J.F., and Suh N.P. Mechanics of crack propagation in delamination wear. Wear 44 (1977) 39-56
    • (1977) Wear , vol.44 , pp. 39-56
    • Fleming, J.F.1    Suh, N.P.2
  • 26
    • 0017522722 scopus 로고
    • Mechanics of subsurface void nucleation in delamination wear
    • Jahanmir S., and Suh N.P. Mechanics of subsurface void nucleation in delamination wear. Wear 44 (1977) 17-38
    • (1977) Wear , vol.44 , pp. 17-38
    • Jahanmir, S.1    Suh, N.P.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.