Volumn 27, Issue 1, 2008, Pages 7-15

Mechanical and thermal cycling effects on the flexural strength of glass ceramics fused to titanium

Author keywords

Aging; Flexural strength; Titanium

Indexed keywords

ALUMINUM OXIDE; BIOMEDICAL AND DENTAL MATERIALS; GLASS; TITANIUM; TITANIUM DIOXIDE; WATER;

EID: 42449111293     PISSN: 02874547     EISSN: None     Source Type: Journal    
DOI: 10.4012/dmj.27.7     Document Type: Article
Times cited : (43)

References (45)
  • 1
    • 0030155746 scopus 로고    scopus 로고
    • Titanium for prosthodontic applications: A review of the literature
    • Wang RR, Fenton A. Titanium for prosthodontic applications: a review of the literature. Quintessence Int 1996; 27: 401-408.
    • (1996) Quintessence Int , vol.27 , pp. 401-408
    • Wang, R.R.1    Fenton, A.2
  • 2
    • 0027616999 scopus 로고
    • Titanium and titanium alloys as dental materials
    • Lautenschlager EP, Monaghan P. Titanium and titanium alloys as dental materials. Int Dent J 1993; 43: 245-253.
    • (1993) Int Dent J , vol.43 , pp. 245-253
    • Lautenschlager, E.P.1    Monaghan, P.2
  • 3
    • 0028500487 scopus 로고
    • Bonding of low-fusing dental porcelain to commercially pure titanium
    • Könönen M, Kivilahti J. Bonding of low-fusing dental porcelain to commercially pure titanium. J Biomed Mater Res 1994; 28: 1027-1035.
    • (1994) J Biomed Mater Res , vol.28 , pp. 1027-1035
    • Könönen, M.1    Kivilahti, J.2
  • 6
    • 0025444240 scopus 로고
    • Oxidation effects on porcelain-titanium interface reactions and bond strength
    • Kimura H, Horng CJ, Okazaki M, Takahashi J. Oxidation effects on porcelain-titanium interface reactions and bond strength. Dent Mater J 1990; 9: 91-99.
    • (1990) Dent Mater J , vol.9 , pp. 91-99
    • Kimura, H.1    Horng, C.J.2    Okazaki, M.3    Takahashi, J.4
  • 7
    • 0025439635 scopus 로고
    • Oxide adherence and porcelain bonding to titanium and Ti-6Al-4V alloy
    • Adachi M, Mackert JR Jr, Parry EE, Fairhurst CW. Oxide adherence and porcelain bonding to titanium and Ti-6Al-4V alloy. J Dent Res 1990; 69: 1230-1235.
    • (1990) J Dent Res , vol.69 , pp. 1230-1235
    • Adachi, M.1    Mackert Jr, J.R.2    Parry, E.E.3    Fairhurst, C.W.4
  • 8
    • 0035000757 scopus 로고    scopus 로고
    • Fusing of dental ceramics to titanium
    • Könönen M, Kivilahti J. Fusing of dental ceramics to titanium. J Dent Res 2001; 80: 840-854.
    • (2001) J Dent Res , vol.80 , pp. 840-854
    • Könönen, M.1    Kivilahti, J.2
  • 9
    • 46349087472 scopus 로고    scopus 로고
    • Anusavice KJ. Phillips: Materiais dentários, Trad Dourado et al., 11th ed, Elsevier, Rio de Janeiro, 2005, p.763.
    • Anusavice KJ. Phillips: Materiais dentários, Trad Dourado et al., 11th ed, Elsevier, Rio de Janeiro, 2005, p.763.
  • 10
    • 0030276530 scopus 로고    scopus 로고
    • The physical properties of low-fusing porcelains for titanium
    • Esquivel JF, Chai J, Wozniak WT. The physical properties of low-fusing porcelains for titanium. Int J Prosthodont 1996; 9: 563-571.
    • (1996) Int J Prosthodont , vol.9 , pp. 563-571
    • Esquivel, J.F.1    Chai, J.2    Wozniak, W.T.3
  • 11
    • 0027142077 scopus 로고
    • Mold filling and porosity in castings of titanium
    • Herø H, Syverud M, Waarli M. Mold filling and porosity in castings of titanium. Dent Mater 1993; 19: 15-18.
    • (1993) Dent Mater , vol.19 , pp. 15-18
    • Herø, H.1    Syverud, M.2    Waarli, M.3
  • 12
    • 0028504438 scopus 로고
    • A comparison of the hardness of different types of titanium and conventional metal ceramics
    • King AW, Lautenschlager E, Chai J, Gilbert J. A comparison of the hardness of different types of titanium and conventional metal ceramics. J Prosthet Dent 1994; 72: 314-319.
    • (1994) J Prosthet Dent , vol.72 , pp. 314-319
    • King, A.W.1    Lautenschlager, E.2    Chai, J.3    Gilbert, J.4
  • 13
    • 16144367589 scopus 로고
    • Mold filling of Ti casting using investments with different gas permeability
    • Syverud M, Herø H. Mold filling of Ti casting using investments with different gas permeability. Dent Mater 1995; 11: 14-18.
    • (1995) Dent Mater , vol.11 , pp. 14-18
    • Syverud, M.1    Herø, H.2
  • 14
    • 0033087402 scopus 로고    scopus 로고
    • Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain
    • Yilmaz H, Dinçer C. Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain. J Dent 1999; 27: 215-222.
    • (1999) J Dent , vol.27 , pp. 215-222
    • Yilmaz, H.1    Dinçer, C.2
  • 16
    • 0030161883 scopus 로고    scopus 로고
    • Designs of bond strength tests for metal ceramic complexes: Review of the literature
    • Hammad IA, Talic YF. Designs of bond strength tests for metal ceramic complexes: review of the literature. J Prosthet Dent 1996; 75: 602-608.
    • (1996) J Prosthet Dent , vol.75 , pp. 602-608
    • Hammad, I.A.1    Talic, Y.F.2
  • 17
    • 0031083224 scopus 로고    scopus 로고
    • Relationship between static chemical and cyclic mechanical fatigue in a feldspathic porcelain
    • White SN, Li ZC, Yu Z, Kipnis V. Relationship between static chemical and cyclic mechanical fatigue in a feldspathic porcelain. Dent Mater 1997; 13: 103-110.
    • (1997) Dent Mater , vol.13 , pp. 103-110
    • White, S.N.1    Li, Z.C.2    Yu, Z.3    Kipnis, V.4
  • 18
    • 0033222301 scopus 로고    scopus 로고
    • The fatigue strength of the interface between Ag-Pd alloy and hydrothermal ceramic
    • Poljak-Guberina R, Catovic A, Jerolimov V, Franz M, Bergman V. The fatigue strength of the interface between Ag-Pd alloy and hydrothermal ceramic. Dent Mater 1999; 15: 417-420.
    • (1999) Dent Mater , vol.15 , pp. 417-420
    • Poljak-Guberina, R.1    Catovic, A.2    Jerolimov, V.3    Franz, M.4    Bergman, V.5
  • 19
    • 0030160162 scopus 로고    scopus 로고
    • Three-point bending strength of ceramics fused to cast titanium
    • Pröbster L, Maiwald U, Weber H. Three-point bending strength of ceramics fused to cast titanium. Eur J Oral Sci 1996; 104: 313-319.
    • (1996) Eur J Oral Sci , vol.104 , pp. 313-319
    • Pröbster, L.1    Maiwald, U.2    Weber, H.3
  • 20
    • 0031617238 scopus 로고    scopus 로고
    • Interfacial reactions of cast titanium with mold materials
    • Wang RR, Welsch GE, Castro-Cedeno M. Interfacial reactions of cast titanium with mold materials. Int J Prosthodont 1998; 11: 33-43.
    • (1998) Int J Prosthodont , vol.11 , pp. 33-43
    • Wang, R.R.1    Welsch, G.E.2    Castro-Cedeno, M.3
  • 21
    • 46349108044 scopus 로고    scopus 로고
    • Evaluation of low-fusing ceramic systems combined with titanium grades II and V by bending test and scanning electron microscopy
    • Garbelini WJ, Henriques GEP, Tróia Júnior M, Mesquita MF, Dezan CC. Evaluation of low-fusing ceramic systems combined with titanium grades II and V by bending test and scanning electron microscopy. J Appl Oral Sci 2003; 11: 354-360.
    • (2003) J Appl Oral Sci , vol.11 , pp. 354-360
    • Garbelini, W.J.1    Henriques, G.E.P.2    Tróia Júnior, M.3    Mesquita, M.F.4    Dezan, C.C.5
  • 22
    • 2942544834 scopus 로고    scopus 로고
    • Evaluation of shear bond strength at the interface of two porcelains and pure titanium injected into the casting mold at three different temperatures
    • Bondioli IR, Bottino MR. Evaluation of shear bond strength at the interface of two porcelains and pure titanium injected into the casting mold at three different temperatures. J Prosthet Dent 2004; 91: 541-547.
    • (2004) J Prosthet Dent , vol.91 , pp. 541-547
    • Bondioli, I.R.1    Bottino, M.R.2
  • 23
    • 4243558954 scopus 로고    scopus 로고
    • International Organization for Standardization, Geneva
    • International Organization for Standardization. ISO 9693: Metal-ceramic dental restorative systems, Geneva, 1999, pp.1-14.
    • (1999) ISO 9693: Metal-ceramic dental restorative systems , pp. 1-14
  • 24
    • 0017658030 scopus 로고
    • Ceramo-metal restorations
    • Riley EJ. Ceramo-metal restorations. Dent Clin North Am 1977; 21: 669-682.
    • (1977) Dent Clin North Am , vol.21 , pp. 669-682
    • Riley, E.J.1
  • 25
    • 0028402743 scopus 로고
    • Bond characteristics of porcelain fused to milled titanium
    • Gilbert JL, Covey DA, Lautenschlager EP. Bond characteristics of porcelain fused to milled titanium. Dent Mater 1994; 10: 134-140.
    • (1994) Dent Mater , vol.10 , pp. 134-140
    • Gilbert, J.L.1    Covey, D.A.2    Lautenschlager, E.P.3
  • 26
    • 0029181886 scopus 로고
    • Bonding characteristic of low fusing porcelain bonded to pure titanium and palladium-copper alloy
    • Pang IC, Gilbert JL, Chai J, Lautenschlager EP. Bonding characteristic of low fusing porcelain bonded to pure titanium and palladium-copper alloy. J Prosthet Dent 1995; 73: 17-25.
    • (1995) J Prosthet Dent , vol.73 , pp. 17-25
    • Pang, I.C.1    Gilbert, J.L.2    Chai, J.3    Lautenschlager, E.P.4
  • 27
    • 0030162904 scopus 로고    scopus 로고
    • Strength of porcelain fused to titanium beams
    • White SN, Ho L, Caputo AA, Goo E. Strength of porcelain fused to titanium beams. J Prosthet Dent 1996; 75: 640-648.
    • (1996) J Prosthet Dent , vol.75 , pp. 640-648
    • White, S.N.1    Ho, L.2    Caputo, A.A.3    Goo, E.4
  • 28
    • 17344374992 scopus 로고    scopus 로고
    • The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminumvanadium alloy
    • Tróia Jr MG, Henriques GEP, Nóbilo MAA, Mesquita MF. The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminumvanadium alloy. Dent Mater 2003; 19: 790-796.
    • (2003) Dent Mater , vol.19 , pp. 790-796
    • Tróia Jr, M.G.1    Henriques, G.E.P.2    Nóbilo, M.A.A.3    Mesquita, M.F.4
  • 29
    • 0043071591 scopus 로고    scopus 로고
    • Adhesion of porcelain to titanium and a titanium alloy
    • Suansuwan N, Swain MV. Adhesion of porcelain to titanium and a titanium alloy. J Dent 2003; 31: 509-518.
    • (2003) J Dent , vol.31 , pp. 509-518
    • Suansuwan, N.1    Swain, M.V.2
  • 30
    • 0033222608 scopus 로고    scopus 로고
    • New approach for evaluating metal-porcelain interfacial bonding
    • Suansuwan N, Swain MV. New approach for evaluating metal-porcelain interfacial bonding. Int J Prosthodont 1999; 12: 547-552.
    • (1999) Int J Prosthodont , vol.12 , pp. 547-552
    • Suansuwan, N.1    Swain, M.V.2
  • 31
    • 0035342531 scopus 로고    scopus 로고
    • Porcelain adherence to dental cast CP titanium: Effects of surface modifications
    • Cai Z, Bunce N, Nunn ME, Okabe T. Porcelain adherence to dental cast CP titanium: effects of surface modifications. Biomater 2001; 22: 979-986.
    • (2001) Biomater , vol.22 , pp. 979-986
    • Cai, Z.1    Bunce, N.2    Nunn, M.E.3    Okabe, T.4
  • 32
    • 0020339536 scopus 로고
    • Effect of magnesia investments in the dental casting of pure titanium or titanium alloys
    • Ida K, Togaya T, Tsutsumi S, Takeuchi M. Effect of magnesia investments in the dental casting of pure titanium or titanium alloys. Dent Mater J 1982; 1: 8-21.
    • (1982) Dent Mater J , vol.1 , pp. 8-21
    • Ida, K.1    Togaya, T.2    Tsutsumi, S.3    Takeuchi, M.4
  • 33
    • 4644297571 scopus 로고    scopus 로고
    • Pure titanium casting into zirconia-modified magnesia-based investment molds
    • Hung CC, Hou GL, Tsai CC, Huang CC. Pure titanium casting into zirconia-modified magnesia-based investment molds. Dent Mater 2004; 20: 846-851.
    • (2004) Dent Mater , vol.20 , pp. 846-851
    • Hung, C.C.1    Hou, G.L.2    Tsai, C.C.3    Huang, C.C.4
  • 34
    • 46349092544 scopus 로고    scopus 로고
    • German Standard Institution. DIN 13.927 metal-ceramic system, Beuth, Berlin, 1990.
    • German Standard Institution. DIN 13.927 metal-ceramic system, Beuth, Berlin, 1990.
  • 35
    • 0028894635 scopus 로고
    • Fracture toughness and flexural strength of dental ceramics for titanium
    • Kvam K, Derand T, Austrheim EK. Fracture toughness and flexural strength of dental ceramics for titanium. Biomaterials 1995; 16: 73-76.
    • (1995) Biomaterials , vol.16 , pp. 73-76
    • Kvam, K.1    Derand, T.2    Austrheim, E.K.3
  • 36
    • 0141798905 scopus 로고    scopus 로고
    • Monotonic flexure and fatigue strength of composites for provisional and definitive restorations
    • Scherrer SS, Wiskott AH, Coto-Hunziker V, Belser UC. Monotonic flexure and fatigue strength of composites for provisional and definitive restorations. J Prosthet Dent 2003; 89: 579-588.
    • (2003) J Prosthet Dent , vol.89 , pp. 579-588
    • Scherrer, S.S.1    Wiskott, A.H.2    Coto-Hunziker, V.3    Belser, U.C.4
  • 37
    • 0034317060 scopus 로고    scopus 로고
    • Fatigue of biomaterials: A review
    • Teoh SH. Fatigue of biomaterials: a review. Int Biomat Fatigue 2000; 22: 825-837.
    • (2000) Int Biomat Fatigue , vol.22 , pp. 825-837
    • Teoh, S.H.1
  • 39
    • 0024345249 scopus 로고
    • Studies of Ti alloys for dental castings
    • Taira M, Moser JB, Greener EH. Studies of Ti alloys for dental castings. Dent Mater 1989; 5: 45-50.
    • (1989) Dent Mater , vol.5 , pp. 45-50
    • Taira, M.1    Moser, J.B.2    Greener, E.H.3
  • 40
    • 0032195704 scopus 로고    scopus 로고
    • A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry
    • Özcan M, Pfeiffer P, Nergiz İ. A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry. Quintessence Int 1998; 29: 713-724.
    • (1998) Quintessence Int , vol.29 , pp. 713-724
    • Özcan, M.1    Pfeiffer, P.2    Nergiz, I.3
  • 41
    • 0142093511 scopus 로고    scopus 로고
    • Effect of laboratory procedures and thermocycling on the shear bond strength of resin-metal bonding systems
    • Kim JY, Pfeiffer P, Niedermeier W. Effect of laboratory procedures and thermocycling on the shear bond strength of resin-metal bonding systems. J Prosthet Dent 2003; 90: 184-189.
    • (2003) J Prosthet Dent , vol.90 , pp. 184-189
    • Kim, J.Y.1    Pfeiffer, P.2    Niedermeier, W.3
  • 42
    • 3242656250 scopus 로고    scopus 로고
    • Comparative strength of metal-ceramic and metal-composite bonds after extended thermocycling
    • Shimoe S, Tanoue N, Yanagida H, Atsuta M, Koizumi H, Matsumura H. Comparative strength of metal-ceramic and metal-composite bonds after extended thermocycling. J Oral Rehabil 2004; 31: 689-694.
    • (2004) J Oral Rehabil , vol.31 , pp. 689-694
    • Shimoe, S.1    Tanoue, N.2    Yanagida, H.3    Atsuta, M.4    Koizumi, H.5    Matsumura, H.6
  • 43
    • 33749072477 scopus 로고    scopus 로고
    • Effect of mechanical cycling on the flexural strength of densely sintered ceramics
    • Itinoche KM, Özcan M, Bottino MA, Oyafuso D. Effect of mechanical cycling on the flexural strength of densely sintered ceramics. Dent Mater 2006; 22: 1029-1034.
    • (2006) Dent Mater , vol.22 , pp. 1029-1034
    • Itinoche, K.M.1    Özcan, M.2    Bottino, M.A.3    Oyafuso, D.4
  • 44
    • 0033071448 scopus 로고    scopus 로고
    • Thermal cycling procedures for laboratory testing of dental restorations
    • Gale MS, Darwell BW. Thermal cycling procedures for laboratory testing of dental restorations. J Dent 1999; 27: 89-99.
    • (1999) J Dent , vol.27 , pp. 89-99
    • Gale, M.S.1    Darwell, B.W.2
  • 45
    • 0033072233 scopus 로고    scopus 로고
    • In vitro study of the effect of thermo- and load-cycling on the bond strength of porcelain repair systems
    • Leibrock A, Degenhart M, Behr M, Rosentritt M, Handel G. In vitro study of the effect of thermo- and load-cycling on the bond strength of porcelain repair systems. J Oral Rehabil 1999; 26: 130-137.
    • (1999) J Oral Rehabil , vol.26 , pp. 130-137
    • Leibrock, A.1    Degenhart, M.2    Behr, M.3    Rosentritt, M.4    Handel, G.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.