Volumn 36, Issue 3, 2008, Pages 186-193

Water uptake and strength characteristics of a nanofilled resin-based composite

Author keywords

Bi axial flexure strength; Nanotechnology; Near infrared spectroscopy; Resin composite; Water sorption

Indexed keywords

FILTEK SUPREME; FILTEK SUPREME TRANSLUCENT; FILTEK Z250; NANOCOMPOSITE; RESIN; UNCLASSIFIED DRUG;

EID: 39149088948     PISSN: 03005712     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jdent.2007.11.015     Document Type: Article
Times cited : (136)

References (42)
  • 1
    • 2942579251 scopus 로고    scopus 로고
    • Amalgam toxicity-environmental and occupational hazards
    • Hörsted-Bindslev P. Amalgam toxicity-environmental and occupational hazards. Journal of Dentistry 32 (2004) 359-365
    • (2004) Journal of Dentistry , vol.32 , pp. 359-365
    • Hörsted-Bindslev, P.1
  • 3
    • 33845305843 scopus 로고    scopus 로고
    • A retrospective clinical study on longevity of posterior composite and amalgam restorations
    • Opdam N.J.M., Bronkhorst E.M., Roeters J.M., and Loomans B.A.C. A retrospective clinical study on longevity of posterior composite and amalgam restorations. Dental Materials 23 (2007) 2-8
    • (2007) Dental Materials , vol.23 , pp. 2-8
    • Opdam, N.J.M.1    Bronkhorst, E.M.2    Roeters, J.M.3    Loomans, B.A.C.4
  • 4
    • 27644560202 scopus 로고    scopus 로고
    • Outcome of direct restorations placed within the general dental services in England and Wales. Part 1. Variation by type of restoration and re-intervention
    • Lucarotti P.S.K., Holder R.L., and Burke F.J.T. Outcome of direct restorations placed within the general dental services in England and Wales. Part 1. Variation by type of restoration and re-intervention. Journal of Dentistry 33 (2005) 805-815
    • (2005) Journal of Dentistry , vol.33 , pp. 805-815
    • Lucarotti, P.S.K.1    Holder, R.L.2    Burke, F.J.T.3
  • 5
    • 39149086760 scopus 로고    scopus 로고
    • Bowen RL. Dental filling materials comprising of vinyl-silane fused silica and binder consisting of the reaction product of bispenol and glycidyl methacrylate. US Patent 3,066,112; 1962.
    • Bowen RL. Dental filling materials comprising of vinyl-silane fused silica and binder consisting of the reaction product of bispenol and glycidyl methacrylate. US Patent 3,066,112; 1962.
  • 8
    • 39149107512 scopus 로고    scopus 로고
    • Exploring whether 'nano' is always necessary
    • Harris J., and Ure D. Exploring whether 'nano' is always necessary. Nanotechnology Perceptions 2 (2006) 1-15
    • (2006) Nanotechnology Perceptions , vol.2 , pp. 1-15
    • Harris, J.1    Ure, D.2
  • 9
    • 33749599209 scopus 로고    scopus 로고
    • Nanomedicine for implants: a review of studies and necessary experimental tools
    • Lui H., and Webster T.J. Nanomedicine for implants: a review of studies and necessary experimental tools. Biomaterials 28 (2007) 354-369
    • (2007) Biomaterials , vol.28 , pp. 354-369
    • Lui, H.1    Webster, T.J.2
  • 10
    • 39149105348 scopus 로고    scopus 로고
    • CARE Group Of Professional Services. Ivoclar Vivadent Inc. Nanofillers?: a microfill by any other name is still a microfill. Nanofillers; August 2003.
    • CARE Group Of Professional Services. Ivoclar Vivadent Inc. Nanofillers?: a microfill by any other name is still a microfill. Nanofillers; August 2003.
  • 11
    • 25144479062 scopus 로고    scopus 로고
    • The reliability of standardized flexure strength testing procedures for a light-activated resin-based composite
    • Palin W.M., Fleming G.J.P., and Marquis O.M. The reliability of standardized flexure strength testing procedures for a light-activated resin-based composite. Dental Materials 21 (2005) 911-919
    • (2005) Dental Materials , vol.21 , pp. 911-919
    • Palin, W.M.1    Fleming, G.J.P.2    Marquis, O.M.3
  • 13
    • 0025617576 scopus 로고
    • Influence of the test method on failure stress of brittle dental materials
    • Ban S., and Anusavice K.J. Influence of the test method on failure stress of brittle dental materials. Journal of Dental Research 69 (1990) 1791-1799
    • (1990) Journal of Dental Research , vol.69 , pp. 1791-1799
    • Ban, S.1    Anusavice, K.J.2
  • 14
    • 0038621198 scopus 로고
    • Determination of water by near-infrared spectrophotometry
    • Keyworth D.A. Determination of water by near-infrared spectrophotometry. Talanta 8 (1961) 461-469
    • (1961) Talanta , vol.8 , pp. 461-469
    • Keyworth, D.A.1
  • 15
    • 0026245543 scopus 로고
    • NIR-spectroscopic investigation of water sorption characteristics of dental resins and composites
    • Venz S., and Dickens B. NIR-spectroscopic investigation of water sorption characteristics of dental resins and composites. Journal of Biomedical Materials Research 25 (1991) 1231-1248
    • (1991) Journal of Biomedical Materials Research , vol.25 , pp. 1231-1248
    • Venz, S.1    Dickens, B.2
  • 16
    • 0026831219 scopus 로고
    • Measurement of water sorption by resin composites adhesives with near-infrared spectroscopy
    • Diaz-Arnold A.M., and Williams V.D. Measurement of water sorption by resin composites adhesives with near-infrared spectroscopy. Journal of Dental Research 71 (1992) 438-442
    • (1992) Journal of Dental Research , vol.71 , pp. 438-442
    • Diaz-Arnold, A.M.1    Williams, V.D.2
  • 17
    • 0018449925 scopus 로고
    • Long-term water sorption and solubility of composite filling materials
    • Pearson J. Long-term water sorption and solubility of composite filling materials. Journal of Dentistry 7 (1979) 64-68
    • (1979) Journal of Dentistry , vol.7 , pp. 64-68
    • Pearson, J.1
  • 18
    • 0025113813 scopus 로고
    • Water sorption and mechanical properties of dental composites
    • Bastoli C., Romano G., and Migliaresi C. Water sorption and mechanical properties of dental composites. Biomaterials 11 (1990) 219-223
    • (1990) Biomaterials , vol.11 , pp. 219-223
    • Bastoli, C.1    Romano, G.2    Migliaresi, C.3
  • 19
    • 0030307272 scopus 로고    scopus 로고
    • Filler leachability of composites stored in distilled water or artificial saliva
    • Söderholm K.J.M., Mukherjee R., and Longmate J. Filler leachability of composites stored in distilled water or artificial saliva. Journal of Dental Research 75 (1996) 1692-1699
    • (1996) Journal of Dental Research , vol.75 , pp. 1692-1699
    • Söderholm, K.J.M.1    Mukherjee, R.2    Longmate, J.3
  • 21
    • 23444437486 scopus 로고    scopus 로고
    • The influence of short and medium-term water immersion on the hydrolytic stability of novel low-shrink dental composites
    • Palin W.M., Fleming G.J., Burke F.J., Marquis P.M., and Randall R.C. The influence of short and medium-term water immersion on the hydrolytic stability of novel low-shrink dental composites. Dental Materials 21 (2005) 852-863
    • (2005) Dental Materials , vol.21 , pp. 852-863
    • Palin, W.M.1    Fleming, G.J.2    Burke, F.J.3    Marquis, P.M.4    Randall, R.C.5
  • 22
    • 0032618888 scopus 로고    scopus 로고
    • Effect of water on the physical properties of resin-modified glass ionomer cements
    • Catteni-Lorente M.A., Dupuis V., Payan F., Moya F., and Meyer J.M. Effect of water on the physical properties of resin-modified glass ionomer cements. Dental Materials 15 (1999) 71-78
    • (1999) Dental Materials , vol.15 , pp. 71-78
    • Catteni-Lorente, M.A.1    Dupuis, V.2    Payan, F.3    Moya, F.4    Meyer, J.M.5
  • 23
    • 0037978003 scopus 로고    scopus 로고
    • Hygroscopic expansion and solubility of composite restoratives
    • Martin N., Jedynakiewicz N.M., and Fisher A.C. Hygroscopic expansion and solubility of composite restoratives. Dental Materials 19 (2003) 77-86
    • (2003) Dental Materials , vol.19 , pp. 77-86
    • Martin, N.1    Jedynakiewicz, N.M.2    Fisher, A.C.3
  • 24
    • 0032488231 scopus 로고    scopus 로고
    • In vitro aging of dental composites in water-effect of degree of conversion, filler volume and filler/matrix coupling
    • Ferracane J.L., Berge H.X., and Condon J.R. In vitro aging of dental composites in water-effect of degree of conversion, filler volume and filler/matrix coupling. Journal of Biomedical Materials Research 42 (1998) 465-472
    • (1998) Journal of Biomedical Materials Research , vol.42 , pp. 465-472
    • Ferracane, J.L.1    Berge, H.X.2    Condon, J.R.3
  • 25
    • 22544463664 scopus 로고    scopus 로고
    • Effects of resin hydrophilicity on water sorption and changes in modulus of elasticity
    • Ito S., Masanori H., Wadgaonkar B., Svizero N., Carvalho M., Yiu C., et al. Effects of resin hydrophilicity on water sorption and changes in modulus of elasticity. Biomaterials 26 (2005) 6449-6459
    • (2005) Biomaterials , vol.26 , pp. 6449-6459
    • Ito, S.1    Masanori, H.2    Wadgaonkar, B.3    Svizero, N.4    Carvalho, M.5    Yiu, C.6
  • 26
    • 0025583354 scopus 로고
    • Influence of water exposure on the tensile strength of composites
    • Söderholm K.J.M., and Roberts M.J. Influence of water exposure on the tensile strength of composites. Journal of Dental Research 69 (1990) 1812-1816
    • (1990) Journal of Dental Research , vol.69 , pp. 1812-1816
    • Söderholm, K.J.M.1    Roberts, M.J.2
  • 28
    • 0023900123 scopus 로고
    • Influence of filler type and water exposure on flexural strength of experimental composite resins
    • Calais J.G., and Söderholm K.J.M. Influence of filler type and water exposure on flexural strength of experimental composite resins. Journal of Dental Research 67 (1988) 836-840
    • (1988) Journal of Dental Research , vol.67 , pp. 836-840
    • Calais, J.G.1    Söderholm, K.J.M.2
  • 30
    • 0032618887 scopus 로고    scopus 로고
    • The influence of clinically induced variability on the biaxial fracture strength of cemented aluminous core porcelain discs
    • Fleming G.J.P., Shelton R.M., and Marquis P.M. The influence of clinically induced variability on the biaxial fracture strength of cemented aluminous core porcelain discs. Dental Materials 15 (1999) 62-70
    • (1999) Dental Materials , vol.15 , pp. 62-70
    • Fleming, G.J.P.1    Shelton, R.M.2    Marquis, P.M.3
  • 31
    • 0035430297 scopus 로고    scopus 로고
    • An evaluation of the technique of a hydrothermal low-fusing dental ceramic
    • Palin W.M., Fleming G.J.P., and Marquis P.M. An evaluation of the technique of a hydrothermal low-fusing dental ceramic. Journal of Dentistry 29 (2001) 443-449
    • (2001) Journal of Dentistry , vol.29 , pp. 443-449
    • Palin, W.M.1    Fleming, G.J.P.2    Marquis, P.M.3
  • 33
    • 34047201755 scopus 로고    scopus 로고
    • Adhesive and bending failure of thermal sprayed hydroapatite coatings: effect of nanostructures at interface ad crack propagation phenomenon during bending
    • Li H., Khor K.A., and Cheang P. Adhesive and bending failure of thermal sprayed hydroapatite coatings: effect of nanostructures at interface ad crack propagation phenomenon during bending. Engineering fracture mechanics 74 (2007) 1894-1903
    • (2007) Engineering fracture mechanics , vol.74 , pp. 1894-1903
    • Li, H.1    Khor, K.A.2    Cheang, P.3
  • 34
    • 0021980488 scopus 로고
    • Alternative interpretations of water sorption values of composite resins
    • Fan P.L., Edahl A., Leung R.L., and Stanford J.W. Alternative interpretations of water sorption values of composite resins. Journal of Dental Research 64 (1985) 78-80
    • (1985) Journal of Dental Research , vol.64 , pp. 78-80
    • Fan, P.L.1    Edahl, A.2    Leung, R.L.3    Stanford, J.W.4
  • 36
    • 38949174245 scopus 로고    scopus 로고
    • Fleming GJP, Awan M, Cooper PR, Sloan AJ. The potential of a resin-composite to be cured to a 4 mm depth. Dental Materials; in press. http://dx.doi.org/10.1016/j.dental.2007.05.016.
    • Fleming GJP, Awan M, Cooper PR, Sloan AJ. The potential of a resin-composite to be cured to a 4 mm depth. Dental Materials; in press. http://dx.doi.org/10.1016/j.dental.2007.05.016.
  • 37
    • 0029267011 scopus 로고
    • Hydrolytic stability of silanated zirconia-silica-urethane dimethacrylate composites
    • Mohsen N.M., and Craig R.G. Hydrolytic stability of silanated zirconia-silica-urethane dimethacrylate composites. Journal of Oral Rehabilitation 22 (1995) 213-220
    • (1995) Journal of Oral Rehabilitation , vol.22 , pp. 213-220
    • Mohsen, N.M.1    Craig, R.G.2
  • 38
    • 15244353651 scopus 로고    scopus 로고
    • Systematic variation of interfacial phase reactivity in dental nanocomposites
    • Wilson K.S., Zhang K., and Atonucci J.M. Systematic variation of interfacial phase reactivity in dental nanocomposites. Biomaterials 26 (2005) 5095-5103
    • (2005) Biomaterials , vol.26 , pp. 5095-5103
    • Wilson, K.S.1    Zhang, K.2    Atonucci, J.M.3
  • 41
    • 0035427334 scopus 로고    scopus 로고
    • The fracture toughness behaviour of interpenetrating phase composites
    • Wegner L.D., and Gibson L.J. The fracture toughness behaviour of interpenetrating phase composites. International Journal of Mechanical Sciences 43 (2001) 1771-1791
    • (2001) International Journal of Mechanical Sciences , vol.43 , pp. 1771-1791
    • Wegner, L.D.1    Gibson, L.J.2
  • 42
    • 0344306444 scopus 로고    scopus 로고
    • Synthesis and characterisation of a novel polymer-ceramic system for biodegradable composite applications
    • Yang L., Wang J., Hong J., Santerre J.P., and Pilliar R.M. Synthesis and characterisation of a novel polymer-ceramic system for biodegradable composite applications. Journal of Biomedical Research A 66 (2003) 622-632
    • (2003) Journal of Biomedical Research A , vol.66 , pp. 622-632
    • Yang, L.1    Wang, J.2    Hong, J.3    Santerre, J.P.4    Pilliar, R.M.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.