Volumn 24, Issue 3, 2008, Pages 351-356

Influence of thermal and mechanical cycling on the flexural strength of ceramics with titanium or gold alloy frameworks

Author keywords

Ceramic; Flexural strength; Gold; Mechanical cycling; Thermal cycling; Titanium

Indexed keywords

BENDING STRENGTH; GOLD ALLOYS; MECHANICAL TESTING; THERMAL CYCLING; THICKNESS MEASUREMENT; TITANIUM ALLOYS;

EID: 38549127722     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2007.06.008     Document Type: Article
Times cited : (46)

References (32)
  • 1
    • 0036561294 scopus 로고    scopus 로고
    • Clinical study on the reasons and location of the failures of metal-ceramic restorations and survival of repairs
    • Özcan M., and Niedermeier W. Clinical study on the reasons and location of the failures of metal-ceramic restorations and survival of repairs. Int J Prosthodont 15 (2002) 299-302
    • (2002) Int J Prosthodont , vol.15 , pp. 299-302
    • Özcan, M.1    Niedermeier, W.2
  • 2
    • 0024345249 scopus 로고
    • Studies of Ti alloys for dental castings
    • Taira M., Moser J.B., and Greener E.H. Studies of Ti alloys for dental castings. Dent Mater 5 (1989) 45-50
    • (1989) Dent Mater , vol.5 , pp. 45-50
    • Taira, M.1    Moser, J.B.2    Greener, E.H.3
  • 4
    • 0025444240 scopus 로고
    • Oxidation effects on porcelain-titanium interface reactions and bond strength
    • Kimura H., Horng C.J., Okazaki M., and Takahashi J. Oxidation effects on porcelain-titanium interface reactions and bond strength. Dent Mater J 9 (1990) 91-99
    • (1990) Dent Mater J , vol.9 , pp. 91-99
    • Kimura, H.1    Horng, C.J.2    Okazaki, M.3    Takahashi, J.4
  • 6
    • 0030155746 scopus 로고    scopus 로고
    • Titanium for prosthodontic applications: a review of the literature
    • Wang R.R., and Fenton A. Titanium for prosthodontic applications: a review of the literature. Quintessence Int 27 (1996) 401-408
    • (1996) Quintessence Int , vol.27 , pp. 401-408
    • Wang, R.R.1    Fenton, A.2
  • 7
    • 0027616999 scopus 로고
    • Titanium and titanium alloys as dental materials
    • Lautenschlager E.P., and Monaghan P. Titanium and titanium alloys as dental materials. Int Dent J 43 (1993) 245-253
    • (1993) Int Dent J , vol.43 , pp. 245-253
    • Lautenschlager, E.P.1    Monaghan, P.2
  • 8
    • 0033222608 scopus 로고    scopus 로고
    • New approach for evaluating metal-porcelain interfacial bonding
    • Suansuwan N., and Swain M.V. New approach for evaluating metal-porcelain interfacial bonding. Int J Prosthodont 12 (1999) 547-552
    • (1999) Int J Prosthodont , vol.12 , pp. 547-552
    • Suansuwan, N.1    Swain, M.V.2
  • 10
    • 0029262154 scopus 로고
    • Stress fatigue: basic principles and prosthodontic implications
    • Wiskott H.W., Nicholls J.I., and Belser U.C. Stress fatigue: basic principles and prosthodontic implications. Int J Prosthodont 8 (1995) 105-116
    • (1995) Int J Prosthodont , vol.8 , pp. 105-116
    • Wiskott, H.W.1    Nicholls, J.I.2    Belser, U.C.3
  • 11
    • 0030160162 scopus 로고    scopus 로고
    • Three-point bending strength of ceramics fused to cast titanium
    • Probster L., Maiwald U., and Weber H. Three-point bending strength of ceramics fused to cast titanium. Eur J Oral Sci 104 (1996) 313-319
    • (1996) Eur J Oral Sci , vol.104 , pp. 313-319
    • Probster, L.1    Maiwald, U.2    Weber, H.3
  • 12
    • 33749072477 scopus 로고    scopus 로고
    • Effect of mechanical cycling on the flexural strength of reinforced ceramics
    • Itinoche K., Özcan M., Bottino M.A., and Oyafuso D.K. Effect of mechanical cycling on the flexural strength of reinforced ceramics. Dent Mater 22 (2006) 1029-1034
    • (2006) Dent Mater , vol.22 , pp. 1029-1034
    • Itinoche, K.1    Özcan, M.2    Bottino, M.A.3    Oyafuso, D.K.4
  • 13
    • 38549158553 scopus 로고    scopus 로고
    • International Organization for Standardization. Metal-ceramic dental restorative systems: ISO 9693. ISO, 1999.
  • 14
    • 38549095650 scopus 로고    scopus 로고
    • Longevity of repaired composite and metal-ceramic restorations: 3.5 year clinical study
    • [Abstract# 0076]
    • Özcan M. Longevity of repaired composite and metal-ceramic restorations: 3.5 year clinical study. J Dent Res 85 (2006) [Abstract# 0076]
    • (2006) J Dent Res , vol.85
    • Özcan, M.1
  • 15
    • 0029181886 scopus 로고
    • Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy
    • Pang I.C., Gilbert J.L., Chai J., and Lautenschlager E.P. Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy. J Prosthet Dent 73 (1995) 17-25
    • (1995) J Prosthet Dent , vol.73 , pp. 17-25
    • Pang, I.C.1    Gilbert, J.L.2    Chai, J.3    Lautenschlager, E.P.4
  • 16
    • 0030119324 scopus 로고    scopus 로고
    • Castability, opaque masking, and porcelain bonding of 17 porcelain-fused-to-metal alloys
    • O'Connor R.P., Mackert Jr. J.R., Myers M.L., and Parry E.E. Castability, opaque masking, and porcelain bonding of 17 porcelain-fused-to-metal alloys. J Prosthet Dent 75 (1996) 367-374
    • (1996) J Prosthet Dent , vol.75 , pp. 367-374
    • O'Connor, R.P.1    Mackert Jr., J.R.2    Myers, M.L.3    Parry, E.E.4
  • 17
    • 0141608992 scopus 로고    scopus 로고
    • Effects of interfacial variables on ceramic adherence to cast and machined commercially pure titanium
    • Sadeq A., Cai Z., Woody R.D., and Miller A.W. Effects of interfacial variables on ceramic adherence to cast and machined commercially pure titanium. J Prosthet Dent 90 (2003) 10-17
    • (2003) J Prosthet Dent , vol.90 , pp. 10-17
    • Sadeq, A.1    Cai, Z.2    Woody, R.D.3    Miller, A.W.4
  • 18
    • 0020339536 scopus 로고
    • Effect of magnesia investments in the dental casting of pure titanium or titanium alloys
    • Ida K., Togaya T., Tsutsumi S., and Takeuchi M. Effect of magnesia investments in the dental casting of pure titanium or titanium alloys. Dent Mater J 1 (1982) 8-21
    • (1982) Dent Mater J , vol.1 , pp. 8-21
    • Ida, K.1    Togaya, T.2    Tsutsumi, S.3    Takeuchi, M.4
  • 19
    • 4644297571 scopus 로고    scopus 로고
    • Pure titanium casting into zirconia-modified magnesia-based investment molds
    • Hung C.C., Hou G.L., Tsai C.C., and Huang C.C. Pure titanium casting into zirconia-modified magnesia-based investment molds. Dent Mater 20 (2004) 846-851
    • (2004) Dent Mater , vol.20 , pp. 846-851
    • Hung, C.C.1    Hou, G.L.2    Tsai, C.C.3    Huang, C.C.4
  • 20
    • 2942544834 scopus 로고    scopus 로고
    • Evaluation of shear bond strength at the interface of two porcelains and pure titanium injected into the casting mold at three different temperatures
    • Bondioli I.R., and Bottino M.A. Evaluation of shear bond strength at the interface of two porcelains and pure titanium injected into the casting mold at three different temperatures. J Prosthet Dent 91 (2004) 541-547
    • (2004) J Prosthet Dent , vol.91 , pp. 541-547
    • Bondioli, I.R.1    Bottino, M.A.2
  • 21
    • 0036497972 scopus 로고    scopus 로고
    • Ceramic bonding to a dental gold-titanium alloy
    • Fischer J. Ceramic bonding to a dental gold-titanium alloy. Biomaterials 23 (2002) 1303-1311
    • (2002) Biomaterials , vol.23 , pp. 1303-1311
    • Fischer, J.1
  • 22
    • 84989535713 scopus 로고
    • Bond strength of porcelain on cast vs. wrought titanium
    • Derand T., and Hero H. Bond strength of porcelain on cast vs. wrought titanium. Scand J Dent Res 100 (1992) 184-188
    • (1992) Scand J Dent Res , vol.100 , pp. 184-188
    • Derand, T.1    Hero, H.2
  • 23
    • 17344374992 scopus 로고    scopus 로고
    • The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminium-vanadium alloy
    • Troia Jr. M.G., Henriques G.E., Nobilo M.A., and Mesquita M.F. The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminium-vanadium alloy. Dent Mater 19 (2003) 790-796
    • (2003) Dent Mater , vol.19 , pp. 790-796
    • Troia Jr., M.G.1    Henriques, G.E.2    Nobilo, M.A.3    Mesquita, M.F.4
  • 24
    • 0028894635 scopus 로고
    • Fracture toughness and flexural strength of dental ceramics for titanium
    • Kvam K., Derand T., and Austrheim E.K. Fracture toughness and flexural strength of dental ceramics for titanium. Biomaterials 16 (1995) 73-76
    • (1995) Biomaterials , vol.16 , pp. 73-76
    • Kvam, K.1    Derand, T.2    Austrheim, E.K.3
  • 25
    • 0141798905 scopus 로고    scopus 로고
    • Monotonic flexure and fatigue strength of composites for provisional and definitive restorations
    • Scherrer S.S., Wiskott A.H., Coto-Hunziker V., and Belser U.C. Monotonic flexure and fatigue strength of composites for provisional and definitive restorations. J Prosthet Dent 89 (2003) 579-588
    • (2003) J Prosthet Dent , vol.89 , pp. 579-588
    • Scherrer, S.S.1    Wiskott, A.H.2    Coto-Hunziker, V.3    Belser, U.C.4
  • 26
    • 0034317060 scopus 로고    scopus 로고
    • Fatigue of biomaterials: a review
    • Teoh S.H. Fatigue of biomaterials: a review. Int Biomat Fatigue 22 (2000) 825-837
    • (2000) Int Biomat Fatigue , vol.22 , pp. 825-837
    • Teoh, S.H.1
  • 27
    • 0032195704 scopus 로고    scopus 로고
    • A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry
    • Özcan M., Pfeiffer P., and Nergiz I. A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry. Quintessence Int 29 (1998) 713-724
    • (1998) Quintessence Int , vol.29 , pp. 713-724
    • Özcan, M.1    Pfeiffer, P.2    Nergiz, I.3
  • 28
    • 0033222301 scopus 로고    scopus 로고
    • The fatigue strength of the interface between Ag-Pd alloy and hydrothermal ceramic
    • Poljak-Guberina R., Catovic A., Jerolimov V., Franz M., and Bergman V. The fatigue strength of the interface between Ag-Pd alloy and hydrothermal ceramic. Dent Mater 15 (1999) 417-420
    • (1999) Dent Mater , vol.15 , pp. 417-420
    • Poljak-Guberina, R.1    Catovic, A.2    Jerolimov, V.3    Franz, M.4    Bergman, V.5
  • 29
    • 0142093511 scopus 로고    scopus 로고
    • Effect of laboratory procedures and thermocycling on the shear bond strength of resin-metal bonding systems
    • Kim J.Y., Pfeiffer P., and Niedermeier W. Effect of laboratory procedures and thermocycling on the shear bond strength of resin-metal bonding systems. J Prosthet Dent 90 (2003) 184-189
    • (2003) J Prosthet Dent , vol.90 , pp. 184-189
    • Kim, J.Y.1    Pfeiffer, P.2    Niedermeier, W.3
  • 30
    • 3242656250 scopus 로고    scopus 로고
    • Comparative strength of metal-ceramic and metal-composite bonds after extended thermocycling
    • Shimoe S., Tanoue N., Yanagida H., Atsuta M., Koizumi H., and Matsumura H. Comparative strength of metal-ceramic and metal-composite bonds after extended thermocycling. J Oral Rehabil 31 (2004) 689-694
    • (2004) J Oral Rehabil , vol.31 , pp. 689-694
    • Shimoe, S.1    Tanoue, N.2    Yanagida, H.3    Atsuta, M.4    Koizumi, H.5    Matsumura, H.6
  • 31
    • 0035321760 scopus 로고    scopus 로고
    • Fracture strength of four different types of anterior 3-unit bridges after thermo-mechanical fatigue in the dual-axis chewing simulator
    • Kheradmandan S., Koutayas S.O., Bernhard M., and Strub J.R. Fracture strength of four different types of anterior 3-unit bridges after thermo-mechanical fatigue in the dual-axis chewing simulator. J Oral Rehabil 28 (2001) 361-369
    • (2001) J Oral Rehabil , vol.28 , pp. 361-369
    • Kheradmandan, S.1    Koutayas, S.O.2    Bernhard, M.3    Strub, J.R.4
  • 32
    • 0034327953 scopus 로고    scopus 로고
    • Prospective clinical 5-year study of ceramic-veneered titanium restorations with the Procera system
    • Lovgren R., Andersson B., Carlsson G.E., and Odman P. Prospective clinical 5-year study of ceramic-veneered titanium restorations with the Procera system. J Prosthet Dent 84 (2000) 514-521
    • (2000) J Prosthet Dent , vol.84 , pp. 514-521
    • Lovgren, R.1    Andersson, B.2    Carlsson, G.E.3    Odman, P.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.