Properties of silicon nitride for aluminum melts prepared by nitrided pressureless sintering

Author keywords

Aluminum; Nitrided pressureless sintering; Reaction sintering; Silicon nitride

Indexed keywords

ALUMINUM; CHEMICAL PROPERTIES; MECHANICAL PROPERTIES; METAL MELTING; NITRIDATION; SINTERING; THERMODYNAMIC PROPERTIES;

EID: 38349054681     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2007.09.032     Document Type: Article
Times cited : (28)

References (19)
  • 1
    • 0031234167 scopus 로고    scopus 로고
    • Role of microstructure in Hertzian contact damage in silicon nitride. 1: Mechanical characterization
    • Lee S.K., Wuttiphan S., and Lawn B.R. Role of microstructure in Hertzian contact damage in silicon nitride. 1: Mechanical characterization. J. Am. Ceram. Soc. 80 (1997) 2367-2381
    • (1997) J. Am. Ceram. Soc. , vol.80 , pp. 2367-2381
    • Lee, S.K.1    Wuttiphan, S.2    Lawn, B.R.3
  • 2
    • 0032046733 scopus 로고    scopus 로고
    • Role of Microstructure in Hertzian contact damage in silicon nitride: II, Strength degradation
    • Lee S.K., and Lawn B.R. Role of Microstructure in Hertzian contact damage in silicon nitride: II, Strength degradation. J. Am. Ceram. Soc. 81 (1998) 997-1003
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 997-1003
    • Lee, S.K.1    Lawn, B.R.2
  • 3
    • 0031700569 scopus 로고    scopus 로고
    • Wear of nitrogen ceramics and composites in contact with bearing steel under oscillating sliding condition
    • Mukerji J., and Prakash B. Wear of nitrogen ceramics and composites in contact with bearing steel under oscillating sliding condition. Ceramics International 24 (1998) 19-24
    • (1998) Ceramics International , vol.24 , pp. 19-24
    • Mukerji, J.1    Prakash, B.2
  • 4
    • 0033750188 scopus 로고    scopus 로고
    • Silicon nitride and related materials
    • Riley F.L. Silicon nitride and related materials. J. Am. Ceram. Soc. 83 (2000) 245-265
    • (2000) J. Am. Ceram. Soc. , vol.83 , pp. 245-265
    • Riley, F.L.1
  • 5
    • 0018467004 scopus 로고
    • Reaction-bonded silicon nitride: Its formation and properties
    • Moulson A.J. Reaction-bonded silicon nitride: Its formation and properties. J. Mater. Sci. 14 (1979) 1017-1021
    • (1979) J. Mater. Sci. , vol.14 , pp. 1017-1021
    • Moulson, A.J.1
  • 6
    • 0032074380 scopus 로고    scopus 로고
    • 4/SiC composite by reaction-bonding and gas pressure sintering
    • 4/SiC composite by reaction-bonding and gas pressure sintering. J. Am. Ceram. Soc. 81 (1998) 1262-1268
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 1262-1268
    • Lee, S.Y.1
  • 7
    • 0036391793 scopus 로고    scopus 로고
    • Mechanical reliability evaluation of silicon nitride ceramic components after exposure in industrial gas turbines
    • Lin H.T., and Ferber M.K. Mechanical reliability evaluation of silicon nitride ceramic components after exposure in industrial gas turbines. J. Am. Ceram. Soc. 22 (2002) 2789-2797
    • (2002) J. Am. Ceram. Soc. , vol.22 , pp. 2789-2797
    • Lin, H.T.1    Ferber, M.K.2
  • 8
    • 33748901342 scopus 로고    scopus 로고
    • Effect of deposition conditions on mechanical properties of low-temperature PECVD silicon nitride films
    • Huang H., Winchester K.J., Suvorova A., Lawn B.R., Liu Y., Hu X.Z., et al. Effect of deposition conditions on mechanical properties of low-temperature PECVD silicon nitride films. Mater. Sci. & Eng. A435-36 (2006) 453-459
    • (2006) Mater. Sci. & Eng. , vol.A435-36 , pp. 453-459
    • Huang, H.1    Winchester, K.J.2    Suvorova, A.3    Lawn, B.R.4    Liu, Y.5    Hu, X.Z.6
  • 9
    • 33746063649 scopus 로고    scopus 로고
    • Preparation and properties of silicon nitride ceramics by nitrided pressureless sintering (NPS) process
    • Han I.S., Cheon S.H., Chung Y.H., Seo D.W., Lee S.W., Woo S.K., et al. Preparation and properties of silicon nitride ceramics by nitrided pressureless sintering (NPS) process. Key Eng. Mater. 317-318 (2006) 125-130
    • (2006) Key Eng. Mater. , vol.317-318 , pp. 125-130
    • Han, I.S.1    Cheon, S.H.2    Chung, Y.H.3    Seo, D.W.4    Lee, S.W.5    Woo, S.K.6
  • 10
    • 27644554082 scopus 로고    scopus 로고
    • Industrial applications of ceramic matrix composites
    • Kelly A., and Zweben C. (Eds), Elsevier, Amsterdam [Chapter 6.28]
    • Richerson D.W. Industrial applications of ceramic matrix composites. In: Kelly A., and Zweben C. (Eds). Comprehensive Composite Materials Vol. 6 (2000), Elsevier, Amsterdam 549-570 [Chapter 6.28]
    • (2000) Comprehensive Composite Materials , vol.6 , pp. 549-570
    • Richerson, D.W.1
  • 11
    • 0025627349 scopus 로고
    • Preparation of sialons by the nitrided pressureless sintering (NPS) technique
    • Brown I.W.M., Pompe R., and Carlsson R. Preparation of sialons by the nitrided pressureless sintering (NPS) technique. J. Eur. Ceram. Soc. 6 (1990) 191-200
    • (1990) J. Eur. Ceram. Soc. , vol.6 , pp. 191-200
    • Brown, I.W.M.1    Pompe, R.2    Carlsson, R.3
  • 12
    • 0036577719 scopus 로고    scopus 로고
    • Improvement of mechanical properties in RBSC by boron carbide addition
    • Han I.S., Lee K.S., Seo D.W., and Woo S.K. Improvement of mechanical properties in RBSC by boron carbide addition. J. Mater. Sci. 21 (2002) 703-706
    • (2002) J. Mater. Sci. , vol.21 , pp. 703-706
    • Han, I.S.1    Lee, K.S.2    Seo, D.W.3    Woo, S.K.4
  • 13
    • 0032095426 scopus 로고    scopus 로고
    • Model of strength degradation from Hertzian contact damage in tough ceramics
    • Lawn B.R., Lee S.K., Peterson I.M., and Wuttiphan S. Model of strength degradation from Hertzian contact damage in tough ceramics. J. Am. Ceram. Soc. 81 (1998) 1509-1520
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 1509-1520
    • Lawn, B.R.1    Lee, S.K.2    Peterson, I.M.3    Wuttiphan, S.4
  • 14
    • 0032137856 scopus 로고    scopus 로고
    • Indentation of ceramics with spheres: A Century after Hertz
    • Lawn B.R. Indentation of ceramics with spheres: A Century after Hertz. J. Am. Ceram. Soc. 81 (1998) 1977-1994
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 1977-1994
    • Lawn, B.R.1
  • 15
    • 0032028115 scopus 로고    scopus 로고
    • Contact-induced transverse fractures in brittle layers on soft substrates: A study on silicon nitride bilayers
    • Lee K.S., Wuttiphan S., Hu X.Z., Lee S.K., Lawn B.R., and Lawn. Contact-induced transverse fractures in brittle layers on soft substrates: A study on silicon nitride bilayers. J. Am. Ceram. Soc. 81 (1998) 571-580
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 571-580
    • Lee, K.S.1    Wuttiphan, S.2    Hu, X.Z.3    Lee, S.K.4    Lawn, B.R.5    Lawn6
  • 16
    • 0032139565 scopus 로고    scopus 로고
    • Effect of starting powder on damage resistance of silicon nitrides
    • Lee S.K., Lee K.S., Lawn B.R., and Kim D.K. Effect of starting powder on damage resistance of silicon nitrides. J. Am. Ceram. Soc. 81 (1998) 2061-2070
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 2061-2070
    • Lee, S.K.1    Lee, K.S.2    Lawn, B.R.3    Kim, D.K.4
  • 17
    • 0032165250 scopus 로고    scopus 로고
    • Contact damage and strength degradation in brittle/quasi-plastic silicon nitride bilayers
    • Lee K.S., Lee K., Lawn B.R., and Kim D.K. Contact damage and strength degradation in brittle/quasi-plastic silicon nitride bilayers. J. Am. Ceram. Soc. 81 (1998) 2394-2404
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 2394-2404
    • Lee, K.S.1    Lee, K.2    Lawn, B.R.3    Kim, D.K.4
  • 18
    • 0032496546 scopus 로고    scopus 로고
    • A simple indentation stress-strain relation for contacts with spheres on bilayer structures
    • Hu X.Z., and Lawn B.R. A simple indentation stress-strain relation for contacts with spheres on bilayer structures. Thin Solid Films 322 (1998) 225-232
    • (1998) Thin Solid Films , vol.322 , pp. 225-232
    • Hu, X.Z.1    Lawn, B.R.2
  • 19
    • 0036346962 scopus 로고    scopus 로고
    • and Lawn B. R., Thermal shock resistance of silicon nitrides using an indentation-quench test
    • Lee S.K., Moretti D., and Readey M.J. and Lawn B. R., Thermal shock resistance of silicon nitrides using an indentation-quench test. J. Am. Ceram. Soc. 85 (2002) 279-281
    • (2002) J. Am. Ceram. Soc. , vol.85 , pp. 279-281
    • Lee, S.K.1    Moretti, D.2    Readey, M.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.