Volumn 28, Issue 2, 2008, Pages 479-491

Mullite-refractory metal (Mo, Nb) composites

Author keywords

Ceramic metal composites; Mechanical properties; Mullite; Wear resistance

Indexed keywords

CRACK PROPAGATION; ELECTRIC CONDUCTIVITY; ELECTRIC DISCHARGE MACHINING; MULLITE; PARTICLE SIZE; REFRACTORY METALS; VOLUME FRACTION; WEAR RESISTANCE;

EID: 35748945739     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2007.03.020     Document Type: Article
Times cited : (34)

References (38)
  • 1
    • 35748943307 scopus 로고    scopus 로고
    • Thermal shock testing on mullite/Mo FGM diks using an infrared radiation/water flow technique
    • Jin G., Takeuchi M., Honda S., Nishikawa T., and Awaji H. Thermal shock testing on mullite/Mo FGM diks using an infrared radiation/water flow technique. J. Ceram. Soc. Jap. 112 5 (2004) S286-S290
    • (2004) J. Ceram. Soc. Jap. , vol.112 , Issue.5
    • Jin, G.1    Takeuchi, M.2    Honda, S.3    Nishikawa, T.4    Awaji, H.5
  • 3
    • 33744965533 scopus 로고    scopus 로고
    • Lighting in the solid state
    • Janeway P.A. Lighting in the solid state. Am. Ceram. Soc. Bull. 85 5 (2006) 17-20
    • (2006) Am. Ceram. Soc. Bull. , vol.85 , Issue.5 , pp. 17-20
    • Janeway, P.A.1
  • 4
    • 84979956641 scopus 로고
    • Mullite for structural, electronic, and optical applications
    • Aksay I.A., Dabbs D.M., and Sarikaya M. Mullite for structural, electronic, and optical applications. J. Am. Ceram. Soc. 74 10 (1991) 2343-2358
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.10 , pp. 2343-2358
    • Aksay, I.A.1    Dabbs, D.M.2    Sarikaya, M.3
  • 6
    • 0020833778 scopus 로고
    • Mechanical properties of mullite
    • Mahn T.-I., and Mazdiyasni K.S. Mechanical properties of mullite. J. Am. Ceram. Soc. 66 10 (1983) 699-703
    • (1983) J. Am. Ceram. Soc. , vol.66 , Issue.10 , pp. 699-703
    • Mahn, T.-I.1    Mazdiyasni, K.S.2
  • 7
    • 18244419840 scopus 로고
    • Sintering and mechanical properties of stoichiometric mullite
    • Kanzaki S., Tabata H., Kumazawa T., and Ohta S. Sintering and mechanical properties of stoichiometric mullite. J. Am. Ceram. Soc. 68 1 (1985) C-6-C-7
    • (1985) J. Am. Ceram. Soc. , vol.68 , Issue.1
    • Kanzaki, S.1    Tabata, H.2    Kumazawa, T.3    Ohta, S.4
  • 8
    • 0023139048 scopus 로고
    • Microstructure and mechanical properties of mullite prepared by the sol-gel method
    • Ismail M.G.M.U., Nakai Z., and Somiya S. Microstructure and mechanical properties of mullite prepared by the sol-gel method. J. Am. Ceram.Soc. 70 1 (1987) C-6-C-7
    • (1987) J. Am. Ceram.Soc. , vol.70 , Issue.1
    • Ismail, M.G.M.U.1    Nakai, Z.2    Somiya, S.3
  • 9
    • 0025229061 scopus 로고
    • Microstructure and mechanical properties of mullite ceramics
    • Ohnishi H., Kawanami T., Nakahira A., and Niihara K. Microstructure and mechanical properties of mullite ceramics. Yogyo Kyokaishi 98 6 (1990) 541-547
    • (1990) Yogyo Kyokaishi , vol.98 , Issue.6 , pp. 541-547
    • Ohnishi, H.1    Kawanami, T.2    Nakahira, A.3    Niihara, K.4
  • 10
    • 0032662992 scopus 로고    scopus 로고
    • Fabrication and mechanical properties of SiC platelet reinforced mullite matrix composites
    • Rezaie H.R., Rainforth W.M., and Lee W.E. Fabrication and mechanical properties of SiC platelet reinforced mullite matrix composites. J. Eur. Ceram. Soc. 19 (1999) 1777-1787
    • (1999) J. Eur. Ceram. Soc. , vol.19 , pp. 1777-1787
    • Rezaie, H.R.1    Rainforth, W.M.2    Lee, W.E.3
  • 11
    • 0036720930 scopus 로고    scopus 로고
    • Microstructure and mechanical properties of SiC-mullite nanocomposite prepared by spark plasma sintering
    • Gao L., Jin X., Kawaoka H., Sekino T., and Niihara K. Microstructure and mechanical properties of SiC-mullite nanocomposite prepared by spark plasma sintering. Mater. Sci. Eng. A334 (2002) 262-266
    • (2002) Mater. Sci. Eng. , vol.A334 , pp. 262-266
    • Gao, L.1    Jin, X.2    Kawaoka, H.3    Sekino, T.4    Niihara, K.5
  • 12
    • 0032097356 scopus 로고    scopus 로고
    • Fatigue crack growth behavior in mullite/alumina functionally graded ceramics
    • Bartolomé J.F., Moya J.S., Requena J., Llorca J., and Anglada M. Fatigue crack growth behavior in mullite/alumina functionally graded ceramics. J. Am. Ceram. Soc. 81 6 (1998) 1502-1508
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.6 , pp. 1502-1508
    • Bartolomé, J.F.1    Moya, J.S.2    Requena, J.3    Llorca, J.4    Anglada, M.5
  • 13
    • 0021493847 scopus 로고
    • Microstructure and mechanical properties of mullite/ZrO2 composites
    • Moya J.S., and Osendi M.I. Microstructure and mechanical properties of mullite/ZrO2 composites. J. Mater. Sci. 19 9 (1984) 2909-2914
    • (1984) J. Mater. Sci. , vol.19 , Issue.9 , pp. 2909-2914
    • Moya, J.S.1    Osendi, M.I.2
  • 15
    • 0036862602 scopus 로고    scopus 로고
    • Influence of the metal particle size on the crack growth resistance in mullite/molybdenum composites
    • Bartolomé J.F., Díaz M., Requena J., and Moya J.S. Influence of the metal particle size on the crack growth resistance in mullite/molybdenum composites. J. Am. Ceram. Soc. 85 11 (2002) 2778-2784
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.11 , pp. 2778-2784
    • Bartolomé, J.F.1    Díaz, M.2    Requena, J.3    Moya, J.S.4
  • 17
    • 0034964808 scopus 로고    scopus 로고
    • Influence of MgO on microstructure and properties of mullite-Mo composites fabricated by pulse electric current sintering
    • Sivakumar R., Jayaseelan D.D., Nishikawa T., Honda S., and Awaji H. Influence of MgO on microstructure and properties of mullite-Mo composites fabricated by pulse electric current sintering. Ceram. Inter. 27 5 (2001) 537-541
    • (2001) Ceram. Inter. , vol.27 , Issue.5 , pp. 537-541
    • Sivakumar, R.1    Jayaseelan, D.D.2    Nishikawa, T.3    Honda, S.4    Awaji, H.5
  • 19
    • 0024838548 scopus 로고
    • High toughness ceramics and ceramic composites
    • Rühle M., and Evans A.G. High toughness ceramics and ceramic composites. Prog. Mater. Sci. 33 (1989) 85
    • (1989) Prog. Mater. Sci. , vol.33 , pp. 85
    • Rühle, M.1    Evans, A.G.2
  • 20
    • 58149368795 scopus 로고
    • EDM-future steps towards the machining of ceramics
    • Koning W., Dauw D.F., Levy G., and Panten U. EDM-future steps towards the machining of ceramics. Ann. CIRP 37 1 (1988) 623-631
    • (1988) Ann. CIRP , vol.37 , Issue.1 , pp. 623-631
    • Koning, W.1    Dauw, D.F.2    Levy, G.3    Panten, U.4
  • 21
    • 0041707722 scopus 로고    scopus 로고
    • Determination of standard free energy of formation for niobium silicides by emf measurements
    • Fujiwara H., Ueda Y., Awasthi A., Hrishnamurthy N., and Garg S.P. Determination of standard free energy of formation for niobium silicides by emf measurements. J. Electrochem. Soc. 150 8 (2003) J43-J48
    • (2003) J. Electrochem. Soc. , vol.150 , Issue.8
    • Fujiwara, H.1    Ueda, Y.2    Awasthi, A.3    Hrishnamurthy, N.4    Garg, S.P.5
  • 22
    • 0000327659 scopus 로고
    • Objective evaluation of short-crack toughness curve using indentation flaws: case study on alumina-based ceramics
    • Braun L.M., Benninson S.J., and Lawn B.R. Objective evaluation of short-crack toughness curve using indentation flaws: case study on alumina-based ceramics. J. Am. Ceram. Soc. 75 11 (1992) 3049-3057
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.11 , pp. 3049-3057
    • Braun, L.M.1    Benninson, S.J.2    Lawn, B.R.3
  • 23
    • 0026875935 scopus 로고
    • An improved technique for determining hardness and elastic-modulus using load and displacement sensing indentation experiments
    • Oliver W.C., and Pharr G.M. An improved technique for determining hardness and elastic-modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7 (1992) 1564
    • (1992) J. Mater. Res. , vol.7 , pp. 1564
    • Oliver, W.C.1    Pharr, G.M.2
  • 25
    • 33745369020 scopus 로고    scopus 로고
    • Damage tolerance of nanolayer grained ceramics and qualtitative estimation
    • Bao Y.W., Hu C.F., and Zhou Y.C. Damage tolerance of nanolayer grained ceramics and qualtitative estimation. Mater. Sci. Technol. 22 2 (2006) 227-230
    • (2006) Mater. Sci. Technol. , vol.22 , Issue.2 , pp. 227-230
    • Bao, Y.W.1    Hu, C.F.2    Zhou, Y.C.3
  • 27
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: I
    • Anstis G.R., Chankitul P., Lawn B.R., and Marshall D.B. A critical evaluation of indentation techniques for measuring fracture toughness: I. J. Am. Ceram. Soc. 64 9 (1981) 533-538
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.9 , pp. 533-538
    • Anstis, G.R.1    Chankitul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 28
    • 0028201618 scopus 로고
    • Flaw tolerance and toughness curves in two-phase particulate composites: SiC/glass system
    • Cai H., Padture N.P., Hooks B.M., and Lawn B.R. Flaw tolerance and toughness curves in two-phase particulate composites: SiC/glass system. J. Eur. Ceram. Soc. 13 (1994) 149-157
    • (1994) J. Eur. Ceram. Soc. , vol.13 , pp. 149-157
    • Cai, H.1    Padture, N.P.2    Hooks, B.M.3    Lawn, B.R.4
  • 29
    • 0030401342 scopus 로고    scopus 로고
    • Short-crack toughness and abrasive machining of silicon nitride
    • Xu H.H.K., Jahanmir S., Ives L.K., Job L.S., and Ritchie K.T. Short-crack toughness and abrasive machining of silicon nitride. J. Am. Ceram. Soc. 79 12 (1996) 3055-3064
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.12 , pp. 3055-3064
    • Xu, H.H.K.1    Jahanmir, S.2    Ives, L.K.3    Job, L.S.4    Ritchie, K.T.5
  • 30
    • 0000398636 scopus 로고
    • Grain boundary segregation and intergranular fracture in molybdenum
    • Kumar A., and Eyre B.L. Grain boundary segregation and intergranular fracture in molybdenum. Proc. R. Soc. Lond. A370 (1980) 431-458
    • (1980) Proc. R. Soc. Lond. , vol.A370 , pp. 431-458
    • Kumar, A.1    Eyre, B.L.2
  • 32
    • 35748960030 scopus 로고    scopus 로고
    • Kameo K., New routes for tailoring metal- and ceramic-based composites for tribological applications, PhD Thesis, Institu für Verbundwerkstoffe, Technische Universität Kaiserslautern, Germany, 2005.
  • 33
    • 0033878998 scopus 로고    scopus 로고
    • Experimental evidence of a giant capacitance in insulator conductor composites at the percolation threshold
    • Pecharroman C., and Moya J.S. Experimental evidence of a giant capacitance in insulator conductor composites at the percolation threshold. Adv. Mater. 12 4 (2000) 294-297
    • (2000) Adv. Mater. , vol.12 , Issue.4 , pp. 294-297
    • Pecharroman, C.1    Moya, J.S.2
  • 34
    • 35748931286 scopus 로고    scopus 로고
    • ® for Windows, Outokumpu Research, Oy, Finland, 2002.
  • 36
    • 0028518939 scopus 로고
    • New route for hydroxiapatite coatings on Ti-based human implants
    • Tomsia A.P., Moya J.S., and Guitian F. New route for hydroxiapatite coatings on Ti-based human implants. Scripta Metallur. et Materialia 31 8 (1994) 995-1000
    • (1994) Scripta Metallur. et Materialia , vol.31 , Issue.8 , pp. 995-1000
    • Tomsia, A.P.1    Moya, J.S.2    Guitian, F.3
  • 37
    • 0019553011 scopus 로고
    • The Lorenz and electron transport properties of NbO
    • Hsieh N., and Fine M.E. The Lorenz and electron transport properties of NbO. J. Appl. Phys. 52 4 (1981) 2876-2883
    • (1981) J. Appl. Phys. , vol.52 , Issue.4 , pp. 2876-2883
    • Hsieh, N.1    Fine, M.E.2
  • 38
    • 0031139718 scopus 로고    scopus 로고
    • Effect of product conductivity on field-activated combustion synthesis
    • Feng A., and Munir A. Effect of product conductivity on field-activated combustion synthesis. J. Am. Ceram. Soc. 80 5 (1997) 1222-1230
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.5 , pp. 1222-1230
    • Feng, A.1    Munir, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.