Volumn 24, Issue 5, 2004, Pages 785-790

Mullite/Mo interfaces formed by intrusion bonding

Author keywords

Diffusion bonding; Fracture; Interfaces; Microstructure; Mullite Mo

Indexed keywords

BENDING STRENGTH; INTERFACES (MATERIALS); MICROSTRUCTURE; MOLYBDENUM COMPOUNDS;

EID: 0242539950     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0955-2219(03)00339-X     Document Type: Article
Times cited : (10)

References (15)
  • 1
    • 18244431765 scopus 로고    scopus 로고
    • Structure and composition of metal/ceramic interfaces
    • Rühle M. Structure and composition of metal/ceramic interfaces Key Engineering Materials 116 1996 1-40
    • (1996) Key Engineering Materials , vol.116 , pp. 1-40
    • Rühle, M.1
  • 3
    • 0022769492 scopus 로고
    • Some aspects of the mechanical strength of ceramic/metal bonded systems
    • Evans A.G. Lu M.C. Schmauder S. Rühle M. Some aspects of the mechanical strength of ceramic/metal bonded systems Acta Metall. 34 1986 1643-1655
    • (1986) Acta Metall. , vol.34 , pp. 1643-1655
    • Evans, A.G.1    Lu, M.C.2    Schmauder, S.3    Rühle, M.4
  • 6
    • 0022665805 scopus 로고
    • Chemical reactions and adherence at glass/metal interfaces: And analysis
    • Tomsia A.P. Pask J.A. Chemical reactions and adherence at glass/metal interfaces: And analysis Dental Materials 2 1986 10-16
    • (1986) Dental Materials , vol.2 , pp. 10-16
    • Tomsia, A.P.1    Pask, J.A.2
  • 7
    • 84979956641 scopus 로고
    • Mullite for structural, electronic, and optical applications
    • Aksay I.A. Dabbs D.M. Sarikaya M.J. Mullite for structural, electronic, and optical applications J. Am. Ceram. Soc. 74 1991 2343-2358
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 2343-2358
    • Aksay, I.A.1    Dabbs, D.M.2    Sarikaya, M.J.3
  • 8
    • 84927622572 scopus 로고
    • High-temperature compressive creep of polycrystalline mullite
    • Hynes A.P. Doremus R.H. High-temperature compressive creep of polycrystalline mullite J. Am. Ceram. Soc. 74 1991 2469-2475
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 2469-2475
    • Hynes, A.P.1    Doremus, R.H.2
  • 12
    • 0000398636 scopus 로고
    • Grain boundary segregation and intergranular fracture in molybdenum
    • Kumar A. Eyre B.L. Grain boundary segregation and intergranular fracture in molybdenum Proc. R. Soc. Lond. A 370 1980 431-458
    • (1980) Proc. R. Soc. Lond. A , vol.370 , pp. 431-458
    • Kumar, A.1    Eyre, B.L.2
  • 15
    • 0029236765 scopus 로고
    • Effects of composite processing on the strength of sapphire fiber-reinforced composites
    • Davis J.B. Yang J. Evans A.G. Effects of composite processing on the strength of sapphire fiber-reinforced composites Acta Metal Mater. 43 1995 259-268
    • (1995) Acta Metal Mater. , vol.43 , pp. 259-268
    • Davis, J.B.1    Yang, J.2    Evans, A.G.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.