1
-
-
0029324743
-
Ceramic Composites of Monazite and Alumina
-
P. E. D. Morgan D. B. Marshall Ceramic Composites of Monazite and Alumina J. Am. Ceram. Soc., 78 [6] 1553 63 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.6
, pp. 1553-63
-
-
Morgan, P.E.D.1
Marshall, D.B.2
-
2
-
-
0037302361
-
Effectiveness of Monazite Coatings in Oxide/Oxide Composites after Long Term Exposure at High Temperature
-
K. A. Keller, T. Mah, T. A. Parthasarathy, E. E. Boakye, P. Mogilevsky M. K. Cinibulk Effectiveness of Monazite Coatings in Oxide/Oxide Composites After Long Term Exposure at High Temperature J. Am. Ceram. Soc., 86 [2] 325 32 (2003).
-
(2003)
J. Am. Ceram. Soc.
, vol.86
, Issue.2
, pp. 325-32
-
-
Keller, K.A.1
Mah, T.2
Parthasarathy, T.A.3
Boakye, E.E.4
Mogilevsky, P.5
Cinibulk, M.K.6
-
3
-
-
0036884672
-
Mullite (Nextel™ 720) Fibre-Reinforced Mullite Matrix Composites Exhibiting Favourable Thermomechanical Properties
-
C. Kaya, E. G. Butler, A. Selcuk, A. R. Boccaccini M. H. Lewis Mullite (Nextel™ 720) Fibre-Reinforced Mullite Matrix Composites Exhibiting Favourable Thermomechanical Properties J. Eur. Ceram. Soc., 22, 2333 42 (2002).
-
(2002)
J. Eur. Ceram. Soc.
, vol.22
, pp. 2333-42
-
-
Kaya, C.1
Butler, E.G.2
Selcuk, A.3
Boccaccini, A.R.4
Lewis, M.H.5
-
5
-
-
1442360594
-
Effects of Sintering Condition on Mechanical Properties of Monazite-Coated Alumina-Fiber/Alumina-Matrix Composites Fabricated by Hot-Pressing
-
P.-Y. Lee, M. Imai T. Yano Effects of Sintering Condition on Mechanical Properties of Monazite-Coated Alumina-Fiber/Alumina-Matrix Composites Fabricated by Hot-Pressing J. Ceram. Soc. Jpn., 112 [1] 29 34 (2004).
-
(2004)
J. Ceram. Soc. Jpn.
, vol.112
, Issue.1
, pp. 29-34
-
-
Lee, P.-Y.1
Imai, M.2
Yano, T.3
-
6
-
-
0041639510
-
Monazite Coatings on Fibers: II, Coating without Strength Degradation
-
E. E. Boakye, R. S. Hay, P. Mogilevsky L. M. Douglas Monazite Coatings on Fibers: II, Coating without Strength Degradation J. Am. Ceram. Soc., 84 [12] 2793 801 (2001).
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.12
, pp. 2793-801
-
-
Boakye, E.E.1
Hay, R.S.2
Mogilevsky, P.3
Douglas, L.M.4
-
7
-
-
1542335547
-
Fiber Strength Retention of la and Ce-PO4 Coated Nextel™ 720
-
E. E. Boakye P. Mogilevsky Fiber Strength Retention of La and Ce-PO4 Coated Nextel™ 720 J. Am. Ceram. Soc., 87 [2] 314 6 (2004).
-
(2004)
J. Am. Ceram. Soc.
, vol.87
, Issue.2
, pp. 314-6
-
-
Boakye, E.E.1
Mogilevsky, P.2
-
9
-
-
27644499061
-
Synthesis of Spherical Rhabdophane Particles
-
E. E. Boakye, P. Mogilevsky R. S. Hay Synthesis of Spherical Rhabdophane Particles J. Am. Ceram. Soc., 88 [10] 2740 6 (2005).
-
(2005)
J. Am. Ceram. Soc.
, vol.88
, Issue.10
, pp. 2740-6
-
-
Boakye, E.E.1
Mogilevsky, P.2
Hay, R.S.3
-
10
-
-
84918121905
-
Low-Temperature Sintering of Aluminum Oxide
-
T.-S. Yeh M. D. Sacks Low-Temperature Sintering of Aluminum Oxide J. Am. Ceram. Soc., 71 [10] 841 4 (1988).
-
(1988)
J. Am. Ceram. Soc.
, vol.71
, Issue.10
, pp. 841-4
-
-
Yeh, T.-S.1
Sacks, M.D.2
-
11
-
-
0242569558
-
Evolution of Texture in Rhabdophane-Derived Monazite Coatings
-
P. Mogilevsky, R. S. Hay, E. E. Boakye K. A. Keller Evolution of Texture in Rhabdophane-Derived Monazite Coatings J. Am. Ceram. Soc., 86 [10] 1767 72 (2003).
-
(2003)
J. Am. Ceram. Soc.
, vol.86
, Issue.10
, pp. 1767-72
-
-
Mogilevsky, P.1
Hay, R.S.2
Boakye, E.E.3
Keller, K.A.4
-
12
-
-
0031140724
-
Statistical Tensile Strength of Nextel 610 and Nextel 720 Fibres
-
D. M. Wilson Statistical Tensile Strength of Nextel 610 and Nextel 720 Fibres J. Mater. Sci., 32, 2535 42 (1997).
-
(1997)
J. Mater. Sci.
, vol.32
, pp. 2535-42
-
-
Wilson, D.M.1
-
13
-
-
0035427193
-
High Performance Oxide Fibers for Metal and Ceramic Composites
-
D. M. Wilson L. R. Visser High Performance Oxide Fibers for Metal and Ceramic Composites Composites A, A32, 1143 5 (2001).
-
(2001)
Composites A
, vol.32
, pp. 1143-5
-
-
Wilson, D.M.1
Visser, L.R.2
-
14
-
-
0033318831
-
Grain Growth and Tensile Strength of 3M Nextel 720 after Thermal Exposure
-
R. S. Hay, E. E. Boakye, M. D. Petry, Y. Berta, K. V. Lehmden J. Welch Grain Growth and Tensile Strength of 3M Nextel 720 after Thermal Exposure Ceram. Eng. Sci. Proc., 20 [3] 153 6 (1999).
-
(1999)
Ceram. Eng. Sci. Proc.
, vol.20
, Issue.3
, pp. 153-6
-
-
Hay, R.S.1
Boakye, E.E.2
Petry, M.D.3
Berta, Y.4
Lehmden, K.V.5
Welch, J.6
-
15
-
-
0025489301
-
Sol-Gel Coatings on Continuous Ceramic Fibers
-
R. S. Hay E. E. Hermes Sol-Gel Coatings on Continuous Ceramic Fibers Ceram. Eng. Sci. Proc., 11 [9-10] 1526 32 (1990).
-
(1990)
Ceram. Eng. Sci. Proc.
, vol.11
, Issue.910
, pp. 1526-32
-
-
Hay, R.S.1
Hermes, E.E.2
-
16
-
-
0033189440
-
Continuous Coating of Oxide Fiber Tows Using Liquid Precursors: Monazite Coatings on Nextel 720
-
E. Boakye, R. S. Hay M. D. Petry Continuous Coating of Oxide Fiber Tows Using Liquid Precursors: Monazite Coatings on Nextel 720 J. Am. Ceram. Soc., 82 [9] 2321 3 (1999).
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, Issue.9
, pp. 2321-3
-
-
Boakye, E.1
Hay, R.S.2
Petry, M.D.3
-
17
-
-
0000994914
-
Sol-Gel Coating of Fiber Tows
-
R. S. Hay Sol-Gel Coating of Fiber Tows Ceram. Eng. Sci. Proc., 12 [7-8] 1064 71 (1991).
-
(1991)
Ceram. Eng. Sci. Proc.
, vol.12
, Issue.78
, pp. 1064-71
-
-
Hay, R.S.1
-
18
-
-
0031251201
-
TEM Specimen Preparation and Characterization of Ceramic Coatings on Fiber Tows
-
R. S. Hay, J. R. Welch M. K. Cinibulk TEM Specimen Preparation and Characterization of Ceramic Coatings on Fiber Tows Thin Solid Films, 308-309, 389 92 (1997).
-
(1997)
Thin Solid Films
, vol.308-309
, pp. 389-92
-
-
Hay, R.S.1
Welch, J.R.2
Cinibulk, M.K.3
-
19
-
-
32044439156
-
Measurement of Fiber Coating Thickness Variation
-
R. S. Hay, G. Fair, P. Mogilevsky E. E. Boakye Measurement of Fiber Coating Thickness Variation Ceram. Eng. Sci. Proc., 26 [2] 11 18 (2005).
-
(2005)
Ceram. Eng. Sci. Proc.
, vol.26
, Issue.2
, pp. 11-18
-
-
Hay, R.S.1
Fair, G.2
Mogilevsky, P.3
Boakye, E.E.4
-
20
-
-
0031259137
-
Validity of Using Average Diameter for Determination of Tensile Strength and Weibull Modulus of Ceramic Filaments
-
M. D. Petry, T. Mah R. J. Kerans Validity of Using Average Diameter for Determination of Tensile Strength and Weibull Modulus of Ceramic Filaments J. Am. Ceram. Soc., 80 [10] 2741 4 (1997).
-
(1997)
J. Am. Ceram. Soc.
, vol.80
, Issue.10
, pp. 2741-4
-
-
Petry, M.D.1
Mah, T.2
Kerans, R.J.3
-
21
-
-
0035297424
-
Extraction of Weibull Parameters of Fiber Strength from Means and Standard Deviations of Failure Loads and Fiber Diameters
-
T. A. Parthasarathy Extraction of Weibull Parameters of Fiber Strength from Means and Standard Deviations of Failure Loads and Fiber Diameters J. Am. Ceram. Soc., 84 [3] 588 92 (2001).
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.3
, pp. 588-92
-
-
Parthasarathy, T.A.1
-
22
-
-
0035791597
-
Monazite Coatings on Fibers: I, Effect of Temperature and Alumina Doping on Coated Fiber Tensile Strength
-
R. S. Hay E. Boakye Monazite Coatings on Fibers: I, Effect of Temperature and Alumina Doping on Coated Fiber Tensile Strength J. Am. Ceram. Soc., 84 [12] 2783 92 (2001).
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.12
, pp. 2783-92
-
-
Hay, R.S.1
Boakye, E.2
-
23
-
-
0029409954
-
Cracking during Pyrolysis of Oxide Thin Films - Phenomenology, Mechanisms, and Mechanics
-
S.-Y. Chen I.-W. Chen Cracking during Pyrolysis of Oxide Thin Films - Phenomenology, Mechanisms, and Mechanics J. Am. Ceram. Soc., 78 [11] 2929 3 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.11
, pp. 2929-3
-
-
Chen, S.-Y.1
Chen, I.-W.2
-
24
-
-
0034005073
-
Effect of Coating Deposition Temperature on Monazite Coated Fiber
-
R. S. Hay, E. E. Boakye M. D. Petry Effect of Coating Deposition Temperature on Monazite Coated Fiber J. Eur. Ceram. Soc., 20, 589 97 (2000).
-
(2000)
J. Eur. Ceram. Soc.
, vol.20
, pp. 589-97
-
-
Hay, R.S.1
Boakye, E.E.2
Petry, M.D.3
-
25
-
-
8644279597
-
Zirconia-Silica-Carbon Coatings on Ceramic Fibers
-
E. E. Boakye, R. S. Hay, M. D. Petry T. A. Parthasarathy Zirconia-Silica-Carbon Coatings on Ceramic Fibers J Am. Ceram. Soc., 87 [10] 1967 76 (2004).
-
(2004)
J Am. Ceram. Soc.
, vol.87
, Issue.10
, pp. 1967-76
-
-
Boakye, E.E.1
Hay, R.S.2
Petry, M.D.3
Parthasarathy, T.A.4
-
26
-
-
34248326630
-
-
Unpublished.
-
J. B. Davis, Unpublished.
-
-
-
Davis, J.B.1
-
27
-
-
0036862965
-
Interface Design for Oxidation Resistant Ceramic Composites
-
R. J. Kerans, R. S. Hay, T. A. Parthasarathy M. K. Cinibulk Interface Design for Oxidation Resistant Ceramic Composites J. Am. Ceram. Soc., 85 [11] 2599 632 (2002).
-
(2002)
J. Am. Ceram. Soc.
, vol.85
, Issue.11
, pp. 2599-632
-
-
Kerans, R.J.1
Hay, R.S.2
Parthasarathy, T.A.3
Cinibulk, M.K.4
-
28
-
-
0003391933
-
-
University Press, Cambridge
-
J. W. Martin, R. D. Doherty B. Cantor, Stability of Microstructure in Metallic Systems, 2nd edition, University Press, Cambridge, 1997.
-
(1997)
Stability of Microstructure in Metallic Systems, 2nd Edition
-
-
Martin, J.W.1
Doherty, R.D.2
Cantor, B.3
-
29
-
-
2742601760
-
Sintering and Properties of Monazite-Type CePO4
-
Y. Hikichi, T. Nomura, Y. Tanimura, S. Suzuki M. Miyamoto Sintering and Properties of Monazite-Type CePO4 J. Am. Ceram. Soc., 73 [12] 3594 6 (1990).
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.12
, pp. 3594-6
-
-
Hikichi, Y.1
Nomura, T.2
Tanimura, Y.3
Suzuki, S.4
Miyamoto, M.5
-
30
-
-
0010059981
-
A Physicochemical Study of Lanthanide Orthophosphate
-
I. A. Bondar, A. I. Domanski, L. P. Mezentseva, M. G. Degen N. E. Kalinina A Physicochemical Study of Lanthanide Orthophosphate Russ. J. Inorg. Chem., 21 [8] 1126 9 (1976).
-
(1976)
Russ. J. Inorg. Chem.
, vol.21
, Issue.8
, pp. 1126-9
-
-
Bondar, I.A.1
Domanski, A.I.2
Mezentseva, L.P.3
Degen, M.G.4
Kalinina, N.E.5
-
31
-
-
84889466161
-
-
Wiley-Interscience, New York
-
R. W. Balluffi, S. M. Allen W. C. Carter, Kinetics of Materials, 1st ed, Wiley-Interscience, New York, 2005.
-
(2005)
Kinetics of Materials, 1st Ed
-
-
Balluffi, R.W.1
Allen, S.M.2
Carter, W.C.3
-
32
-
-
84979418085
-
Grain Growth in Very Porous Al2O3 Powder Compacts
-
C. Greskovich W. Lay Grain Growth in Very Porous Al2O3 Powder Compacts J. Am. Ceram. Soc., 55 [3] 142 6 (1972).
-
(1972)
J. Am. Ceram. Soc.
, vol.55
, Issue.3
, pp. 142-6
-
-
Greskovich, C.1
Lay, W.2
-
33
-
-
0024130260
-
Grain-Growth Transition during Sintering of Colloidally Prepared Alumina Powder Compacts
-
C. P. Cameron R. Raj Grain-Growth Transition During Sintering of Colloidally Prepared Alumina Powder Compacts J. Am. Ceram. Soc., 71 [12] 1031 5 (1988).
-
(1988)
J. Am. Ceram. Soc.
, vol.71
, Issue.12
, pp. 1031-5
-
-
Cameron, C.P.1
Raj, R.2
-
34
-
-
0027626947
-
Processing of Nanocrystalline Ceramics for Applications in Superplasticity
-
M. J. Mayo, D. C. Hague D. Chen Processing of Nanocrystalline Ceramics for Applications in Superplasticity Mater. Sci. Eng., A166, 145 59 (1993).
-
(1993)
Mater. Sci. Eng.
, vol.166
, pp. 145-59
-
-
Mayo, M.J.1
Hague, D.C.2
Chen, D.3
|