Volumn 27, Issue 2-3, 2007, Pages 1223-1228

Thermal diffusivity measurement of SiC fibre reinforced BMAS glass ceramic composites exposed mechanical damage

Author keywords

BMAS; Composites; Fatigue; Glass ceramics; Thermal properties

Indexed keywords

BARIUM MAGNESIUM ALUMINIUM SILICATE (BMAS); GLASS CERAMIC MATRIX COMPOSITES; MECHANICAL DAMAGE; THERMAL DIFFUSIVITY;

EID: 33750985347     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2006.04.027     Document Type: Article
Times cited : (3)

References (26)
  • 1
    • 0000369297 scopus 로고
    • High temperature materials-a general review
    • Meetham G.V.J. High temperature materials-a general review. J. Mater. Sci. 26 (1991) 853-860
    • (1991) J. Mater. Sci. , vol.26 , pp. 853-860
    • Meetham, G.V.J.1
  • 2
    • 0000048240 scopus 로고
    • Recent developments in fiber reinforced high temperature ceramic composites
    • Mah T., Mendiratta M.G., Katz A.P., and Mazdiyasni K.S. Recent developments in fiber reinforced high temperature ceramic composites. Ceram. Bull. 6 2 (1987) 304-308
    • (1987) Ceram. Bull. , vol.6 , Issue.2 , pp. 304-308
    • Mah, T.1    Mendiratta, M.G.2    Katz, A.P.3    Mazdiyasni, K.S.4
  • 3
    • 0022659398 scopus 로고
    • Fiber reinforced glasses and glass ceramics for high performance applications
    • Prewo P.M., Brennan J.J., and Layden G.K. Fiber reinforced glasses and glass ceramics for high performance applications. Am. Ceram. Soc. Bull. 65 (1986) 305-313
    • (1986) Am. Ceram. Soc. Bull. , vol.65 , pp. 305-313
    • Prewo, P.M.1    Brennan, J.J.2    Layden, G.K.3
  • 4
    • 0020173673 scopus 로고
    • Silicon carbide fibre reinforced glass ceramic matrix composites exhibiting high strength and toughness
    • Brennan J.J., and Prewo K.M. Silicon carbide fibre reinforced glass ceramic matrix composites exhibiting high strength and toughness. J. Mater. Sci. 17 (1982) 2371-2383
    • (1982) J. Mater. Sci. , vol.17 , pp. 2371-2383
    • Brennan, J.J.1    Prewo, K.M.2
  • 5
    • 84880382006 scopus 로고    scopus 로고
    • Brennan, J. J., Chyung, K. and Taylor, M. P., High strength thermally stable magnesium aluminosilicate glass ceramic matrix SiC fibre composite, USA patent No.: 4589900, 1986.
  • 6
    • 0030196051 scopus 로고    scopus 로고
    • Microstructure property relationships of the fibre reinforced magnesium alumina silicates. I. Mechanical properties and failure characteristic
    • Kumar A., and Knowles K.M. Microstructure property relationships of the fibre reinforced magnesium alumina silicates. I. Mechanical properties and failure characteristic. Acta Met. 44 (1996) 2923-2934
    • (1996) Acta Met. , vol.44 , pp. 2923-2934
    • Kumar, A.1    Knowles, K.M.2
  • 7
    • 0031131332 scopus 로고    scopus 로고
    • Effect of preparation parameters on the properties of unidirectional SiC fibre reinforced MAS and BMAS glass-ceramics
    • Reich C., and Brückner B. Effect of preparation parameters on the properties of unidirectional SiC fibre reinforced MAS and BMAS glass-ceramics. Compos. Technol. 57 (1997) 533-541
    • (1997) Compos. Technol. , vol.57 , pp. 533-541
    • Reich, C.1    Brückner, B.2
  • 8
    • 0032688480 scopus 로고    scopus 로고
    • Influence of the laminate lay-up on the fatigue behaviour of SiC-fibre/BMAS-matrix composites
    • Vanwijgenhoven E., Wevers M., and Biest O.V.D. Influence of the laminate lay-up on the fatigue behaviour of SiC-fibre/BMAS-matrix composites. Compos.: Part A (1999) 623-635
    • (1999) Compos.: Part A , pp. 623-635
    • Vanwijgenhoven, E.1    Wevers, M.2    Biest, O.V.D.3
  • 10
    • 0037409623 scopus 로고    scopus 로고
    • In situ speckle observation of Tyrano/BMAS composites in shear strength measurements
    • Tanebe Y., Ishiguro Y., and Yasuda E. In situ speckle observation of Tyrano/BMAS composites in shear strength measurements. Compos., Part B 34 (2003) 399-403
    • (2003) Compos., Part B , vol.34 , pp. 399-403
    • Tanebe, Y.1    Ishiguro, Y.2    Yasuda, E.3
  • 11
    • 0001131974 scopus 로고
    • Effect of heat treatment in air on the structure and properties of barium osumilite reinforced with Nicalon fibres
    • Bleay S.M., and Scott V.D. Effect of heat treatment in air on the structure and properties of barium osumilite reinforced with Nicalon fibres. J. Mater. Sci. 27 (1992) 825-838
    • (1992) J. Mater. Sci. , vol.27 , pp. 825-838
    • Bleay, S.M.1    Scott, V.D.2
  • 12
  • 13
    • 0002519642 scopus 로고
    • Effect of silicon fibre or whisker reinforcement on the thermal diffusivity, conductivity of an osumilite glass ceramics
    • Johnson L.F., Hasselman D.P.H., and Chung K.J. Effect of silicon fibre or whisker reinforcement on the thermal diffusivity, conductivity of an osumilite glass ceramics. J. Am. Ceram. Soc. 70 (1987) c135-c138
    • (1987) J. Am. Ceram. Soc. , vol.70
    • Johnson, L.F.1    Hasselman, D.P.H.2    Chung, K.J.3
  • 14
    • 0029546829 scopus 로고
    • Thermal expansion behaviour of unidirectionally SiC fibre reinforced MAS and BMAS glass ceramics
    • Reich C., and Bruckner R. Thermal expansion behaviour of unidirectionally SiC fibre reinforced MAS and BMAS glass ceramics. Glastech. Berl. Glass Sci. Technol. 68 12 (1995) 404-409
    • (1995) Glastech. Berl. Glass Sci. Technol. , vol.68 , Issue.12 , pp. 404-409
    • Reich, C.1    Bruckner, R.2
  • 15
    • 84880361455 scopus 로고    scopus 로고
    • Yi{dotless}lmaz, R. and Taylor, R., Effect of heat treatment in air on the thermal properties of SiC fibre reinforced composite, part 1 a barium osumilite (BMAS) matrix glass ceramic composite, J. Mater. Sci., 2006, in press.
  • 16
    • 0027684421 scopus 로고
    • Fatigue behaviour of borosilicate glass-ceramic matrix, Nicalon (silicon carbide) fibre composites
    • Ramakrishnan V., and Jayaraman N. Fatigue behaviour of borosilicate glass-ceramic matrix, Nicalon (silicon carbide) fibre composites. J. Mater. Sci. 28 (1993) 5580-5591
    • (1993) J. Mater. Sci. , vol.28 , pp. 5580-5591
    • Ramakrishnan, V.1    Jayaraman, N.2
  • 18
    • 0027628109 scopus 로고
    • Damage development and moduli reductions in Nicalon-calcium aluminosilicate composites under static fatigue and cyclic fatigue
    • Karandikar P.G., and Shou T.W. Damage development and moduli reductions in Nicalon-calcium aluminosilicate composites under static fatigue and cyclic fatigue. J. Am. Ceram. Soc. 76 7 (1993) 1720-1728
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.7 , pp. 1720-1728
    • Karandikar, P.G.1    Shou, T.W.2
  • 19
    • 0003088381 scopus 로고
    • The effects of thermal fatigue on a SiC fibre/aluminosilicate glass composite
    • Zawada L.P., and Wetherhold R.C. The effects of thermal fatigue on a SiC fibre/aluminosilicate glass composite. J. Mater. Sci. 26 (1991) 648-654
    • (1991) J. Mater. Sci. , vol.26 , pp. 648-654
    • Zawada, L.P.1    Wetherhold, R.C.2
  • 20
    • 0020223822 scopus 로고
    • Thermal diffusivity of composites
    • Taylor R.E. Thermal diffusivity of composites. High Temp. High Press 15 (1983) 299-309
    • (1983) High Temp. High Press , vol.15 , pp. 299-309
    • Taylor, R.E.1
  • 21
    • 0019085249 scopus 로고
    • Construction of apparatus for the heat pulse thermal diffusivity measurements from 300 to 3000 K
    • Taylor R. Construction of apparatus for the heat pulse thermal diffusivity measurements from 300 to 3000 K. J. Phys. E: Sci. Instrum. 13 (1980) 1193-1199
    • (1980) J. Phys. E: Sci. Instrum. , vol.13 , pp. 1193-1199
    • Taylor, R.1
  • 22
    • 0023414650 scopus 로고
    • Structure and chemistry of fibre matrix interfaces in silicon carbide fibre reinforced glass ceramic composites: an electron microscopy study
    • Cooper R.F., and Chyung K. Structure and chemistry of fibre matrix interfaces in silicon carbide fibre reinforced glass ceramic composites: an electron microscopy study. J. Mater. Sci. 22 (1987) 3148-3160
    • (1987) J. Mater. Sci. , vol.22 , pp. 3148-3160
    • Cooper, R.F.1    Chyung, K.2
  • 23
    • 85024664396 scopus 로고
    • Effect of micro-cracking on thermal conductivity: analysis and experiment
    • Edi. D.C Larsen Plenum Press, New York pp. 413-431
    • Hasselman D.P.H. Effect of micro-cracking on thermal conductivity: analysis and experiment. Thermal Conductivity Vol. 16 (1983), Edi. D.C Larsen Plenum Press, New York pp. 413-431
    • (1983) Thermal Conductivity , vol.16
    • Hasselman, D.P.H.1
  • 24
    • 84985080569 scopus 로고
    • Role of thermal barrier in effective thermal diffusivity/conductivity of SiC fibre reinforced reaction bonded silicon nitride
    • Bhatt H., Donaldson K.Y., Hasselman D.P.H., and Bhatt R.T. Role of thermal barrier in effective thermal diffusivity/conductivity of SiC fibre reinforced reaction bonded silicon nitride. J. Am. Ceram. Soc. 73 (1990) 312-316
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 312-316
    • Bhatt, H.1    Donaldson, K.Y.2    Hasselman, D.P.H.3    Bhatt, R.T.4
  • 25
    • 0025958642 scopus 로고
    • Role of interfacial debonding and matrix cracking in the effective thermal diffusivity of SiC fibre reinforced chemical vapour deposited SiC matrix composites
    • Hasselman D.P.H., Venkatesawaron A., and Yu M. Role of interfacial debonding and matrix cracking in the effective thermal diffusivity of SiC fibre reinforced chemical vapour deposited SiC matrix composites. J. Mater. Sci. Lett. 17 (1991) 1037-1042
    • (1991) J. Mater. Sci. Lett. , vol.17 , pp. 1037-1042
    • Hasselman, D.P.H.1    Venkatesawaron, A.2    Yu, M.3
  • 26
    • 0000057425 scopus 로고
    • Role of interfacial debonding and matrix cracking in the effective thermal diffusivity of SiC fibre reinforced chemical vapour infiltrated silicon carbide matrix composites
    • Hasselman D.P.H., Venkatesawaron A., and Tawil H. Role of interfacial debonding and matrix cracking in the effective thermal diffusivity of SiC fibre reinforced chemical vapour infiltrated silicon carbide matrix composites. J. Am. Ceram. Soc. 74 (1991) 1631-1634
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 1631-1634
    • Hasselman, D.P.H.1    Venkatesawaron, A.2    Tawil, H.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.