2
-
-
0343511291
-
Growth of sapphire filaments from the melt
-
LaBelle Jr. H.E., and Mlavsky A.I. Growth of sapphire filaments from the melt. Nature 216 (1967) 574-575
-
(1967)
Nature
, vol.216
, pp. 574-575
-
-
LaBelle Jr., H.E.1
Mlavsky, A.I.2
-
6
-
-
0009743869
-
Growth of single-crystal sapphire-clad ruby fibers
-
Burrus C.A., and Coldren L.A. Growth of single-crystal sapphire-clad ruby fibers. Appl Phys Lett 31 6 (1977) 383-384
-
(1977)
Appl Phys Lett
, vol.31
, Issue.6
, pp. 383-384
-
-
Burrus, C.A.1
Coldren, L.A.2
-
7
-
-
0001625903
-
Crystallization of fibres inside a matrix: a new way of fabrication of composites
-
Mileiko S.T., and Kazmin V.I. Crystallization of fibres inside a matrix: a new way of fabrication of composites. J Mater Sci 27 (1992) 2165-2172
-
(1992)
J Mater Sci
, vol.27
, pp. 2165-2172
-
-
Mileiko, S.T.1
Kazmin, V.I.2
-
8
-
-
0027094721
-
Structure and mechanical properties of oxide fibre reinforced metal-matrix composites produced by the internal crystallization method
-
Mileiko S.T., and Kazmin V.I. Structure and mechanical properties of oxide fibre reinforced metal-matrix composites produced by the internal crystallization method. Compos Sci Technol 45 (1992) 209-220
-
(1992)
Compos Sci Technol
, vol.45
, pp. 209-220
-
-
Mileiko, S.T.1
Kazmin, V.I.2
-
9
-
-
0032690193
-
Sapphire fibres grown by a modified internal crystallization method
-
Kurlov V.N., Kiiko V.M., Kolchin A.A., and Mileiko S.T. Sapphire fibres grown by a modified internal crystallization method. J Cryst Growth 204 4 (1999) 499-504
-
(1999)
J Cryst Growth
, vol.204
, Issue.4
, pp. 499-504
-
-
Kurlov, V.N.1
Kiiko, V.M.2
Kolchin, A.A.3
Mileiko, S.T.4
-
11
-
-
27644540872
-
Oxide fibers produced by internal crystallization method and their usage in oxide-matrix composites
-
Krenkel W., Naslain R., and Schneider H. (Eds), Wiley-VCh, Weinheim
-
Mileiko S.T., Kiiko V.M., Kolchin A.A., and Kurlov V.N. Oxide fibers produced by internal crystallization method and their usage in oxide-matrix composites. In: Krenkel W., Naslain R., and Schneider H. (Eds). High temperature ceramic matrix composites (2001), Wiley-VCh, Weinheim 633-638
-
(2001)
High temperature ceramic matrix composites
, pp. 633-638
-
-
Mileiko, S.T.1
Kiiko, V.M.2
Kolchin, A.A.3
Kurlov, V.N.4
-
12
-
-
0036779043
-
Fabrication, properties and usage of single-crystalline YAG fibres
-
Mileiko S.T., Kurlov V.N., Kolchin A.A., and Kiiko V.M. Fabrication, properties and usage of single-crystalline YAG fibres. J Eur Ceram Soc 22 11 (2002) 1831-1837
-
(2002)
J Eur Ceram Soc
, vol.22
, Issue.11
, pp. 1831-1837
-
-
Mileiko, S.T.1
Kurlov, V.N.2
Kolchin, A.A.3
Kiiko, V.M.4
-
13
-
-
0035251936
-
Fabrication and some properties of single crystalline mullite fibers
-
Mileiko S.T., Kiiko V.M., Starostin M.Yu., Kolchin A.A., and Kozhevnikov L.S. Fabrication and some properties of single crystalline mullite fibers. Scripta Mater 44 2 (2001) 249-255
-
(2001)
Scripta Mater
, vol.44
, Issue.2
, pp. 249-255
-
-
Mileiko, S.T.1
Kiiko, V.M.2
Starostin, M.Yu.3
Kolchin, A.A.4
Kozhevnikov, L.S.5
-
14
-
-
0141573478
-
Mullite single crystal fibers produced by the internal crystallization method (ICM)
-
Rüscher C.H., Mileiko S.T., and Schneider H. Mullite single crystal fibers produced by the internal crystallization method (ICM). J Eur Ceram Soc 23 (2003) 3113-3117
-
(2003)
J Eur Ceram Soc
, vol.23
, pp. 3113-3117
-
-
Rüscher, C.H.1
Mileiko, S.T.2
Schneider, H.3
-
15
-
-
0033213435
-
Evaluation of room temperature strength of oxide fibres produced by the internal crystallization method
-
Kiiko V.M., and Mileiko S.T. Evaluation of room temperature strength of oxide fibres produced by the internal crystallization method. Compos Sci Technol 59 13 (1999) 1977-1981
-
(1999)
Compos Sci Technol
, vol.59
, Issue.13
, pp. 1977-1981
-
-
Kiiko, V.M.1
Mileiko, S.T.2
-
16
-
-
0036470941
-
Oxide-fibre/Ni-based matrix composites - III: a creep model and analysis of experimental data
-
Mileiko S.T. Oxide-fibre/Ni-based matrix composites - III: a creep model and analysis of experimental data. Compos Sci Technol 62 2 (2002) 195-204
-
(2002)
Compos Sci Technol
, vol.62
, Issue.2
, pp. 195-204
-
-
Mileiko, S.T.1
-
17
-
-
33750471786
-
-
Wilson DM, Visser LR. High performance oxide fibers for metal and ceramic composites. Presented at the processing of fibers and composites conference, Barga, Italy, 2000.
-
-
-
-
18
-
-
0017471175
-
High-temperature mechanical properties of mullite under compression
-
Dokko P.C., Pask J.A., and Mazdiyasni K.S. High-temperature mechanical properties of mullite under compression. J Am Ceram Soc 60 (1977) 150-155
-
(1977)
J Am Ceram Soc
, vol.60
, pp. 150-155
-
-
Dokko, P.C.1
Pask, J.A.2
Mazdiyasni, K.S.3
-
19
-
-
0036472026
-
Oxide-fibre/Ni-based matrix composites - I: fabrication and microstructure
-
Mileiko S.T., Kiiko V.M., Kolchin A.A., Serebryakov A.V., Korzhov V.P., Starostin M.Yu., et al. Oxide-fibre/Ni-based matrix composites - I: fabrication and microstructure. Compos Sci Technol 62 2 (2002) 167-179
-
(2002)
Compos Sci Technol
, vol.62
, Issue.2
, pp. 167-179
-
-
Mileiko, S.T.1
Kiiko, V.M.2
Kolchin, A.A.3
Serebryakov, A.V.4
Korzhov, V.P.5
Starostin, M.Yu.6
-
20
-
-
0035946847
-
High temperature creep properties of sapphire-fibre/titanium-aluminide-matrix composites
-
Mileiko S.T., Povarova K.B., Serebryakov A.V., Korzhov V.P., Kolchin A.A., Kiiko V.M., et al. High temperature creep properties of sapphire-fibre/titanium-aluminide-matrix composites. Scripta Mater 44 10 (2001) 2463-2469
-
(2001)
Scripta Mater
, vol.44
, Issue.10
, pp. 2463-2469
-
-
Mileiko, S.T.1
Povarova, K.B.2
Serebryakov, A.V.3
Korzhov, V.P.4
Kolchin, A.A.5
Kiiko, V.M.6
-
21
-
-
33745774577
-
Wettability and interface considerations in advanced heat-resistant Ni-base composites
-
Asthana R., Mileiko S.T., and Sobczak N. Wettability and interface considerations in advanced heat-resistant Ni-base composites. Bull Polish Acad Sci (Technical Sciences) 54 2 (2006) 147-166
-
(2006)
Bull Polish Acad Sci (Technical Sciences)
, vol.54
, Issue.2
, pp. 147-166
-
-
Asthana, R.1
Mileiko, S.T.2
Sobczak, N.3
-
22
-
-
33750462940
-
-
Mileiko ST. Composites reinforced with single crystalline oxide fibres: experiments and modeling. J Mater Sci, in press.
-
-
-
-
23
-
-
0000167449
-
Strength degradation of sapphire fibers during pressure casting of a sapphire-reinforced Ni-base superalloy
-
Asthana R., Tewari S.N., and Draper S.L. Strength degradation of sapphire fibers during pressure casting of a sapphire-reinforced Ni-base superalloy. Metall Mater Trans 29A (1998) 1527-1530
-
(1998)
Metall Mater Trans
, vol.29 A
, pp. 1527-1530
-
-
Asthana, R.1
Tewari, S.N.2
Draper, S.L.3
-
24
-
-
0009686715
-
Interface response to solidification in sapphire-reinforced Ni-base composites
-
Asthana R., and Tewari S.N. Interface response to solidification in sapphire-reinforced Ni-base composites. Adv Compos Mater 9 4 (2000) 265-307
-
(2000)
Adv Compos Mater
, vol.9
, Issue.4
, pp. 265-307
-
-
Asthana, R.1
Tewari, S.N.2
-
25
-
-
0041132666
-
Role of interfacially active metals in the apparent adherence of nickel to sapphire
-
Plenum Press
-
Sutton W.H., and Feingold E. Role of interfacially active metals in the apparent adherence of nickel to sapphire. Materials science research vol. 3 (1966), Plenum Press 577-611
-
(1966)
Materials science research
, vol.3
, pp. 577-611
-
-
Sutton, W.H.1
Feingold, E.2
-
26
-
-
0035421874
-
Evaluation of the fibre/matrix interface strength by the pushing-out of fibres of non-symmetrical cross-section
-
Prokopenko V.M., and Mileiko S.T. Evaluation of the fibre/matrix interface strength by the pushing-out of fibres of non-symmetrical cross-section. Compos Sci Technol 61 11 (2001) 1649-1652
-
(2001)
Compos Sci Technol
, vol.61
, Issue.11
, pp. 1649-1652
-
-
Prokopenko, V.M.1
Mileiko, S.T.2
-
27
-
-
0031186142
-
In situ rare-earth hexaaluminate interphases
-
Cain M.G., Cain R.L., Lewis M.H., and Gent J. In situ rare-earth hexaaluminate interphases. J Am Ceram Soc 80 7 (1997) 1873-1876
-
(1997)
J Am Ceram Soc
, vol.80
, Issue.7
, pp. 1873-1876
-
-
Cain, M.G.1
Cain, R.L.2
Lewis, M.H.3
Gent, J.4
-
28
-
-
0030084731
-
Concept for a damage tolerant ceramic composite with "strong" interfaces
-
Tu W., Lange F.F., and Evans A.G. Concept for a damage tolerant ceramic composite with "strong" interfaces. J Am Ceram Soc 79 (1996) 417-424
-
(1996)
J Am Ceram Soc
, vol.79
, pp. 417-424
-
-
Tu, W.1
Lange, F.F.2
Evans, A.G.3
-
29
-
-
0033996724
-
Aluminosilicate fiber/mullite matrix composites with favorable high-temperature properties
-
Kanka B., and Schneider H. Aluminosilicate fiber/mullite matrix composites with favorable high-temperature properties. J Eur Ceram Soc 20 (2000) 619-623
-
(2000)
J Eur Ceram Soc
, vol.20
, pp. 619-623
-
-
Kanka, B.1
Schneider, H.2
-
30
-
-
0035361193
-
Oxide/oxide composites with fibres produced by using internal crystallization method
-
Kolchin A.A., Kiiko V.M., Sarkissyan N.S., and Mileiko S.T. Oxide/oxide composites with fibres produced by using internal crystallization method. Compos Sci Technol 61 8 (2001) 1079-1082
-
(2001)
Compos Sci Technol
, vol.61
, Issue.8
, pp. 1079-1082
-
-
Kolchin, A.A.1
Kiiko, V.M.2
Sarkissyan, N.S.3
Mileiko, S.T.4
-
31
-
-
33750481070
-
-
Kolchin AA, Korzhov VP, Maleev IV, Kiiko VM, Mileiko ST. Creep of a model sapphire/alumina composite. J Compos Mater, submitted for publication.
-
-
-
-
32
-
-
0036471161
-
Oxide-fibre/Ni-based matrix composites - II: mechanical behaviour
-
Mileiko S.T., Kiiko V.M., Kolchin A.A., Korzhov V.P., and Prokopenko V.M. Oxide-fibre/Ni-based matrix composites - II: mechanical behaviour. Compos Sci Technol 62 2 (2002) 181-193
-
(2002)
Compos Sci Technol
, vol.62
, Issue.2
, pp. 181-193
-
-
Mileiko, S.T.1
Kiiko, V.M.2
Kolchin, A.A.3
Korzhov, V.P.4
Prokopenko, V.M.5
|