1
-
-
0020249827
-
A compliant, high failure strain, fibre-reinforced glass matrix composite
-
K. M. Prewo, "A Compliant, High Failure Strain, Fibre-Reinforced Glass Matrix Composite," J. Mater. Sci., 17 [12] 3549-63 (1982).
-
(1982)
J. Mater. Sci.
, vol.17
, Issue.12
, pp. 3549-3563
-
-
Prewo, K.M.1
-
2
-
-
0023828660
-
Tensile performance of carbon-fibre-reinforced glass
-
V. C. Nardone and K. M. Prewo, "Tensile Performance of Carbon-Fibre-Reinforced Glass," J. Mater. Sci., 23 [1] 168 (1988).
-
(1988)
J. Mater. Sci.
, vol.23
, Issue.1
, pp. 168
-
-
Nardone, V.C.1
Prewo, K.M.2
-
3
-
-
0023400958
-
Fatigue and stress rupture of silicon carbide fibre-reinforced glass-ceramics
-
K. M. Prewo, "Fatigue and Stress Rupture of Silicon Carbide Fibre-Reinforced Glass-Ceramics," J. Mater. Sci., 22 [8] 2595-701 (1987).
-
(1987)
J. Mater. Sci.
, vol.22
, Issue.8
, pp. 2595-2701
-
-
Prewo, K.M.1
-
4
-
-
18144406062
-
-
French Pat. No. 2526785, Nov. 18
-
J. Jamet, D. Damange, and J. Loubeau, "Nouveaux Matériaux Composites Alumine-Alumine à Rupture Fortement Dissipative et Lour Préparation," French Pat. No. 2526785, Nov. 18, 1983.
-
(1983)
Nouveaux Matériaux Composites Alumine-Alumine À Rupture Fortement Dissipative et Lour Préparation
-
-
Jamet, J.1
Damange, D.2
Loubeau, J.3
-
5
-
-
0024749360
-
The mechanical behavior of ceramic matrix composites
-
A. G. Evans and D. B. Marshall, "The Mechanical Behavior of Ceramic Matrix Composites," Acta Metall., 37 [ 10] 2567-83 (1989).
-
(1989)
Acta Metall.
, vol.37
, Issue.10
, pp. 2567-2583
-
-
Evans, A.G.1
Marshall, D.B.2
-
6
-
-
0022060228
-
Failure mechanisms in ceramic-fiber/ceramic-matrix composites
-
D. B. Marshall and A. G. Evans, "Failure Mechanisms in Ceramic-Fiber/Ceramic-Matrix Composites," J. Am. Ceram. Soc., 68 [5] 225-31 (1985).
-
(1985)
J. Am. Ceram. Soc.
, vol.68
, pp. 5225-5231
-
-
Marshall, D.B.1
Evans, A.G.2
-
7
-
-
0020173673
-
Silicon carbide fibre reinforced glass-ceramic matrix composites exhibiting high strength and toughness
-
J. J. Brennan and K. M. Prewo, "Silicon Carbide Fibre Reinforced Glass-Ceramic Matrix Composites Exhibiting High Strength and Toughness," J. Mater. Sci., 17 [8] 2371-83 (1982).
-
(1982)
J. Mater. Sci.
, vol.17
, Issue.8
, pp. 2371-2383
-
-
Brennan, J.J.1
Prewo, K.M.2
-
8
-
-
0020115708
-
Silicon carbide yarn reinforced glass matrix composites
-
J. J. Brennan and K. M. Prewo, "Silicon Carbide Yarn Reinforced Glass Matrix Composites," J. Mater. Sci., 17 [4] 1201-206 (1982).
-
(1982)
J. Mater. Sci.
, vol.17
, Issue.4
, pp. 1201-1206
-
-
Brennan, J.J.1
Prewo, K.M.2
-
9
-
-
0018985511
-
High-strength silicon carbide fibre-reinforced glass-matrix composites
-
J. J. Brennan and K. M. Prewo, "High-Strength Silicon Carbide Fibre-Reinforced Glass-Matrix Composites," J. Mater. Sci., 15 [2] 463-68 (1980).
-
(1980)
J. Mater. Sci.
, vol.15
, Issue.2
, pp. 463-468
-
-
Brennan, J.J.1
Prewo, K.M.2
-
10
-
-
0042606298
-
Theoretical analysis of the fiber pullout and pushout tests
-
R. J. Kerans and T. A. Parthasarathy, "Theoretical Analysis of the Fiber Pullout and Pushout Tests," J. Am. Ceram. Soc., 74 [7] 1585-96 (1991).
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.7
, pp. 1585-1596
-
-
Kerans, R.J.1
Parthasarathy, T.A.2
-
11
-
-
0029172028
-
Silicon carbide/calcium aluminosilicate: A notch-insensitive ceramic-matrix composite
-
C. Cady, T. J. Mackin, and A. G. Evans, "Silicon Carbide/Calcium Aluminosilicate: A Notch-Insensitive Ceramic-Matrix Composite," J. Am. Ceram. Soc., 78 [1] 77-82 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.1
, pp. 77-82
-
-
Cady, C.1
Mackin, T.J.2
Evans, A.G.3
-
12
-
-
0028400567
-
Tensile fracture behaviour of fibre-reinforced ceramic-matrix composite with hole
-
S. Mall, D. E. Bullock, and J. J. Pernot, "Tensile Fracture Behaviour of Fibre-Reinforced Ceramic-Matrix Composite with Hole," Composites, 25 [3] 237-45 (1994).
-
(1994)
Composites
, vol.25
, Issue.3
, pp. 237-245
-
-
Mall, S.1
Bullock, D.E.2
Pernot, J.J.3
-
13
-
-
0024662856
-
Microstructural studies of the interfacial zone of a SiC-fiber-reinforced lithium aluminum silicate glass-ceramic
-
E. Bischoff, M. Rühle, O. Sbaizero, and A. G. Evans, "Microstructural Studies of the Interfacial Zone of a SiC-Fiber-Reinforced Lithium Aluminum Silicate Glass-Ceramic," J. Am. Ceram. Soc., 72 [5] 741-45 (1989).
-
(1989)
J. Am. Ceram. Soc.
, vol.72
, Issue.5
, pp. 741-745
-
-
Bischoff, E.1
Rühle, M.2
Sbaizero, O.3
Evans, A.G.4
-
14
-
-
0003187712
-
Interfacial characterization of glass and glass-ceramic matrix/nicalon SiC fiber composites
-
Proceedings of the Twenty-First University Conference on Ceramic Science. Edited by R. E. Tressler, G. L. Messing, C. G. Pantano, and R. E. Newnham. Plenum Press, New York
-
J. J. Brennan, "Interfacial Characterization of Glass and Glass-Ceramic Matrix/Nicalon SiC Fiber Composites"; pp. 549-60 in Tailoring Multiphase and Composite Ceramics, Proceedings of the Twenty-First University Conference on Ceramic Science. Edited by R. E. Tressler, G. L. Messing, C. G. Pantano, and R. E. Newnham. Plenum Press, New York, 1986.
-
(1986)
Tailoring Multiphase and Composite Ceramics
, pp. 549-560
-
-
Brennan, J.J.1
-
15
-
-
0029358865
-
Oxidation embrittlement probe for ceramic-matrix composites
-
F. E. Heredia, J. McNuIty, F. W. Zok, and A. G. Evans, "Oxidation Embrittlement Probe for Ceramic-Matrix Composites," J. Am. Ceram. Soc., 78 [8] 2097-100 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.8
, pp. 2097-2100
-
-
Heredia, F.E.1
McNuity, J.2
Zok, F.W.3
Evans, A.G.4
-
16
-
-
0000563079
-
Fugitive interface coating in oxide-oxide composites: A viability study
-
T. Mah, K. Keller, T. A. Parthasarathy, and J. Guth, "Fugitive Interface Coating in Oxide-Oxide Composites: A Viability Study," Ceram. Eng. Sci. Proc., 12 [9-10] 1802-15 (1991).
-
(1991)
Ceram. Eng. Sci. Proc.
, vol.12
, Issue.9-10
, pp. 1802-1815
-
-
Mah, T.1
Keller, K.2
Parthasarathy, T.A.3
Guth, J.4
-
17
-
-
84986347515
-
Fiber coating concepts for brittle-matrix composites
-
J. B. Davis, J. P. A. Löfvander, A. G. Evans, E. Bischoff, and M. L. Emiliani, "Fiber Coating Concepts for Brittle-Matrix Composites," J. Am. Ceram. Soc., 76 [5] 1249-57 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, Issue.5
, pp. 1249-1257
-
-
Davis, J.B.1
Löfvander, J.P.A.2
Evans, A.G.3
Bischoff, E.4
Emiliani, M.L.5
-
18
-
-
0029236765
-
Effects of composite processing on the strength of sapphire fiber-reinforced composites
-
J. B. Davis, J. Y. Yang, and A. G. Evans, "Effects of Composite Processing on the Strength of Sapphire Fiber-Reinforced Composites," Acta Metall. Mater., 43 [1] 259-68 (1995).
-
(1995)
Acta Metall. Mater.
, vol.43
, Issue.1
, pp. 259-268
-
-
Davis, J.B.1
Yang, J.Y.2
Evans, A.G.3
-
19
-
-
0022421965
-
-
M. F. Ashby, K. E. Easterling, R. Harrysson, and S. K. Maite, Proc. R. Soc. London, A398, 261 (1985).
-
(1985)
Proc. R. Soc. London
, vol.A398
, pp. 261
-
-
Ashby, M.F.1
Easterling, K.E.2
Harrysson, R.3
Maite, S.K.4
-
21
-
-
28844483519
-
The mechanical behavior of a laminar ceramic/fiber-reinforced epoxy composite
-
C. A. Folsom, F. W. Zok, F. F. Lange, and D. B. Marshall, "The Mechanical Behavior of a Laminar Ceramic/Fiber-Reinforced Epoxy Composite," J. Am. Ceram. Soc., 75 [9] 1-7 (1992).
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, Issue.9
, pp. 1-7
-
-
Folsom, C.A.1
Zok, F.W.2
Lange, F.F.3
Marshall, D.B.4
-
22
-
-
0027573301
-
The mechanics of crack growth in layered materials
-
M. Y. He, F. E. Heredia, D. J. Wissuchek, M. C. Shaw, and A. G. Evans, "The Mechanics of Crack Growth in Layered Materials," Acta Metall. Mater., 41 [4] 1223-28 (1993).
-
(1993)
Acta Metall. Mater.
, vol.41
, Issue.4
, pp. 1223-1228
-
-
He, M.Y.1
Heredia, F.E.2
Wissuchek, D.J.3
Shaw, M.C.4
Evans, A.G.5
|