4
-
-
17144364171
-
Ab-initio calculation of titanium silicon carbide
-
Z. M. Sun and Y. C. Zhou, "Ab-Initio Calculation of Titanium Silicon Carbide," Phys. Rev. B, 60 [3] 1441-3 (1999).
-
(1999)
Phys. Rev. B
, vol.60
, Issue.3
, pp. 1441-1443
-
-
Sun, Z.M.1
Zhou, Y.C.2
-
5
-
-
0035371819
-
2-based ceramic at 900-1300 degrees in air
-
2-Based Ceramic at 900-1300 Degrees in Air," Corros. Sci., 43 [6] 1095-109 (2001).
-
(2001)
Corros. Sci.
, vol.43
, Issue.6
, pp. 1095-1109
-
-
Sun, Z.M.1
Zhou, Y.C.2
Li, M.S.3
-
7
-
-
0033742212
-
Titanium silicon carbide: A ceramic or a metal
-
Y. C. Zhou, Z. M. Sun, J. H. Sun, Y. Zhang, and J. Zhou, "Titanium Silicon Carbide: A Ceramic or A Metal," Z. Metallkd., 91 [4] 329-34 (2000).
-
(2000)
Z. Metallkd.
, vol.91
, Issue.4
, pp. 329-334
-
-
Zhou, Y.C.1
Sun, Z.M.2
Sun, J.H.3
Zhang, Y.4
Zhou, J.5
-
11
-
-
6944232701
-
2
-
2," J. Mater. Sci., 39, 6635-7 (2004).
-
(2004)
J. Mater. Sci.
, vol.39
, pp. 6635-6637
-
-
Zhai, H.X.1
Huang, Z.Y.2
Zhou, Y.3
Zhang, Z.L.4
Wang, Y.F.5
Ai, M.X.6
-
12
-
-
33646596364
-
2
-
2," J. Am. Ceram. Soc., 88, 3245-8 (2005).
-
(2005)
J. Am. Ceram. Soc.
, vol.88
, pp. 3245-3248
-
-
Sarkar, D.1
Basu, B.2
Cho, S.J.3
Chu, M.C.4
Hwang, S.S.5
Park, S.W.6
-
13
-
-
14744298412
-
2 ceramic tools in dry high-speed machining of hardened steel
-
2 Ceramic Tools in Dry High-Speed Machining of Hardened Steel," J. Eur. Ceram. Soc., 25, 1073-9 (2005).
-
(2005)
J. Eur. Ceram. Soc.
, vol.25
, pp. 1073-1079
-
-
Deng, J.X.1
Cao, T.K.2
Liu, L.L.3
-
15
-
-
0035427243
-
2 under room-temperature compression
-
2 Under Room-Temperature Compression," J. Eur. Ceram. Soc., 21, 1007-11 (2001).
-
(2001)
J. Eur. Ceram. Soc.
, vol.21
, pp. 1007-1011
-
-
Zhou, Y.C.1
Sun, Z.M.2
-
16
-
-
0031197257
-
Evaluated material properties for a sintered α-alumina
-
R. G. Munro, "Evaluated Material Properties for a Sintered α-Alumina," J. Am. Ceram. Soc., 80, 1919-28 (1997).
-
(1997)
J. Am. Ceram. Soc.
, vol.80
, pp. 1919-1928
-
-
Munro, R.G.1
-
17
-
-
0036430609
-
2 composites by SPS
-
2 Composites by SPS," Key. Eng. Mater., 224, 347-50 (2002).
-
(2002)
Key. Eng. Mater.
, vol.224
, pp. 347-350
-
-
Luo, Y.M.1
Pan, W.2
Li, S.Q.3
Wang, R.G.4
Li, J.Q.5
-
19
-
-
3142658297
-
2 with improved oxidation resistance by substitution of 51 with Al
-
2 with Improved Oxidation Resistance by Substitution of 51 with Al," Mater. Res. Innov., 8, 97-102 (2004).
-
(2004)
Mater. Res. Innov.
, vol.8
, pp. 97-102
-
-
Zhou, Y.C.1
Zhang, H.B.2
Liu, M.Y.3
Wang, J.Y.4
Bao, Y.W.5
-
21
-
-
0033491110
-
Reciprocating friction and wear behavior of a ceramic-matrix graphite composite for possible use in diesel engine valve guides
-
P. J. Blau, B. Dumont, D. N. Braski, T. Jenkins, E. S. Zanoria, and M. C. Long, "Reciprocating Friction and Wear Behavior of a Ceramic-Matrix Graphite Composite for Possible Use in Diesel Engine Valve Guides," Wear, 225, 1338-49 (1999).
-
(1999)
Wear
, vol.225
, pp. 1338-1349
-
-
Blau, P.J.1
Dumont, B.2
Braski, D.N.3
Jenkins, T.4
Zanoria, E.S.5
Long, M.C.6
-
22
-
-
0033626712
-
Reciprocating friction and wear of two silicon nitride-based ceramics against type 316 stainless steel
-
B. Dumont, P. J. Blau, and G. M. Crosbie, "Reciprocating Friction and Wear of Two Silicon Nitride-Based Ceramics against Type 316 Stainless Steel," Wear, 238, 93-109 (2000).
-
(2000)
Wear
, vol.238
, pp. 93-109
-
-
Dumont, B.1
Blau, P.J.2
Crosbie, G.M.3
-
23
-
-
0032787279
-
Failure modes of plasma sprayed WC-15% Co coated rolling elements
-
R. Ahmed and M. Hadfield, "Failure Modes of Plasma Sprayed WC-15% Co Coated Rolling Elements," Wear, 230, 39-55 (1999).
-
(1999)
Wear
, vol.230
, pp. 39-55
-
-
Ahmed, R.1
Hadfield, M.2
-
25
-
-
0029111075
-
Investigation into the impact wear behaviour of ceramic coatings
-
R. Bantle and A. Matthews, "Investigation into the Impact Wear Behaviour of Ceramic Coatings," Surf. Coat. Technol., 74, 857-68 (1995).
-
(1995)
Surf. Coat. Technol.
, vol.74
, pp. 857-868
-
-
Bantle, R.1
Matthews, A.2
-
27
-
-
10044234187
-
Effects of the ratio of hardness to young's modulus on the friction and wear behavior of bilayer coatings
-
W. Y. Ni, Y. T. Cheng, M. J. Lukitsch, A. M. Weiner, L. C. Lev, and D. S. Grummon, "Effects of the Ratio of Hardness to Young's Modulus on the Friction and Wear Behavior of Bilayer Coatings," Appl. Phys. Lett., 85 [18] 4028-30 (2004).
-
(2004)
Appl. Phys. Lett.
, vol.85
, Issue.18
, pp. 4028-4030
-
-
Ni, W.Y.1
Cheng, Y.T.2
Lukitsch, M.J.3
Weiner, A.M.4
Lev, L.C.5
Grummon, D.S.6
-
28
-
-
0025130331
-
Tribology of ceramics
-
K. Kato, "Tribology of Ceramics," Wear., 136, 117-33 (1990).
-
(1990)
Wear
, vol.136
, pp. 117-133
-
-
Kato, K.1
-
30
-
-
0345476789
-
Wear by hard particles
-
K. H. Z. Gahr, "Wear by Hard Particles," Tribol. Int., 31, 587-96 (1998).
-
(1998)
Tribol. Int.
, vol.31
, pp. 587-596
-
-
Gahr, K.H.Z.1
-
31
-
-
0029108381
-
Friction and wear behaviour of ceramic-hardened steel couples under reciprocating sliding motion
-
Y. J. He, A. J. A. Winnubst, D. J. Schipper, P. M. V. Bakker, A. J. Burggraaf, and H. Verweij, "Friction and Wear Behaviour of Ceramic-Hardened Steel Couples under Reciprocating Sliding Motion," Wear, 184, 33-43 (1995).
-
(1995)
Wear
, vol.184
, pp. 33-43
-
-
He, Y.J.1
Winnubst, A.J.A.2
Schipper, D.J.3
Bakker, P.M.V.4
Burggraaf, A.J.5
Verweij, H.6
-
32
-
-
0042693214
-
Friction and wear behavior of SiAlON ceramics under fretting contacts
-
B. Basu, J. Vleugels, M. Kalin, and O. V. D. Biest, "Friction and Wear Behavior of SiAlON Ceramics Under Fretting Contacts," Mater. Sci. Eng. A., 359, 228-36 (2003).
-
(2003)
Mater. Sci. Eng. A
, vol.359
, pp. 228-236
-
-
Basu, B.1
Vleugels, J.2
Kalin, M.3
Biest, O.V.D.4
-
33
-
-
4644280261
-
Tribo-oxidalion of cathodic arc ion-plated (V, Ti)N coatings sliding against a steel ball under both unlubricated and boundary-lubricated conditions
-
J. H. Ouyang and S. Sasaki, "Tribo-Oxidalion of Cathodic Arc Ion-Plated (V, Ti)N Coatings Sliding Against a Steel Ball Under Both Unlubricated and Boundary-Lubricated Conditions," Surf. Com. Technol., 187, 343-57 (2004).
-
(2004)
Surf. Com. Technol.
, vol.187
, pp. 343-357
-
-
Ouyang, J.H.1
Sasaki, S.2
-
34
-
-
0034305157
-
Genesis and role of wear debris in sliding wear of ceramics
-
T. E. Fischer, Z. Zhu, H. Kim, and D. S. Shin, "Genesis and Role of Wear Debris in Sliding Wear of Ceramics," Wear, 245, 53-60 (2000).
-
(2000)
Wear
, vol.245
, pp. 53-60
-
-
Fischer, T.E.1
Zhu, Z.2
Kim, H.3
Shin, D.S.4
-
35
-
-
0038127175
-
Self-lubrication mechanism of chlorine implanted TiN coatings
-
T. Akhadejdamrong, T. Aizawa, M. Yoshilake, A. Mitsvio, T. Yamamoto, and Y. Ikuhara, "Self-Lubrication Mechanism of Chlorine Implanted TiN Coatings," Wear. 254, 668-79 (2003).
-
(2003)
Wear
, vol.254
, pp. 668-679
-
-
Akhadejdamrong, T.1
Aizawa, T.2
Yoshilake, M.3
Mitsvio, A.4
Yamamoto, T.5
Ikuhara, Y.6
-
36
-
-
22944450311
-
Self-lubrication mechanism via the in situ formed lubricious oxide tribofilm
-
T. Aizawa, A. Mitsuo, S. Yamamoto, T. Sumitomo, and S. Muraishi, "Self-Lubrication Mechanism Via the In Situ Formed Lubricious Oxide Tribofilm," Wear, 259, 708-18 (2005).
-
(2005)
Wear
, vol.259
, pp. 708-718
-
-
Aizawa, T.1
Mitsuo, A.2
Yamamoto, S.3
Sumitomo, T.4
Muraishi, S.5
|