2
-
-
0032646603
-
Crystallization in pores
-
Scherer GW (1999) Crystallization in pores. Cem. Concr. Res. 29:1347-1358.
-
(1999)
Cem. Concr. Res.
, vol.29
, pp. 1347-1358
-
-
Scherer, G.W.1
-
3
-
-
0001229391
-
The mechanism of masonry decay through crystallisation
-
National Academy of Sciences, Washington DC
-
Lewin SZ (1981) The mechanism of masonry decay through crystallisation. Conservation of Historic Stone Building and Monuments, National Academy of Sciences, Washington DC, 120-144.
-
(1981)
Conservation of Historic Stone Building and Monuments
, pp. 120-144
-
-
Lewin, S.Z.1
-
4
-
-
0033058244
-
Salt weathering: Influence of evaporation rate, supersaturation and crystallisation pattern
-
Rodríguez-Navarro C, Doehne E (1999) Salt weathering: Influence of evaporation rate, supersaturation and crystallisation pattern. Earth Surf. Process. Landforms 24:191-209.
-
(1999)
Earth Surf. Process. Landforms
, vol.24
, pp. 191-209
-
-
Rodríguez-Navarro, C.1
Doehne, E.2
-
6
-
-
0002032092
-
Materials science research for the conservation of sculpture and monuments
-
Scherer GW, Flatt RJ, Wheeler G (2001) Materials science research for the conservation of sculpture and monuments. MRS Bull. 26:44-50.
-
(2001)
MRS Bull.
, vol.26
, pp. 44-50
-
-
Scherer, G.W.1
Flatt, R.J.2
Wheeler, G.3
-
8
-
-
0021371339
-
The relationship between pore structure and durability of brick
-
Robinson GC (1984) The relationship between pore structure and durability of brick. Am. Ceram. Soc. Bull. 63:295-300.
-
(1984)
Am. Ceram. Soc. Bull.
, vol.63
, pp. 295-300
-
-
Robinson, G.C.1
-
10
-
-
0031471258
-
Pore size distribution and the durability of a porous limestone
-
Ordóñez S, Fort R, García del Cura MA (1997) Pore size distribution and the durability of a porous limestone. Q. J. Eng. Geol. 30:221-230.
-
(1997)
Q. J. Eng. Geol.
, vol.30
, pp. 221-230
-
-
Ordóñez, S.1
Fort, R.2
García Del Cura, M.A.3
-
13
-
-
4344618304
-
Stress from crystallization of salt
-
Scherer GW (2004) Stress from crystallization of salt. Cem. Concr. Res 34:1613-1624.
-
(2004)
Cem. Concr. Res
, vol.34
, pp. 1613-1624
-
-
Scherer, G.W.1
-
14
-
-
49449122490
-
Rate of capillary rise in porous media with nonuniform pores
-
Dullien FAL, El-Sayed MS, Batra VK (1977) Rate of capillary rise in porous media with nonuniform pores. J. Colloid Interf. Sci. 60:497-506.
-
(1977)
J. Colloid Interf. Sci.
, vol.60
, pp. 497-506
-
-
Fal, D.1
El-Sayed, M.S.2
Batra, V.K.3
-
15
-
-
0028668076
-
Modelling the capillary imbibition kinectics in sedimentary rocks: Role of petrographical features
-
Hammecker C, Jeannette D (1994) Modelling the capillary imbibition kinectics in sedimentary rocks: Role of petrographical features. Transport in Porous Med. 17:285-303.
-
(1994)
Transport in Porous Med.
, vol.17
, pp. 285-303
-
-
Hammecker, C.1
Jeannette, D.2
-
17
-
-
0041841568
-
Durability of bricks used in the conservation of historic buildings - Influence of composition and microstructure
-
Elert K, Cultrone G, Rodríguez-Navarro C, Sebastian E (2003) Durability of bricks used in the conservation of historic buildings - Influence of composition and microstructure. J. Cult. Herit. 4:91-99.
-
(2003)
J. Cult. Herit.
, vol.4
, pp. 91-99
-
-
Elert, K.1
Cultrone, G.2
Rodríguez-Navarro, C.3
Sebastian, E.4
-
18
-
-
2642515694
-
Durability estimation of porous building stones from pore structure and strength
-
Benavente D, García del Cura MA, Fort R, Ordóñez S (2004) Durability estimation of porous building stones from pore structure and strength. Eng. Geol. 74:113-127.
-
(2004)
Eng. Geol.
, vol.74
, pp. 113-127
-
-
Benavente, D.1
García Del Cura, M.A.2
Fort, R.3
Ordóñez, S.4
-
20
-
-
0035005377
-
Carbonate and silicate phase reactions during ceramic firing
-
Cultrone G, Rodríguez-Navarro C, Sebastian E, Cazalla O, de la Torre M J (2001) Carbonate and silicate phase reactions during ceramic firing. Eur. J. Mineral. 13:621-634.
-
(2001)
Eur. J. Mineral.
, vol.13
, pp. 621-634
-
-
Cultrone, G.1
Rodríguez-Navarro, C.2
Sebastian, E.3
Cazalla, O.4
De La Torre, M.J.5
-
22
-
-
0027642294
-
Evolution of porosity in extruded stoneware as a function of firing temperature
-
Delbrouck O, Janssen J, Ottenburgs R, Van Oyen P, Viaene W (1993) Evolution of porosity in extruded stoneware as a function of firing temperature. Appl. Clay Sci. 7:187-192.
-
(1993)
Appl. Clay Sci.
, vol.7
, pp. 187-192
-
-
Delbrouck, O.1
Janssen, J.2
Ottenburgs, R.3
Van Oyen, P.4
Viaene, W.5
-
23
-
-
0142259917
-
Influence of mineralogy and firing temperature on porosity of bricks
-
Cultrone G, Sebastian E, Elert K, de la Torre MJ, Cazalla O, Rodríguez-Navarro C (2004) Influence of mineralogy and firing temperature on porosity of bricks. J. Eur. Ceram. Soc. 24:547-564.
-
(2004)
J. Eur. Ceram. Soc.
, vol.24
, pp. 547-564
-
-
Cultrone, G.1
Sebastian, E.2
Elert, K.3
De La Torre, M.J.4
Cazalla, O.5
Rodríguez-Navarro, C.6
-
24
-
-
0021426426
-
Measurement of the resistance to deterioration of old and new bricks by means of accelerated aging tests
-
Binda L, Baronio G (1984) Measurement of the resistance to deterioration of old and new bricks by means of accelerated aging tests. Durability of Building Materials 2:139-154.
-
(1984)
Durability of Building Materials
, vol.2
, pp. 139-154
-
-
Binda, L.1
Baronio, G.2
-
25
-
-
0032172881
-
An approach to the chemistry of pyroxenes formed during the firing of Ca-rich silicate ceramics
-
Dondi M, Ercolani G, Fabbri B, Marsigli M (1998) An approach to the chemistry of pyroxenes formed during the firing of Ca-rich silicate ceramics. Clay Miner. 33:443-452.
-
(1998)
Clay Miner.
, vol.33
, pp. 443-452
-
-
Dondi, M.1
Ercolani, G.2
Fabbri, B.3
Marsigli, M.4
-
30
-
-
0001281470
-
Examination of ancient pottery using the scanning electron microscope
-
Tite MS, Maniatis Y (1975) Examination of ancient pottery using the scanning electron microscope. Nature 257:122-123.
-
(1975)
Nature
, vol.257
, pp. 122-123
-
-
Tite, M.S.1
Maniatis, Y.2
-
31
-
-
33745648040
-
-
Develop at the University of Texas Health Science Center at San Antonio (Texas)
-
UTHESCA ImageTool®. Develop at the University of Texas Health Science Center at San Antonio (Texas, 1995), http://www.frommaxrad6.uthesca.edu
-
(1995)
UTHESCA ImageTool®
-
-
-
33
-
-
0026137690
-
A simple approximate solution for horizontal infiltration in a Brooks-Corey medium
-
Zimmerman RW, Bodvarsson G (1991) A simple approximate solution for horizontal infiltration in a Brooks-Corey medium. Transport in Porous Med. 6:195-205.
-
(1991)
Transport in Porous Med.
, vol.6
, pp. 195-205
-
-
Zimmerman, R.W.1
Bodvarsson, G.2
-
35
-
-
0001214155
-
Salt weathering, a neglected geological erosive agent in coastal and arid environments
-
Wellman HW, Wilson AT (1965) Salt weathering, a neglected geological erosive agent in coastal and arid environments. Nature 205:1097-1098.
-
(1965)
Nature
, vol.205
, pp. 1097-1098
-
-
Wellman, H.W.1
Wilson, A.T.2
-
36
-
-
0031547726
-
Salt crystallization in porous construction materials I. Estimation of crystallization pressure
-
La Iglesia A, Gonzalez V, López-Acevedo V, Viedma C (1997) Salt crystallization in porous construction materials I. Estimation of crystallization pressure. J. Cryst. Growth 177:111-118.
-
(1997)
J. Cryst. Growth
, vol.177
, pp. 111-118
-
-
La Iglesia, A.1
Gonzalez, V.2
López-Acevedo, V.3
Viedma, C.4
|