메뉴 건너뛰기




Volumn 89, Issue 5, 2006, Pages 1615-1620

Role of rare-earth oxide additives on mechanical properties and oxidation behavior of Si 3N 4/BN fibrous monolith ceramics

Author keywords

[No Author keywords available]

Indexed keywords

FIBROUS MONOLITHIC (FM); FOUR-POINT FLEXURAL TESTING; RARE-EARTH OXIDE ADDITIVES;

EID: 33646582333     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2006.00911.x     Document Type: Article
Times cited : (7)

References (26)
  • 1
    • 0027667720 scopus 로고
    • Fibrous monolithic ceramics: I, fabrication, microstructure, and indentation behavior
    • S. Baskaran, S. D. Nunn, D. Popovic, and J. W. Halloran, "Fibrous Monolithic Ceramics: I, Fabrication, Microstructure, and Indentation Behavior," J. Am. Ceram. Soc., 76 [9] 2209-16 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.9 , pp. 2209-2216
    • Baskaran, S.1    Nunn, S.D.2    Popovic, D.3    Halloran, J.W.4
  • 3
    • 0033749005 scopus 로고    scopus 로고
    • Elevated-temperature mechanical properties of silicon nitride/boron nitride fibrous monolithic ceramics
    • R. W. Trice and J. W. Halloran, "Elevated-Temperature Mechanical Properties of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics," J. Am. Ceram. Soc., 83 [2] 311-6 (2000).
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.2 , pp. 311-316
    • Trice, R.W.1    Halloran, J.W.2
  • 5
    • 0033188958 scopus 로고    scopus 로고
    • Influences of microstructure and temperature on the interfacial fracture energy of silicon nitride/boron nitride fibrous monolithic ceramics
    • R. W. Trice and J. W. Halloran, "Influences of Microstructure and Temperature on the Interfacial Fracture Energy of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics," J. Am. Ceram. Soc., 82 [9] 2502-8 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.9 , pp. 2502-2508
    • Trice, R.W.1    Halloran, J.W.2
  • 8
    • 0036602527 scopus 로고    scopus 로고
    • Thermal expansion of unidirectional and cross-ply fibrous monoliths
    • M. Y. He, D. Singh, J. C. McNulty, and F. W. Zok, "Thermal Expansion of Unidirectional and Cross-Ply Fibrous Monoliths," Compos. Sci. Technol., 62, 967-76 (2002).
    • (2002) Compos. Sci. Technol. , vol.62 , pp. 967-976
    • He, M.Y.1    Singh, D.2    McNulty, J.C.3    Zok, F.W.4
  • 9
    • 0017554683 scopus 로고
    • Grain boundary in a hot-pressed MgO fluxed silicon nitride
    • D. R. Clarke and G. Thomas, "Grain Boundary in a Hot-Pressed MgO Fluxed Silicon Nitride," J. Am. Ceram. Soc., 60 [11-12] 491-5 (1977).
    • (1977) J. Am. Ceram. Soc. , vol.60 , Issue.11-12 , pp. 491-495
    • Clarke, D.R.1    Thomas, G.2
  • 10
    • 0023126048 scopus 로고
    • On the equilibrium thickness of intergranular glass phases in ceramic materials
    • D. R. Clarke, "On the Equilibrium Thickness of Intergranular Glass Phases in Ceramic Materials," J. Am. Ceram. Soc., 70 [1] 15-22 (1987).
    • (1987) J. Am. Ceram. Soc. , vol.70 , Issue.1 , pp. 15-22
    • Clarke, D.R.1
  • 11
    • 0029270930 scopus 로고
    • Microstructure of silicon nitride ceramics sintered with rare-earth oxides
    • Y. Goto and G. Thomas, "Microstructure of Silicon Nitride Ceramics Sintered with Rare-Earth Oxides," Acta Metall. Mater., 43 [3] 923-30 (1995).
    • (1995) Acta Metall. Mater. , vol.43 , Issue.3 , pp. 923-930
    • Goto, Y.1    Thomas, G.2
  • 12
    • 0012725032 scopus 로고    scopus 로고
    • The microstructure and boundary phases of in-sitn reinforced silicon nitride
    • M. Liu and S. Nemat-Nasser, "The Microstructure and Boundary Phases of In-Sitn Reinforced Silicon Nitride," Mater. Sc. Eng., A254, 242-52 (1998).
    • (1998) Mater. Sc. Eng. , vol.A254 , pp. 242-252
    • Liu, M.1    Nemat-Nasser, S.2
  • 13
    • 0001518019 scopus 로고
    • Strength and creep behavior of rare-earth disilicate-silicon nitride ceramics
    • M. K. Cinibulk, G. Thomas, and S. M. Johnson, "Strength and Creep Behavior of Rare-Earth Disilicate-Silicon Nitride Ceramics," J. Am. Ceram. Soc., 75 [8] 2050-5 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.8 , pp. 2050-2055
    • Cinibulk, M.K.1    Thomas, G.2    Johnson, S.M.3
  • 14
    • 0026789421 scopus 로고
    • Oxidation behavior of rare-earth disilicate-silicon nitride ceramics
    • M. K. Cinibulk,G. Thomas, and S. M. Johnson, "Oxidation Behavior of Rare-Earth Disilicate-Silicon Nitride Ceramics," J. Am. Ceram. Soc., 75 [8] 2044-9 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.8 , pp. 2044-2049
    • Cinibulk, M.K.1    Thomas, G.2    Johnson, S.M.3
  • 16
    • 0036607724 scopus 로고    scopus 로고
    • Development of a self-forming ytterbium silicate skin on silicon nitride by controlled oxidation
    • S. K. Lee and M. J. Readey, "Development of a Self-Forming Ytterbium Silicate Skin on Silicon Nitride by Controlled Oxidation," J. Am. Ceram. Soc., 85 [6] 1435-40 (2002).
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.6 , pp. 1435-1440
    • Lee, S.K.1    Readey, M.J.2
  • 18
    • 0001121946 scopus 로고
    • 3 by laser raman spectroscopy
    • 3 by Laser Raman Spectroscopy," J Catal., 89, 433-41 (1984).
    • (1984) J Catal. , vol.89 , pp. 433-441
    • Chan, S.S.1    Bell, A.T.2
  • 19
    • 0009801861 scopus 로고
    • Some properties of strontium-doped lanthanum chromite
    • B. D. Meadowcroft, "Some Properties of Strontium-Doped Lanthanum Chromite," Br. J. Appl. Phys., 2 [2] 1225-33 (1969).
    • (1969) Br. J. Appl. Phys. , vol.2 , Issue.2 , pp. 1225-1233
    • Meadowcroft, B.D.1
  • 20
    • 0037377466 scopus 로고    scopus 로고
    • Long-term stability of monoxide ceramics in an oxidative environment at 1500°C
    • H. Klemm, C. Taut, and G. Wotting, "Long-Term Stability of Monoxide Ceramics in an Oxidative Environment at 1500°C," J. Eur. Ceram. Soc., 23, 619-27 (2003).
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 619-627
    • Klemm, H.1    Taut, C.2    Wotting, G.3
  • 21
    • 2042476047 scopus 로고    scopus 로고
    • Silicon nitride oxidation behavior at 1000°C and 1200°C
    • S. P. Taguchi and S. Ribeiro, "Silicon Nitride Oxidation Behavior at 1000°C and 1200°C," J. Mater. Process. Techn., 147, 336-42 (2004).
    • (2004) J. Mater. Process. Techn. , vol.147 , pp. 336-342
    • Taguchi, S.P.1    Ribeiro, S.2
  • 24
    • 0033079046 scopus 로고    scopus 로고
    • High-temperature oxidation of boron nitride: I, monolithic boron nitride
    • N. S. Jacobson and G. N. Morscher, "High-Temperature Oxidation of Boron Nitride: I, Monolithic Boron Nitride," J. Am. Ceram. Soc., 82 [2] 393-8 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.2 , pp. 393-398
    • Jacobson, N.S.1    Morscher, G.N.2
  • 25
    • 0032626259 scopus 로고    scopus 로고
    • High-temperature oxidation of boron nitride: II, boron nitride layers in composites
    • N. S. Jacobson and G. N. Morscher, "High-Temperature Oxidation of Boron Nitride: II, Boron Nitride Layers in Composites," J. Am. Ceram. Soc., 82 [6] 1473-82 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.6 , pp. 1473-1482
    • Jacobson, N.S.1    Morscher, G.N.2
  • 26
    • 0029227342 scopus 로고
    • Oxidative and hydrolytic stability of boron nitride - A new approach to improving the oxidation resistance of carbonaceous structures
    • C. G. Cofer and J. Economy, "Oxidative and Hydrolytic Stability of Boron Nitride - A New Approach to Improving the Oxidation Resistance of Carbonaceous Structures," Carbon, 33 [4] 389-95 (1995).
    • (1995) Carbon , vol.33 , Issue.4 , pp. 389-395
    • Cofer, C.G.1    Economy, J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.