Volumn 25, Issue 4, 2004, Pages 197-202

Sliding contact damage of Y-α/β composite SiAlON ceramics

Author keywords

[No Author keywords available]

Indexed keywords

CERAMIC MATERIALS; COMPOSITE MATERIALS; ETCHING; SILICON NITRIDE; WEAR OF MATERIALS; YTTRIUM;

EID: 31944451453     PISSN: 01966219     EISSN: None     Source Type: Conference Proceeding    
DOI: None     Document Type: Conference Paper
Times cited : (1)

References (11)
  • 1
    • 0027606680 scopus 로고
    • Wear transition diagram for silicon nitride
    • X. Dong and S. Jahanmir, "Wear Transition Diagram for Silicon Nitride," Wear, 165, 169-180 (1993).
    • (1993) Wear , vol.165 , pp. 169-180
    • Dong, X.1    Jahanmir, S.2
  • 2
    • 0027573933 scopus 로고
    • The combined effect of speed and humidity on the wear and friction of silicon nitride
    • M. G Gee and D. Butterfield, "The Combined Effect of Speed and Humidity on the Wear and Friction of Silicon Nitride," Wear, 162-164, 234-245 (1993).
    • (1993) Wear , vol.162-164 , pp. 234-245
    • Gee, M.G.1    Butterfield, D.2
  • 3
    • 0030435043 scopus 로고    scopus 로고
    • Ceramic wear maps
    • S. M. Hsu and M. C. Shen, "Ceramic Wear Maps," Wear, 200,154-175 (1996).
    • (1996) Wear , vol.200 , pp. 154-175
    • Hsu, S.M.1    Shen, M.C.2
  • 4
    • 0031144912 scopus 로고    scopus 로고
    • st report, classification of wear mode-mild wear/severe wear)
    • in Japanese
    • st Report, Classification of Wear Mode-Mild Wear/Severe Wear)," Trans. JSME Ser. C, 63, 1718-1726 (1997), in Japanese.
    • (1997) Trans. JSME Ser. C , vol.63 , pp. 1718-1726
    • Adachi, K.1    Kato, K.2    Chen, N.3
  • 5
    • 0031188885 scopus 로고    scopus 로고
    • nd report, construction of mild-severe wear mode map)
    • in Japanese
    • nd Report, Construction of Mild-Severe Wear Mode Map)," Trans. JSME Ser. C, 63, 2448-2455 (1997), in Japanese.
    • (1997) Trans. JSME Ser. C , vol.63 , pp. 2448-2455
    • Adachi, K.1    Kato, K.2    Chen, N.3
  • 7
    • 0035497613 scopus 로고    scopus 로고
    • Visualization of knoop indentation damage of silicon nitride by plasma etching
    • W. Kanematsu, T. Miyajima and M. Sando, "Visualization of Knoop Indentation Damage of Silicon Nitride by Plasma Etching," J. Am. Ceram. Soc., 84, 2427-2429 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2427-2429
    • Kanematsu, W.1    Miyajima, T.2    Sando, M.3
  • 8
    • 1642423510 scopus 로고    scopus 로고
    • Subsurface damage in scratch testing of silicon nitride
    • In Press
    • W. Kanematsu, "Subsurface damage in scratch testing of silicon nitride," Wear (In Press)
    • Wear
    • Kanematsu, W.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.