Fatigue behavior of arc melted Ti-13Nb-13Zr alloy

Author keywords

Biomaterials; Environmental assisted fatigue; Low cycle fatigue; Titanium alloys

Indexed keywords

BIOCOMPATIBILITY; BIOMATERIALS; CORROSION RESISTANCE; ELASTIC MODULI; FATIGUE OF MATERIALS; HEAT TREATMENT; MEDICAL APPLICATIONS; SODIUM CHLORIDE; SWAGING;

EID: 2942737458     PISSN: 01421123     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijfatigue.2004.01.011     Document Type: Article
Times cited : (42)

References (24)
  • 1
    • 0032170254 scopus 로고    scopus 로고
    • Titanium alloys in total joint replacement: A materials science perspective
    • Long M., Rack H.J. Titanium alloys in total joint replacement: a materials science perspective. Biomaterials. 19:1998;1621-1639.
    • (1998) Biomaterials , vol.19 , pp. 1621-1639
    • Long, M.1    Rack, H.J.2
  • 2
    • 0033078978 scopus 로고    scopus 로고
    • Theoretical study of the effects of alloying elements on the strength and modulus of β-type bio-titanium alloys
    • Song Y., Xu D.S., Yang R., Li D., Wu W.T., Guo Z.X. Theoretical study of the effects of alloying elements on the strength and modulus of β-type bio-titanium alloys. Mater Sci Engng A. 260:1999;269-274.
    • (1999) Mater Sci Engng A , vol.260 , pp. 269-274
    • Song, Y.1    Xu, D.S.2    Yang, R.3    Li, D.4    Wu, W.T.5    Guo, Z.X.6
  • 3
    • 0037210057 scopus 로고    scopus 로고
    • Electrochemical characterization of cast titanium alloys
    • Cai Z., Shafer T., Watanabe J., Nunn M.E., Okabe T. Electrochemical characterization of cast titanium alloys. Biomaterials. 24:2003;213-218.
    • (2003) Biomaterials , vol.24 , pp. 213-218
    • Cai, Z.1    Shafer, T.2    Watanabe, J.3    Nunn, M.E.4    Okabe, T.5
  • 4
    • 0035048541 scopus 로고    scopus 로고
    • A new Ti-15Zr-4Nb-4Ta alloy for medical applications
    • Okazaki Y. A new Ti-15Zr-4Nb-4Ta alloy for medical applications. Curr Opin Solid State Mater Sci. 5:2001;45-53.
    • (2001) Curr Opin Solid State Mater Sci , vol.5 , pp. 45-53
    • Okazaki, Y.1
  • 5
    • 0033120166 scopus 로고    scopus 로고
    • The corrosion behavior of Ti-6Al-4V, Ti-6Al-7Nb and Ti-13Nb-13Zr in protein solutions
    • Khan M.A., Williams R.L., Williams D.F. The corrosion behavior of Ti-6Al-4V, Ti-6Al-7Nb and Ti-13Nb-13Zr in protein solutions. Biomaterials. 20:1999;631-637.
    • (1999) Biomaterials , vol.20 , pp. 631-637
    • Khan, M.A.1    Williams, R.L.2    Williams, D.F.3
  • 6
    • 0034449106 scopus 로고    scopus 로고
    • Titanium alloys for fracture fixation implants
    • Disegi J.A. Titanium alloys for fracture fixation implants. Injury - Int J Care Injured. 31:(Suppl 4):2000;14-17.
    • (2000) Injury - Int J Care Injured , vol.31 , Issue.SUPPL. 4 , pp. 14-17
    • Disegi, J.A.1
  • 7
    • 0032023387 scopus 로고    scopus 로고
    • Mechanical properties of biomedical titanium alloys
    • Niinomi M. Mechanical properties of biomedical titanium alloys. Mater Sci Engng A. 243:1998;231-236.
    • (1998) Mater Sci Engng A , vol.243 , pp. 231-236
    • Niinomi, M.1
  • 8
    • 67349121825 scopus 로고
    • Beta titanium alloys and their role in the titanium industry
    • Bania P.J. Beta titanium alloys and their role in the titanium industry. J Metals. 46:(7):1994;16-19.
    • (1994) J Metals , vol.46 , Issue.7 , pp. 16-19
    • Bania, P.J.1
  • 9
    • 0030142572 scopus 로고    scopus 로고
    • Mechanical and tribological properties and biocompatibility of diffusion hardened Ti-13Nb-13Zr: A new titanium alloy for surgical implants
    • S.A. Brown, & J.E. Lemons. Medical applications of titanium and its alloys: The material and biological issues. Philadelphia, PA: American Society for Testing and Materials
    • Mishra A.K., Davidson J.A., Poggie R.A., Kovacs P., Fitzgerald T.J. Mechanical and tribological properties and biocompatibility of diffusion hardened Ti-13Nb-13Zr: a new titanium alloy for surgical implants. Brown S.A., Lemons J.E. Medical applications of titanium and its alloys: the material and biological issues. ASTM STP 1272. 1996;96-113 American Society for Testing and Materials, Philadelphia, PA.
    • (1996) ASTM STP , vol.1272 , pp. 96-113
    • Mishra, A.K.1    Davidson, J.A.2    Poggie, R.A.3    Kovacs, P.4    Fitzgerald, T.J.5
  • 10
    • 0013342924 scopus 로고    scopus 로고
    • Development of processing methods for Ti-13Nb-13Zr
    • I. Weiss, R. Srinivasan, P.J. Bania, D. Eylon, & S.L. Semiatin. The Minerals, Metals & Materials Society
    • Robare E.W., Bugle C.M., Davidson J.A., Daigle K.P. Development of processing methods for Ti-13Nb-13Zr. Weiss I., Srinivasan R., Bania P.J., Eylon D., Semiatin S.L. Advances in the technology of titanium alloy processing. 1997;283-291 The Minerals, Metals & Materials Society.
    • (1997) Advances in the Technology of Titanium Alloy Processing , pp. 283-291
    • Robare, E.W.1    Bugle, C.M.2    Davidson, J.A.3    Daigle, K.P.4
  • 11
    • 0028309860 scopus 로고
    • New surface-hardened, low modulus, corrosion resistant Ti-13Nb-13Zr alloy for total hip arthroplasty
    • Davidson J.A., Mishra A.K., Kovacs P., Poggie R.A. New surface-hardened, low modulus, corrosion resistant Ti-13Nb-13Zr alloy for total hip arthroplasty. Bio-med Mater Engng. 4:1994;231-243.
    • (1994) Bio-med Mater Engng , vol.4 , pp. 231-243
    • Davidson, J.A.1    Mishra, A.K.2    Kovacs, P.3    Poggie, R.A.4
  • 13
    • 0034317060 scopus 로고    scopus 로고
    • Fatigue of biomaterials: A review
    • Teoh S.H. Fatigue of biomaterials: a review. Int J Fatigue. 22:2000;825-837.
    • (2000) Int J Fatigue , vol.22 , pp. 825-837
    • Teoh, S.H.1
  • 14
    • 0013430807 scopus 로고    scopus 로고
    • Corrosion resistance and corrosion fatigue strength of new titanium alloys for medical implants without V and Al
    • Okazaki Y., Ito Y., Kyo K., Tateishi T. Corrosion resistance and corrosion fatigue strength of new titanium alloys for medical implants without V and Al. Mater Sci Engng A. 213:1996;138-147.
    • (1996) Mater Sci Engng A , vol.213 , pp. 138-147
    • Okazaki, Y.1    Ito, Y.2    Kyo, K.3    Tateishi, T.4
  • 16
    • 0026924789 scopus 로고
    • In vitro corrosion fatigue of 316L cold worked stainless steel
    • Taira M., Lautenschlanger E.P. In vitro corrosion fatigue of 316L cold worked stainless steel. J Biomed Mater Res. 26:1992;1131-1139.
    • (1992) J Biomed Mater Res , vol.26 , pp. 1131-1139
    • Taira, M.1    Lautenschlanger, E.P.2
  • 18
    • 0031675571 scopus 로고    scopus 로고
    • Fatigue crack growth behavior of metallic biomaterials in a physiological environment
    • Nakajima M., Shimizu T., Kanamori T., Tokaji K. Fatigue crack growth behavior of metallic biomaterials in a physiological environment. Fatigue Fract Engng Mater Struct. 21:1998;35-45.
    • (1998) Fatigue Fract Engng Mater Struct , vol.21 , pp. 35-45
    • Nakajima, M.1    Shimizu, T.2    Kanamori, T.3    Tokaji, K.4
  • 19
    • 0012638368 scopus 로고    scopus 로고
    • Fatigue characteristics and microstructure of titanium alloys for biomedical applications
    • Blom A.F. Cradley Heath: EMAS
    • Niinomi M. Fatigue characteristics and microstructure of titanium alloys for biomedical applications. Blom A.F. Fatigue 2002: Proceedings of the Eighth International Fatigue Congress. vol. III:2002;2073-2083 EMAS, Cradley Heath.
    • (2002) Fatigue 2002: Proceedings of the Eighth International Fatigue Congress , vol.3 , pp. 2073-2083
    • Niinomi, M.1
  • 20
    • 0033353149 scopus 로고    scopus 로고
    • Potential ambiguity in the determination of the plastic strain range component in LCF testing
    • Kandil F.A. Potential ambiguity in the determination of the plastic strain range component in LCF testing. Int J Fatigue. 21:1999;1013-1018.
    • (1999) Int J Fatigue , vol.21 , pp. 1013-1018
    • Kandil, F.A.1
  • 21
    • 24244475256 scopus 로고
    • Constant amplitude fatigue life data for notched and unnotched annealed Ti-6Al-4V sheet
    • Wright-Patterson Air Force Base, Ohio
    • Rhode TM, Ertel PW. Constant amplitude fatigue life data for notched and unnotched annealed Ti-6Al-4V sheet. Technical report AD A193 420/7/XAB, Wright-Patterson Air Force Base, Ohio, 1988, 38p.
    • (1988) Technical Report , vol.AD A193 420-7-XAB , pp. 38
    • Rhode, T.M.1    Ertel, P.W.2
  • 22
    • 0029357455 scopus 로고
    • Development of a finite element based strain accumulation model for the prediction of fatigue lives in highly stressed Ti components
    • Putchkov V.I., Dowson L.A., Damrit D. Development of a finite element based strain accumulation model for the prediction of fatigue lives in highly stressed Ti components. Int J Fatigue. 17:1995;385-397.
    • (1995) Int J Fatigue , vol.17 , pp. 385-397
    • Putchkov, V.I.1    Dowson, L.A.2    Damrit, D.3
  • 23
    • 85170371240 scopus 로고
    • The resistance of metals to cyclic deformation
    • Achievement of high fatigue resistance in metals and alloys, Philadelphia, PA: American Society for Testing and Materials
    • Landgraf R.W. The resistance of metals to cyclic deformation. Achievement of high fatigue resistance in metals and alloys, ASTM STP 467. 1970;3-36 American Society for Testing and Materials, Philadelphia, PA.
    • (1970) ASTM STP , vol.467 , pp. 3-36
    • Landgraf, R.W.1
  • 24
    • 0020274131 scopus 로고
    • The cyclic stress-strain response of age-hardenable beta titanium alloys
    • J.C. Williams, Belov A.F. New York: Plenum Press
    • Theodorski G., Koss D.A. The cyclic stress-strain response of age-hardenable beta titanium alloys. Williams J.C., Belov A.F. Titanium and titanium alloys: scientific and technological aspects. vol. I:1982;553-567 Plenum Press, New York.
    • (1982) Titanium and Titanium Alloys: Scientific and Technological Aspects , vol.1 , pp. 553-567
    • Theodorski, G.1    Koss, D.A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.