Volumn 24, Issue 3, 2005, Pages 328-334

Fracture toughness measurement of dental ceramics using the indentation fracture method with different formulas

Author keywords

Dental ceramics; Fracture toughness; Indentation fracture method

Indexed keywords


EID: 28844466307     PISSN: 02874547     EISSN: None     Source Type: Journal    
DOI: 10.4012/dmj.24.328     Document Type: Article
Times cited : (10)

References (45)
  • 1
    • 28844440543 scopus 로고    scopus 로고
    • The mechanical properties of the pressable ceramics and its optimal crystallization
    • Kuroda Y, Shinya A, Matuda T, Katagiri S. The mechanical properties of the pressable ceramics and its optimal crystallization. J J Dent Mater 2003; 22: 221-230.
    • (2003) J J Dent Mater , vol.22 , pp. 221-230
    • Kuroda, Y.1    Shinya, A.2    Matuda, T.3    Katagiri, S.4
  • 2
    • 0033124151 scopus 로고    scopus 로고
    • Effect of glaze thickness on the fracture toughness and hardness of alumina-reinforced porcelain
    • Baharav H, Laufer BZ, Pilo R, Cardash SH. Effect of glaze thickness on the fracture toughness and hardness of alumina-reinforced porcelain. J Prosthet Dent 1999; 81: 515-519.
    • (1999) J Prosthet Dent , vol.81 , pp. 515-519
    • Baharav, H.1    Laufer, B.Z.2    Pilo, R.3    Cardash, S.H.4
  • 4
    • 0347853393 scopus 로고    scopus 로고
    • Mechanical properties of low-fusing porcelains for multi-purpose gold alloys
    • Ohnuki Y. Mechanical properties of low-fusing porcelains for multi-purpose gold alloys. J J Dent Mater 1997; 16: 27-37.
    • (1997) J J Dent Mater , vol.16 , pp. 27-37
    • Ohnuki, Y.1
  • 5
    • 0022702131 scopus 로고
    • Fracture toughness of commercial dental porcelains
    • Morena R, Lockwood PE, Fairhurst CW. Fracture toughness of commercial dental porcelains. Dent Mater 1986; 2: 58-62.
    • (1986) Dent Mater , vol.2 , pp. 58-62
    • Morena, R.1    Lockwood, P.E.2    Fairhurst, C.W.3
  • 6
    • 0030179259 scopus 로고    scopus 로고
    • Effect of different cooling rates on fracture toughness of a glazed alumina reinforced porcelain
    • Baharav H, Laufer BZ, Mizrachi A, Harold S. Effect of different cooling rates on fracture toughness of a glazed alumina reinforced porcelain. J Prosthet Dent 1996; 76: 19-22.
    • (1996) J Prosthet Dent , vol.76 , pp. 19-22
    • Baharav, H.1    Laufer, B.Z.2    Mizrachi, A.3    Harold, S.4
  • 7
    • 0038378501 scopus 로고    scopus 로고
    • Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials
    • Albakry M, Guazzato M, Vincent SM. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials. J Dent 2003; 31: 181-188.
    • (2003) J Dent , vol.31 , pp. 181-188
    • Albakry, M.1    Guazzato, M.2    Vincent, S.M.3
  • 9
    • 0032107537 scopus 로고    scopus 로고
    • Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic
    • Scherrer SS, Denry IL, Wiskott HW. Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic. Dent Mater 1998; 14: 246-255.
    • (1998) Dent Mater , vol.14 , pp. 246-255
    • Scherrer, S.S.1    Denry, I.L.2    Wiskott, H.W.3
  • 10
    • 0030208953 scopus 로고    scopus 로고
    • Biaxial flexural strength and indentation fracture toughness of three new core ceramies
    • Wagner WC, Chu TM. Biaxial flexural strength and indentation fracture toughness of three new core ceramies. J Prosthet Dent 1996; 76: 140-144.
    • (1996) J Prosthet Dent , vol.76 , pp. 140-144
    • Wagner, W.C.1    Chu, T.M.2
  • 11
    • 0025495567 scopus 로고
    • Effects of load and loading time on fracture toughness with indentation method
    • Okada T, Shinya A, Yokozuka S. Effects of load and loading time on fracture toughness with indentation method. Shigaku 1990; 78: 460-486.
    • (1990) Shigaku , vol.78 , pp. 460-486
    • Okada, T.1    Shinya, A.2    Yokozuka, S.3
  • 12
    • 0025495436 scopus 로고
    • Fracture toughness of porcelain using indentation method
    • Ueda H, Shinya A, Tohyama Y, Yokozuka, S. Fracture toughness of porcelain using indentation method. Shigaku 1990; 78: 487-504.
    • (1990) Shigaku , vol.78 , pp. 487-504
    • Ueda, H.1    Shinya, A.2    Tohyama, Y.3    Yokozuka, S.4
  • 13
    • 0025495534 scopus 로고
    • Effects of additive oxide, repeating load on the fracture toughness of calcium phosphate crystalline ceramics (CPCC)
    • Takahashi H, Shinya A, Yokozuka S. Effects of additive oxide, repeating load on the fracture toughness of calcium phosphate crystalline ceramics (CPCC). Shigaku 1990; 78: 505-525.
    • (1990) Shigaku , vol.78 , pp. 505-525
    • Takahashi, H.1    Shinya, A.2    Yokozuka, S.3
  • 14
    • 0035408185 scopus 로고    scopus 로고
    • Effect of water exposure on the fracture toughness and flexure strength of a dental glass
    • Scherrer SS, Denry IL, Wiskott HW, Belser CU. Effect of water exposure on the fracture toughness and flexure strength of a dental glass. Dent Mater 2001; 17: 367-371.
    • (2001) Dent Mater , vol.17 , pp. 367-371
    • Scherrer, S.S.1    Denry, I.L.2    Wiskott, H.W.3    Belser, C.U.4
  • 15
    • 0034328590 scopus 로고    scopus 로고
    • Comparison of two heat-pressed all-ceramic dental materials
    • Gorman CM, McDevitt WE, Hill RG. Comparison of two heat-pressed all-ceramic dental materials. Dent Mater 2000; 16: 389-395.
    • (2000) Dent Mater , vol.16 , pp. 389-395
    • Gorman, C.M.1    McDevitt, W.E.2    Hill, R.G.3
  • 16
    • 0030330338 scopus 로고    scopus 로고
    • Mechanical properties of a new mica-based machinable glass ceramic for CAD/CAM restorations
    • Thompson JY, Bayne SC, Heymann HO. Mechanical properties of a new mica-based machinable glass ceramic for CAD/CAM restorations. J Prosthet Dent 1996; 76: 619-623.
    • (1996) J Prosthet Dent , vol.76 , pp. 619-623
    • Thompson, J.Y.1    Bayne, S.C.2    Heymann, H.O.3
  • 17
    • 0029348306 scopus 로고
    • Relative fracture toughness and hardness of new dental ceramics
    • Seghi RR, Denry IL, Rosenstiel SF. Relative fracture toughness and hardness of new dental ceramics. J Prosthet Dent 1995; 74: 145-150.
    • (1995) J Prosthet Dent , vol.74 , pp. 145-150
    • Seghi, R.R.1    Denry, I.L.2    Rosenstiel, S.F.3
  • 18
    • 0026891164 scopus 로고
    • Effects of ion exchange on hardness and fracture toughness of dental ceramics
    • Seghi RR, Denry IL, Brajevic F. Effects of ion exchange on hardness and fracture toughness of dental ceramics. Int J Prosthodont 1992; 5: 309-314.
    • (1992) Int J Prosthodont , vol.5 , pp. 309-314
    • Seghi, R.R.1    Denry, I.L.2    Brajevic, F.3
  • 19
    • 0024618931 scopus 로고
    • Apparent fracture toughness of metal ceramic restorations with different manipulative variables
    • Rosenstiel SF, Porter SS. Apparent fracture toughness of metal ceramic restorations with different manipulative variables. J Prosthet Dent 1989; 61: 185-191.
    • (1989) J Prosthet Dent , vol.61 , pp. 185-191
    • Rosenstiel, S.F.1    Porter, S.S.2
  • 20
    • 0036134528 scopus 로고    scopus 로고
    • Fracture toughness of dental ceramics: Comparison of bending and indentation method
    • Fischer H, Marx R. Fracture toughness of dental ceramics: Comparison of bending and indentation method. Dent Mater 2002; 18: 12-19.
    • (2002) Dent Mater , vol.18 , pp. 12-19
    • Fischer, H.1    Marx, R.2
  • 22
    • 0034188519 scopus 로고    scopus 로고
    • Mechanical property evaluation of pressable restorative ceramics
    • Drummond JL, King TJ, Bapna MS, Koperski RD. Mechanical property evaluation of pressable restorative ceramics. Dent Mater 2000; 16: 226-233.
    • (2000) Dent Mater , vol.16 , pp. 226-233
    • Drummond, J.L.1    King, T.J.2    Bapna, M.S.3    Koperski, R.D.4
  • 23
    • 0027693235 scopus 로고
    • Fracture toughness of high alumina core dental ceramics: The effect of water and artificial saliva
    • Mante FK, Brantley WA, Dhuru VB, Ziebelt GJ. Fracture toughness of high alumina core dental ceramics: The effect of water and artificial saliva. Int J Prosthodont 1993; 6: 546-552.
    • (1993) Int J Prosthodont , vol.6 , pp. 546-552
    • Mante, F.K.1    Brantley, W.A.2    Dhuru, V.B.3    Ziebelt, G.J.4
  • 24
    • 0028894635 scopus 로고
    • Fracture toughness of dental ceramics for titanium
    • Kvan K, Derand T, Austrheim EK. Fracture toughness of dental ceramics for titanium. Biomater 1995; 16: 73-76.
    • (1995) Biomater , vol.16 , pp. 73-76
    • Kvan, K.1    Derand, T.2    Austrheim, E.K.3
  • 25
    • 0007285056 scopus 로고    scopus 로고
    • A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics
    • Holand W, Schweiger M, Frank M, Rheinberger V. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics. J Biomed Mater Res 2000; 53: 297-303.
    • (2000) J Biomed Mater Res , vol.53 , pp. 297-303
    • Holand, W.1    Schweiger, M.2    Frank, M.3    Rheinberger, V.4
  • 26
    • 84989530091 scopus 로고
    • Fracture toughness measurements of some dental core ceramics: A methodological study
    • Kvan K, Hero H, Öilo G. Fracture toughness measurements of some dental core ceramics: A methodological study. Scand J Dent Res 1991; 99: 527-532.
    • (1991) Scand J Dent Res , vol.99 , pp. 527-532
    • Kvan, K.1    Hero, H.2    Öilo, G.3
  • 28
    • 0042128698 scopus 로고    scopus 로고
    • Influence of microstructure on the fracture toughness of dental ceramics
    • Quinn JB, Sundar V, Lloyd IK. Influence of microstructure on the fracture toughness of dental ceramics. Dent Mater 2003; 19: 603-611.
    • (2003) Dent Mater , vol.19 , pp. 603-611
    • Quinn, J.B.1    Sundar, V.2    Lloyd, I.K.3
  • 30
    • 0019058952 scopus 로고
    • Elastic/plastic indentation damage in ceramics: The median/radial crack system
    • Lawn BR, Evans AG, Marshall BD. Elastic/plastic indentation damage in ceramics: The median/radial crack system. J Am Ceram Soc 1980; 63: 574-581.
    • (1980) J Am Ceram Soc , vol.63 , pp. 574-581
    • Lawn, B.R.1    Evans, A.G.2    Marshall, B.D.3
  • 31
    • 0001641602 scopus 로고
    • Indentation plasticity and fracture of Si3N4 ceramic alloys
    • Lewis MH. Indentation plasticity and fracture of Si3N4 ceramic alloys. J Mater Sci 1981; 16: 3437-3446.
    • (1981) J Mater Sci , vol.16 , pp. 3437-3446
    • Lewis, M.H.1
  • 32
    • 85039343992 scopus 로고
    • The studies of fracture toughness of the fine ceramics
    • Abstract 840-10
    • Miyoshi T, Sagawa N, Sasa T. The studies of fracture toughness of the fine ceramics. J Jpn Soc Mech Eng 1984; Abstract 840-10: 9-16.
    • (1984) J Jpn Soc Mech Eng , pp. 9-16
    • Miyoshi, T.1    Sagawa, N.2    Sasa, T.3
  • 33
    • 0005787430 scopus 로고
    • Indentation microfracture of ceramics - Its application and problems
    • Niihara K. Indentation microfracture of ceramics - Its application and problems. Ceram Jpn 1985; 20: 12-18.
    • (1985) Ceram Jpn , vol.20 , pp. 12-18
    • Niihara, K.1
  • 34
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: Direct crack measurements
    • Anstis GR, Chantikul P, Lawn BR, Marshall BD. A critical evaluation of indentation techniques for measuring fracture toughness: Direct crack measurements. J Am Ceram Soc 1981; 4: 533-538.
    • (1981) J Am Ceram Soc , vol.4 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, B.D.4
  • 35
    • 28844456577 scopus 로고    scopus 로고
    • Evaluation of Young's modulus of human mandible by ultra-micro indentation method
    • Matsushita Y, Kihara M, Koyano K, Murakami Y. Evaluation of Young's modulus of human mandible by ultra-micro indentation method. J Jpn Sci Biomater 2000, 18: 247-252.
    • (2000) J Jpn Sci Biomater , vol.18 , pp. 247-252
    • Matsushita, Y.1    Kihara, M.2    Koyano, K.3    Murakami, Y.4
  • 36
    • 12744273106 scopus 로고    scopus 로고
    • Elastic modulus of resin-based dental restorative materials: A microindentation approach
    • Chung SM, Yap AUJ, Tsai KT, Yap FL. Elastic modulus of resin-based dental restorative materials: a microindentation approach. J Biomed Mater Res B Appl Biomater 2005; 72: 246-253.
    • (2005) J Biomed Mater Res B Appl Biomater , vol.72 , pp. 246-253
    • Chung, S.M.1    Yap, A.U.J.2    Tsai, K.T.3    Yap, F.L.4
  • 37
    • 0019016272 scopus 로고
    • Fracture toughness determination of alumina using four-point-bend specimens and eight straight-through and chevron notches
    • Munz D, Bubsey RT, Shannon JL Jr. Fracture toughness determination of alumina using four-point-bend specimens and eight straight-through and chevron notches. J Am Ceram Soc 1980; 63: 300-305.
    • (1980) J Am Ceram Soc , vol.63 , pp. 300-305
    • Munz, D.1    Bubsey, R.T.2    Shannon Jr., J.L.3
  • 39
    • 0029687551 scopus 로고    scopus 로고
    • Comparison of four modes of fracture toughness testing for dental composites
    • Fujishima A, Ferracane JL. Comparison of four modes of fracture toughness testing for dental composites. Dent Mater 1996; 12: 38-43.
    • (1996) Dent Mater , vol.12 , pp. 38-43
    • Fujishima, A.1    Ferracane, J.L.2
  • 40
    • 0000738741 scopus 로고
    • Fracture toughness determinations by indentation
    • Evans AG, Charles EA. Fracture toughness determinations by indentation. J Am Ceram Soc 1976; 59: 371-372.
    • (1976) J Am Ceram Soc , vol.59 , pp. 371-372
    • Evans, A.G.1    Charles, E.A.2
  • 42
    • 84987344365 scopus 로고
    • Reply to "Comment on elastic/plastic indentation damage in ceramics: The median/radial crack system"
    • Marshall BD, Evans AG. Reply to "Comment on elastic/plastic indentation damage in ceramics: The median/radial crack system". J Am Ceram Soc 1981; 64: C182-183.
    • (1981) J Am Ceram Soc , vol.64
    • Marshall, B.D.1    Evans, A.G.2
  • 45
    • 0035260939 scopus 로고    scopus 로고
    • Determination of elastic properties of metal alloys and dental porcelains
    • Suansuwan N, Swain MV. Determination of elastic properties of metal alloys and dental porcelains. J Oral Rehabil 2001; 28: 133-139.
    • (2001) J Oral Rehabil , vol.28 , pp. 133-139
    • Suansuwan, N.1    Swain, M.V.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.