1
-
-
0036667228
-
Tribological behavior of sialon ceramics sliding against steel lubricated by fluorine containing oils
-
W. Liu C. Ye Y. Chen Z. Ou and D.C. Sun Tribological behavior of sialon ceramics sliding against steel lubricated by fluorine containing oils Trib. Int. 35 2002 503-509
-
(2002)
Trib. Int.
, vol.35
, pp. 503-509
-
-
Liu, W.1
Ye, C.2
Chen, Y.3
Ou, Z.4
Sun, D.C.5
-
2
-
-
0035482623
-
Effect of contact pressure and load on wear of alumina
-
A. Ravikiran and S. Jahanmir Effect of contact pressure and load on wear of alumina Wear 251 2001 980-984
-
(2001)
Wear
, vol.251
, pp. 980-984
-
-
Ravikiran, A.1
Jahanmir, S.2
-
3
-
-
0035526629
-
Tribological properties of unidirectional aligned silicon nitride
-
M. Nakamura K. Hirao Y. Yamauchi and S. Kanzaki Tribological properties of unidirectional aligned silicon nitride J. Am. Ceram. Soc. 84 11 2001 2579-2584
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.11
, pp. 2579-2584
-
-
Nakamura, M.1
Hirao, K.2
Yamauchi, Y.3
Kanzaki, S.4
-
4
-
-
0023728280
-
Dry sliding wear behavior of SiAlON ceramics
-
J.C. Conway P.H. Cohen and D.A. Love Dry sliding wear behavior of SiAlON ceramics Wear 126 1998 79-80
-
(1998)
Wear
, vol.126
, pp. 79-80
-
-
Conway, J.C.1
Cohen, P.H.2
Love, D.A.3
-
5
-
-
0029289227
-
Wear and wear transition mechanisms in silicon carbide during sliding
-
S.-J. Cho C.-D. Um and S.-S Kim Wear and wear transition mechanisms in silicon carbide during sliding J. Am. Ceram. Soc. 78 4 1995 1076-1078
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.4
, pp. 1076-1078
-
-
Cho, S.-J.1
Um, C.-D.2
Kim, S.-S.3
-
6
-
-
0027606680
-
Wear transition diagram of silicon nitride
-
X. Dong and S. Jahanmir Wear transition diagram of silicon nitride Wear 165 1993 169-180
-
(1993)
Wear
, vol.165
, pp. 169-180
-
-
Dong, X.1
Jahanmir, S.2
-
7
-
-
0029406278
-
Influence of speed on the tribochemical reaction products and the associated transitions for the dry sliding of silicon nitride against steel
-
A. Ravikiran and B.N. Parimala Bai Influence of speed on the tribochemical reaction products and the associated transitions for the dry sliding of silicon nitride against steel J. Am. Ceram. Soc. 78 11 1995 3025-3032
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.11
, pp. 3025-3032
-
-
Ravikiran, A.1
Parimala Bai, B.N.2
-
8
-
-
0027573933
-
The combined effect of speed and humidity on the wear and friction of silicon nitride
-
M.G. Gee and D. Butterfield The combined effect of speed and humidity on the wear and friction of silicon nitride Wear 162-164 1993 234-245
-
(1993)
Wear
, vol.162-164
, pp. 234-245
-
-
Gee, M.G.1
Butterfield, D.2
-
10
-
-
84902927213
-
Tribological characteristics of α-alumina in high temperature water
-
S. Kitaoka Y. Yamaguchi and Y. Takahashi Tribological characteristics of α-alumina in high temperature water J. Am. Ceram. Soc. 75 1992 3075-3080
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, pp. 3075-3080
-
-
Kitaoka, S.1
Yamaguchi, Y.2
Takahashi, Y.3
-
11
-
-
0026084678
-
Tribological characteristics of alpha alumina at elevated temperatures
-
X. Dong S. Jahanmir and S.M. Hsu Tribological characteristics of alpha alumina at elevated temperatures J. Am. Ceram. Soc. 74 5 1991 1036-1044
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.5
, pp. 1036-1044
-
-
Dong, X.1
Jahanmir, S.2
Hsu, S.M.3
-
13
-
-
0029152508
-
Tribological behavior of silicon nitride materials under unlubricated sliding between 22 °C and 1000 °C
-
A. Skopp M. Woydt and K.-H. Habig Tribological behavior of silicon nitride materials under unlubricated sliding between 22 °C and 1000 °C Wear 183-186 1995 571-580
-
(1995)
Wear
, vol.183-186
, pp. 571-580
-
-
Skopp, A.1
Woydt, M.2
Habig, K.-H.3
-
14
-
-
44049121717
-
The transition from mild to severe wear in alumina during sliding
-
S.-J. Cho H. Moon B.J. Hockey and S.M. Hsu The transition from mild to severe wear in alumina during sliding Acta Metal. Mater. 40 1 1992 185-192
-
(1992)
Acta Metal. Mater.
, vol.40
, Issue.1
, pp. 185-192
-
-
Cho, S.-J.1
Moon, H.2
Hockey, B.J.3
Hsu, S.M.4
-
15
-
-
0002023796
-
Wear and wear transition mechanisms of ceramics
-
Y. Wang and S.M. Hsu Wear and wear transition mechanisms of ceramics Wear 195 1996 112-122
-
(1996)
Wear
, vol.195
, pp. 112-122
-
-
Wang, Y.1
Hsu, S.M.2
-
16
-
-
0015206088
-
Section-and-etch study of Hertzian fracture mechanics
-
A.G. Mikosza and B.R. Lawn Section-and-etch study of Hertzian fracture mechanics J. Appl. Phys. 42 1971 5540-5545
-
(1971)
J. Appl. Phys.
, vol.42
, pp. 5540-5545
-
-
Mikosza, A.G.1
Lawn, B.R.2
-
17
-
-
1642423510
-
Subsurface damage in scratch testing of silicon nitride
-
W. Kanematsu Subsurface damage in scratch testing of silicon nitride Wear 256 2004 100-107
-
(2004)
Wear
, vol.256
, pp. 100-107
-
-
Kanematsu, W.1
-
18
-
-
0035497613
-
Visualization of Knoop indentation damage of silicon nitride by plasma etching
-
W. Kanematsu T. Miyajima and M. Sando Visualization of Knoop indentation damage of silicon nitride by plasma etching J. Am. Ceram. Soc. 84 10 2001 2427-2429
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.10
, pp. 2427-2429
-
-
Kanematsu, W.1
Miyajima, T.2
Sando, M.3
-
19
-
-
0030088361
-
Transitions in the mechanism of material removal in abrasive wear of alumina
-
H.H.K. Xu and S. Jahanmir Transitions in the mechanism of material removal in abrasive wear of alumina Wear 192 1996 228-232
-
(1996)
Wear
, vol.192
, pp. 228-232
-
-
Xu, H.H.K.1
Jahanmir, S.2
-
22
-
-
0031187556
-
Correlations between tangential forces on the strength of brittle materials
-
N. Axen L. Kahlman and I.M. Hutchings Correlations between tangential forces on the strength of brittle materials Trib. Int. 30 7 1997 467-474
-
(1997)
Trib. Int.
, vol.30
, Issue.7
, pp. 467-474
-
-
Axen, N.1
Kahlman, L.2
Hutchings, I.M.3
-
25
-
-
4244025922
-
Wear mechanism of plasma sprayed alumina coating in sliding contacts with harder asperities
-
Y. Xie and H.M. Hawthorne Wear mechanism of plasma sprayed alumina coating in sliding contacts with harder asperities Wear 225-229 1999 90-103
-
(1999)
Wear
, vol.225-229
, pp. 90-103
-
-
Xie, Y.1
Hawthorne, H.M.2
-
26
-
-
0037124995
-
Effect of contact geometry on the failure modes of thin coatings in the scratch adhesion test
-
Y. Xie and H.M. Hawthorne Effect of contact geometry on the failure modes of thin coatings in the scratch adhesion test Surf. Coat. Technol. 155 2002 121-129
-
(2002)
Surf. Coat. Technol.
, vol.155
, pp. 121-129
-
-
Xie, Y.1
Hawthorne, H.M.2
-
27
-
-
0037415422
-
Effects of indenter radius on the critical load in scratch testing
-
H. Ichimura and Y. Ishii Effects of indenter radius on the critical load in scratch testing Surf. Coat. Technol. 165 2003 1-7
-
(2003)
Surf. Coat. Technol.
, vol.165
, pp. 1-7
-
-
Ichimura, H.1
Ishii, Y.2
-
28
-
-
0021481427
-
Effect of sliding friction forces on the strength of brittle materials
-
B.R. Lawn S.M. Wiederhorn and D.E. Roberts Effect of sliding friction forces on the strength of brittle materials J. Mater. Sci. 19 1984 2561-2569
-
(1984)
J. Mater. Sci.
, vol.19
, pp. 2561-2569
-
-
Lawn, B.R.1
Wiederhorn, S.M.2
Roberts, D.E.3
-
29
-
-
0034305157
-
Genesis and role of wear debris in sliding wear of ceramics
-
T.E. Fischer Z. Zhu H. Kim and D.S. Shin Genesis and role of wear debris in sliding wear of ceramics Wear 245 2000 53-60
-
(2000)
Wear
, vol.245
, pp. 53-60
-
-
Fischer, T.E.1
Zhu, Z.2
Kim, H.3
Shin, D.S.4
|