메뉴 건너뛰기




Volumn 88, Issue 7, 2005, Pages 1967-1972

Advantages of SiC Hi-nicalon or NLM 202 fibers in SiC f-SiBC composites

Author keywords

[No Author keywords available]

Indexed keywords

CREEP RESISTANCE; MICROGRAPHS; OPERATING TEMPERATURE; STRESS LEVEL;

EID: 27644495825     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2005.00241.x     Document Type: Article
Times cited : (8)

References (39)
  • 3
    • 0030652313 scopus 로고    scopus 로고
    • Structure and properties of SYLRAMIC™ silicon carbide fiber - A polycrystalline, stoichiometric β-SiC composition
    • J. Lipowitz, J. A. Rabe, A. Zangvil, and Y. Xu, "Structure and Properties of SYLRAMIC™ Silicon Carbide Fiber - A Polycrystalline, Stoichiometric β-SiC Composition," Ceram. Eng. Sci. Proc., 18 [3] 147-57 (1997).
    • (1997) Ceram. Eng. Sci. Proc. , vol.18 , Issue.3 , pp. 147-157
    • Lipowitz, J.1    Rabe, J.A.2    Zangvil, A.3    Xu, Y.4
  • 4
    • 0001160417 scopus 로고
    • Creep and rupture of advanced SiC fibers
    • Edited by A. Poursartip and K. Street. Woodhouse Publ. Ltd., Whistler, British Columbia, Canada, August
    • J. A. DiCarlo, H. M. Yun, and J. C. Goldsby, "Creep and Rupture of Advanced SiC Fibers;" pp. 315-22 in Proceedings of ICCM-10, Vol. VI, Whistler, BC, Canada. Edited by A. Poursartip and K. Street. Woodhouse Publ. Ltd., Whistler, British Columbia, Canada, August 1995.
    • (1995) Proceedings of ICCM-10, Vol. VI, Whistler, BC, Canada , vol.6 , pp. 315-322
    • DiCarlo, J.A.1    Yun, H.M.2    Goldsby, J.C.3
  • 5
    • 11744302718 scopus 로고
    • High temperature strength and creep behavior of carborundum alpha silicon carbide fibers
    • L. A. Giannuzzi, K. L. Rugg, and R. E. Tressler, "High Temperature Strength and Creep Behavior of Carborundum Alpha Silicon Carbide Fibers," Ceram. Trans., 38, 655-66 (1995).
    • (1995) Ceram. Trans. , vol.38 , pp. 655-666
    • Giannuzzi, L.A.1    Rugg, K.L.2    Tressler, R.E.3
  • 7
    • 0003423336 scopus 로고    scopus 로고
    • Thèse de Doctorat of the University of Caen
    • f-SiBC;" Thèse de Doctorat of the University of Caen, 2000.
    • (2000) f-SiBC
    • Darzens, S.1
  • 9
    • 0033309084 scopus 로고    scopus 로고
    • Thermal stability of low SiC fiber (hi-nicalon) treated in a hot isostatic press
    • T. Shimoo, J. Tsukada, T. Seguchi, and K. Okamura, "Thermal Stability of Low SiC Fiber (Hi-Nicalon) Treated in a Hot Isostatic Press," J. Am. Ceram. Soc., 82 [12] 3508-12 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.12 , pp. 3508-3512
    • Shimoo, T.1    Tsukada, J.2    Seguchi, T.3    Okamura, K.4
  • 10
    • 0029338661 scopus 로고
    • High performance silicon carbide fiber hi-nicalon for ceramic matrix composites
    • M. Takeda, J. Sakamoto, A. Saeki, Y. Imai, and H. Ichikawa, "High Performance Silicon Carbide Fiber Hi-Nicalon for Ceramic Matrix Composites," Ceram. Eng. Sci. Proc., 16 [5] 37-44 (1995).
    • (1995) Ceram. Eng. Sci. Proc. , vol.16 , Issue.5 , pp. 37-44
    • Takeda, M.1    Sakamoto, J.2    Saeki, A.3    Imai, Y.4    Ichikawa, H.5
  • 11
    • 0002493533 scopus 로고
    • Oxygen-free ceramic fibers from organosilicon precursors and E-beam curing
    • H. Ichikawa, K. Okamura, and T. Seguchi, "Oxygen-Free Ceramic Fibers from Organosilicon Precursors and E-Beam Curing," Ceram. Trans., 58, 65-76 (1995).
    • (1995) Ceram. Trans. , vol.58 , pp. 65-76
    • Ichikawa, H.1    Okamura, K.2    Seguchi, T.3
  • 12
    • 0028935218 scopus 로고
    • Microstructure and thermo-mechanical stability of a low-oxygen nicalon fibre
    • M. H. Berger, N. Hochet, and A. R. Bunsell, "Microstructure and Thermo-Mechanical Stability of a Low-Oxygen Nicalon Fibre," J. Microsc., 177 [3] 230-41 (1995).
    • (1995) J. Microsc. , vol.177 , Issue.3 , pp. 230-241
    • Berger, M.H.1    Hochet, N.2    Bunsell, A.R.3
  • 13
    • 0033686358 scopus 로고    scopus 로고
    • Thermal stability of low-oxygen silicon carbide fiber (hi-nicalon) subjected to selected oxidation treatment
    • T. Shimoo, F. Toyoda, and K. Okamura, "Thermal Stability of Low-Oxygen Silicon Carbide Fiber (Hi-Nicalon) Subjected to Selected Oxidation Treatment," J. Am. Ceram. Soc., 83 [6] 1450-6 (2000).
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.6 , pp. 1450-1456
    • Shimoo, T.1    Toyoda, F.2    Okamura, K.3
  • 14
    • 0042870158 scopus 로고    scopus 로고
    • Properties and microstructures of small-diameter SiC-based fibers
    • Edited by A. R. Bunsell and M. H. Berger. Marcel Dekker Inc., New York
    • M. H. Berger, N. Hochet, and A. R. Bunsell, "Properties and Microstructures of Small-Diameter SiC-Based Fibers;" pp. 231-90 in Fine Ceramic Fibers, Edited by A. R. Bunsell and M. H. Berger. Marcel Dekker Inc., New York, 1999.
    • (1999) Fine Ceramic Fibers , pp. 231-290
    • Berger, M.H.1    Hochet, N.2    Bunsell, A.R.3
  • 16
    • 0030946386 scopus 로고    scopus 로고
    • Microstructural evolution of the latest generation of small-diameter SiC-based fibres tested at high temperatures
    • N. Hochet, M. H. Berger, and A. R. Bunsell, "Microstructural Evolution of the Latest Generation of Small-Diameter SiC-Based Fibres Tested at High Temperatures," J. Microsc., 185 [part 2] 243-58 (1997).
    • (1997) J. Microsc. , vol.185 , Issue.2 PART , pp. 243-258
    • Hochet, N.1    Berger, M.H.2    Bunsell, A.R.3
  • 17
    • 0033827951 scopus 로고    scopus 로고
    • Fine diameter ceramic fibres
    • A. R. Bunsell and M. H. Berger, "Fine Diameter Ceramic Fibres," J. Eur. Ceram. Soc., 20 [13] 2249-60 (2000).
    • (2000) J. Eur. Ceram. Soc. , vol.20 , Issue.13 , pp. 2249-2260
    • Bunsell, A.R.1    Berger, M.H.2
  • 18
    • 0030415335 scopus 로고    scopus 로고
    • Mechanical and structural analysis of silicon carbide fiber hi-nicalon type S
    • M. Takeda, J. Sakamoto, A. Saeki, and H. Ichikawa, "Mechanical and Structural Analysis of Silicon Carbide Fiber Hi-Nicalon Type S," Ceram. Eng. Sci. Proc., 17 [4] 35-42 (1996).
    • (1996) Ceram. Eng. Sci. Proc. , vol.17 , Issue.4 , pp. 35-42
    • Takeda, M.1    Sakamoto, J.2    Saeki, A.3    Ichikawa, H.4
  • 19
    • 0033709814 scopus 로고    scopus 로고
    • Recent advances in nicalon fibres including hi-nicalon type S
    • H. Ichikawa, "Recent Advances in Nicalon Fibres Including Hi-Nicalon Type S," Ann. Chim. Sci. Mater., 25, 523-8 (2000).
    • (2000) Ann. Chim. Sci. Mater. , vol.25 , pp. 523-528
    • Ichikawa, H.1
  • 20
    • 0018753215 scopus 로고
    • A thermodynamic and experimental approach of silicon carbide CVD. Application to the CVD-infiltration of porous carbon-carbon composites
    • Edited by T. O. Sedwick and H. Lydtin. The Electrochemical Society, Princeton
    • F. Christin, R. Naslain, and C. Bernard, "A Thermodynamic and Experimental Approach of Silicon Carbide CVD. Application to the CVD-Infiltration of Porous Carbon-Carbon Composites;" pp. 499-514 in Proceedings of the 7th International Conference on CVD, Edited by T. O. Sedwick and H. Lydtin. The Electrochemical Society, Princeton, 1979.
    • (1979) Proceedings of the 7th International Conference on CVD , pp. 499-514
    • Christin, F.1    Naslain, R.2    Bernard, C.3
  • 21
    • 0001679385 scopus 로고
    • Deposition of Si-B-C materials from the vapor phase for applications in ceramic matrix composites
    • S. Goujard and L. Vandenbulcke, "Deposition of Si-B-C Materials from the Vapor Phase for Applications in Ceramic Matrix Composites," Ceram. Trans., 46, 925-35 (1994).
    • (1994) Ceram. Trans. , vol.46 , pp. 925-935
    • Goujard, S.1    Vandenbulcke, L.2
  • 22
    • 0031122726 scopus 로고    scopus 로고
    • Interlaboratory verification of silicon nitride creep properties
    • W. E. Luecke and S. M. Wiederhorn, "Interlaboratory Verification of Silicon Nitride Creep Properties," J. Am. Ceram. Soc., 80, 831-8 (1997).
    • (1997) J. Am. Ceram. Soc. , vol.80 , pp. 831-838
    • Luecke, W.E.1    Wiederhorn, S.M.2
  • 23
    • 0036478962 scopus 로고    scopus 로고
    • Results of an international round-robin for tensile creep rupture of silicon nitride
    • W. E. Luecke, "Results of an International Round-Robin for Tensile Creep Rupture of Silicon Nitride," J. Am. Ceram. Soc., 85 [2] 408-14 (2002).
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.2 , pp. 408-414
    • Luecke, W.E.1
  • 25
  • 27
    • 0022060228 scopus 로고
    • Failure mechanisms in ceramic-fiber/ceramic matrix composites
    • B. Marshall and A. G. Evans, "Failure Mechanisms in Ceramic-Fiber/Ceramic Matrix Composites," J. Am. Ceram. Soc., 68, 225-31 (1985).
    • (1985) J. Am. Ceram. Soc. , vol.68 , pp. 225-231
    • Marshall, B.1    Evans, A.G.2
  • 28
    • 0024641573 scopus 로고
    • Effect of interface mechanical properties on pullout in a SiC-fiber-reinforeed lithium aluminum silicate glass-ceramic
    • M. D. Thouless, O. Sbaizero, L. S. Sigl, and A. G. Evans, "Effect of Interface Mechanical Properties on Pullout in a SiC-Fiber-Reinforeed Lithium Aluminum Silicate Glass-Ceramic," J. Am. Ceram. Soc., 72 [4] 525-32 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.4 , pp. 525-532
    • Thouless, M.D.1    Sbaizero, O.2    Sigl, L.S.3    Evans, A.G.4
  • 29
    • 0025506999 scopus 로고
    • Large scale bridging in brittle matrix composites
    • F. W. Zok and C. L. Hom, "Large Scale Bridging in Brittle Matrix Composites," Acta Metall. Mater., 38, 1895-904 (1990).
    • (1990) Acta Metall. Mater. , vol.38 , pp. 1895-1904
    • Zok, F.W.1    Hom, C.L.2
  • 30
    • 0002699969 scopus 로고
    • Rupture time under creep conditions
    • L. Kachanov, "Rupture Time Under Creep Conditions," Izv Akad Nauk SSR, 8, 26-31 (1958).
    • (1958) Izv Akad Nauk SSR , vol.8 , pp. 26-31
    • Kachanov, L.1
  • 33
    • 27644446812 scopus 로고    scopus 로고
    • Damage quantification of CMCs by image analysis
    • Edited by W. Krenkel, R. Naslain, and H. Schneider. Wiley-VCH, Weinhein, Germany
    • G. Boitier, S. Darzens, L. Chermant, M. Coster, and J. L. Chermant, "Damage Quantification of CMCs by Image Analysis;" pp. 511-6 in High Temperature Ceramic Matrix Composites, HT-CMC4, Edited by W. Krenkel, R. Naslain, and H. Schneider. Wiley-VCH, Weinhein, Germany, 2001.
    • (2001) High Temperature Ceramic Matrix Composites, HT-CMC4 , pp. 511-516
    • Boitier, G.1    Darzens, S.2    Chermant, L.3    Coster, M.4    Chermant, J.L.5
  • 37
    • 0001148590 scopus 로고
    • Creep behavior of ceramic matrix composites
    • J. L. Chermant, "Creep Behavior of Ceramic Matrix Composites," Sil. Ind., 60, 261-73 (1995).
    • (1995) Sil. Ind. , vol.60 , pp. 261-273
    • Chermant, J.L.1
  • 39
    • 27644552545 scopus 로고    scopus 로고
    • Structural Ceramics and Ceramic Composites for High Temperature Applications, Sevilla, Spain, Oct. 7-12
    • (in Structural Ceramics and Ceramic Composites for High Temperature Applications, Euro Conference, Sevilla, Spain, Oct. 7-12, 2001).
    • (2001) Euro Conference


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.