1
-
-
34249927916
-
4-32% SiC Nanocomposite from Amorphous Si-C-N Powder with Improved Strength above 1200°C
-
4-32% SiC Nanocomposite from Amorphous Si-C-N Powder with Improved Strength above 1200°C," J. Mater. Sci. Lett., 10, 112-14 (1990).
-
(1990)
J. Mater. Sci. Lett.
, vol.10
, pp. 112-114
-
-
Niihara, K.1
Izaki, K.2
Kawakami, T.3
-
5
-
-
0031354854
-
4 Matrix Composites
-
4 Matrix Composites," J. Am. Ceram. Soc., 80 [12] 3070-76 (1997).
-
(1997)
J. Am. Ceram. Soc.
, vol.80
, Issue.12
, pp. 3070-3076
-
-
Petrovic, J.J.1
Pena, M.I.2
Reinmanis, I.E.3
Sandlin, M.S.4
Conzone, S.D.5
Kung, H.H.6
Butt, D.P.7
-
6
-
-
0001420039
-
4-SiC Composites with Network Structures of Second Phase
-
4-SiC Composites with Network Structures of Second Phase," Mater. Sci. Eng. A, 261, 270-77 (1999).
-
(1999)
Mater. Sci. Eng. A
, vol.261
, pp. 270-277
-
-
Yamada, K.1
Kamiya, N.2
-
8
-
-
0030244426
-
Influence of Molybdenum Suicide Additions on High-Temperature Oxidation Resistance of Silicon Nitride Materials
-
H. Klemm, K. Tangermann, C. Schubert, and W. Hermel, "Influence of Molybdenum Suicide Additions on High-Temperature Oxidation Resistance of Silicon Nitride Materials," J. Am. Ceram. Soc., 79 [9] 2429-35 (1996).
-
(1996)
J. Am. Ceram. Soc.
, vol.79
, Issue.9
, pp. 2429-2435
-
-
Klemm, H.1
Tangermann, K.2
Schubert, C.3
Hermel, W.4
-
11
-
-
0027700947
-
Properties of Silicon Nitride-Molybdenum Disilicide Particulate Ceramic Composites
-
M.-Y. Kao, "Properties of Silicon Nitride-Molybdenum Disilicide Particulate Ceramic Composites," J. Am. Ceram. Soc., 76 [11] 2879-83 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, Issue.11
, pp. 2879-2883
-
-
Kao, M.-Y.1
-
13
-
-
0030834931
-
2 Composites from Elemental Powders
-
2 Composites from Elemental Powders," J. Am. Ceram. Soc., 80 [1] 269-72 (1996).
-
(1996)
J. Am. Ceram. Soc.
, vol.80
, Issue.1
, pp. 269-272
-
-
Zhang, B.-R.1
Marino, F.2
-
14
-
-
0010191349
-
2/SiC Composite Produced by Self-Propagating HighTemperature Synthesis
-
2/SiC Composite Produced by Self-Propagating HighTemperature Synthesis," J. Mater. Sci., 33, 1653-60 (1998).
-
(1998)
J. Mater. Sci.
, vol.33
, pp. 1653-1660
-
-
Bartlett, A.H.1
Castro, R.G.2
-
18
-
-
0034268370
-
Effect of Binder Content on Shrinkage Behavior of a Multilayered Ceramic Substrate
-
L. S. Chen, S. L. Fu, and W. K. Huang, "Effect of Binder Content on Shrinkage Behavior of a Multilayered Ceramic Substrate," J. Appl. Phys. Jpn., 39 [9A] 5209-10 (2000).
-
(2000)
J. Appl. Phys. Jpn.
, vol.39
, Issue.9 A
, pp. 5209-5210
-
-
Chen, L.S.1
Fu, S.L.2
Huang, W.K.3
-
19
-
-
1842674809
-
Tungsten Oxide
-
Edited by Japan Fine Ceramics Cyclopedia Edit Committee. Gihoudou, Tokyo, Japan
-
K. Kuribayashi, "Tungsten Oxide"; pp. 272-78 in Fine Ceramics Cyclopedia. Edited by Japan Fine Ceramics Cyclopedia Edit Committee. Gihoudou, Tokyo, Japan, 1987.
-
(1987)
Fine Ceramics Cyclopedia
, pp. 272-278
-
-
Kuribayashi, K.1
-
20
-
-
0014648949
-
Studies on the Formation Process of Tungsten Carbide Powder from Tungsten Powder
-
A. Hara and M. Miyake, "Studies on the Formation Process of Tungsten Carbide Powder from Tungsten Powder," J. Jpn. Inst. Met., 33 [12] 1323-28 (1969).
-
(1969)
J. Jpn. Inst. Met.
, vol.33
, Issue.12
, pp. 1323-1328
-
-
Hara, A.1
Miyake, M.2
-
21
-
-
0026102264
-
Processing, Mechanical Properties, and Oxidation Behavior of Silicon Oxinitride Ceramics
-
M. Ohashi, S. Kanzaki, and H. Tabata, "Processing, Mechanical Properties, and Oxidation Behavior of Silicon Oxinitride Ceramics," J. Am. Ceram. Soc., 74 [1] 109-14 (1991).
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.1
, pp. 109-114
-
-
Ohashi, M.1
Kanzaki, S.2
Tabata, H.3
-
22
-
-
0032096296
-
Strengthening and Toughening Mechanism of Ceramic Nanocomposites
-
T. Ohji, Y. K. Jeong, Y. H. Choa, and K. Niihara, "Strengthening and Toughening Mechanism of Ceramic Nanocomposites," J. Am. Ceram. Soc., 81 [6] 1453-60 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, Issue.6
, pp. 1453-1460
-
-
Ohji, T.1
Jeong, Y.K.2
Choa, Y.H.3
Niihara, K.4
|