Volumn 257, Issue 11, 2004, Pages 1154-1166

Tribological behavior of Stellite 21 modified with yttrium

Author keywords

High temperature wear; Micro scratch; Nano indentation; Oxide; Stellite 21; Yttrium

Indexed keywords

COBALT ALLOYS; CORROSION; ENERGY DISPERSIVE SPECTROSCOPY; GAS TURBINES; MICROSTRUCTURE; OXIDATION; SCANNING ELECTRON MICROSCOPY; TRIBOLOGY; WEAR OF MATERIALS; X RAY DIFFRACTION ANALYSIS; YTTRIUM;

EID: 10844232373     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.wear.2004.07.013     Document Type: Article
Times cited : (64)

References (58)
  • 1
    • 10844282598 scopus 로고
    • Cobalt, Cobalt alloys
    • Materials Park, Ohio
    • P. Crook, Cobalt, Cobalt alloys, in: ASM Metal Handbook, vol. 2, Materials Park, Ohio, 1993, pp. 446-456.
    • (1993) ASM Metal Handbook , vol.2 , pp. 446-456
    • Crook, P.1
  • 2
    • 0035360949 scopus 로고    scopus 로고
    • Evidence of tribocorrosion wear in pressurized water reactors
    • E. Lemarie, M. Le Calvar, Evidence of tribocorrosion wear in pressurized water reactors, Wear 249 (2001) 338-344.
    • (2001) Wear , vol.249 , pp. 338-344
    • Lemarie, E.1    Le Calvar, M.2
  • 5
    • 0020707934 scopus 로고
    • Wear-resistant cobalt base alloys
    • K.C. Antony, Wear-resistant cobalt base alloys, J. Metals 35 (1983) 52-60.
    • (1983) J. Metals , vol.35 , pp. 52-60
    • Antony, K.C.1
  • 6
    • 0015557870 scopus 로고
    • The tribological behavior of polycrystalline cobalt as related to crystallographic texture and structure
    • W.J. Huppmann, M.A. Clegg, The tribological behavior of polycrystalline cobalt as related to crystallographic texture and structure, ASLE Trans. 16 (1972) 107-114.
    • (1972) ASLE Trans. , vol.16 , pp. 107-114
    • Huppmann, W.J.1    Clegg, M.A.2
  • 7
    • 0024681449 scopus 로고
    • Comparison of the microstructure and abrasive wear properties of Stellite hardfacing alloys deposited by arc welding and laser cladding
    • S. Atamert, H.K.D.H. Bhadeshia, Comparison of the microstructure and abrasive wear properties of Stellite hardfacing alloys deposited by arc welding and laser cladding, Metals Technol. 20 (1989) 1037-1054.
    • (1989) Metals Technol. , vol.20 , pp. 1037-1054
    • Atamert, S.1    Bhadeshia, H.K.D.H.2
  • 8
    • 0025514553 scopus 로고
    • The microstructure and galling wear of a laser-melted cobalt-base hardfacing alloy
    • S.C. Agarwal, H. Ocken, The microstructure and galling wear of a laser-melted cobalt-base hardfacing alloy, Wear (1990) 140.
    • (1990) Wear , pp. 140
    • Agarwal, S.C.1    Ocken, H.2
  • 9
    • 0031102553 scopus 로고    scopus 로고
    • Microstructural features and mechanical properties of a cobalt-based laser coating
    • V. Otterloo, J. Hosson, Microstructural features and mechanical properties of a cobalt-based laser coating, Acta Mater. 45 (1997) 1225-1236.
    • (1997) Acta Mater. , vol.45 , pp. 1225-1236
    • Otterloo, V.1    Hosson, J.2
  • 10
    • 0033489899 scopus 로고    scopus 로고
    • On the behavior of surface clad layers under high temperature
    • J.N. Aoh, Y.R. Jeng, E.L. Chu, L.T. Wu, On the behavior of surface clad layers under high temperature, Wear 225-229 (1999) 1114-1122.
    • (1999) Wear , vol.225-229 , pp. 1114-1122
    • Aoh, J.N.1    Jeng, Y.R.2    Chu, E.L.3    Wu, L.T.4
  • 11
    • 0242515964 scopus 로고    scopus 로고
    • Effect of molybdenum on the microstructure and wear resistance of cobalt-base Stellite alloys
    • J.C. Shin, J.M. Doh, J.K. Yoon, D.Y. Lee, J.S. Kim, Effect of molybdenum on the microstructure and wear resistance of cobalt-base Stellite alloys, Surf. Coat. Technol. 166 (2003) 117-126.
    • (2003) Surf. Coat. Technol. , vol.166 , pp. 117-126
    • Shin, J.C.1    Doh, J.M.2    Yoon, J.K.3    Lee, D.Y.4    Kim, J.S.5
  • 12
    • 0032664759 scopus 로고    scopus 로고
    • Formation of hep martensite during the isothermal aging of an fee Co-27Cr-5Mo-0.05C implant alloy
    • J.S. Garcia, M.A. Medrano, A.S. Rodriguez, Formation of hep martensite during the isothermal aging of an fee Co-27Cr-5Mo-0.05C implant alloy, Metall. Mater. Trans. A 30 (1999) 1177-1184.
    • (1999) Metall. Mater. Trans. A , vol.30 , pp. 1177-1184
    • Garcia, J.S.1    Medrano, M.A.2    Rodriguez, A.S.3
  • 13
    • 33847252619 scopus 로고
    • Twinning and strain induced fee to hep transformation on the mechanical properties of Co-Ni-Cr-Mo alloys
    • L. Remy, A. Pineau, Twinning and strain induced fee to hep transformation on the mechanical properties of Co-Ni-Cr-Mo alloys, Mater. Sci. Eng. 26 (1976) 123-132.
    • (1976) Mater. Sci. Eng. , vol.26 , pp. 123-132
    • Remy, L.1    Pineau, A.2
  • 14
    • 0018105098 scopus 로고
    • Influence of the fee phase retained at room temperature on the mechanical properties of cobalt
    • G. Bouquet, B. Dubois, Influence of the fee phase retained at room temperature on the mechanical properties of cobalt, Scripta Metall. 12 (1978) 1079-1081.
    • (1978) Scripta Metall. , vol.12 , pp. 1079-1081
    • Bouquet, G.1    Dubois, B.2
  • 15
    • 0021510131 scopus 로고
    • Structure and hardness of Co-Mo-Cr-Si wear resistant alloy
    • A. Halstead, R.D. Rawlings, Structure and hardness of Co-Mo-Cr-Si wear resistant alloy, Metal Sci. 18 (1984) 491-500.
    • (1984) Metal Sci. , vol.18 , pp. 491-500
    • Halstead, A.1    Rawlings, R.D.2
  • 16
    • 0345580847 scopus 로고    scopus 로고
    • Strain induced ε-martensite in a Co-Cr-Mo alloy: Grain size effects
    • P. Huang, H.F. Lopez, Strain induced ε-martensite in a Co-Cr-Mo alloy: grain size effects, Mater. Lett. 39 (1999) 244-248.
    • (1999) Mater. Lett. , vol.39 , pp. 244-248
    • Huang, P.1    Lopez, H.F.2
  • 17
    • 0345580846 scopus 로고    scopus 로고
    • Athermal ε-martensite in a Co-Cr-Mo alloy: Grain size effects
    • P. Huang, H.F. Lopez, Athermal ε-martensite in a Co-Cr-Mo alloy: grain size effects, Mater. Lett. 39 (1999) 249-253.
    • (1999) Mater. Lett. , vol.39 , pp. 249-253
    • Huang, P.1    Lopez, H.F.2
  • 18
    • 0035979872 scopus 로고    scopus 로고
    • Role of aging on the martensitic transformation in a cast cobalt alloy
    • P. Huang, H.F. Lopez, Role of aging on the martensitic transformation in a cast cobalt alloy, Scripta Mater. 45 (2001) 427-433.
    • (2001) Scripta Mater. , vol.45 , pp. 427-433
    • Huang, P.1    Lopez, H.F.2
  • 19
    • 0020500979 scopus 로고
    • The elevated temperature metal to metal wear behavior of selected hardfacing alloys
    • P. Crook, C.C. Li, The elevated temperature metal to metal wear behavior of selected hardfacing alloys, Wear Mater. (1983) 272-279.
    • (1983) Wear Mater. , pp. 272-279
    • Crook, P.1    Li, C.C.2
  • 20
    • 0019441582 scopus 로고
    • Role of stacking fault energy on the galling and wear behavior of a cobalt base alloy
    • K.J. Bhansali, A.E. Miller, Role of stacking fault energy on the galling and wear behavior of a cobalt base alloy, Wear Mater. (1981) 179-182.
    • (1981) Wear Mater. , pp. 179-182
    • Bhansali, K.J.1    Miller, A.E.2
  • 21
    • 0021822994 scopus 로고
    • Reducing the cobalt inventory in light water reactors
    • H. Ocken, Reducing the cobalt inventory in light water reactors, Nucl. Technol. 68 (1984) 18-28.
    • (1984) Nucl. Technol. , vol.68 , pp. 18-28
    • Ocken, H.1
  • 22
    • 0042570414 scopus 로고    scopus 로고
    • Effect of temperature on friction and galling of laser processed Norem 02 and Stellite 21
    • A.J. Persson, S. Jacobson, S. Hogmark, Effect of temperature on friction and galling of laser processed Norem 02 and Stellite 21, Wear 255 (2003) 498-503.
    • (2003) Wear , vol.255 , pp. 498-503
    • Persson, A.J.1    Jacobson, S.2    Hogmark, S.3
  • 23
    • 0028714318 scopus 로고
    • Galling resistance of hardfacing alloys replacing stellite
    • J. Vikstrom, Galling resistance of hardfacing alloys replacing Stellite, Wear 143 (1994) 143-146.
    • (1994) Wear , vol.143 , pp. 143-146
    • Vikstrom, J.1
  • 24
    • 0035691919 scopus 로고    scopus 로고
    • Thermal fatigue characterisitcs of PTA hard-faced steel
    • S.H. Kang, Y.K. Shinoda, Y.K.H.S. Jeong, Thermal fatigue characterisitcs of PTA hard-faced steel, Surf. Eng. 17 (2001) 498-504.
    • (2001) Surf. Eng. , vol.17 , pp. 498-504
    • Kang, S.H.1    Shinoda, Y.K.2    Jeong, Y.K.H.S.3
  • 25
    • 0032119150 scopus 로고    scopus 로고
    • An investigation of Stellite 6 alloy containing 5wt.% Si
    • V. Kuzuku, M. Ceylan, I. Aksoy, An investigation of Stellite 6 alloy containing 5wt.% Si, J. Mater. Process. Technol. 79 (1998) 47-51.
    • (1998) J. Mater. Process. Technol. , vol.79 , pp. 47-51
    • Kuzuku, V.1    Ceylan, M.2    Aksoy, I.3
  • 26
    • 0041568330 scopus 로고    scopus 로고
    • Effects of yttrium on microstructure, mechanical properties and high-temperature wear behavior of cast Stellite 6 alloy
    • L. Wang, D.Y. Li, Effects of yttrium on microstructure, mechanical properties and high-temperature wear behavior of cast Stellite 6 alloy, Wear 255 (2003) 535-544.
    • (2003) Wear , vol.255 , pp. 535-544
    • Wang, L.1    Li, D.Y.2
  • 27
    • 0031996692 scopus 로고    scopus 로고
    • Phase investigation of a cobalt base alloy containing Cr, Ni, W and C
    • V. Kuzuku, M. Ceylan, I. Aksoy, Phase investigation of a cobalt base alloy containing Cr, Ni, W and C, J. Mater. Process. Technol. 74 (1998) 137-141.
    • (1998) J. Mater. Process. Technol. , vol.74 , pp. 137-141
    • Kuzuku, V.1    Ceylan, M.2    Aksoy, I.3
  • 28
    • 0031233012 scopus 로고    scopus 로고
    • Microstructure and phase analyses of Stellite 6 Plus 6 wt.% Mo alloy
    • V. Kuzuku, M. Ceylan, I. Aksoy, Microstructure and Phase Analyses of Stellite 6 Plus 6 wt.% Mo Alloy, J. Mater. Process. Technol. 69 (1997) 257-263.
    • (1997) J. Mater. Process. Technol. , vol.69 , pp. 257-263
    • Kuzuku, V.1    Ceylan, M.2    Aksoy, I.3
  • 29
    • 0030242584 scopus 로고    scopus 로고
    • The effect of elevated temperature and silicon addition on a cobalt-based wear resistant superlloy
    • A. Osma, E.S. Kayali, M.L. Ovecoglu, The effect of elevated temperature and silicon addition on a cobalt-based wear resistant superlloy, J. Mater. Sci. 31 (1996) 4603-4608.
    • (1996) J. Mater. Sci. , vol.31 , pp. 4603-4608
    • Osma, A.1    Kayali, E.S.2    Ovecoglu, M.L.3
  • 30
    • 0036670832 scopus 로고    scopus 로고
    • High-temperature sliding wear of metals
    • F.H. Stott, High-temperature sliding wear of metals, Tribol. Int. 35 (2002) 489-495.
    • (2002) Tribol. Int. , vol.35 , pp. 489-495
    • Stott, F.H.1
  • 32
    • 0022012934 scopus 로고
    • The sliding of wear commercial Fe-12%Cr alloys at high temperatures
    • F.H. Stott, J. Glascott, G.C. Wood, The sliding of wear commercial Fe-12%Cr alloys at high temperatures, Wear 101 (1985) 311-324.
    • (1985) Wear , vol.101 , pp. 311-324
    • Stott, F.H.1    Glascott, J.2    Wood, G.C.3
  • 33
    • 0022146863 scopus 로고
    • The Effectiveness of oxides in reducing sliding wear of alloys
    • F.H. Stott, J. Glascott, G.C. Wood, The Effectiveness of oxides in reducing sliding wear of alloys, Oxid. met. 24 (1985) 99-113.
    • (1985) Oxid. Met. , vol.24 , pp. 99-113
    • Stott, F.H.1    Glascott, J.2    Wood, G.C.3
  • 34
    • 0031594089 scopus 로고    scopus 로고
    • The role of oxidation in the wear of alloys
    • F.H. Stott, The role of oxidation in the wear of alloys, Tribol. Int. 31 (1998) 61-71.
    • (1998) Tribol. Int. , vol.31 , pp. 61-71
    • Stott, F.H.1
  • 35
    • 0000420418 scopus 로고
    • Improvement in properties: Additives in oxidation resistance
    • D.P. Whittle, J. Stringer, Improvement in properties: additives in oxidation resistance, Philos. Trans. R. Soc. London Ser. A 295 (1980) 309-329.
    • (1980) Philos. Trans. R. Soc. London Ser. A , vol.295 , pp. 309-329
    • Whittle, D.P.1    Stringer, J.2
  • 36
    • 0028729919 scopus 로고
    • Interfacial scaling reactions and the reactive element effect
    • B. Pieraggi, R.A. Rapp, Interfacial scaling reactions and the reactive element effect, Mater. High Temp. 24 (1994) 229-234.
    • (1994) Mater. High Temp. , vol.24 , pp. 229-234
    • Pieraggi, B.1    Rapp, R.A.2
  • 37
    • 0027842013 scopus 로고
    • General aspects of the reactive element effect
    • J. Jedlinski, General aspects of the reactive element effect, Corros. Sci. 35 (1993) 863-869.
    • (1993) Corros. Sci. , vol.35 , pp. 863-869
    • Jedlinski, J.1
  • 38
    • 0024766809 scopus 로고
    • The reactive element effect in high-temperature corrosion
    • J. Stringer, The reactive element effect in high-temperature corrosion, Mater. Sci. Eng. A 120 (1989) 129-137.
    • (1989) Mater. Sci. Eng. A , vol.120 , pp. 129-137
    • Stringer, J.1
  • 39
    • 0033702694 scopus 로고    scopus 로고
    • Effects of a reactive element on isothermal and cyclic oxidation of chromia forming alloys: SEM/EDX, TEM and SIMS investigations
    • S. Chevalier, G. Bonnet, Effects of a reactive element on isothermal and cyclic oxidation of chromia forming alloys: SEM/EDX, TEM and SIMS investigations, Mater. High Temp. 17 (2000) 247-256.
    • (2000) Mater. High Temp. , vol.17 , pp. 247-256
    • Chevalier, S.1    Bonnet, G.2
  • 40
    • 0027840330 scopus 로고
    • Role of the rare earth elements on high-temperature oxidation behavior of Fe-Cr, Ni-cr and Ni-Cr-Al alloys
    • L.V. Ramanathan, Role of the rare earth elements on high-temperature oxidation behavior of Fe-Cr, Ni-cr and Ni-Cr-Al alloys, Corros. Sci. 35 (1993) 871-878.
    • (1993) Corros. Sci. , vol.35 , pp. 871-878
    • Ramanathan, L.V.1
  • 42
    • 0002125494 scopus 로고
    • The reactive elements effect on high-temperature oxidation
    • K. Przybylski, G.J. Yurek, The reactive elements effect on high-temperature oxidation, Mater. Sci. Forum 43 (1989) 1-6.
    • (1989) Mater. Sci. Forum , vol.43 , pp. 1-6
    • Przybylski, K.1    Yurek, G.J.2
  • 44
    • 0024717440 scopus 로고
    • Improved high-temperature oxidation behavior of alloys by ion implantation
    • M.J. Bennett, A.T. Tuson, Improved high-temperature oxidation behavior of alloys by ion implantation, Mater. Sci. Eng. 116 (1989) 79-87.
    • (1989) Mater. Sci. Eng. , vol.116 , pp. 79-87
    • Bennett, M.J.1    Tuson, A.T.2
  • 45
    • 0029408489 scopus 로고
    • The Effect of reactive element additions on the selective oxidation, growth and adhesion of chromia scales
    • P. Y. Hou, J. Stringer, The Effect of reactive element additions on the selective oxidation, growth and adhesion of chromia scales, Mater. Sci. Eng. 202 (1995) 1-10.
    • (1995) Mater. Sci. Eng. , vol.202 , pp. 1-10
    • Hou, P.Y.1    Stringer, J.2
  • 46
    • 0342264692 scopus 로고    scopus 로고
    • Effect of yttrium and erbium ion implantation on the oxidation behavior of the AISI 304 austenitic steel
    • F.J. Perez, M.J. Cristobal, M.P. Hierro, F. Pedraza, G. Arnau, P. Merino, Effect of yttrium and erbium ion implantation on the oxidation behavior of the AISI 304 austenitic steel, Surf. Coat. Technol. 126 (2000) 116-122.
    • (2000) Surf. Coat. Technol. , vol.126 , pp. 116-122
    • Perez, F.J.1    Cristobal, M.J.2    Hierro, M.P.3    Pedraza, F.4    Arnau, G.5    Merino, P.6
  • 47
    • 34249758359 scopus 로고
    • The influence of alloying elements on the development and maintenance of protective scales
    • F.H. Stott, J. Glascott, G.C. Wood, The influence of alloying elements on the development and maintenance of protective scales, Oxid. Met. 44 (1995) 113-141.
    • (1995) Oxid. Met. , vol.44 , pp. 113-141
    • Stott, F.H.1    Glascott, J.2    Wood, G.C.3
  • 48
    • 0000680021 scopus 로고    scopus 로고
    • Effects of yttrium on sliding wear of 304 stainless steel in dilute sulphuric acid and air
    • T. Zhang, D.Y. Li, Effects of yttrium on sliding wear of 304 stainless steel in dilute sulphuric acid and air, Mater. Sci. Technol. 15 (1999) 1441-1446.
    • (1999) Mater. Sci. Technol. , vol.15 , pp. 1441-1446
    • Zhang, T.1    Li, D.Y.2
  • 49
    • 0035975576 scopus 로고    scopus 로고
    • Beneficial effects of yttrium on the mechanical failure and chemical stability of the passive film of 304 stainless steel
    • X. Wang, D.Y. Li, Beneficial effects of yttrium on the mechanical failure and chemical stability of the passive film of 304 stainless steel, Mater. Sci. Eng. A 315 (2001) 158-165.
    • (2001) Mater. Sci. Eng. A , vol.315 , pp. 158-165
    • Wang, X.1    Li, D.Y.2
  • 50
    • 0036789086 scopus 로고    scopus 로고
    • Effects of yttrium on mechanical properties and chemical stability of passive film of alumide coating on 1045 steel
    • X. Wang, D.Y. Li, Effects of yttrium on mechanical properties and chemical stability of passive film of alumide coating on 1045 steel, Surf. Coat. Technol. 160 (2002) 20-28.
    • (2002) Surf. Coat. Technol. , vol.160 , pp. 20-28
    • Wang, X.1    Li, D.Y.2
  • 51
    • 0343914331 scopus 로고
    • Méthode d'analyse quantitative des variétés allotropiques du cobalt par les rayons X
    • M. Sage, C. Guillaud, Méthode d'analyse quantitative des variétés allotropiques du cobalt par les rayons X, Rev. Metall. 37 (1950) 139-145.
    • (1950) Rev. Metall. , vol.37 , pp. 139-145
    • Sage, M.1    Guillaud, C.2
  • 52
    • 0029253103 scopus 로고
    • Micro-structural properties of wear resistant alloys
    • H. Berns, Micro-structural properties of wear resistant alloys, Wear 181-183 (1995) 271-279.
    • (1995) Wear , vol.181-183 , pp. 271-279
    • Berns, H.1
  • 54
    • 0020843331 scopus 로고
    • A study of the aging behavior of a cobalt based implant alloy
    • R.N. Taylor, R.B. Waterhouse, A study of the aging behavior of a cobalt based implant alloy, J. Mater. Sci. 18 (1983) 3265-3280.
    • (1983) J. Mater. Sci. , vol.18 , pp. 3265-3280
    • Taylor, R.N.1    Waterhouse, R.B.2
  • 55
    • 0000605365 scopus 로고    scopus 로고
    • Effects of grain size on development of athermal and strain induced ε-martensite in a Co-Cr-Mo implant alloy
    • P. Huang, H.F. Lopez, Effects of grain size on development of athermal and strain induced ε-martensite in a Co-Cr-Mo implant alloy, Mater. Sci. Technol. 15 (1999) 157-164.
    • (1999) Mater. Sci. Technol. , vol.15 , pp. 157-164
    • Huang, P.1    Lopez, H.F.2
  • 56
    • 0017459201 scopus 로고
    • Friction and wear properties of Stellite 31 at temperatures from 293 to 1073K
    • F.H. Stoot, C.W. Stevenson, G.C. Wood, Friction and wear properties of Stellite 31 at temperatures from 293 to 1073K, Metals Technol. 4 (1977) 66-74.
    • (1977) Metals Technol. , vol.4 , pp. 66-74
    • Stoot, F.H.1    Stevenson, C.W.2    Wood, G.C.3
  • 57
    • 0037465025 scopus 로고    scopus 로고
    • The reactive element effect on thermally grown chromia scale residual stress
    • S. Chevalier, C. Valot, G. Bonnet, J.C. Colson, J.P. Larpin, The reactive element effect on thermally grown chromia scale residual stress, Mater. Sci. Eng. A 343 (2003) 257-264.
    • (2003) Mater. Sci. Eng. A , vol.343 , pp. 257-264
    • Chevalier, S.1    Valot, C.2    Bonnet, G.3    Colson, J.C.4    Larpin, J.P.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.