Volumn 30, Issue 2, 2004, Pages 213-217

R-curve behavior of laminated SiC/BN ceramics

Author keywords

B. Interface; C. Fracture; C. Mechanical properties; D. SiC

Indexed keywords

BENDING STRENGTH; CASTING; CRACKS; CUBIC BORON NITRIDE; DELAMINATION; FRACTURE; HOT PRESSING; INDENTATION; LAMINATED COMPOSITES; SILICON CARBIDE; SINTERING;

EID: 0742324192     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0272-8842(03)00091-9     Document Type: Article
Times cited : (25)

References (20)
  • 1
    • 0005376605 scopus 로고
    • Structural ceramic microlaminates by electrophoretic deposition
    • Sarkar P., Haung X., Nicholson P.S. Structural ceramic microlaminates by electrophoretic deposition. J. Am. Ceram. Soc. 75(10):1992;2907-2909.
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.10 , pp. 2907-2909
    • Sarkar, P.1    Haung, X.2    Nicholson, P.S.3
  • 3
    • 0024716116 scopus 로고
    • Alumina and alumina/zirconia multilayer composites obtained by slip casting
    • Requena J., Moreno R., Moya J.S. Alumina and alumina/zirconia multilayer composites obtained by slip casting. J. Am. Ceram. Soc. 72(8):1989;1511-1513.
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.8 , pp. 1511-1513
    • Requena, J.1    Moreno, R.2    Moya, J.S.3
  • 4
    • 0028493771 scopus 로고
    • Processing of tape-cast laminates prepared from fine alumina/zirconia powders
    • Plucknett K.P., Caceres C.H., Hughers C., Wilkinson D.S. Processing of tape-cast laminates prepared from fine alumina/zirconia powders. J. Am. Ceram. Soc. 77(8):1994;2145-2153.
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.8 , pp. 2145-2153
    • Plucknett, K.P.1    Caceres, C.H.2    Hughers, C.3    Wilkinson, D.S.4
  • 5
    • 84985162794 scopus 로고
    • Design of laminated ceramic composite for improved strength and toughness
    • Russo C.J., Harmer M.P., Chan H.M., Miller G.A. Design of laminated ceramic composite for improved strength and toughness. J. Am. Ceram. Soc. 75(12):1992;3396-3400.
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.12 , pp. 3396-3400
    • Russo, C.J.1    Harmer, M.P.2    Chan, H.M.3    Miller, G.A.4
  • 6
    • 0025682555 scopus 로고
    • Coat of alumina sheet with needle-like mullite
    • Katsuki H., Hirata Y. Coat of alumina sheet with needle-like mullite. J. Ceram. Soc. Jpn. 98:1990;1114-1119.
    • (1990) J. Ceram. Soc. Jpn. , vol.98 , pp. 1114-1119
    • Katsuki, H.1    Hirata, Y.2
  • 7
    • 0034308150 scopus 로고    scopus 로고
    • Multilayer Al2O3/SiC ceramics with improved mechanical behavior
    • She J., Inoue T., Ueno K. Multilayer Al2O3/SiC ceramics with improved mechanical behavior. Ceram. Int. 20:2000;1771-1775.
    • (2000) Ceram. Int. , vol.20 , pp. 1771-1775
    • She, J.1    Inoue, T.2    Ueno, K.3
  • 10
    • 0026944173 scopus 로고
    • The fabrication and failure of laminar ceramic composites
    • Clegg W.J. The fabrication and failure of laminar ceramic composites. Acta Metall. Mater. 40(11):1992;3085-3093.
    • (1992) Acta Metall. Mater. , vol.40 , Issue.11 , pp. 3085-3093
    • Clegg, W.J.1
  • 11
    • 0030126078 scopus 로고    scopus 로고
    • Hertzian contact response of tailored silicon nitride multilayers
    • Liu H., Lawn B.R., Hsu S.M. Hertzian contact response of tailored silicon nitride multilayers. J. Am. Ceram. Soc. 79(4):1996;1009.
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.4 , pp. 1009
    • Liu, H.1    Lawn, B.R.2    Hsu, S.M.3
  • 12
    • 0030242049 scopus 로고    scopus 로고
    • Fracture behavior of multilayer silicon nitride/boron nitride ceramics
    • Liu H., Hsu S.M. Fracture behavior of multilayer silicon nitride/boron nitride ceramics. J. Am. Ceram. Soc. 79(9):1996;2452-2457.
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.9 , pp. 2452-2457
    • Liu, H.1    Hsu, S.M.2
  • 13
    • 0031122607 scopus 로고    scopus 로고
    • Fracture resistance behavior of multilayered silicon nitride
    • Ohji T., Shigegaki Y., Miyajima T. Fracture resistance behavior of multilayered silicon nitride. J. Am. Ceram. Soc. 80(4):1997;991-994.
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.4 , pp. 991-994
    • Ohji, T.1    Shigegaki, Y.2    Miyajima, T.3
  • 14
    • 0035381709 scopus 로고    scopus 로고
    • Selection of interfacial layer of laminated silicon carbide matrix composites
    • in Chinese
    • Yuan G.J., Luo Y.M., Chen D.M. Selection of interfacial layer of laminated silicon carbide matrix composites. J. Chinese Ceram. Soc. 29(3):2001;226-231 (in Chinese).
    • (2001) J. Chinese Ceram. Soc. , vol.29 , Issue.3 , pp. 226-231
    • Yuan, G.J.1    Luo, Y.M.2    Chen, D.M.3
  • 15
    • 0032467713 scopus 로고    scopus 로고
    • Oxidation resistance of SiC/SiC micro and minicomposites with a highly crystallised Bn interphase
    • Rebillat F., Guette A., Espitalier L. Oxidation resistance of SiC/SiC micro and minicomposites with a highly crystallised Bn interphase. J. Eur. Ceram. Soc. 18:1998;1809-1819.
    • (1998) J. Eur. Ceram. Soc. , vol.18 , pp. 1809-1819
    • Rebillat, F.1    Guette, A.2    Espitalier, L.3
  • 16
    • 0031234167 scopus 로고    scopus 로고
    • Role of microstructure-strength properties in ceramics: I, effect of crack size on toughness
    • Lee S.K., Wuttiphan S., Fairbanks C.J. Role of microstructure-strength properties in ceramics. I, effect of crack size on toughness J. Am. Ceram. Soc. 80(9):1997;2367-2381.
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.9 , pp. 2367-2381
    • Lee, S.K.1    Wuttiphan, S.2    Fairbanks, C.J.3
  • 17
    • 0025418269 scopus 로고
    • Direct observation and analysis of indentation cracking in glass and ceramics
    • Cook R.F. Direct observation and analysis of indentation cracking in glass and ceramics. J. Am. Ceram. Soc. 73:1990;787-817.
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 787-817
    • Cook, R.F.1
  • 18
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness-direct crack measurements
    • Antis G.T. A critical evaluation of indentation techniques for measuring fracture toughness-direct crack measurements. J. Am. Ceram. Soc. 64(2):1981;533.
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.2 , pp. 533
    • Antis, G.T.1
  • 19
    • 84987306805 scopus 로고
    • A simple method for determining elastic-modulus-to-hardness ratios using Knoop indentation measurements
    • Marshall D.B., Noma T., Evans A.G. A simple method for determining elastic-modulus-to-hardness ratios using Knoop indentation measurements. J. Am. Ceram. Soc. 65(10):1982;175-176.
    • (1982) J. Am. Ceram. Soc. , vol.65 , Issue.10 , pp. 175-176
    • Marshall, D.B.1    Noma, T.2    Evans, A.G.3
  • 20
    • 0022162478 scopus 로고
    • Microstructure-strength properties in ceramics: Effect of crack size on toughness
    • Cook R.F. Microstructure-strength properties in ceramics. effect of crack size on toughness J. Am. Ceram. Soc. 68(11):1985;604-615.
    • (1985) J. Am. Ceram. Soc. , vol.68 , Issue.11 , pp. 604-615
    • Cook, R.F.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.