3
-
-
0027627834
-
Interface characterization by TEM, AES and SIMS in tough SiC (ex-PCS) fibre-SiC (CVI) matrix composites with a BN interphase
-
Dugne O. Prouhet S. Guette A. Naslain R. Fourmeaux R. Khin Y. Sevely J. Rocher J.P. Cotteret J. Interface characterization by TEM, AES and SIMS in tough SiC (ex-PCS) fibre-SiC (CVI) matrix composites with a BN interphase J. Mater. Sci. 28 1993 3409-3422.
-
(1993)
J. Mater. Sci.
, vol.28
, pp. 3409-3422
-
-
Dugne, O.1
Prouhet, S.2
Guette, A.3
Naslain, R.4
Fourmeaux, R.5
Khin, Y.6
Sevely, J.7
Rocher, J.P.8
Cotteret, J.9
-
5
-
-
0029227342
-
Oxidative and hydrolitic stability of boron nitride. A new approach to improving the oxidation resistance of carbonaceous structures
-
Cofer C.G. Economy J. Oxidative and hydrolitic stability of boron nitride. A new approach to improving the oxidation resistance of carbonaceous structures Carbon 33 4 1995 389-395.
-
(1995)
Carbon
, vol.33
, Issue.4
, pp. 389-395
-
-
Cofer, C.G.1
Economy, J.2
-
6
-
-
0032663646
-
Chemical and mechanical alterations of SiC Nicalon fiber properties during CVD/CVI process of boron nitride
-
Rebillat F. Guette A. Robin-Brosse C. Chemical and mechanical alterations of SiC Nicalon fiber properties during CVD/CVI process of boron nitride Acta. Mater. 47 5 1999 1685-1696.
-
(1999)
Acta. Mater.
, vol.47
, Issue.5
, pp. 1685-1696
-
-
Rebillat, F.1
Guette, A.2
Robin-Brosse, C.3
-
7
-
-
0012058575
-
Chemical and mechanical degradation of Hi-Nicalon and Hi-Nicalon S fibers under CVD/CVI BN processing condition
-
Rebillat F. Guette A. Espitalier L. Naslain R. Chemical and mechanical degradation of Hi-Nicalon and Hi-Nicalon S fibers under CVD/CVI BN processing condition Key Eng. Mater. 164-165 1999 31-34.
-
(1999)
Key Eng. Mater.
, vol.164-165
, pp. 31-34
-
-
Rebillat, F.1
Guette, A.2
Espitalier, L.3
Naslain, R.4
-
11
-
-
0024700593
-
Stability to moisture for chemically vapour-deposited boron nitride
-
Matsuda T. Stability to moisture for chemically vapour-deposited boron nitride J. Mater. Sci. 24 1989 2353-2358.
-
(1989)
J. Mater. Sci.
, vol.24
, pp. 2353-2358
-
-
Matsuda, T.1
-
13
-
-
0000343773
-
Preparation and properties of thin film boron nitride
-
Rand M.J. Roberts J.F. Preparation and properties of thin film boron nitride J. Electrochem. Soc. 115 4 1968 423-429.
-
(1968)
J. Electrochem. Soc.
, vol.115
, Issue.4
, pp. 423-429
-
-
Rand, M.J.1
Roberts, J.F.2
-
14
-
-
0012094391
-
Influence of isothermal chemical vapor deposition and chemical vapor infiltration conditions on the deposition kinetics and structure of boron nitride
-
Leparoux M. Vandenbulcke L. Clinard C. Influence of isothermal chemical vapor deposition and chemical vapor infiltration conditions on the deposition kinetics and structure of boron nitride J. Am. Ceram. Soc. 82 5 1999 1187-1195.
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, Issue.5
, pp. 1187-1195
-
-
Leparoux, M.1
Vandenbulcke, L.2
Clinard, C.3
-
15
-
-
0242377524
-
Turbostratic boron nitride, thermal transformation to ordered-layer-lattice boron nitride
-
Thomas J. Weston N.E. O'Connor T.E. Turbostratic boron nitride, thermal transformation to ordered-layer-lattice boron nitride J. Am. Chem. Soc. 84 24 1963 4619-4622.
-
(1963)
J. Am. Chem. Soc.
, vol.84
, Issue.24
, pp. 4619-4622
-
-
Thomas, J.1
Weston, N.E.2
O'Connor, T.E.3
-
16
-
-
33746621208
-
Light Scattering of boron nitride microcrystals
-
Nemanich R.J. Solin S.A. Martin R.M. Light Scattering of boron nitride microcrystals Phys. Rev. 23 1 1981 6348-6356.
-
(1981)
Phys. Rev.
, vol.23
, Issue.1
, pp. 6348-6356
-
-
Nemanich, R.J.1
Solin, S.A.2
Martin, R.M.3
-
17
-
-
0027682039
-
3 and hBN crystallinity on cBN synthesis
-
3 and hBN crystallinity on cBN synthesis J. Am. Ceram. Soc. 76 10 1993 2525-2528.
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, Issue.10
, pp. 2525-2528
-
-
Choi, Y.1
Kang, S.2
-
18
-
-
85031065354
-
Oxidation resistance of CVD BN coatings: Correlation with processing conditions and with precursor gas systems
-
Beijing, 25-29 June CR-ROM ed. Y. Zhang. ID1373, ISBN 7-900075-46-1
-
Le Gallet, S., Rebillat, F., Guette, A. and Naslain, R., Oxidation resistance of CVD BN coatings: correlation with processing conditions and with precursor gas systems. In: Proceedings of the 13th International Conference on Composite Materials, Beijing, 25-29 June 2001, CR-ROM ed. Y. Zhang. ID1373, ISBN 7-900075-46-1.
-
(2001)
Proceedings of the 13th International Conference on Composite Materials
-
-
Le Gallet, S.1
Rebillat, F.2
Guette, A.3
Naslain, R.4
-
20
-
-
0008627857
-
Investigation of the BN films prepared by low pressure chemical vapor deposition
-
Huang J. Pan C. Lii D. Investigation of the BN films prepared by low pressure chemical vapor deposition Surface and Coatings Technology 122 1999 166-175.
-
(1999)
Surface and Coatings Technology
, vol.122
, pp. 166-175
-
-
Huang, J.1
Pan, C.2
Lii, D.3
-
21
-
-
0023965374
-
Density and deposition rate of chemical vapour deposited boron nitride
-
Matsuda T. Nakae H. Hirai T. Density and deposition rate of chemical vapour deposited boron nitride J. Mater. Sci. 23 1988 509-514.
-
(1988)
J. Mater. Sci.
, vol.23
, pp. 509-514
-
-
Matsuda, T.1
Nakae, H.2
Hirai, T.3
-
22
-
-
0000076009
-
3-Ar: 1. influence of temperature and total pressure on the kinetic control by mass transfer or chemical reactions
-
and Prouhet, S., Vignoles, G., Langlais, F., Guette, A. and Naslain, R., 2. Influence of the precursor composition and chemical mechanisms, ibid. 971-989
-
3-Ar: 1. influence of temperature and total pressure on the kinetic control by mass transfer or chemical reactions. Eur. J. Solid State Inorg. Chem., 1993, 30, 953-969 and Prouhet, S., Vignoles, G., Langlais, F., Guette, A. and Naslain, R., 2. Influence of the precursor composition and chemical mechanisms, ibid. 971-989.
-
(1993)
Eur. J. Solid State Inorg. Chem.
, vol.30
, pp. 953-969
-
-
Prouhet, S.1
Langlais, F.2
Guette, A.3
Naslain, R.4
Rey, J.5
-
23
-
-
0141572670
-
CVD mechanism of pyrolytic boron nitride
-
Pennington, ed. G.W. Cullen (The Electrochem. Soc.)
-
Tanji, H., Monden, K. and Ide, M., CVD mechanism of pyrolytic boron nitride. In: Proceedings of the 10th International Conference on CVD, Pennington, 1987, ed. G.W. Cullen (The Electrochem. Soc.). pp. 562-569.
-
(1987)
Proceedings of the 10th International Conference on CVD
, pp. 562-569
-
-
Tanji, H.1
Monden, K.2
Ide, M.3
|