1
-
-
0024613751
-
The role of the fiber-matrix interface in ceramic composites
-
R. J. Kerans, R. S. Hay, N. J. Pagano, and T. A. Parthasarathy, "The Role of the Fiber-Matrix Interface in Ceramic Composites," Am. Ceram. Soc. Bull., 68 [2] 429-42 (1989).
-
(1989)
Am. Ceram. Soc. Bull.
, vol.68
, Issue.2
, pp. 429-442
-
-
Kerans, R.J.1
Hay, R.S.2
Pagano, N.J.3
Parthasarathy, T.A.4
-
2
-
-
0028484874
-
Review: The physics and mechanics of fibre-reinforced brittle-matrix composites
-
A. G. Evans and F. W. Zok, "Review: The Physics and Mechanics of Fibre-Reinforced Brittle-Matrix Composites," J. Mater. Sci., 29, 3857-96 (1994).
-
(1994)
J. Mater. Sci.
, vol.29
, pp. 3857-3896
-
-
Evans, A.G.1
Zok, F.W.2
-
3
-
-
0022128977
-
High-temperature mechanical behavior of fiber-reinforced glass-ceramic-matrix composites
-
T. Mah, M. G. Mendiratta, A. P. Katz, R. Ruh, and K. S. Mazdiyasni, "High-Temperature Mechanical Behavior of Fiber-Reinforced Glass-Ceramic-Matrix Composites," J. Am. Ceram. Soc., 68 [9] C-248-C-251 (1985).
-
(1985)
J. Am. Ceram. Soc.
, vol.68
, Issue.9
-
-
Mah, T.1
Mendiratta, M.G.2
Katz, A.P.3
Ruh, R.4
Mazdiyasni, K.S.5
-
4
-
-
0025448282
-
Effect of interfaces on the properties of fiber-reinforced ceramics
-
H. C. Cao, E. Bischoff, O. Sbaizero, M. Ruhle, A. G. Evans, D. B. Marshall, and J. J. Brennan, "Effect of Interfaces on the Properties of Fiber-Reinforced Ceramics," J. Am. Ceram. Soc., 73 [6] 1691-99 (1990).
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.6
, pp. 1691-1699
-
-
Cao, H.C.1
Bischoff, E.2
Sbaizero, O.3
Ruhle, M.4
Evans, A.G.5
Marshall, D.B.6
Brennan, J.J.7
-
5
-
-
0003187712
-
Interfacial characterization of glass and glass-ceramic matrix/nicalon SiC fiber composites
-
J. J. Brennan, "Interfacial Characterization of Glass and Glass-Ceramic Matrix/Nicalon SiC Fiber Composites," Mater. Sci. Res., 20, 546-60 (1986).
-
(1986)
Mater. Sci. Res.
, vol.20
, pp. 546-560
-
-
Brennan, J.J.1
-
6
-
-
0018985511
-
High-strength silicon carbide-fiber-reinforced glass-matrix composites
-
K. Prewo and J. J. Brennan, "High-Strength Silicon Carbide-Fiber-Reinforced Glass-Matrix Composites," J. Mater. Sci., 15 [2] 463-68 (1980).
-
(1980)
J. Mater. Sci.
, vol.15
, Issue.2
, pp. 463-468
-
-
Prewo, K.1
Brennan, J.J.2
-
7
-
-
0009517614
-
Interfacial chemistry and bonding in fiber-reinforced glass and glass-ceramic-matrix composites
-
Edited by J. A. Pask and A. G. Evans. Plenum, New York
-
J. J. Brennan, "Interfacial Chemistry and Bonding in Fiber-Reinforced Glass and Glass-Ceramic-Matrix Composites"; pp. 387-99 in Ceramic Microstructures '86: Role of Interfaces. Edited by J. A. Pask and A. G. Evans. Plenum, New York, 1986.
-
(1986)
Ceramic Microstructures '86: Role of Interfaces
, pp. 387-399
-
-
Brennan, J.J.1
-
8
-
-
0023414650
-
Structure and chemistry of fiber-matrix interfaces in silicon carbide-fibre-reinforced glass-ceramic composites: An electron microscopy study
-
R. F. Cooper and K. Chyung, "Structure and Chemistry of Fiber-Matrix Interfaces in Silicon Carbide-Fibre-Reinforced Glass-Ceramic Composites: An Electron Microscopy Study," J. Mater. Sci., 22, 3148-60 (1987).
-
(1987)
J. Mater. Sci.
, vol.22
, pp. 3148-3160
-
-
Cooper, R.F.1
Chyung, K.2
-
9
-
-
0001567977
-
Effect of boron nitride coating on fiber-matrix interactions
-
R. N. Singh and M. K. Brun, "Effect of Boron Nitride Coating on Fiber-Matrix Interactions," Ceram. Eng. Sci. Proc., 8 [7-8] 634-43 (1987).
-
(1987)
Ceram. Eng. Sci. Proc.
, vol.8
, Issue.7-8
, pp. 634-643
-
-
Singh, R.N.1
Brun, M.K.2
-
10
-
-
84985161054
-
Boron nitride interphase in ceramic-matrix composites
-
R. Naslain, O. Dugne, A. Guette, J. Sevely, C. R. Brosse, J. P. Rocher, and J. Cotteret, "Boron Nitride Interphase in Ceramic-Matrix Composites," J. Am. Ceram. Soc., 74 [10] 2482-88 (1991).
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.10
, pp. 2482-2488
-
-
Naslain, R.1
Dugne, O.2
Guette, A.3
Sevely, J.4
Brosse, C.R.5
Rocher, J.P.6
Cotteret, J.7
-
11
-
-
0028442172
-
Interfacial microstructure and chemistry of SiC/BN dual-coated nicalon-fiber-reinforced glass-ceramic-matrix composites
-
E. Y. Sun, S. R. Nutt, and J. J. Brennan, "Interfacial Microstructure and Chemistry of SiC/BN Dual-Coated Nicalon-Fiber-Reinforced Glass-Ceramic-Matrix Composites," J. Am. Ceram. Soc., 77 [5] 1329-39 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, Issue.5
, pp. 1329-1339
-
-
Sun, E.Y.1
Nutt, S.R.2
Brennan, J.J.3
-
12
-
-
0024700593
-
Stability to moisture for chemically vapour deposited boron nitride
-
T. Matsuda, "Stability to Moisture for Chemically Vapour Deposited Boron Nitride," J. Mater. Sci., 24, 2353-58 (1989).
-
(1989)
J. Mater. Sci.
, vol.24
, pp. 2353-2358
-
-
Matsuda, T.1
-
13
-
-
33644805769
-
Ceramic bodies of controlled porosity and process for making same
-
U.S. Pat. No. 5 017 522, May 21
-
A. G. Hegedus, "Ceramic Bodies of Controlled Porosity and Process for Making Same," U.S. Pat. No. 5 017 522, May 21, 1991.
-
(1991)
-
-
Hegedus, A.G.1
-
14
-
-
4243492181
-
Fiber-reinforced ceramic composite member
-
U.S. Pat. No. 5 488 017, Jan. 30
-
A. Szweda, M. L. Millard, and M. G. Harrison, "Fiber-Reinforced Ceramic Composite Member," U.S. Pat. No. 5 488 017, Jan. 30, 1996.
-
(1996)
-
-
Szweda, A.1
Millard, M.L.2
Harrison, M.G.3
-
15
-
-
4243775734
-
Fiber-reinforced ceramic-matrix composite member and method for making
-
U.S. Pat. No. 5 601 674, Feb. 11
-
A. Szweda, M. L. Millard, and M. G. Harrison, "Fiber-Reinforced Ceramic-Matrix Composite Member and Method for Making," U.S. Pat. No. 5 601 674, Feb. 11, 1997.
-
(1997)
-
-
Szweda, A.1
Millard, M.L.2
Harrison, M.G.3
-
16
-
-
0038088894
-
Thermal aging effects in oxide/oxide ceramic-matrix composites
-
Edited by J. D. Buckley, NASA, Washington, DC
-
T. J. Dunyak, D. R. Chang, and M. L. Millard, "Thermal Aging Effects in Oxide/Oxide Ceramic-Matrix Composites"; pp. 675-90 in 17th Conference on Metal Matrix, Carbon, and Ceramic Matrix Composites, NASA Conference Publication 3235, Part 2. Edited by J. D. Buckley, NASA, Washington, DC, 1993.
-
(1993)
17th Conference on Metal Matrix, Carbon, and Ceramic Matrix Composites, NASA Conference Publication 3235, Part 2
, pp. 675-690
-
-
Dunyak, T.J.1
Chang, D.R.2
Millard, M.L.3
-
17
-
-
0038765483
-
Mechanical behavior of CMCs for flaps and seals
-
Edited by W. S. Coblenz. ARPA Ceramic Technology Insertion Program (DARPA), Annapolis, MD
-
L. P. Zawada and S. S. Lee, "Mechanical Behavior of CMCs for Flaps and Seals"; pp. 267-322 in Defense Advanced Projects Agency Conference Publication. Edited by W. S. Coblenz. ARPA Ceramic Technology Insertion Program (DARPA), Annapolis, MD, 1994.
-
(1994)
Defense Advanced Projects Agency Conference Publication
, pp. 267-322
-
-
Zawada, L.P.1
Lee, S.S.2
-
18
-
-
0007076230
-
Evaluation of the fatigue performance of five CMCs for aerospace applications
-
Edited by G. Lutjering and H. Nowack. Elsevier Science, Tarrytown, NY
-
L. P. Zawada and S. S. Lee, "Evaluation of the Fatigue Performance of Five CMCs for Aerospace Applications"; pp. 1669-74 in Sixth International Fatigue Congress, Vol. III. Edited by G. Lutjering and H. Nowack. Elsevier Science, Tarrytown, NY, 1996.
-
(1996)
Sixth International Fatigue Congress
, vol.3
, pp. 1669-1674
-
-
Zawada, L.P.1
Lee, S.S.2
-
19
-
-
0029771716
-
Crack branching in all-oxide ceramic composites
-
T. J. Lu, "Crack Branching in All-Oxide Ceramic Composites," J. Am. Ceram. Soc., 79 [1] 266-74 (1996).
-
(1996)
J. Am. Ceram. Soc.
, vol.79
, Issue.1
, pp. 266-274
-
-
Lu, T.J.1
-
20
-
-
0030084731
-
Concept for a damage-tolerant ceramic composite with 'strong' interfaces
-
W.-C. Tu, F. F. Lange, and A. G. Evans, "Concept for a Damage-Tolerant Ceramic Composite with 'Strong' Interfaces," J. Am. Ceram. Soc., 79 [2] 417-24 (1996).
-
(1996)
J. Am. Ceram. Soc.
, vol.79
, Issue.2
, pp. 417-424
-
-
Tu, W.-C.1
Lange, F.F.2
Evans, A.G.3
-
21
-
-
85039670146
-
Oxide-oxide CMCs for engine exhaust systems
-
HAVE FORM, U.S. Ar Force, Fort Walton Beach, FL
-
D. M. Carper and M. L. Millard, "Oxide-Oxide CMCs for Engine Exhaust Systems," HAVE FORM, U.S. Ar Force, Fort Walton Beach, FL, 1997.
-
(1997)
-
-
Carper, D.M.1
Millard, M.L.2
-
22
-
-
0035530960
-
Mechanical properties of porous-matrix ceramic composites
-
F. W. Zok and C. G. Levi, "Mechanical Properties of Porous-Matrix Ceramic Composites," Adv. Eng. Mater., 3 [1-2] 15-23 (2001).
-
(2001)
Adv. Eng. Mater.
, vol.3
, Issue.1-2
, pp. 15-23
-
-
Zok, F.W.1
Levi, C.G.2
-
23
-
-
0030244427
-
Preparation of thin sections of coated fibers for characterization by transmission electron microscopy
-
M. K. Cinibulk, J. R. Welch, and R. S. Hay, "Preparation of Thin Sections of Coated Fibers for Characterization by Transmission Electron Microscopy," J. Am. Ceram. Soc., 79 [9] 2481-84 (1996).
-
(1996)
J. Am. Ceram. Soc.
, vol.79
, Issue.9
, pp. 2481-2484
-
-
Cinibulk, M.K.1
Welch, J.R.2
Hay, R.S.3
-
24
-
-
0025509459
-
A fracture mechanics test automation system for a basic research laboratory
-
G. A. Hartman and N. E. Ashbaugh, "A Fracture Mechanics Test Automation System for a Basic Research Laboratory," ASTM, STP STP 1092, 95-110 (1990).
-
(1990)
ASTM, STP
, vol.1092
, pp. 95-110
-
-
Hartman, G.A.1
Ashbaugh, N.E.2
-
25
-
-
0026626917
-
Fatigue test methodology and results for ceramic-matrix composites at room and elevated temperatures
-
L. M. Butkus, L. P. Zawada, and G. A. Hartman, "Fatigue Test Methodology and Results for Ceramic-Matrix Composites at Room and Elevated Temperatures," ASTM, STP STP 1157, 52-68 (1990).
-
(1990)
ASTM, STP
, vol.1157
, pp. 52-68
-
-
Butkus, L.M.1
Zawada, L.P.2
Hartman, G.A.3
-
26
-
-
0027677610
-
Crack growth and damage in constrained sintering films
-
R. K. Bordia and A. Jagota, "Crack Growth and Damage in Constrained Sintering Films," J. Am. Ceram. Soc., 76 [10] 2475-85 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, Issue.10
, pp. 2475-2485
-
-
Bordia, R.K.1
Jagota, A.2
-
27
-
-
0024704051
-
Observations and analysis of sintering damage
-
C. P. Ostertag, P. G. Charalambrides, and A. G. Evans, "Observations and Analysis of Sintering Damage," Acta Metall., 37 [7] 2077-84 (1989).
-
(1989)
Acta Metall.
, vol.37
, Issue.7
, pp. 2077-2084
-
-
Ostertag, C.P.1
Charalambrides, P.G.2
Evans, A.G.3
-
29
-
-
0028478715
-
Microstructural observations on constrained densification of alumina powder containing a periodic array of sapphire fibers
-
D. C. C. Lam and F. F. Lange, "Microstructural Observations on Constrained Densification of Alumina Powder Containing a Periodic Array of Sapphire Fibers," J. Am. Ceram. Soc., 77 [7] 1976-78 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, Issue.7
, pp. 1976-1978
-
-
Lam, D.C.C.1
Lange, F.F.2
-
30
-
-
0023435572
-
Sintering with rigid inclusions
-
G. W. Scherer, "Sintering with Rigid Inclusions," J. Am. Ceram. Soc., 70 [10] 719-25 (1987).
-
(1987)
J. Am. Ceram. Soc.
, vol.70
, Issue.10
, pp. 719-725
-
-
Scherer, G.W.1
-
31
-
-
79958282441
-
Formation of mullite from sol-gel mixtures and kaolinite
-
J. A. Pask and A. P. Tomsia, "Formation of Mullite from Sol-Gel Mixtures and Kaolinite," J. Am. Ceram. Soc., 74 [10] 2367-73 (1991).
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.10
, pp. 2367-2373
-
-
Pask, J.A.1
Tomsia, A.P.2
-
32
-
-
0000741620
-
Mullite formation from nonstoichiometric diphasic precursors
-
D. X. Li and W. J. Thomson, "Mullite Formation from Nonstoichiometric Diphasic Precursors," J. Am. Ceram. Soc., 74 [10] 2382-87 (1991).
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.10
, pp. 2382-2387
-
-
Li, D.X.1
Thomson, W.J.2
-
33
-
-
0021523156
-
Viscous sintering of a bimodal pore-size distribution
-
G. W. Scherer, "Viscous Sintering of a Bimodal Pore-Size Distribution," J. Am. Ceram. Soc., 67 [11] 709-15 (1984).
-
(1984)
J. Am. Ceram. Soc.
, vol.67
, Issue.11
, pp. 709-715
-
-
Scherer, G.W.1
-
34
-
-
84986384837
-
Viscous sintering with a pore-size distribution and rigid inclusions
-
G. W. Scherer, "Viscous Sintering with a Pore-Size Distribution and Rigid Inclusions," J. Am. Ceram. Soc., 71 [10] C-447-C-448 (1988).
-
(1988)
J. Am. Ceram. Soc.
, vol.71
, Issue.10
-
-
Scherer, G.W.1
-
35
-
-
0031696788
-
Coarsening in a viscous matrix
-
G. W. Scherer, "Coarsening in a Viscous Matrix," J. Am. Ceram. Soc., 81 [1] 49-54 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, Issue.1
, pp. 49-54
-
-
Scherer, G.W.1
-
36
-
-
0002940727
-
Effect of atmosphere on surface tension of glass
-
N. M. Parikh, "Effect of Atmosphere on Surface Tension of Glass," J. Am. Ceram. Soc., 41 [1] 18-22 (1958).
-
(1958)
J. Am. Ceram. Soc.
, vol.41
, Issue.1
, pp. 18-22
-
-
Parikh, N.M.1
-
37
-
-
0000138840
-
Viscosity of vitreous silica
-
G. Hetherington, K. H. Jack, and J. C. Kennedy, "Viscosity of Vitreous Silica," Phys. Chem. Glasses, 5 [5] 130-36 (1964).
-
(1964)
Phys. Chem. Glasses
, vol.5
, Issue.5
, pp. 130-136
-
-
Hetherington, G.1
Jack, K.H.2
Kennedy, J.C.3
-
38
-
-
85061368529
-
"Theory of solid-state and viscous sintering" Ch. 8
-
Marcel-Dekker, New York
-
M. N. Rahaman, "Theory of Solid-State and Viscous Sintering"; Ch. 8, pp. 374-444 in Ceramic Processing and Sintering, 1st ed. Marcel-Dekker, New York, 1995.
-
(1995)
Ceramic Processing and Sintering, 1st Ed.
, pp. 374-444
-
-
Rahaman, M.N.1
-
39
-
-
0001826050
-
Single and multiple fracture
-
Edited by J. C. Aveston, C. G. Cooper, and C. G. Cooper, and A. Kelly, IPC Science and Technology Press, Guildford, U.K.
-
J. C. Aveston, C. G. Cooper, and A. Kelly, "Single and Multiple Fracture"; pp. 15-26 in Properties of Fiber Composites, Proceedings of National Physics Laboratory Conference. Edited by J. C. Aveston, C. G. Cooper, and C. G. Cooper, and A. Kelly, IPC Science and Technology Press, Guildford, U.K., 1971.
-
(1971)
Properties of Fiber Composites, Proceedings of National Physics Laboratory Conference
, pp. 15-26
-
-
Aveston, J.C.1
Cooper, C.G.2
Kelly, A.3
-
40
-
-
0028479093
-
Microstructure and properties of nextel™ 610 fiber reinforced ceramic and metal matrix composites
-
A. S. Fareed and G. H. Schiroky, "Microstructure and Properties of Nextel™ 610 Fiber Reinforced Ceramic and Metal Matrix Composites," Ceram. Eng. Sci. Proc., 15 [4] 344-52 (1994).
-
(1994)
Ceram. Eng. Sci. Proc.
, vol.15
, Issue.4
, pp. 344-352
-
-
Fareed, A.S.1
Schiroky, G.H.2
-
41
-
-
0033204919
-
In-plane mechanical properties of an all-oxide ceramic composite
-
J. A. Heathcote, X.-Y. Gong, J. Y. Yang, U. Ramamurty, and F. W. Zok, "In-Plane Mechanical Properties of an All-Oxide Ceramic Composite," J. Am. Ceram. Soc., 82 [10] 2721-30 (1999).
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, Issue.10
, pp. 2721-2730
-
-
Heathcote, J.A.1
Gong, X.-Y.2
Yang, J.Y.3
Ramamurty, U.4
Zok, F.W.5
-
42
-
-
0031461008
-
Shear strength of continuous-fiber ceramic composites
-
E. Lara-Curzio and M. K. Ferber, "Shear Strength of Continuous-Fiber Ceramic Composites," Thermal and Mechanical Test Methods and Behavior of Continuous Fiber Ceramic Composites, ASTM, STP 1309, 31-48 (1997).
-
(1997)
Thermal and Mechanical Test Methods and Behavior of Continuous Fiber Ceramic Composites, ASTM, STP
, vol.1309
, pp. 31-48
-
-
Lara-Curzio, E.1
Ferber, M.K.2
-
43
-
-
0029273402
-
Fatigue of ceramic-matrix composites
-
A. G. Evans, F. W. Zok and R. M. McMeeking, "Fatigue of Ceramic-Matrix Composites," Acta Metall. Mater., 43 [3] 859-75 (1995).
-
(1995)
Acta Metall. Mater.
, vol.43
, Issue.3
, pp. 859-875
-
-
Evans, A.G.1
Zok, F.W.2
McMeeking, R.M.3
-
44
-
-
84985080200
-
Experimental observations of frictional heating in a fiber-reinforced ceramic
-
J. W. Holmes and C. Cho, "Experimental Observations of Frictional Heating in a Fiber-Reinforced Ceramic," J. Am. Ceram. Soc., 75 [4] 928-38 (1992).
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, Issue.4
, pp. 928-938
-
-
Holmes, J.W.1
Cho, C.2
-
45
-
-
4243779500
-
Monotonic and fatigue loading behavior of an oxide/oxide ceramic-matrix composite
-
M.A. Thesis, Air Force Institute of Technology, Wright-Patterson Air Force Base, OH
-
S. G. Steel, "Monotonic and Fatigue Loading Behavior of an Oxide/Oxide Ceramic-Matrix Composite"; M.A. Thesis, Air Force Institute of Technology, Wright-Patterson Air Force Base, OH, 2000.
-
(2000)
-
-
Steel, S.G.1
-
46
-
-
0001682670
-
Elevated temperature creep behavior of continuous-fiber-reinforced ceramics
-
Edited by S. V. Nair and K. Jakus, Butterworth-Hienneman, Kent, U.K.
-
J. W. Holmes and X. Wu, "Elevated Temperature Creep Behavior of Continuous-Fiber-Reinforced Ceramics"; pp. 193-260 in Elevated Temperature Creep Behavior of Continuous Fiber-Reinforced Ceramics. Edited by S. V. Nair and K. Jakus, Butterworth-Hienneman, Kent, U.K., 1995.
-
(1995)
Elevated Temperature Creep Behavior of Continuous Fiber-Reinforced Ceramics
, pp. 193-260
-
-
Holmes, J.W.1
Wu, X.2
-
47
-
-
0027694319
-
High-temperature creep and the interfacial mechanical response of a ceramic-matrix composite
-
D. W. Meyer, R. F. Cooper, and M. E. Plesha, "High-Temperature Creep and the Interfacial Mechanical Response of a Ceramic-Matrix Composite," Acta Metall. Mater., 41 [11] 3157-70 (1993).
-
(1993)
Acta Metall. Mater.
, vol.41
, Issue.11
, pp. 3157-3170
-
-
Meyer, D.W.1
Cooper, R.F.2
Plesha, M.E.3
-
48
-
-
0026801696
-
Creep rupture studies of two alumina-based ceramic fibers
-
D. J. Pysher and R. E. Tressler, "Creep Rupture Studies of Two Alumina-Based Ceramic Fibers," J. Mater. Sci., 27, 423-28 (1992).
-
(1992)
J. Mater. Sci.
, vol.27
, pp. 423-428
-
-
Pysher, D.J.1
Tressler, R.E.2
-
49
-
-
0008404443
-
Tensile creep rupture behavior of alumina-based polycrystalline oxide fibers
-
D. J. Pysher and R. E. Tressler, "Tensile Creep Rupture Behavior of Alumina-Based Polycrystalline Oxide Fibers," Ceram. Eng. Sci. Proc., 13 [7-8] 218-26 (1992).
-
(1992)
Ceram. Eng. Sci. Proc.
, vol.13
, Issue.7-8
, pp. 218-226
-
-
Pysher, D.J.1
Tressler, R.E.2
-
50
-
-
0027632588
-
High-temperature properties of nextel 610 and alumina-based nanocomposite fibers
-
D. M. Wilson, D. C. Lunenburg, and S. L. Lieder, "High-Temperature Properties of Nextel 610 and Alumina-Based Nanocomposite Fibers," Ceram. Eng. Sci. Proc., 14 [7-78] 609-21 (1993).
-
(1993)
Ceram. Eng. Sci. Proc.
, vol.14
, Issue.7-8
, pp. 609-621
-
-
Wilson, D.M.1
Lunenburg, D.C.2
Lieder, S.L.3
-
51
-
-
0033672704
-
Creep deformation and rupture behavior of a notched oxide/oxide nextel 720/AS composite
-
R. John, D. J. Buchanan, and L. P. Zawada, "Creep Deformation and Rupture Behavior of a Notched Oxide/Oxide Nextel 720/AS Composite," Ceram. Eng. Sci. Proc., 21 [3] 567-73 (2000).
-
(2000)
Ceram. Eng. Sci. Proc.
, vol.21
, Issue.3
, pp. 567-573
-
-
John, R.1
Buchanan, D.J.2
Zawada, L.P.3
-
52
-
-
0039783509
-
Notch-sensitivity of a woven oxide/oxide ceramic-matrix composite
-
R. John, D. J. Buchanan, and L. P. Zawada, "Notch-Sensitivity of a Woven Oxide/Oxide Ceramic-Matrix Composite," Mechanical, Thermal, and Environmental Testing and Performance of Ceramic Composites and Components, ASTM, STP 1392, 160-71 (2000).
-
(2000)
Mechanical, Thermal, and Environmental Testing and Performance of Ceramic Composites and Components, ASTM, STP
, vol.1392
, pp. 160-171
-
-
John, R.1
Buchanan, D.J.2
Zawada, L.P.3
-
53
-
-
0039782479
-
Damage accumulation in 2-D woven SiC/SiC ceramic-matrix composites
-
G. N. Morscher, J. Z. Gyekenyesi, and R. T. Bhatt, "Damage Accumulation in 2-D Woven SiC/SiC Ceramic-Matrix Composites," Mechanical, Thermal, and Environmental Testing and Performance of Ceramic Composites and Components, ASTM, STP 1392, 306-19 (2000).
-
(2000)
Mechanical, Thermal, and Environmental Testing and Performance of Ceramic Composites and Components, ASTM, STP
, vol.1392
, pp. 306-319
-
-
Morscher, G.N.1
Gyekenyesi, J.Z.2
Bhatt, R.T.3
-
54
-
-
0032117635
-
Mechanical behavior and high-temperature performance of a woven nicalon™/SiNC ceramic-matrix composite
-
S. S. Lee, L. P. Zawada, J. M. Staehler, and C. A. Folsom, "Mechanical Behavior and High-Temperature Performance of a Woven Nicalon™/SiNC Ceramic-Matrix Composite," J. Am. Ceram. Soc., 81 [7] 1797-11 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, Issue.7
, pp. 1797-1711
-
-
Lee, S.S.1
Zawada, L.P.2
Staehler, J.M.3
Folsom, C.A.4
-
55
-
-
0034226676
-
Performance of four ceramic-matrix composite divergent flap inserts following ground testing on an F110 turbofan engine
-
J. M. Staehler and L. P. Zawada, "Performance of Four Ceramic-Matrix Composite Divergent Flap Inserts Following Ground Testing on an F110 Turbofan Engine," J. Am. Ceram. Soc., 83 [7] 1727-1738 (2000).
-
(2000)
J. Am. Ceram. Soc.
, vol.83
, Issue.7
, pp. 1727-1738
-
-
Staehler, J.M.1
Zawada, L.P.2
-
56
-
-
0032316030
-
Longitudinal and transthickness tensile behavior of several oxide/oxide composites
-
L. P. Zawada, "Longitudinal and Transthickness Tensile Behavior of Several Oxide/Oxide Composites," Ceram. Eng. Sci. Proc., 19 [3] 327-39 (1998).
-
(1998)
Ceram. Eng. Sci. Proc.
, vol.19
, Issue.3
, pp. 327-339
-
-
Zawada, L.P.1
-
57
-
-
0033189440
-
Continuous coating of oxide fiber tows using liquid precursors: Monazite coatings on nextel 720
-
E. Boakye, R. S. Hay, and M. D. Petry, "Continuous Coating of Oxide Fiber Tows Using Liquid Precursors: Monazite Coatings on Nextel 720," J. Am. Ceram. Soc., 82 [9] 2321-31 (1999).
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, Issue.9
, pp. 2321-2331
-
-
Boakye, E.1
Hay, R.S.2
Petry, M.D.3
-
58
-
-
0034005073
-
Effect of coating deposition temperature on monazite coated fiber
-
R. S. Hay, E. E. Boakye, and M. D. Petry, "Effect of Coating Deposition Temperature on Monazite Coated Fiber," J. Eur. Ceram. Soc., 20, 589-97 (2000).
-
(2000)
J. Eur. Ceram. Soc.
, vol.20
, pp. 589-597
-
-
Hay, R.S.1
Boakye, E.E.2
Petry, M.D.3
-
59
-
-
0041639510
-
Monazite coatings on fibers: II, coating without strength degradation
-
E. E. Boakye, R. S. Hay, P. Mogilesky, and L. M. Douglas, "Monazite Coatings on Fibers: II, Coating without Strength Degradation," J. Am. Ceram. Soc., 84 [12] 2793-801 (2001).
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.12
, pp. 2793-2801
-
-
Boakye, E.E.1
Hay, R.S.2
Mogilesky, P.3
Douglas, L.M.4
-
60
-
-
0033225105
-
Notched fracture behavior of an oxide/oxide ceramic-matrix composite
-
V. A. Kramb, R. John, and L. P. Zawada, "Notched Fracture Behavior of an Oxide/Oxide Ceramic-Matrix Composite," J. Am. Ceram. Soc., 82 [11] 3087-96 (1999).
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, Issue.11
, pp. 3087-3096
-
-
Kramb, V.A.1
John, R.2
Zawada, L.P.3
-
61
-
-
0035427193
-
High-performance oxide fibers for metal and ceramic composites
-
D. M. Wilson and L. R. Visser, "High-Performance Oxide Fibers for Metal and Ceramic Composites," Composites, Part A, 32, 1143-53 (2001).
-
(2001)
Composites, Part A
, vol.32
, pp. 1143-1153
-
-
Wilson, D.M.1
Visser, L.R.2
-
62
-
-
0027696843
-
Effect of high-temperature exposure on the tensile strength of alumina fiber nextel 610
-
Z. R. Xu, K. K. Chawla, and X. Li, "Effect of High-Temperature Exposure on the Tensile Strength of Alumina Fiber Nextel 610," Mater. Sci. Eng. A, 171, 249-56 (1993).
-
(1993)
Mater. Sci. Eng. A
, vol.171
, pp. 249-256
-
-
Xu, Z.R.1
Chawla, K.K.2
Li, X.3
-
63
-
-
0032139153
-
Processing and performance of an all-oxide ceramic composite
-
C. G. Levi, J. Y. Yang, B. J. Dalgleish, F. W. Zok, and A. G. Evans, "Processing and Performance of an All-Oxide Ceramic Composite," J. Am. Ceram. Soc., 81 [8] 2077-86 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, Issue.8
, pp. 2077-2086
-
-
Levi, C.G.1
Yang, J.Y.2
Dalgleish, B.J.3
Zok, F.W.4
Evans, A.G.5
|