1
-
-
0002379975
-
Ceramics in clinical applications, past, present and future
-
Vincenzinc P (ed). Amsterdam: Elsevier Science
-
Hulbert SF, Bokros JC, Hench LL, Wilson J, Heimke G. Ceramics in clinical applications, past, present and future. In: Vincenzinc P (ed). High Tech Ceramics. Amsterdam: Elsevier Science, 1987:3-27.
-
(1987)
High Tech Ceramics
, pp. 3-27
-
-
Hulbert, S.F.1
Bokros, J.C.2
Hench, L.L.3
Wilson, J.4
Heimke, G.5
-
2
-
-
0039274148
-
All ceramic bridges with the slip casting technique
-
Paris, September
-
Sadoun M. All ceramic bridges with the slip casting technique. Presented at the 7th International Symposium on Ceramics, Paris, September, 1988.
-
(1988)
7th International Symposium on Ceramics
-
-
Sadoun, M.1
-
3
-
-
0027546239
-
A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain
-
Andersson M, Oden A. A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain. Acta Odontol Scand 1993;51:59-64.
-
(1993)
Acta Odontol Scand
, vol.51
, pp. 59-64
-
-
Andersson, M.1
Oden, A.2
-
4
-
-
0026148632
-
Porcelain-composite interface microleakage with various porcelain surface treatments
-
Sorensen JA, Kang SK, Avera SP. Porcelain-composite interface microleakage with various porcelain surface treatments. Dent Mater 1991;7:118-123.
-
(1991)
Dent Mater
, vol.7
, pp. 118-123
-
-
Sorensen, J.A.1
Kang, S.K.2
Avera, S.P.3
-
5
-
-
0024676323
-
Etched porcelain resin-bonded full veneer crowns: In vitro fracture resistance
-
Jensen ME, Sheth JJ, Tolliver D. Etched porcelain resin-bonded full veneer crowns: In vitro fracture resistance. Comp Cont Ed Dent 1989;10:336-346.
-
(1989)
Comp Cont Ed Dent
, vol.10
, pp. 336-346
-
-
Jensen, M.E.1
Sheth, J.J.2
Tolliver, D.3
-
6
-
-
0141585469
-
Dicor crown strength improvement due to bonding
-
Eden GT, Kaztez JM. Dicor crown strength improvement due to bonding. J Dent Res 1987;66:207-211.
-
(1987)
J Dent Res
, vol.66
, pp. 207-211
-
-
Eden, G.T.1
Kaztez, J.M.2
-
8
-
-
0029299001
-
Adhesion of composite to porcelain with various surface conditions
-
Aida M, Hayakawa T, Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent 1995;73:464-470.
-
(1995)
J Prosthet Dent
, vol.73
, pp. 464-470
-
-
Aida, M.1
Hayakawa, T.2
Mizukawa, K.3
-
9
-
-
0028441251
-
Bonding of resin cements to an aluminous ceramic: A new surface treatment
-
Sadoun M, Asmussen E. Bonding of resin cements to an aluminous ceramic: A new surface treatment. Dent Mater 1994;10:185-189.
-
(1994)
Dent Mater
, vol.10
, pp. 185-189
-
-
Sadoun, M.1
Asmussen, E.2
-
10
-
-
0026253546
-
Tensile strength of the bond to In-Ceram after varying modes of surface conditioning
-
Kern M, Neikes MJ, Strub JR. Tensile strength of the bond to In-Ceram after varying modes of surface conditioning. Dtsch Zahnarztl Z 1991;46:758-761.
-
(1991)
Dtsch Zahnarztl Z
, vol.46
, pp. 758-761
-
-
Kern, M.1
Neikes, M.J.2
Strub, J.R.3
-
11
-
-
0026194688
-
Bond strength of etched In-Ceram to tooth enamel
-
Pape FW, Pfeiffer P, Marx R. Bond strength of etched In-Ceram to tooth enamel. Zahnärztl Welt 1991;100:450-453.
-
(1991)
Zahnärztl Welt
, vol.100
, pp. 450-453
-
-
Pape, F.W.1
Pfeiffer, P.2
Marx, R.3
-
12
-
-
0141697178
-
Bond strength of resin cement to In-Ceram core material
-
Kraivixien R, Pietrobon N, Nathanson D. Bond strength of resin cement to In-Ceram core material. J Dent Res 1992;71:533-537.
-
(1992)
J Dent Res
, vol.71
, pp. 533-537
-
-
Kraivixien, R.1
Pietrobon, N.2
Nathanson, D.3
-
13
-
-
0028435067
-
Sandblasting and silica coating of glass-infiltrated alumina ceramic: Volume loss, morphology, and changes in the surface composition
-
Kern M, Thompson VP. Sandblasting and silica coating of glass-infiltrated alumina ceramic: Volume loss, morphology, and changes in the surface composition. J Prosthet Dent 1994;71:453-461.
-
(1994)
J Prosthet Dent
, vol.71
, pp. 453-461
-
-
Kern, M.1
Thompson, V.P.2
-
14
-
-
0029266741
-
Bonding to glass infiltrated alumina ceramic: Adhesive methods and their durability
-
Kern M, Thompson VP. Bonding to glass infiltrated alumina ceramic: Adhesive methods and their durability. J Prosthet Dent 1995;73:240-249.
-
(1995)
J Prosthet Dent
, vol.73
, pp. 240-249
-
-
Kern, M.1
Thompson, V.P.2
-
15
-
-
0034202903
-
Effects of surface treatments on shear bond strengths between a resin cement and an alumina core
-
Madani M, Chu FCS, McDonald AV, Smales RJ. Effects of surface treatments on shear bond strengths between a resin cement and an alumina core. J Prosthet Dent 2000;83:644-647.
-
(2000)
J Prosthet Dent
, vol.83
, pp. 644-647
-
-
Madani, M.1
Chu, F.C.S.2
McDonald, A.V.3
Smales, R.J.4
-
16
-
-
0031991726
-
Shear bond strength of a resin cement to densely sintered high-purity alumina with various surface conditions
-
Awliya W, Oden A, Yaman P, Dennison J, Razzoog M. Shear bond strength of a resin cement to densely sintered high-purity alumina with various surface conditions. Acta Odontol Scand 1998;56:9-13.
-
(1998)
Acta Odontol Scand
, vol.56
, pp. 9-13
-
-
Awliya, W.1
Oden, A.2
Yaman, P.3
Dennison, J.4
Razzoog, M.5
-
17
-
-
0034189689
-
Bonding to densely sintered alumina surfaces: Effect of sandblasting and silica coating on shear bond strength of luting cements
-
Blixt M, Adamczak E, Linden L-A, Oden A, Arvidson K. Bonding to densely sintered alumina surfaces: Effect of sandblasting and silica coating on shear bond strength of luting cements. Int J Prosthodont 2000;13:221-226.
-
(2000)
Int J Prosthodont
, vol.13
, pp. 221-226
-
-
Blixt, M.1
Adamczak, E.2
Linden, L.-A.3
Oden, A.4
Arvidson, K.5
-
18
-
-
0020839571
-
Porcelain laminate veneers bonded to etched enamel
-
Horn HR. Porcelain laminate veneers bonded to etched enamel. Dent Clin North Am 1983;27:671-675.
-
(1983)
Dent Clin North Am
, vol.27
, pp. 671-675
-
-
Horn, H.R.1
-
19
-
-
0024616164
-
Porcelain-to-composite bond strengths using four organosilane materials
-
Bailey JH. Porcelain-to-composite bond strengths using four organosilane materials. J Prosthet Dent 1989;61:174-177.
-
(1989)
J Prosthet Dent
, vol.61
, pp. 174-177
-
-
Bailey, J.H.1
-
20
-
-
0032171898
-
Effect of etchant, etching period, and silane priming on bond strength to porcelain of composite resin
-
Chen JH, Matsumura H, Atsuta M. Effect of etchant, etching period, and silane priming on bond strength to porcelain of composite resin. Oper Dent 1998;23:250-257.
-
(1998)
Oper Dent
, vol.23
, pp. 250-257
-
-
Chen, J.H.1
Matsumura, H.2
Atsuta, M.3
-
21
-
-
0030207640
-
Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair
-
Kupiec KA, Wuertz KM, Barkmeier WW, Wilwerding TM. Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair. J Prosthet Dent 1996;76:119-124.
-
(1996)
J Prosthet Dent
, vol.76
, pp. 119-124
-
-
Kupiec, K.A.1
Wuertz, K.M.2
Barkmeier, W.W.3
Wilwerding, T.M.4
-
22
-
-
0028523833
-
Effect of porcelain surface treatments on bond strengths of composite bonded to porcelain
-
Thurmond JW, Barkmeier WW, Wilwerding TM. Effect of porcelain surface treatments on bond strengths of composite bonded to porcelain. J Prosthet Dent 1994;72:355-359.
-
(1994)
J Prosthet Dent
, vol.72
, pp. 355-359
-
-
Thurmond, J.W.1
Barkmeier, W.W.2
Wilwerding, T.M.3
-
23
-
-
0034251718
-
To silanate or not to silanate: Making a clinical decision
-
Barghi N. To silanate or not to silanate: Making a clinical decision. Compend Contin Educ 2000;21:659-664.
-
(2000)
Compend Contin Educ
, vol.21
, pp. 659-664
-
-
Barghi, N.1
-
24
-
-
0027336936
-
Molecular orientation of silane at the surface of colloidal silica
-
Söderholm KJM, Shang SW. Molecular orientation of silane at the surface of colloidal silica. J Dent Res 1993;72:1050-1054.
-
(1993)
J Dent Res
, vol.72
, pp. 1050-1054
-
-
Söderholm, K.J.M.1
Shang, S.W.2
-
25
-
-
0031265663
-
Shear bond strength of feldspathic porcelain of two luting cements in combination with three surface treatments
-
Matsumura H, Kato H, Atsuta M. Shear bond strength of feldspathic porcelain of two luting cements in combination with three surface treatments. J Prosthet Dent 1997;78:511-517.
-
(1997)
J Prosthet Dent
, vol.78
, pp. 511-517
-
-
Matsumura, H.1
Kato, H.2
Atsuta, M.3
-
26
-
-
0026194688
-
Haftfestigkeit von geätztem In-Ceram an Zahnschmeiz
-
Pape FW, Pfeiffer P, Marx R. Haftfestigkeit von geätztem In-Ceram an Zahnschmeiz [Bond strength of acid-etched In-Ceram to enamel]. Zahnärztl Welt 1991;100:450-453.
-
(1991)
Zahnärztl Welt
, vol.100
, pp. 450-453
-
-
Pape, F.W.1
Pfeiffer, P.2
Marx, R.3
-
27
-
-
0025468236
-
Chemische und thermische Kompatibilität vollkeramischer Verbundsysteme
-
Schmid M, Fischer J, Hoffmann C, Strub JR. Chemische und thermische Kompatibilität vollkeramischer Verbundsysteme [Chemical and thermal compatibility of all-ceramic systems]. Dtsch Zahnärztl Z 1990;45:505-508.
-
(1990)
Dtsch Zahnärztl Z
, vol.45
, pp. 505-508
-
-
Schmid, M.1
Fischer, J.2
Hoffmann, C.3
Strub, J.R.4
-
28
-
-
0034132457
-
Shear bond strength of resin luting cement to glass-infiltrated porous aluminum oxide cores
-
Sen D. Shear bond strength of resin luting cement to glass-infiltrated porous aluminum oxide cores. J Prosthet Dent 2000;83:210-215.
-
(2000)
J Prosthet Dent
, vol.83
, pp. 210-215
-
-
Sen, D.1
-
29
-
-
0026856210
-
Bond strengths of composite to porcelain treated with new porcelain repair agents
-
Wolf DM, Powers JM. Bond strengths of composite to porcelain treated with new porcelain repair agents. Dent Mater 1992;8:158-161.
-
(1992)
Dent Mater
, vol.8
, pp. 158-161
-
-
Wolf, D.M.1
Powers, J.M.2
|