1
-
-
0018344605
-
An evaluation of beta titanium alloys for use in orthodontic appliances
-
Goldberg J., Burstone C.J. An evaluation of beta titanium alloys for use in orthodontic appliances. J Dent Res. 58:1979;593-600.
-
(1979)
J Dent Res
, vol.58
, pp. 593-600
-
-
Goldberg, J.1
Burstone, C.J.2
-
2
-
-
0018831556
-
Beta titanium: A new orthodontic alloy
-
Burstone C.J., Goldberg A.J. Beta titanium. a new orthodontic alloy Am J Orthod. 77:1980;121-132.
-
(1980)
Am J Orthod
, vol.77
, pp. 121-132
-
-
Burstone, C.J.1
Goldberg, A.J.2
-
3
-
-
0019582294
-
Comparison of nickel-titanium and beta titanium wire sizes to conventional orthodontic arch wire materials
-
Kusy R.P. Comparison of nickel-titanium and beta titanium wire sizes to conventional orthodontic arch wire materials. Am J Orthod. 79:1981;625-629.
-
(1981)
Am J Orthod
, vol.79
, pp. 625-629
-
-
Kusy, R.P.1
-
4
-
-
0020794903
-
The flexure modulus of elasticity of orthodontic wire
-
Goldberg A.J., Morton J., Burstone C.J. The flexure modulus of elasticity of orthodontic wire. J Dent Res. 62:1983;856-858.
-
(1983)
J Dent Res
, vol.62
, pp. 856-858
-
-
Goldberg, A.J.1
Morton, J.2
Burstone, C.J.3
-
5
-
-
0021383662
-
Age hardening of orthodontic beta titanium alloys
-
Goldberg A.J., Shastry C.V. Age hardening of orthodontic beta titanium alloys. J Biomed Mater Res. 18:1984;155-163.
-
(1984)
J Biomed Mater Res
, vol.18
, pp. 155-163
-
-
Goldberg, A.J.1
Shastry, C.V.2
-
8
-
-
0023391429
-
Geometric and material parameters of a nickel-titanium and a beta titanium orthodontic arch wire alloy
-
Kusy R.P., Stush A.M. Geometric and material parameters of a nickel-titanium and a beta titanium orthodontic arch wire alloy. Dent Mater. 3:1987;207-217.
-
(1987)
Dent Mater
, vol.3
, pp. 207-217
-
-
Kusy, R.P.1
Stush, A.M.2
-
9
-
-
0025503750
-
Dynamic mechanical properties of straight titanium alloy arch wires
-
Kusy R.P., Wilson T.W. Dynamic mechanical properties of straight titanium alloy arch wires. Dent Mater. 6:1990;228-236.
-
(1990)
Dent Mater
, vol.6
, pp. 228-236
-
-
Kusy, R.P.1
Wilson, T.W.2
-
10
-
-
0035882635
-
Degradation and fracture of Ni-Ti superelastic wire in an oral cavity
-
Yokoyama K., Hamada K., Moriyama K., Asaoka K. Degradation and fracture of Ni-Ti superelastic wire in an oral cavity. Biomaterials. 22:2001;2257-2262.
-
(2001)
Biomaterials
, vol.22
, pp. 2257-2262
-
-
Yokoyama, K.1
Hamada, K.2
Moriyama, K.3
Asaoka, K.4
-
11
-
-
0034981405
-
Fracture analysis of hydrogen-charged nickel-titanium superelastic alloy
-
Yokoyama K., Hamada K., Asaoka K. Fracture analysis of hydrogen-charged nickel-titanium superelastic alloy. Mater Trans. 42:2001;141-144.
-
(2001)
Mater Trans
, vol.42
, pp. 141-144
-
-
Yokoyama, K.1
Hamada, K.2
Asaoka, K.3
-
12
-
-
0036010384
-
Fracture mechanisms of retrieved titanium screw thread in dental implant
-
Yokoyama K., Ichikawa T., Murakami H., Miyamoto Y., Asaoka K. Fracture mechanisms of retrieved titanium screw thread in dental implant. Biomaterials. 23:2002;2459-2465.
-
(2002)
Biomaterials
, vol.23
, pp. 2459-2465
-
-
Yokoyama, K.1
Ichikawa, T.2
Murakami, H.3
Miyamoto, Y.4
Asaoka, K.5
-
13
-
-
0000088442
-
Hydrogen embrittlement of nickel-titanium alloy in biological environment
-
Asaoka K., Yokoyama K., Nagumo M. Hydrogen embrittlement of nickel-titanium alloy in biological environment. Metall Mater Trans A. 33A:2002;495-501.
-
(2002)
Metall Mater Trans A
, vol.33 A
, pp. 495-501
-
-
Asaoka, K.1
Yokoyama, K.2
Nagumo, M.3
-
14
-
-
0037454510
-
Susceptibility to delayed fracture of Ni-Ti superelastic alloy
-
Yokoyama K., Watabe S., Hamada K., Sakai J., Asaoka K., Nagumo M. Susceptibility to delayed fracture of Ni-Ti superelastic alloy. Mater Sci Eng A. 341:2003;91-97.
-
(2003)
Mater Sci Eng A
, vol.341
, pp. 91-97
-
-
Yokoyama, K.1
Watabe, S.2
Hamada, K.3
Sakai, J.4
Asaoka, K.5
Nagumo, M.6
-
15
-
-
85031203157
-
Hydrogen embrittlement of Ni-Ti superelastic alloy in fluoride solution
-
in press
-
Yokoyama K, Kaneko K, Moriyama K, Asaoka K, Sakai J, Nagumo M. Hydrogen embrittlement of Ni-Ti superelastic alloy in fluoride solution. J Biomed Mater Res, in press.
-
J Biomed Mater Res
-
-
Yokoyama, K.1
Kaneko, K.2
Moriyama, K.3
Asaoka, K.4
Sakai, J.5
Nagumo, M.6
-
16
-
-
0021981642
-
Accelerated oxide grown on titanium implants during autoclaving caused by fluorine contamination
-
Lausmaa J., Kasemo B., Hansson S. Accelerated oxide grown on titanium implants during autoclaving caused by fluorine contamination. Biomaterials. 6:1985;23-27.
-
(1985)
Biomaterials
, vol.6
, pp. 23-27
-
-
Lausmaa, J.1
Kasemo, B.2
Hansson, S.3
-
17
-
-
0026124943
-
The effect of oral topical fluorides on the surface of commercially pure titanium
-
Siirilä H.S., Könönen M. The effect of oral topical fluorides on the surface of commercially pure titanium. Int J Oral Maxillofac Implants. 6:1991;50-54.
-
(1991)
Int J Oral Maxillofac Implants
, vol.6
, pp. 50-54
-
-
Siirilä, H.S.1
Könönen, M.2
-
19
-
-
0029330528
-
SEM observations on stress corrosion cracking of commercially pure titanium in a topical fluoride solution
-
Könönen M.H.O., Lavonius E.T., Kivilahti J.K. SEM observations on stress corrosion cracking of commercially pure titanium in a topical fluoride solution. Dent Mater. 11:1995;269-272.
-
(1995)
Dent Mater
, vol.11
, pp. 269-272
-
-
Könönen, M.H.O.1
Lavonius, E.T.2
Kivilahti, J.K.3
-
20
-
-
0029415082
-
Influence of fluoride on titanium in an acidic environment measured by polarization resistance technique
-
Boere G. Influence of fluoride on titanium in an acidic environment measured by polarization resistance technique. J Appl Biomater. 6:1995;283-288.
-
(1995)
J Appl Biomater
, vol.6
, pp. 283-288
-
-
Boere, G.1
-
21
-
-
0029685412
-
Corrosive properties of fluoride-containing odontologic gels against titanium
-
Toumelin-Chemla F., Rouelle F., Burdairon G. Corrosive properties of fluoride-containing odontologic gels against titanium. J Dent. 24:1996;109-115.
-
(1996)
J Dent
, vol.24
, pp. 109-115
-
-
Toumelin-Chemla, F.1
Rouelle, F.2
Burdairon, G.3
-
22
-
-
0000823852
-
Electrochemical corrosion behavior of titanium castings: Part 1. Effects of degree of surface polishing and kind of solution
-
Mimura H., Miyagawa Y. Electrochemical corrosion behavior of titanium castings. Part 1. Effects of degree of surface polishing and kind of solution Jpn J Dent Mater Dev. 15:1996;283-285.
-
(1996)
Jpn J Dent Mater Dev
, vol.15
, pp. 283-285
-
-
Mimura, H.1
Miyagawa, Y.2
-
23
-
-
0001041398
-
The influence of fluoride concentration on the corrosion of titanium and titanium alloys
-
Oda Y., Kawada E., Yoshinari M., Hasegawa K., Okabe T. The influence of fluoride concentration on the corrosion of titanium and titanium alloys. Jpn J Dent Mater Dev. 15:1996;317-322.
-
(1996)
Jpn J Dent Mater Dev
, vol.15
, pp. 317-322
-
-
Oda, Y.1
Kawada, E.2
Yoshinari, M.3
Hasegawa, K.4
Okabe, T.5
-
24
-
-
0031864346
-
Effects of fluorides on titanium and other dental alloys in dentistry
-
Reclaru L., Meyer J-.M. Effects of fluorides on titanium and other dental alloys in dentistry. Biomaterials. 19:1998;85-92.
-
(1998)
Biomaterials
, vol.19
, pp. 85-92
-
-
Reclaru, L.1
Meyer, J.-M.2
-
25
-
-
0033278195
-
Effect of fluoride concentration and pH on corrosion behavior of titanium for dental use
-
Nakagawa M., Matsuya S., Shiraishi T., Ohta M. Effect of fluoride concentration and pH on corrosion behavior of titanium for dental use. J Dent Res. 78:1999;1568-1572.
-
(1999)
J Dent Res
, vol.78
, pp. 1568-1572
-
-
Nakagawa, M.1
Matsuya, S.2
Shiraishi, T.3
Ohta, M.4
-
26
-
-
0035757573
-
Corrosion behavior of pure titanium and titanium alloys in fluoride-containing solutions
-
Nakagawa M., Matsuya S., Udoh K. Corrosion behavior of pure titanium and titanium alloys in fluoride-containing solutions. Dent Mater J. 20:2001;305-314.
-
(2001)
Dent Mater J
, vol.20
, pp. 305-314
-
-
Nakagawa, M.1
Matsuya, S.2
Udoh, K.3
-
27
-
-
0036617834
-
Effects of fluoride and dissolved oxygen concentrations on the corrosion behavior of pure titanium and titanium alloys
-
Nakagawa M., Matsuya S., Udoh K. Effects of fluoride and dissolved oxygen concentrations on the corrosion behavior of pure titanium and titanium alloys. Dent Mater J. 21:2002;83-92.
-
(2002)
Dent Mater J
, vol.21
, pp. 83-92
-
-
Nakagawa, M.1
Matsuya, S.2
Udoh, K.3
-
28
-
-
0036027441
-
Effects of fluoride concentration and elastic tensile strain on the corrosion resistance of commercially pure titanium
-
Huang H-.H. Effects of fluoride concentration and elastic tensile strain on the corrosion resistance of commercially pure titanium. Biomaterials. 23:2002;59-63.
-
(2002)
Biomaterials
, vol.23
, pp. 59-63
-
-
Huang, H.-H.1
-
29
-
-
0036210742
-
Influence of fluoride content and pH on the corrosion resistance of titanium and its alloys
-
Schiff N., Grosgogeat B., Lissac M., Dalard F. Influence of fluoride content and pH on the corrosion resistance of titanium and its alloys. Biomaterials. 23:2002;1995-2002.
-
(2002)
Biomaterials
, vol.23
, pp. 1995-2002
-
-
Schiff, N.1
Grosgogeat, B.2
Lissac, M.3
Dalard, F.4
-
30
-
-
0022785742
-
Evidence of FCC titanium hydride formation in β titanium alloy: An X-ray diffraction study
-
Shih D.S., Birnbaum H.K. Evidence of FCC titanium hydride formation in β titanium alloy. an X-ray diffraction study Scr Metall. 20:1986;1261-1264.
-
(1986)
Scr Metall
, vol.20
, pp. 1261-1264
-
-
Shih, D.S.1
Birnbaum, H.K.2
-
31
-
-
0012167791
-
Bending strength of hydrogen-charged Ti-13V-11Cr-3Al alloy
-
Nakasa K., Liu J. Bending strength of hydrogen-charged Ti-13V-11Cr-3Al alloy. J Jpn Inst Metals. 55:1991;922-927.
-
(1991)
J Jpn Inst Metals
, vol.55
, pp. 922-927
-
-
Nakasa, K.1
Liu, J.2
-
32
-
-
0003850107
-
Effects of internal hydrogen on microstructures and mechanical properties of β21S and Ti-15-3
-
D. Eylon, R.R. Boyer, & D.A. Koss. Warrendale, PA: TMS
-
Lederich R.J., Schwartz D.S., Sastry S.M.L. Effects of internal hydrogen on microstructures and mechanical properties of β21S and Ti-15-3. Eylon D., Boyer R.R., Koss D.A. Beta titanium alloys in the 1990s. 1993;159-169 TMS, Warrendale, PA.
-
(1993)
Beta Titanium Alloys in the 1990s
, pp. 159-169
-
-
Lederich, R.J.1
Schwartz, D.S.2
Sastry, S.M.L.3
-
33
-
-
0003850107
-
The effects of hydrogen on the room temperature mechanical properties of Ti-15V-3Cr-3Al-3Sn and Ti-15Mo-3Nb-3Al
-
D. Eylon, R.R. Boyer, & D.A. Koss. Warrendale, PA: TMS
-
Young G.A. Jr., Scully J.R. The effects of hydrogen on the room temperature mechanical properties of Ti-15V-3Cr-3Al-3Sn and Ti-15Mo-3Nb-3Al. Eylon D., Boyer R.R., Koss D.A. Beta titanium alloys in the 1990s. 1993;147-158 TMS, Warrendale, PA.
-
(1993)
Beta Titanium Alloys in the 1990s
, pp. 147-158
-
-
Young G.A., Jr.1
Scully, J.R.2
-
34
-
-
0027544305
-
Effects of hydrogen on the mechanical properties of a Ti-Mo-Nb-Al alloy
-
Young G.A. Jr., Scully J.R. Effects of hydrogen on the mechanical properties of a Ti-Mo-Nb-Al alloy. Scr Metall Mater. 28:1993;507-512.
-
(1993)
Scr Metall Mater
, vol.28
, pp. 507-512
-
-
Young G.A., Jr.1
Scully, J.R.2
-
35
-
-
0001038062
-
Hydrogen embrittlement of solution heat-treated and aged β-titanium alloys Ti-15% V-3% Cr-3% Al-3% Sn and Ti-15% Mo-3% Nb-3% Al
-
Young G.A. Jr., Scully J.R. Hydrogen embrittlement of solution heat-treated and aged β-titanium alloys Ti-15% V-3% Cr-3% Al-3% Sn and Ti-15% Mo-3% Nb-3% Al. Corrosion. 50:1994;919-933.
-
(1994)
Corrosion
, vol.50
, pp. 919-933
-
-
Young G.A., Jr.1
Scully, J.R.2
-
36
-
-
0031140736
-
Hydrogen trapping in aged β-titanium alloys
-
Pound B.G. Hydrogen trapping in aged β-titanium alloys. Acta Mater. 45:1997;2059-2068.
-
(1997)
Acta Mater
, vol.45
, pp. 2059-2068
-
-
Pound, B.G.1
-
37
-
-
0035802962
-
The effects of hydrogen on the deformation and fracture of β-titanium
-
Teter D.F., Robertson I.M., Birnbaum H.K. The effects of hydrogen on the deformation and fracture of β-titanium. Acta Mater. 49:2001;4313-4323.
-
(2001)
Acta Mater
, vol.49
, pp. 4313-4323
-
-
Teter, D.F.1
Robertson, I.M.2
Birnbaum, H.K.3
-
38
-
-
0019047366
-
Model of sustained load cracking by hydride growth in Ti alloys
-
Pardee W.J., Paton N.E. Model of sustained load cracking by hydride growth in Ti alloys. Metall Trans A. 11A:1980;1391-1400.
-
(1980)
Metall Trans A
, vol.11 A
, pp. 1391-1400
-
-
Pardee, W.J.1
Paton, N.E.2
-
39
-
-
0023827822
-
Hydrogen embrittlement of β titanium: In situ tem studies
-
Shin D.S., Robertson I.M., Birnbaum H.K. Hydrogen embrittlement of β titanium. in situ tem studies Acta Metall. 36:1988;111-124.
-
(1988)
Acta Metall
, vol.36
, pp. 111-124
-
-
Shin, D.S.1
Robertson, I.M.2
Birnbaum, H.K.3
-
40
-
-
0001504590
-
Hydrogen embrittlement of grade 2 and grade 3 titanium in 6% sodium chloride solution
-
Wang Z.F., Briant C.L., Kumar K.S. Hydrogen embrittlement of grade 2 and grade 3 titanium in 6% sodium chloride solution. Corrosion. 54:1998;553-560.
-
(1998)
Corrosion
, vol.54
, pp. 553-560
-
-
Wang, Z.F.1
Briant, C.L.2
Kumar, K.S.3
|