2
-
-
85045807506
-
-
K. Shiraogori, H. Sato, F. Kamikubo, T. Fukuzufu, Desalination 22 (1977): p. 403.
-
(1977)
Desalination
, vol.22
, pp. 403
-
-
Shiraogori, K.1
Sato, H.2
Kamikubo, F.3
Fukuzufu, T.4
-
3
-
-
84885313868
-
Determination of Cathodic Potential Limits for Prevention of Titanium Tube Hydride Embrittlement in Salt Water
-
paper no. 110, April 17-21, 1989, New Orleans, Louisiana Houston TX: NACE
-
R. W. Schutz, J.S. Grauman, "Determination of Cathodic Potential Limits for Prevention of Titanium Tube Hydride Embrittlement in Salt Water," CORROSION/89, paper no. 110, April 17-21, 1989, New Orleans, Louisiana (Houston TX: NACE, 1989).
-
(1989)
CORROSION/89
-
-
Schutz, R.W.1
Grauman, J.S.2
-
4
-
-
0018811963
-
-
T. Fukuzuku, K. Shimogori, H. Satoh, F. Kamikabo, Desalination 31 (1979): p. 389.
-
(1979)
Desalination
, vol.31
, pp. 389
-
-
Fukuzuku, T.1
Shimogori, K.2
Satoh, H.3
Kamikabo, F.4
-
5
-
-
0542444965
-
Hydrogen Pickup by Titanium Held Cathodic in Seawater
-
paper no. 6A1, June 6-11, Paris, France
-
H. Satoh, T. Fukuzuka, K. Shimogori, H. Tanabe, "Hydrogen Pickup by Titanium Held Cathodic in Seawater," 2nd Int. Cong. Hydrogen in Metals, paper no. 6A1, June 6-11, 1977, Paris, France.
-
(1977)
2nd Int. Cong. Hydrogen in Metals
-
-
Satoh, H.1
Fukuzuka, T.2
Shimogori, K.3
Tanabe, H.4
-
6
-
-
0016083429
-
Experience of Welded Titanium Tubes in Air Cooling Zone of Surface Condensers
-
July
-
T. Nosetani, "Experience of Welded Titanium Tubes in Air Cooling Zone of Surface Condensers," Sumitomo Light Metal Technical Reports 15, 3 (July, 1974).
-
(1974)
Sumitomo Light Metal Technical Reports
, vol.15
, Issue.3
-
-
Nosetani, T.1
-
7
-
-
0016871720
-
-
S. Sato, K. Nagata, Y. Watanabe, T. Nakamura, T. Hanada, Corros. Eng. Jpn. 25 (1976): p. 311.
-
(1976)
Corros. Eng. Jpn.
, vol.25
, pp. 311
-
-
Sato, S.1
Nagata, K.2
Watanabe, Y.3
Nakamura, T.4
Hanada, T.5
-
8
-
-
0542397431
-
-
A.J. Sedriks, MP 34, 2 (1994): p. 56.
-
(1994)
MP
, vol.34
, Issue.2
, pp. 56
-
-
Sedriks, A.J.1
-
9
-
-
0008702696
-
The Environment-Induced Cracking of Hexagonal Materials: Magnesium, Titanium, and Zirconium
-
eds. R.P. Gangloff, M.B. Ives, NACE-10 Houston, TX: NACE
-
D. Hardie, "The Environment-Induced Cracking of Hexagonal Materials: Magnesium, Titanium, and Zirconium," in Environment-Induced Cracking of Metals, eds. R.P. Gangloff, M.B. Ives, NACE-10 (Houston, TX: NACE, 1990), p. 347.
-
(1990)
Environment-Induced Cracking of Metals
, pp. 347
-
-
Hardie, D.1
-
19
-
-
0017542224
-
-
R. Dutton, N. Nuttall, M.P. Puls, L.A. Simpson, Met. Trans. 8A (1977): p. 1,553.
-
(1977)
Met. Trans.
, vol.8 A
, pp. 1553
-
-
Dutton, R.1
Nuttall, N.2
Puls, M.P.3
Simpson, L.A.4
-
24
-
-
0029701949
-
Diffusion of Hydrogen in Titanium
-
Moran, Wyoming Warrendale, PA: TMS
-
O.S. Abdul-Hamid, R.M. Latanision, "Diffusion of Hydrogen in Titanium," Proc. 5th Int. Conf. Effect of Hydrogen on the Behavior of Materials, Moran, Wyoming (Warrendale, PA: TMS, 1994), p. 205.
-
(1994)
Proc. 5th Int. Conf. Effect of Hydrogen on the Behavior of Materials
, pp. 205
-
-
Abdul-Hamid, O.S.1
Latanision, R.M.2
-
27
-
-
0542397427
-
-
S. Yamanaka, T. Tanaka, S. Tsuboi, M. Miyake, Fusion Eng. 10 (1989): p. 303.
-
(1989)
Fusion Eng.
, vol.10
, pp. 303
-
-
Yamanaka, S.1
Tanaka, T.2
Tsuboi, S.3
Miyake, M.4
-
28
-
-
0022805614
-
-
T.H. Qyach-Kamimura, D. David, G. Beranger, A. Falanga, G. Lozes, J. Less-Common Met. 125 (1986): p. 59.
-
(1986)
J. Less-Common Met.
, vol.125
, pp. 59
-
-
Qyach-Kamimura, T.H.1
David, D.2
Beranger, G.3
Falanga, A.4
Lozes, G.5
|