Volumn 254, Issue 1-2, 2003, Pages 94-102

Wear behaviour of α-Si3N4 ceramics reinforced by rod-like β-Si3N4 grains

Author keywords

Si3N4; Si3N4; Grain morphology

Indexed keywords

ANISOTROPY; CERAMIC MATERIALS; CRACK INITIATION; LUBRICANTS; MICROSTRUCTURE; SILICON NITRIDE; TRIBOLOGY;

EID: 0037253907     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0043-1648(02)00293-4     Document Type: Article
Times cited : (35)

References (25)
  • 1
    • 0002480796 scopus 로고
    • Nitrogen ceramics, 1976-1981
    • F.L. Riley (Ed.), Martinus Nijhoff Publishers, The Hague, The Netherlands
    • R.N. Katz, Nitrogen ceramics, 1976-1981, in: F.L. Riley (Ed.), Progress in Nitrogen Ceramics, Martinus Nijhoff Publishers, The Hague, The Netherlands, 1983, pp. 3-20.
    • (1983) Progress in Nitrogen Ceramics , pp. 3-20
    • Katz, R.N.1
  • 2
    • 0002435715 scopus 로고
    • Sialons: A study in materials development
    • S. Hampsshire (Ed.), Elsevier Applied Science Publishers, New York
    • K.H. Jack, Sialons: a study in materials development in: S. Hampsshire (Ed.), Non-Oxide Technical and Engineering Ceramics, Elsevier Applied Science Publishers, New York, 1986, pp. 1-30.
    • (1986) Non-Oxide Technical and Engineering Ceramics , pp. 1-30
    • Jack, K.H.1
  • 3
    • 0027271173 scopus 로고
    • 4 based ceramics
    • I.W. Chen, P.F. Becher, M. Mitomo, G. Petzow, T.S. Yen (Eds.), Material Research Society, Pittsburgh, PA
    • 4 based ceramics, in: I.W. Chen, P.F. Becher, M. Mitomo, G. Petzow, T.S. Yen (Eds.), Silicon Nitride Ceramics, Material Research Society, Pittsburgh, PA, 1993, pp. 3-14.
    • (1993) Silicon Nitride Ceramics , pp. 3-14
    • Hoffmann, M.J.1    Petzow, G.2
  • 7
    • 0033131102 scopus 로고    scopus 로고
    • Wear behaviour of Si3N4 ceramic cutting tool material against stainless steel in dry and water-lubricated conditions
    • 4 ceramic cutting tool material against stainless steel in dry and water-lubricated conditions, Ceram. Int. 25 (1999) 309-315.
    • (1999) Ceram. Int. , vol.25 , pp. 309-315
    • Zhao, X.1    Liu, J.2    Zhu, B.3    Miao, H.4    Luo, Z.5
  • 8
    • 0028422272 scopus 로고
    • Processing, microstructure, and wear behavior of silicon nitride hot-pressed with alumina and yttria
    • A. Zutshi, R.A. Haber, D.E. Niesz, J.W. Adams, J.B.Wachtman, M.K. Ferber, S.M. Hsu, Processing, microstructure, and wear behavior of silicon nitride hot-pressed with alumina and yttria, J. Am. Ceram. Soc. 77 (4) (1994) 883-890.
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.4 , pp. 883-890
    • Zutshi, A.1    Haber, R.A.2    Niesz, D.E.3    Adams, J.W.4    Wachtman, J.B.5    Ferber, M.K.6    Hsu, S.M.7
  • 9
    • 0032178162 scopus 로고    scopus 로고
    • The tribochemistry of silicon nitride: Effects of friction, temperature and sliding velocity
    • V.A. Muratov, T. Lungvaranunt, T.E. Fidcher, The tribochemistry of silicon nitride: effects of friction, temperature and sliding velocity, Tribol. Int. 31 (10) (1998) 601-611.
    • (1998) Tribol. Int. , vol.31 , Issue.10 , pp. 601-611
    • Muratov, V.A.1    Lungvaranunt, T.2    Fidcher, T.E.3
  • 10
    • 0032661099 scopus 로고    scopus 로고
    • Surface quality of tribochemically polished silicon nitride
    • S.R. Hah, C.B. burk, T.E. Fischer, Surface quality of tribochemically polished silicon nitride, J. Electrochem. Soc. 146 (4) (1999) 1505-1509.
    • (1999) J. Electrochem. Soc. , vol.146 , Issue.4 , pp. 1505-1509
    • Hah, S.R.1    Burk, C.B.2    Fischer, T.E.3
  • 13
    • 0029325006 scopus 로고
    • Processing strategy for producing highly anisotropic silicon nitride
    • K. Hirao, M. Ohashi, M.E. Brito, S. Kanzaki, Processing strategy for producing highly anisotropic silicon nitride, J. Am. Ceram. Soc. 78 (6) (1995) 1687-1690.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.6 , pp. 1687-1690
    • Hirao, K.1    Ohashi, M.2    Brito, M.E.3    Kanzaki, S.4
  • 14
    • 0001603167 scopus 로고    scopus 로고
    • Effect of seed alignment on microstructures and mechanical properties of silicon nitride
    • R.M. German, G.L. Messing, R.G. Cornwall (Eds.), The Pennsylvania State University, PA, USA
    • K. Hirao, M.E. Brito, M. Toriyama, S. Kanzaki, H. Teshima, Effect of seed alignment on microstructures and mechanical properties of silicon nitride, in: R.M. German, G.L. Messing, R.G. Cornwall (Eds.), Proceedings of Sintering Science and Technology, The Pennsylvania State University, PA, USA, 2000, pp. 343-348.
    • (2000) Proceedings of Sintering Science and Technology , pp. 343-348
    • Hirao, K.1    Brito, M.E.2    Toriyama, M.3    Kanzaki, S.4    Teshima, H.5
  • 15
    • 0033355115 scopus 로고    scopus 로고
    • Fabrication and mechanical properties of silicon nitride ceramics with unidirectionally oriented rodlike grains
    • in Japanese
    • H. Teshima, K. Hirao, M. Toriyama, S. kanzaki, Fabrication and mechanical properties of silicon nitride ceramics with unidirectionally oriented rodlike grains, J. Ceram. Soc. Jpn. 107 (12) (1999) 1216- 1220 (in Japanese).
    • (1999) J. Ceram. Soc. Jpn. , vol.107 , Issue.12 , pp. 1216-1220
    • Teshima, H.1    Hirao, K.2    Toriyama, M.3    Kanzaki, S.4
  • 17
    • 0019058952 scopus 로고
    • Elastic/plastic indentation damage in ceramics: The median/radial crack system
    • B.R. Lawn, A.G. Evans, D.B. Marshall, Elastic/plastic indentation damage in ceramics: the median/radial crack system, J. Am. Ceram. Soc. 63 (9-10) (1980) 574-581.
    • (1980) J. Am. Ceram. Soc. , vol.63 , Issue.9-10 , pp. 574-581
    • Lawn, B.R.1    Evans, A.G.2    Marshall, D.B.3
  • 19
    • 0001645790 scopus 로고    scopus 로고
    • Development of new silicon nitride materials for automotive applications
    • K. Niihara, S. Hirano, S. Kanzaki, K. Komeya, K. Morinaga (Eds), Japan Fine Ceramics Association
    • M. Sato, K. Sakaue, T. Fukudome, S. Wakida, Development of new silicon nitride materials for automotive applications, in: K. Niihara, S. Hirano, S. Kanzaki, K. Komeya, K. Morinaga (Eds), Proceedings of the 6th International Symposium on Ceramic Materials and Components for Engines, Japan Fine Ceramics Association, 1997, pp. 173-176.
    • (1997) Proceedings of the 6th International Symposium on Ceramic Materials and Components for Engines , pp. 173-176
    • Sato, M.1    Sakaue, K.2    Fukudome, T.3    Wakida, S.4
  • 21
    • 0032206823 scopus 로고    scopus 로고
    • Microhardness load size effect in individual grains of a gas pressure sintered silicon nitride
    • J. Dusza, M. Steen, Microhardness load size effect in individual grains of a gas pressure sintered silicon nitride, J. Am. Ceram. Soc. 81 (11) (1998) 3022-3024.
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.11 , pp. 3022-3024
    • Dusza, J.1    Steen, M.2
  • 22
    • 0026115117 scopus 로고
    • Microstructure design of toughened ceramics
    • P.F. Becher, Microstructure design of toughened ceramics, J. Am. Ceram. Soc. 74 (1991) 255-269.
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 255-269
    • Becher, P.F.1
  • 23
    • 0027627698 scopus 로고
    • Toughness anisotropy in textured ceramic composites
    • F. Lee, M.S. Sandlin, K.J. Bowman, Toughness anisotropy in textured ceramic composites, J. Am. Ceram. Soc. 76 (7) (1993) 1793-1800.
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.7 , pp. 1793-1800
    • Lee, F.1    Sandlin, M.S.2    Bowman, K.J.3
  • 25
    • 0035526629 scopus 로고    scopus 로고
    • Tribological properties of uni-directionally aligned silicon nitride
    • M. Nakamura, K. Hirao, Y. Yamauchi, S. Kanzaki, Tribological properties of uni-directionally aligned silicon nitride, J. Am. Ceram. Soc. 84 (11) (2001) 2579-2584.
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.11 , pp. 2579-2584
    • Nakamura, M.1    Hirao, K.2    Yamauchi, Y.3    Kanzaki, S.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.