Surface layer formed by selective oxidation in high-purity copper-titanium binary alloys

Author keywords

Copper titanium alloy; Internal oxidation; Secondary ion mass spectrometry; Selective oxidation; X ray photoelectron spectroscopy

Indexed keywords

COPPER ALLOYS; DIFFUSION; OXIDATION; PARTIAL PRESSURE; SECONDARY ION MASS SPECTROMETRY; TITANIUM ALLOYS; X RAY PHOTOELECTRON SPECTROSCOPY;