1
-
-
84974883811
-
Requirements for engineering ceramics in gas turbine engines
-
A. Bennett, "Requirements for Engineering Ceramics in Gas Turbine Engines," Mater. Sci. Technol., 2, 895-99 (1986).
-
(1986)
Mater. Sci. Technol.
, vol.2
, pp. 895-899
-
-
Bennett, A.1
-
2
-
-
0016618571
-
Silicon/silicon carbide composites
-
W. B. Hillig, R. L. Mehan, C. R. Morelock, V. J. Decarlo, and W. Laskow, "Silicon/Silicon Carbide Composites," Am. Ceram. Soc. Bull., 54, 1054-56 (1975).
-
(1975)
Am. Ceram. Soc. Bull.
, vol.54
, pp. 1054-1056
-
-
Hillig, W.B.1
Mehan, R.L.2
Morelock, C.R.3
Decarlo, V.J.4
Laskow, W.5
-
3
-
-
0022663873
-
Fiber-reinforced silicon carbide
-
E. Fitzer and R. Gadow, "Fiber-Reinforced Silicon Carbide," Am. Ceram. Soc. Bull., 65, 326-35 (1986).
-
(1986)
Am. Ceram. Soc. Bull.
, vol.65
, pp. 326-335
-
-
Fitzer, E.1
Gadow, R.2
-
4
-
-
0029324484
-
Reaction-infiltrated, net-shape sic composites
-
L. Hozer, J. Lee, and Y. Chiang, "Reaction-Infiltrated, Net-Shape SiC Composites," Mater. Sci. Eng., A195, 131-43 (1995).
-
(1995)
Mater. Sci. Eng.
, vol.A195
, pp. 131-143
-
-
Hozer, L.1
Lee, J.2
Chiang, Y.3
-
5
-
-
0022660888
-
Sic/Sic composite ceramics
-
P. J. Lamicq, G. A. Bernhart, M. M. Dauchier, and J. G. Mace, "SiC/SiC Composite Ceramics," Am. Ceram. Soc. Bull., 65, 336-38 (1986).
-
(1986)
Am. Ceram. Soc. Bull.
, vol.65
, pp. 336-338
-
-
Lamicq, P.J.1
Bernhart, G.A.2
Dauchier, M.M.3
Mace, J.G.4
-
6
-
-
0030196487
-
Densification of ultrafine SiC powders
-
R. Vassen, A. Kaiser, J. Forster, H. P. Buchkremer, and D. Stover, "Densification of Ultrafine SiC Powders," J. Mater. Sci., 31, 3623-37 (1996).
-
(1996)
J. Mater. Sci.
, vol.31
, pp. 3623-3637
-
-
Vassen, R.1
Kaiser, A.2
Forster, J.3
Buchkremer, H.P.4
Stover, D.5
-
7
-
-
0032632519
-
Fabrication of nanograined silicon carbide by ultra high-pressure hot isostatic pressing
-
Y. Shinoda, T. Nagano, and F. Wakai, "Fabrication of Nanograined Silicon Carbide by Ultra High-Pressure Hot Isostatic Pressing," J. Am. Ceram. Soc., 82, 771-73 (1999).
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, pp. 771-773
-
-
Shinoda, Y.1
Nagano, T.2
Wakai, F.3
-
8
-
-
0002645801
-
Fabrication of ceramic composites: Forced CVI
-
T. M. Besmann, J. C. McLaughlin, and H. Lin, "Fabrication of Ceramic Composites: Forced CVI," J. Nucl. Mater., 219, 31-35 (1995).
-
(1995)
J. Nucl. Mater.
, vol.219
, pp. 31-35
-
-
Besmann, T.M.1
McLaughlin, J.C.2
Lin, H.3
-
13
-
-
0033908888
-
1 and its composites
-
1 and its Composites," J. Mater. Sci., 35, 863-72 (2000).
-
(2000)
J. Mater. Sci.
, vol.35
, pp. 863-872
-
-
Zhu, Q.1
Shobu, K.2
Tani, E.3
Kishi, K.4
Umebayashi, S.5
-
16
-
-
0033316519
-
1 composites
-
1 Composites," J. Am. Ceram. Soc., 82, 2276-78 (1999).
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, pp. 2276-2278
-
-
Zhu, Q.1
Shobu, K.2
Tani, E.3
Kishi, K.4
Umebayashi, S.5
-
17
-
-
84987368857
-
Critical evaluation of indentation techniques for measuring fracture toughness: II, strength method
-
P. Chantikul, G. R. Anstis, B. R. Lawn, and D. B. Marshall, "Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: II, Strength Method," J. Am. Ceram. Soc., 64, 539-43 (1981).
-
(1981)
J. Am. Ceram. Soc.
, vol.64
, pp. 539-543
-
-
Chantikul, P.1
Anstis, G.R.2
Lawn, B.R.3
Marshall, D.B.4
-
18
-
-
0029309781
-
Reactive melt infiltration of silicon-molybdenum alloys into microporous carbon preforms
-
M. Singh and D. R. Behrendt, "Reactive Melt Infiltration of Silicon-Molybdenum Alloys into Microporous Carbon Preforms," Mater. Sci. Eng., A194, 193-200 (1995).
-
(1995)
Mater. Sci. Eng.
, vol.A194
, pp. 193-200
-
-
Singh, M.1
Behrendt, D.R.2
-
19
-
-
0005548986
-
-
JANAF Thermochemical Tables, 3rd ed. American Chemical Society, New York
-
W. Chase Jr., C. W. Davies, J. R. Doweny Jr., D. J. Frurip, R. A. McDonald, and A. N. Syverud in JANAF Thermochemical Tables, 3rd ed. J. Phys. Chem. Ref. Data, Vol. 14. Suppl. 1. American Chemical Society, New York, 1985.
-
(1985)
J. Phys. Chem. Ref. Data
, vol.14
, Issue.SUPPL. 1
-
-
Chase W., Jr.1
Davies, C.W.2
Doweny J.R., Jr.3
Frurip, D.J.4
McDonald, R.A.5
Syverud, A.N.6
-
20
-
-
0028465881
-
Reactive melt infiltration of silicon-niobium alloys in microporous carbons
-
M. Singh and D. R. Behrendt, "Reactive Melt Infiltration of Silicon-Niobium Alloys in Microporous Carbons," J. Mater. Res., 9, 1701-708 (1994).
-
(1994)
J. Mater. Res.
, vol.9
, pp. 1701-1708
-
-
Singh, M.1
Behrendt, D.R.2
-
21
-
-
0028544430
-
Microstructure and mechanical properties of Reaction-Formed Silicon Carbide (RFSC) ceramics
-
M. Singh and D. R. Behrendt, "Microstructure and Mechanical Properties of Reaction-Formed Silicon Carbide (RFSC) Ceramics," Mater. Sci. Eng., A187, 183-87 (1994).
-
(1994)
Mater. Sci. Eng.
, vol.A187
, pp. 183-187
-
-
Singh, M.1
Behrendt, D.R.2
-
22
-
-
84985163670
-
Perspective on the development of high-toughness ceramics
-
A. G. Evans, "Perspective on the Development of High-Toughness Ceramics," J. Am. Ceram. Soc., 73, 187-206 (1990).
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, pp. 187-206
-
-
Evans, A.G.1
-
23
-
-
0032108335
-
Microstructure and fracture toughness of in-situ toughened SiC-TiC composites
-
K. Cho, H. Choi, and J. Lee, "Microstructure and Fracture Toughness of In-situ Toughened SiC-TiC Composites," J. Mater. Sci. Lett., 17, 1081-84 (1998).
-
(1998)
J. Mater. Sci. Lett.
, vol.17
, pp. 1081-1084
-
-
Cho, K.1
Choi, H.2
Lee, J.3
-
24
-
-
0026840695
-
Crack healing behavior of hot pressed silicon nitride due to oxidation
-
S. R. Choi and V. Tikare, "Crack Healing Behavior of Hot Pressed Silicon Nitride due to Oxidation," Scr. Metall. Mater., 26, 1263-68 (1992).
-
(1992)
Scr. Metall. Mater.
, vol.26
, pp. 1263-1268
-
-
Choi, S.R.1
Tikare, V.2
-
25
-
-
0031190166
-
High temperature fracture toughness of single crystal yttrium-aluminium garnet
-
W. R. Blumenthal and S. T. Taylor, "High Temperature Fracture Toughness of Single Crystal Yttrium-Aluminium Garnet," Acta Metall. Mater., 45, 3071-78 (1997).
-
(1997)
Acta Metall. Mater.
, vol.45
, pp. 3071-3078
-
-
Blumenthal, W.R.1
Taylor, S.T.2
-
26
-
-
0023997851
-
On the toughness of brittle materials reinforced with a ductile phase
-
L. S. Sigl, P. A. Mataga, B. J. Dalgleish, R. M. McMeeking, and A. G. Evans, "On the Toughness of Brittle Materials Reinforced with a Ductile Phase," Acta Metall., 36, 945-53 (1988).
-
(1988)
Acta Metall.
, vol.36
, pp. 945-953
-
-
Sigl, L.S.1
Mataga, P.A.2
Dalgleish, B.J.3
McMeeking, R.M.4
Evans, A.G.5
-
27
-
-
0027091113
-
Toughening mechanisms for ceramic materials
-
R. W. Steinbrech, "Toughening Mechanisms for Ceramic Materials," J. Ear. Ceram. Soc., 10, 131-42 (1992).
-
(1992)
J. Ear. Ceram. Soc.
, vol.10
, pp. 131-142
-
-
Steinbrech, R.W.1
-
28
-
-
0004217652
-
-
Wiley, New York
-
W. D. Kingery, H. K. Bowen, and D. R. Uhlmann, Introduction to Ceramics, 2nd ed. Wiley, New York, 1975.
-
(1975)
Introduction to Ceramics, 2nd Ed.
-
-
Kingery, W.D.1
Bowen, H.K.2
Uhlmann, D.R.3
-
29
-
-
0002378537
-
Grain boundary deformation processes
-
Edited by R. C. Bradt and R. E. Tressler. Plenum, New York
-
T. G. Langdon, "Grain Boundary Deformation Processes"; pp. 101-26 in Deformation of Ceramic Materials. Edited by R. C. Bradt and R. E. Tressler. Plenum, New York, 1975.
-
(1975)
Deformation of Ceramic Materials
, pp. 101-126
-
-
Langdon, T.G.1
-
30
-
-
84977687573
-
Creep of polycrystalline silicon carbide
-
T. L. Francis and R. L. Coble, "Creep of Polycrystalline Silicon Carbide," J. Am. Ceram. Soc., 51, 115-16 (1968).
-
(1968)
J. Am. Ceram. Soc.
, vol.51
, pp. 115-116
-
-
Francis, T.L.1
Coble, R.L.2
-
31
-
-
84977692571
-
Deformation behavior of dense polycrystalline SiC
-
P. L. Farnsworth and R. L. Coble, "Deformation Behavior of Dense Polycrystalline SiC," J. Am. Ceram. Soc., 49, 264-68 (1966).
-
(1966)
J. Am. Ceram. Soc.
, vol.49
, pp. 264-268
-
-
Farnsworth, P.L.1
Coble, R.L.2
-
32
-
-
0021444296
-
Kinetics and mechanisms of high-temperature creep in silicon carbide: I, reaction-bonded
-
C. H. Carter, R. F. Davis, and J. Bentley, "Kinetics and Mechanisms of High-Temperature Creep in Silicon Carbide: I, Reaction-Bonded," J. Am. Ceram. Soc., 67, 409-17 (1984).
-
(1984)
J. Am. Ceram. Soc.
, vol.67
, pp. 409-417
-
-
Carter, C.H.1
Davis, R.F.2
Bentley, J.3
-
34
-
-
84980280980
-
Sintering of low density glasses: I, theory
-
G. W. Scherer, "Sintering of Low Density Glasses: I, Theory," J. Am. Ceram, Soc., 60, 236-39 (1977).
-
(1977)
J. Am. Ceram, Soc.
, vol.60
, pp. 236-239
-
-
Scherer, G.W.1
-
35
-
-
0032050590
-
Oxidation behavior of chemically-vapor-deposited silicon carbide and silicon nitride from 1200° to 1600°C
-
D. S. Fox, "Oxidation Behavior of Chemically-Vapor-Deposited Silicon Carbide and Silicon Nitride from 1200° to 1600°C," J. Am. Ceram. Soc., 81, 945-50 (1998).
-
(1998)
J. Am. Ceram. Soc.
, vol.81
, pp. 945-950
-
-
Fox, D.S.1
|