A miniature specimen mechanical testing technique scaled to articulating surface of polyethylene components for total joint arthroplasty

Author keywords

Degradation; Mechanical properties; Polyethylene; Small punch test

Indexed keywords

BIOMECHANICS; DUCTILITY; FRACTURE TOUGHNESS; MECHANICAL TESTING; POLYETHYLENES; STRENGTH OF MATERIALS;

EID: 0033104526     PISSN: 00219304     EISSN: None     Source Type: Journal    
DOI: 10.1002/(SICI)1097-4636(1999)48:1<75::AID-JBM13>3.0.CO;2-H     Document Type: Article
Times cited : (49)

References (26)
  • 1
  • 2
    • 0031039389 scopus 로고    scopus 로고
    • Degradation rate of ultra-high molecular weight polyethylene
    • Kurtz SM, Rimnac CM, Bartel DL. Degradation rate of ultra-high molecular weight polyethylene. J Orthop Res 1997;15: 57-61.
    • (1997) J Orthop Res , vol.15 , pp. 57-61
    • Kurtz, S.M.1    Rimnac, C.M.2    Bartel, D.L.3
  • 3
    • 0345218243 scopus 로고
    • The effects of post-irradiation aging on the stresses and strains in UHMWPE tibial components for TKR
    • Kurtz SM, Bartel DL, Rimnac CM. The effects of post-irradiation aging on the stresses and strains in UHMWPE Tibial Components for TKR. 2nd Combined Mtg. ORS U.S.A., Canada, Eur 1995;2:70.
    • (1995) 2nd Combined Mtg. ORS U.S.A., Canada, Eur , vol.2 , pp. 70
    • Kurtz, S.M.1    Bartel, D.L.2    Rimnac, C.M.3
  • 5
    • 0028818758 scopus 로고
    • Impact of gamma sterilization on clinical performance of polyethylene in the hip
    • Sutula LC, Collier JP, Saum KA, et al. Impact of gamma sterilization on clinical performance of polyethylene in the hip. Clin Orthop 1995;319:28-40.
    • (1995) Clin Orthop , vol.319 , pp. 28-40
    • Sutula, L.C.1    Collier, J.P.2    Saum, K.A.3
  • 6
    • 0001738320 scopus 로고    scopus 로고
    • Gamma sterilization of UHMWPE articular implants: An analysis of the oxidation problem
    • Premnath V, Harris WH, Jasty M, Merrill EW. Gamma sterilization of UHMWPE articular implants: an analysis of the oxidation problem. Biomaterials 1996;17:1741-1753.
    • (1996) Biomaterials , vol.17 , pp. 1741-1753
    • Premnath, V.1    Harris, W.H.2    Jasty, M.3    Merrill, E.W.4
  • 8
    • 0030415661 scopus 로고
    • Oxidative degradation and embrittlement of ultra-high molecular weight polyethylene. Analysis of 107 Components
    • Muratoglu O, Liu A, Jasty M, Bragdon CR, Elder JR, Harris WH. Oxidative degradation and embrittlement of ultra-high molecular weight polyethylene. Analysis of 107 components. Trans 21st Soc Biomater 1995;18:808.
    • (1995) Trans 21st Soc Biomater , vol.18 , pp. 808
    • Muratoglu, O.1    Liu, A.2    Jasty, M.3    Bragdon, C.R.4    Elder, J.R.5    Harris, W.H.6
  • 9
  • 10
    • 0029999567 scopus 로고    scopus 로고
    • Safety and efficacy of ethylene oxide sterilized polyethylene in total knee arthroplasty
    • Ries MD. Weaver K. Beals N. Safety and efficacy of ethylene oxide sterilized polyethylene in total knee arthroplasty. Clin Orthop 1996:331:159-163.
    • (1996) Clin Orthop , vol.331 , pp. 159-163
    • Ries, M.D.1    Weaver, K.2    Beals, N.3
  • 11
    • 0023688210 scopus 로고
    • Radiation sterilization of polymeric implant materials
    • Bruck SD, Mueller EP. Radiation sterilization of polymeric implant materials. J Biomed Mater Res 1988;22:133-144.
    • (1988) J Biomed Mater Res , vol.22 , pp. 133-144
    • Bruck, S.D.1    Mueller, E.P.2
  • 15
    • 0031412462 scopus 로고    scopus 로고
    • Validation of a small punch testing technique to characterize the mechanical behavior of ultra-high molecular weight polyethylene
    • Kurtz SM, Foulds JR, Jewett CW, Srivastav S, Edidin AA. Validation of a small punch testing technique to characterize the mechanical behavior of ultra-high molecular weight polyethylene. Biomaterials 1998;18:1659-1663.
    • (1998) Biomaterials , vol.18 , pp. 1659-1663
    • Kurtz, S.M.1    Foulds, J.R.2    Jewett, C.W.3    Srivastav, S.4    Edidin, A.A.5
  • 17
    • 0000082414 scopus 로고
    • Development of an accelerated aging method for evaluation of long-term irradiation effects on UHMWPE implants
    • Sun DC, Stark C, Dumbleton JH. Development of an accelerated aging method for evaluation of long-term irradiation effects on UHMWPE implants. Polym Prepr 1994;35:969-970.
    • (1994) Polym Prepr , vol.35 , pp. 969-970
    • Sun, D.C.1    Stark, C.2    Dumbleton, J.H.3
  • 18
    • 0001614608 scopus 로고    scopus 로고
    • A simple accelerated aging method for simulations of long-term oxidative aging effects in UHMWPE implants
    • Sun DC, Scmidig G, Stark C, Dumbleton JH. A simple accelerated aging method for simulations of long-term oxidative aging effects in UHMWPE implants. Trans 43rd Orthop Res Soc 1997;22:493.
    • (1997) Trans 43rd Orthop Res Soc , vol.22 , pp. 493
    • Sun, D.C.1    Scmidig, G.2    Stark, C.3    Dumbleton, J.H.4
  • 19
    • 0024174065 scopus 로고
    • Ionizing irradiation for sterilization and modification of high molecular weight polyethylenes
    • Streicher RM. Ionizing irradiation for sterilization and modification of high molecular weight polyethylenes. Plast Rubber Proc Applic 1988;10:221-229.
    • (1988) Plast Rubber Proc Applic , vol.10 , pp. 221-229
    • Streicher, R.M.1
  • 20
    • 0003649802 scopus 로고    scopus 로고
    • Marked improvement in the wear resistance of a new form of UHMWPE in a physiologic hip simulator
    • Jasty M, Bragdon CR, O'Connor DO, et al. Marked improvement in the wear resistance of a new form of UHMWPE in a physiologic hip simulator. Trans 43rd Orthop Res Soc 1997;22:785.
    • (1997) Trans 43rd Orthop Res Soc , vol.22 , pp. 785
    • Jasty, M.1    Bragdon, C.R.2    O'Connor, D.O.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.