Volumn 103, Issue 31, 1999, Pages 6562-6566

Rate-Dependent Fracture at Adhesive Interface

Author keywords

[No Author keywords available]

Indexed keywords


EID: 0000510334     PISSN: 15206106     EISSN: None     Source Type: Journal    
DOI: 10.1021/jp9906482     Document Type: Article
Times cited : (119)

References (46)
  • 7
    • 0028301942 scopus 로고
    • Brown, H. R. Science 1994, 263, 1411; Macromolecules 1993, 26, 1666.
    • (1994) Science , vol.263 , pp. 1411
    • Brown, H.R.1
  • 8
    • 0027560777 scopus 로고
    • Brown, H. R. Science 1994, 263, 1411; Macromolecules 1993, 26, 1666.
    • (1993) Macromolecules , vol.26 , pp. 1666
  • 20
    • 0032098009 scopus 로고    scopus 로고
    • Ahn, D.; Shull, K. R. Langmuir 1998, 14, 3646; Langmuir 1998, 14, 3637; Shull, K. R.; Crosby, A. J. Eng. Mater. Technol. 1997, 119, 211.
    • (1998) Langmuir , vol.14 , pp. 3646
    • Ahn, D.1    Shull, K.R.2
  • 21
    • 0032097633 scopus 로고    scopus 로고
    • Ahn, D.; Shull, K. R. Langmuir 1998, 14, 3646; Langmuir 1998, 14, 3637; Shull, K. R.; Crosby, A. J. Eng. Mater. Technol. 1997, 119, 211.
    • (1998) Langmuir , vol.14 , pp. 3637
  • 23
    • 0018101150 scopus 로고
    • Bell, G. I. Science 1978, 200, 618.
    • (1978) Science , vol.200 , pp. 618
    • Bell, G.I.1
  • 24
    • 0029914159 scopus 로고    scopus 로고
    • Full kinetic equations of bond rupture, including the reverse reaction rates, were first described by Hammer et al. See the following papers for details: Brunk, D. K.; Goetz, D. J.; Hammer, D. A. Biophys. J. 1996, 71, 2902. Chang, K.-C; Hammer, D. A. Langmuir 1996, 12, 2271. Hammer, D. A.; Apte, S. M. Biophys. J. 1992, 62, 35-37.
    • (1996) Biophys. J. , vol.71 , pp. 2902
    • Brunk, D.K.1    Goetz, D.J.2    Hammer, D.A.3
  • 25
    • 0001505304 scopus 로고    scopus 로고
    • Full kinetic equations of bond rupture, including the reverse reaction rates, were first described by Hammer et al. See the following papers for details: Brunk, D. K.; Goetz, D. J.; Hammer, D. A. Biophys. J. 1996, 71, 2902. Chang, K.-C; Hammer, D. A. Langmuir 1996, 12, 2271. Hammer, D. A.; Apte, S. M. Biophys. J. 1992, 62, 35-37.
    • (1996) Langmuir , vol.12 , pp. 2271
    • Chang, K.-C.1    Hammer, D.A.2
  • 26
    • 0026690271 scopus 로고
    • Full kinetic equations of bond rupture, including the reverse reaction rates, were first described by Hammer et al. See the following papers for details: Brunk, D. K.; Goetz, D. J.; Hammer, D. A. Biophys. J. 1996, 71, 2902. Chang, K.-C; Hammer, D. A. Langmuir 1996, 12, 2271. Hammer, D. A.; Apte, S. M. Biophys. J. 1992, 62, 35-37.
    • (1992) Biophys. J. , vol.62 , pp. 35-37
    • Hammer, D.A.1    Apte, S.M.2
  • 27
    • 0031001349 scopus 로고    scopus 로고
    • and the references therein
    • Evans, E.; Ritchie, K. Biophys. J. 1997, 72, 1541 and the references therein.
    • (1997) Biophys. J. , vol.72 , pp. 1541
    • Evans, E.1    Ritchie, K.2
  • 35
    • 85086292668 scopus 로고    scopus 로고
    • note
    • -13, even when the velocity of crack propagation is only 1 Å/s. Thus eq 9 is well justified.
  • 40
    • 0346816743 scopus 로고    scopus 로고
    • note
    • Note that the velocity of stretching of the polymer used in eq 9 is in the direction vertical to the crack plane, which is obtained as V = a da/dt, where a is the radius of contact.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.