메뉴 건너뛰기




Volumn 87, Issue 4, 2004, Pages 241-247

Depth profile of UV-induced wood surface degradation

Author keywords

Clear wood stain; Photostabilisers; Thin strip method; UV exposure; Wood surface degradation

Indexed keywords

IRON COMPOUNDS; SURFACE TREATMENT; TENSILE PROPERTIES; ULTRAVIOLET RADIATION; WEATHERING; WOOD PRODUCTS;

EID: 9644281521     PISSN: 14764865     EISSN: None     Source Type: Journal    
DOI: 10.1007/BF02699671     Document Type: Article
Times cited : (17)

References (30)
  • 1
    • 0023964869 scopus 로고
    • Role of pigment concentration in the weathering of semi-transparent stains
    • Feist W C, Role of pigment concentration in the weathering of semi-transparent stains', Forest Prod J, 38, (2), 41-44, 1988
    • (1988) Forest Prod J , vol.38 , Issue.2 , pp. 41-44
    • Feist, W.C.1
  • 3
    • 0000347453 scopus 로고
    • The photodegradation of wood during irradiation. Part I: Effects on structural integrity of thin wood strips
    • Derbyshire H and E R Miller, The photodegradation of wood during irradiation. Part I: Effects on structural integrity of thin wood strips', Holz als Roh-und Werkstoff, 39, 341-50, 1981
    • (1981) Holz als Roh-und Werkstoff , vol.39 , pp. 341-350
    • Derbyshire, H.1    Miller, E.R.2
  • 4
    • 9644256381 scopus 로고
    • Durability of exterior wood stains
    • Feist W C, E A Mraz and J M Black, 'Durability of exterior wood stains', Forest Prod J, 27, (1), 13-16, 1977
    • (1977) Forest Prod J , vol.27 , Issue.1 , pp. 13-16
    • Feist, W.C.1    Mraz, E.A.2    Black, J.M.3
  • 5
    • 4243639871 scopus 로고
    • Research Paper FPL 339, US Department of Agriculture, Forest Service, Forest Products Laboratory, Madison, WII
    • Feist W C, 'Protection of wood surfaces with chromium trioxide', Research Paper FPL 339, US Department of Agriculture, Forest Service, Forest Products Laboratory, Madison, WII, 1979
    • (1979) Protection of Wood Surfaces with Chromium Trioxide
    • Feist, W.C.1
  • 6
    • 0002054928 scopus 로고
    • Photoprotection of wood surfaces by wood-ion complexes
    • Hon D N-S and S T Chang, 'Photoprotection of wood surfaces by wood-ion complexes', Wood and Fiber Science, 17, (1), 92-100, 1985
    • (1985) Wood and Fiber Science , vol.17 , Issue.1 , pp. 92-100
    • Hon, D.N.-S.1    Chang, S.T.2
  • 7
    • 84961488613 scopus 로고
    • A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds
    • Evans P D and K J Schmalzl, 'A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds', Holzforschung, 43, (5), 289-92, 1989
    • (1989) Holzforschung , vol.43 , Issue.5 , pp. 289-292
    • Evans, P.D.1    Schmalzl, K.J.2
  • 8
    • 0012855342 scopus 로고
    • Weathering durability of chromium-treated southern pine
    • Feist W C and R S Williams, 'Weathering durability of chromium-treated southern pine', Forest Prod J, 41, (1), 8-14, 1991
    • (1991) Forest Prod J , vol.41 , Issue.1 , pp. 8-14
    • Feist, W.C.1    Williams, R.S.2
  • 9
    • 0022045653 scopus 로고
    • Protection of wood surfaces against photodegradation
    • Hon D N -S, S T Chang and W C Feist, 'Protection of wood surfaces against photodegradation', J Appl Polymer Sci, 30, 1429-48, 1985
    • (1985) J Appl Polymer Sci , vol.30 , pp. 1429-1448
    • Hon, D.N.-S.1    Chang, S.T.2    Feist, W.C.3
  • 10
    • 0020767292 scopus 로고
    • Effect of grafted UV stabilisers on wood surface erosion and clear coating performance
    • Williams R S, 'Effect of grafted UV stabilisers on wood surface erosion and clear coating performance', J Appl Polymer Sci, 28, 2093-103, 1983
    • (1983) J Appl Polymer Sci , vol.28 , pp. 2093-2103
    • Williams, R.S.1
  • 11
    • 0024303255 scopus 로고
    • Einfluß von UV-Absorbern auf die Wetterbeständigkeit farbloser Acryldispersionen
    • Kastien H, 'Einfluß von UV-Absorbern auf die Wetterbestä ndigkeit farbloser Acryldispersionen', Farbe und Lack, 95, (1), 16-19, 1989
    • (1989) Farbe und Lack , vol.95 , Issue.1 , pp. 16-19
    • Kastien, H.1
  • 12
    • 0346810695 scopus 로고
    • Lichtschutzmittel in Lacken: Möglichkeiten und Grenzen
    • October
    • Böhnke H and E Hess, 'Lichtschutzmittel in Lacken: Möglichkeiten und Grenzen', Farbe und Lack, 95, (10), 715-9, October 1989
    • (1989) Farbe und Lack , vol.95 , Issue.10 , pp. 715-719
    • Böhnke, H.1    Hess, E.2
  • 13
    • 0028740698 scopus 로고
    • Möglichkeiten der UV-Stabilisierung farbloser Holz- Außenanstriche
    • Heinskill J, 'Möglichkeiten der UV-Stabilisierung farbloser Holz-Außenanstriche', Farbe und Lack, 100, (12), 1011-5, 1994
    • (1994) Farbe und Lack , vol.100 , Issue.12 , pp. 1011-1015
    • Heinskill, J.1
  • 14
    • 85039465926 scopus 로고    scopus 로고
    • Challenges and solutions for the 21st century
    • The Paint Research Association, 8 Waldegrave Road, Teddington Middlesex, TW11 8LD, UK
    • Rogez D and M Koehler, 'Challenges and solutions for the 21st century', Paper 24, Second Woodcoatings Congress, The Paint Research Association, 8 Waldegrave Road, Teddington Middlesex, TW11 8LD, UK, 2000
    • (2000) Paper 24, Second Woodcoatings Congress
    • Rogez, D.1    Koehler, M.2
  • 15
    • 0006452325 scopus 로고
    • Seasonal effects on the atmospheric corrosion of spruce micro-sections
    • Raczkowski J, 'Seasonal effects on the atmospheric corrosion of spruce micro-sections', Holz Roh-Werkst, 38, 231-4, 1980
    • (1980) Holz Roh-Werkst , vol.38 , pp. 231-234
    • Raczkowski, J.1
  • 16
    • 9644269586 scopus 로고
    • The international research group on wood preservation, Document No IRG/WP/3289, IRG Secretariat, Sweden
    • Banks W B and P D Evans, 'The degradation of wood surfaces by water', The international research group on wood preservation, Document No IRG/WP/3289, IRG Secretariat, Sweden, 1984
    • (1984) The Degradation of Wood Surfaces by Water
    • Banks, W.B.1    Evans, P.D.2
  • 17
    • 0000133246 scopus 로고
    • Degradation of wood surfaces by water. Changes in mechanical properties of the thin wood strips
    • Evans P D and W B Banks, 'Degradation of wood surfaces by water. Changes in mechanical properties of the thin wood strips', Holz als Roh-und Werkstoff, 46, (11), 427-35, 1988
    • (1988) Holz als Roh-und Werkstoff , vol.46 , Issue.11 , pp. 427-435
    • Evans, P.D.1    Banks, W.B.2
  • 18
    • 84905989337 scopus 로고
    • Degradation of wood surfaces by water. Weight losses and changes in ultrastructural and chemical composition
    • Evans P D and W B Banks, 'Degradation of wood surfaces by water. Weight losses and changes in ultrastructural and chemical composition', Holz als Roh-und Werkstoff, 48, (3), 159-63, 1990
    • (1990) Holz als Roh-und Werkstoff , vol.48 , Issue.3 , pp. 159-163
    • Evans, P.D.1    Banks, W.B.2
  • 19
    • 85039484647 scopus 로고
    • Assessment of wood photodegradation by microtensile testing
    • Paper presented, Tampere, Finland, 6th to 12th August
    • Derbyshire H, E R Miller, J Sell and H Turkulin, 'Assessment of wood photodegradation by microtensile testing', Paper presented at the XX IUFRO World Congress, Tampere, Finland, 6th to 12th August 1995
    • (1995) XX IUFRO World Congress
    • Derbyshire, H.1    Miller, E.R.2    Sell, J.3    Turkulin, H.4
  • 20
    • 65749312825 scopus 로고
    • Investigations into the photodegradation of wood using microtensile testing. Part 1: The application of microtensile testing to measurement of photodegradation rates
    • Derbyshire H, E R Miller and H Turkulin, 'Investigations into the photodegradation of wood using microtensile testing. Part 1: The application of microtensile testing to measurement of photodegradation rates', Holz als Roh-und Werkstoff, 53, (5), 339-45, 1995
    • (1995) Holz als Roh-und Werkstoff , vol.53 , Issue.5 , pp. 339-345
    • Derbyshire, H.1    Miller, E.R.2    Turkulin, H.3
  • 21
    • 0002157223 scopus 로고    scopus 로고
    • Investigations into the photodegradation of wood using microtensile testing. Part 2: An investigation of the changes in tensile strength of different softwood species during natural weathering
    • Derbyshire H, E R Miller and H Turkulin, 'Investigations into the photodegradation of wood using microtensile testing. Part 2: An investigation of the changes in tensile strength of different softwood species during natural weathering', Holz als Roh-und Werkstoff, 54, (1), 1-6, 1996
    • (1996) Holz als Roh-und Werkstoff , vol.54 , Issue.1 , pp. 1-6
    • Derbyshire, H.1    Miller, E.R.2    Turkulin, H.3
  • 23
    • 0036555303 scopus 로고    scopus 로고
    • Investigations into the photodegradation of wood using microtensile testing, Part 4: Tensile properties and fractography of weathered wood
    • Turkulin H and J Sell,' Investigations into the photodegradation of wood using microtensile testing, Part 4:Tensile properties and fractography of weathered wood', Holz als Roh-und Werkstoff, 60, 96-105, 2002
    • (2002) Holz als Roh-und Werkstoff , vol.60 , pp. 96-105
    • Turkulin, H.1    Sell, J.2
  • 24
    • 85039483622 scopus 로고    scopus 로고
    • Challenges and solutions for the 21 st century
    • The Paint Research Association, 8 Waldegrave Road, Teddington Middlesex, TW11 8LD, UK
    • Kiguchi M, P Evans, J Eksted and S Williams, Challenges and solutions for the 21 st century', Paper 23, Second Woodcoatings Congress, The Paint Research Association, 8 Waldegrave Road, Teddington Middlesex, TW11 8LD, UK, 2000
    • (2000) Paper 23, Second Woodcoatings Congress
    • Kiguchi, M.1    Evans, P.2    Eksted, J.3    Williams, S.4
  • 25
    • 0000276283 scopus 로고
    • Tensile strength behaviour as a function of cellulose in wood
    • Ifju G, 'Tensile strength behaviour as a function of cellulose in wood', For Prod J, 21, (8), 366-72, 1964
    • (1964) For Prod J , vol.21 , Issue.8 , pp. 366-372
    • Ifju, G.1
  • 26
    • 0012448447 scopus 로고
    • Measuring penetration of light into wood by detection of photoinduced free radicals
    • Hon D N-S and G Ifju, 'Measuring penetration of light into wood by detection of photoinduced free radicals', Wood Science, 11, (2), 1978
    • (1978) Wood Science , vol.11 , Issue.2
    • Hon, D.N.-S.1    Ifju, G.2
  • 27
    • 0011197564 scopus 로고
    • FT-IR studies of weathering effects in western red cedar and southern pine
    • 7th to 8th November, Rotorua, New Zealand
    • Horn B A, J Qiu, N L Owen and W C Feist, 'FT-IR studies of weathering effects in western red cedar and southern pine', Chemical Modification of Lignocellulosics, FRI Bull, 176, 7th to 8th November, Rotorua, New Zealand, 1992
    • (1992) Chemical Modification of Lignocellulosics, FRI Bull , pp. 176
    • Horn, B.A.1    Qiu, J.2    Owen, N.L.3    Feist, W.C.4
  • 29
    • 0011197564 scopus 로고
    • FT-IR studies of weathering effects in western red cedar and southern pine
    • 7th to 8th November, Rotorua, New Zealand, New Zealand Forest Research Institute
    • Horn B A, J Qiu J, N L Owen N.L., and W C Feist W C, 'FT-IR studies of weathering effects in western red cedar and southern pine'. Chemical Modification of Lignocellulosics. FRI Bull, 67-76, 176, 7th to 8th November, Rotorua, New Zealand, New Zealand Forest Research Institute, 1992
    • (1992) Chemical Modification of Lignocellulosics. FRI Bull , pp. 67-76
    • Horn, B.A.1    Qiu, J.J.2    Owen, N.L.3    Feist, W.C.4
  • 30
    • 0036555303 scopus 로고    scopus 로고
    • Investigations into the photodegradation of wood using microtensile testing. Part 4: Tensile properties and fractography of weathered wood
    • Turkulin H and J Sell, 'Investigations into the photodegradation of wood using microtensile testing. Part 4: Tensile properties and fractography of weathered wood', Holz als Roh-und Werkstoff, 60, (2), 96-105, 2002
    • (2002) Holz als Roh-und Werkstoff , vol.60 , Issue.2 , pp. 96-105
    • Turkulin, H.1    Sell, J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.