-
2
-
-
33744990376
-
A Polymer Electrolyte Fuel Cell Life Test: 3 Years of Continuous Operation
-
Cleghorn, S. J. C., Mayfield, D. K., Moore, D. A., Moore, J. C., Rusch, G., Sherman, T. W., Sisofo, N. T., and Beuscher, U., 2006, "A Polymer Electrolyte Fuel Cell Life Test: 3 Years of Continuous Operation," J. Power Sources, 158, pp. 446-454.
-
(2006)
J. Power Sources
, vol.158
, pp. 446-454
-
-
Cleghorn, S. J. C.1
Mayfield, D. K.2
Moore, D. A.3
Moore, J. C.4
Rusch, G.5
Sherman, T. W.6
Sisofo, N. T.7
Beuscher, U.8
-
3
-
-
0029246672
-
Low Platinum Loading Electrodes for Polymer Electrolyte Fuel Cells Fabricated Using Thermoplastic Ionomers
-
Wilson, M. S., Valerio, J. A., and Gottesfeld, S., 1995, "Low Platinum Loading Electrodes for Polymer Electrolyte Fuel Cells Fabricated Using Thermoplastic Ionomers," Electrochim. Acta, 40, pp. 355-363.
-
(1995)
Electrochim. Acta
, vol.40
, pp. 355-363
-
-
Wilson, M. S.1
Valerio, J. A.2
Gottesfeld, S.3
-
4
-
-
0000069747
-
Performance and Endurance of a PEMFC Operated with Synthetic Reformate Gas Feed
-
Sishtla, C., Koncar, G., Platon, R., Gamburzev, S., Appleby, A. J., and Velev, O., 1998, "Performance and Endurance of a PEMFC Operated with Synthetic Reformate Gas Feed," J. Power Sources, 71, pp. 249-255.
-
(1998)
J. Power Sources
, vol.71
, pp. 249-255
-
-
Sishtla, C.1
Koncar, G.2
Platon, R.3
Gamburzev, S.4
Appleby, A. J.5
Velev, O.6
-
5
-
-
0033889730
-
Development of High Performance PEFC Module Operated by Reformate Gas
-
Isono, T., Suzuki, S., Kaneko, M., Akiyama, Y., and Yonezu, I., 2000, "Development of High Performance PEFC Module Operated by Reformate Gas," J. Power Sources, 86, pp. 269-273.
-
(2000)
J. Power Sources
, vol.86
, pp. 269-273
-
-
Isono, T.1
Suzuki, S.2
Kaneko, M.3
Akiyama, Y.4
Yonezu, I.5
-
6
-
-
0012829283
-
Membrane Durability in PEM Fuel Cells
-
Liu, W., Ruth, K., and Rusch, G., 2001, "Membrane Durability in PEM Fuel Cells," J. New Mater. Electrochem. Syst., 4, pp. 227-231.
-
(2001)
J. New Mater. Electrochem. Syst
, vol.4
, pp. 227-231
-
-
Liu, W.1
Ruth, K.2
Rusch, G.3
-
7
-
-
12744279500
-
Durability of PEFCs at High Humidity Conditions
-
Xie, J., Wood, D. L., III, Wayne, D. M., Zawodzinski, T. A., Atanassov, P., and Borup, R. L., 2005, "Durability of PEFCs at High Humidity Conditions," J. Electrochem. Soc., 152, pp. A104-A113.
-
(2005)
J. Electrochem. Soc
, vol.152
, pp. A104-A113
-
-
Xie, J.1
Wood, D. L.2
Wayne, D. M.3
Zawodzinski, T. A.4
Atanassov, P.5
Borup, R. L.6
-
8
-
-
1542378759
-
Aging Mechanism and Lifetime of PEFC and DMFC
-
Knight, S. D., Colbow, K. M., St-Pierre, J., and Wilkinson, D. P., 2004, "Aging Mechanism and Lifetime of PEFC and DMFC," J. Power Sources, 127, pp. 127-134.
-
(2004)
J. Power Sources
, vol.127
, pp. 127-134
-
-
Knight, S. D.1
Colbow, K. M.2
St-Pierre, J.3
Wilkinson, D. P.4
-
9
-
-
51449109289
-
-
Salt Lake City, Utah, Oct 20-24
-
Endoh, E., Terazono, S., and Widjaja, H., 2002, Abstract 89, The Electrochemical Society Meeting Abstracts, Vol. 2002-2, Salt Lake City, Utah, Oct 20-24.
-
(2002)
Abstract 89, The Electrochemical Society Meeting Abstracts
, vol.2002-2
-
-
Endoh, E.1
Terazono, S.2
Widjaja, H.3
-
10
-
-
34047180439
-
Investigation of Catalyst Degradation After Single Cell Life Tests
-
Tada, T., Toshima, N., Yamamoto, Y., and Inoue, M., 2007, "Investigation of Catalyst Degradation After Single Cell Life Tests," Electrochemistry (Toyko, Jpn.), 75, pp. 221-230.
-
(2007)
Electrochemistry (Toyko, Jpn.)
, vol.75
, pp. 221-230
-
-
Tada, T.1
Toshima, N.2
Yamamoto, Y.3
Inoue, M.4
-
11
-
-
33845271880
-
Accelerated Testing and Lifetime Modeling for the Development of Durable Fuel Cell MEAs
-
Pierpont, D., Hicks, M., Watschke, T., and Turner, P., 2006, "Accelerated Testing and Lifetime Modeling for the Development of Durable Fuel Cell MEAs," ECS Trans., 1, pp. 229-237.
-
(2006)
ECS Trans
, vol.1
, pp. 229-237
-
-
Pierpont, D.1
Hicks, M.2
Watschke, T.3
Turner, P.4
-
12
-
-
45249116376
-
DOE Fuel Cell Program: Durability Technical Targets and Testing Protocols
-
Garland, N. L., Benjamin, T. G., and Kopasz, J. P., 2007, "DOE Fuel Cell Program: Durability Technical Targets and Testing Protocols," ECS Trans., 11, pp. 923-931.
-
(2007)
ECS Trans
, vol.11
, pp. 923-931
-
-
Garland, N. L.1
Benjamin, T. G.2
Kopasz, J. P.3
-
13
-
-
60649121973
-
Study of MEA Degradation in Operating PEM Fuel Cells
-
Lucern, Switzerland, July 4-8
-
Escribano, S., Morin, A., Solan, S., Sommacal, B., Capron, P., Rougeaux, I., and Gebel, G., 2005, "Study of MEA Degradation in Operating PEM Fuel Cells," 3rd European PEFC Forum, Lucern, Switzerland, July 4-8.
-
(2005)
3rd European PEFC Forum
-
-
Escribano, S.1
Morin, A.2
Solan, S.3
Sommacal, B.4
Capron, P.5
Rougeaux, I.6
Gebel, G.7
-
14
-
-
33845273519
-
Durable PEM Fuel Cell Electrode Materials: Requirements and Benchmarking Methodologies
-
Makharia, R., Kocha, S. S., Yu, P. T., Sweikart, M. A., Gu, W., Wagner, F. T., and Gasteiger, H. A., 2006, "Durable PEM Fuel Cell Electrode Materials: Requirements and Benchmarking Methodologies," ECS Trans., 1, pp. 3-18.
-
(2006)
ECS Trans
, vol.1
, pp. 3-18
-
-
Makharia, R.1
Kocha, S. S.2
Yu, P. T.3
Sweikart, M. A.4
Gu, W.5
Wagner, F. T.6
Gasteiger, H. A.7
-
15
-
-
3042754028
-
Degradation Study of MEA for PEMFCs under Low Humidity Conditions
-
Endoh, E., Terazono, S., Widjaja, H., and Takimoto, Y., 2004, "Degradation Study of MEA for PEMFCs under Low Humidity Conditions," Electrochem. Solid-State Lett., 7, pp. A209-A211.
-
(2004)
Electrochem. Solid-State Lett
, vol.7
, pp. A209-A211
-
-
Endoh, E.1
Terazono, S.2
Widjaja, H.3
Takimoto, Y.4
-
16
-
-
45249100418
-
Preferential Thinning Behaviours of the Anode Side of the PEM Under Durability Test
-
Shim, J. Y., Tsushima, S., and Hirai, S., 2007, "Preferential Thinning Behaviours of the Anode Side of the PEM Under Durability Test," ECS Trans., 11, pp. 1151-1156.
-
(2007)
ECS Trans
, vol.11
, pp. 1151-1156
-
-
Shim, J. Y.1
Tsushima, S.2
Hirai, S.3
-
17
-
-
45249091211
-
Analysis ofMembrane Degradation Behaviour During OCV Hold Test
-
Ohma, A., Yamamoto, S., and Shinohara, K., 2007, "Analysis ofMembrane Degradation Behaviour During OCV Hold Test," ECS Trans., 11, pp. 1181-1192.
-
(2007)
ECS Trans
, vol.11
, pp. 1181-1192
-
-
Ohma, A.1
Yamamoto, S.2
Shinohara, K.3
-
18
-
-
34247636667
-
Investigation of the Ag-SiO2/Sulfonated Poly(Biphenyl Ether Sulfone) Composite Membranes for Fuel Cell
-
Xing, D., Zhang, H., Wang, L., Zhai, Y., and Yi, B., 2007, "Investigation of the Ag-SiO2/Sulfonated Poly(Biphenyl Ether Sulfone) Composite Membranes for Fuel Cell," J. Membr. Sci., 296, pp. 9-14.
-
(2007)
J. Membr. Sci
, vol.296
, pp. 9-14
-
-
Xing, D.1
Zhang, H.2
Wang, L.3
Zhai, Y.4
Yi, B.5
-
19
-
-
33846960700
-
Degradation Rates of PEM Fuel Cells Running at Open Circuit Voltage
-
Aarhaug, T. A., and Svensson, A. M., 2006, "Degradation Rates of PEM Fuel Cells Running at Open Circuit Voltage," ECS Trans., 3, pp. 775-780.
-
(2006)
ECS Trans
, vol.3
, pp. 775-780
-
-
Aarhaug, T. A.1
Svensson, A. M.2
-
20
-
-
40549124041
-
Reinforced Membrane Durability in Proton Exchange Membrane Fuel Cell Stacks for Automotive Applications
-
Ralph, T. R., Barnwell, D. E., Bouwman, P. J., Hodgkinson, A. J., Petch, M. I., and Pollington, M., 2008, "Reinforced Membrane Durability in Proton Exchange Membrane Fuel Cell Stacks for Automotive Applications," J. Electrochem. Soc., 155, pp. B411-B422.
-
(2008)
J. Electrochem. Soc
, vol.155
, pp. B411-B422
-
-
Ralph, T. R.1
Barnwell, D. E.2
Bouwman, P. J.3
Hodgkinson, A. J.4
Petch, M. I.5
Pollington, M.6
-
21
-
-
33845603536
-
The Stability of Pt/C Catalyst in H3PO4/PBI PEMFC During High Temperature Life Test
-
Zhai, Y., Zhang, H., Xing, D., and Shao, Z., 2007, "The Stability of Pt/C Catalyst in H3PO4/PBI PEMFC During High Temperature Life Test," J. Power Sources, 164, pp. 126-133.
-
(2007)
J. Power Sources
, vol.164
, pp. 126-133
-
-
Zhai, Y.1
Zhang, H.2
Xing, D.3
Shao, Z.4
-
22
-
-
34547235518
-
Single PEM Fuel Cell Design and Validation for High Temperature MEA Testing and Diagnosis up to 300_C
-
Tang, Y., Zhang, J., Song, C., and Zhang, J., 2007, "Single PEM Fuel Cell Design and Validation for High Temperature MEA Testing and Diagnosis up to 300_C," Electrochem. Solid-State Lett., 10, pp. B142-B146.
-
(2007)
Electrochem. Solid-State Lett
, vol.10
, pp. B142-B146
-
-
Tang, Y.1
Zhang, J.2
Song, C.3
Zhang, J.4
-
23
-
-
85150840508
-
High Temperature PEM Fuel Cell Catalysts and Catalyst Layers
-
J. Zhang, ed., Springer-Verlag, London, Chap. 18
-
Song, C., Hui, R., and Zhang, J., 2007, "High Temperature PEM Fuel Cell Catalysts and Catalyst Layers," PEM Fuel Cell Electrocatalysts and Catalyst Layers, J. Zhang, ed., Springer-Verlag, London, Chap. 18.
-
(2007)
PEM Fuel Cell Electrocatalysts and Catalyst Layers
-
-
Song, C.1
Hui, R.2
Zhang, J.3
-
24
-
-
22244432179
-
Propane Fuel Cells Using Phosphoric-Acid-Doped Polybenzimidazole Membranes
-
Cheng, C., Luo, J., Chuang, K. T., and Sanger, A. R., 2005, "Propane Fuel Cells Using Phosphoric-Acid-Doped Polybenzimidazole Membranes" J. Phys. Chem. B, 109, pp. 13036-13042.
-
(2005)
J. Phys. Chem. B
, vol.109
, pp. 13036-13042
-
-
Cheng, C.1
Luo, J.2
Chuang, K. T.3
Sanger, A. R.4
-
25
-
-
2342556324
-
Fourier Transform Infra-Red Spectroscopy on the Thermo-Oxidative Degradation of Polybenzimidazole and of a Polybenzimidazole/Polyetherimide Blend
-
Musto, P., Karasz, F. E., and MacKnight, W. J., 1993, "Fourier Transform Infra-Red Spectroscopy on the Thermo-Oxidative Degradation of Polybenzimidazole and of a Polybenzimidazole/Polyetherimide Blend," Polymer, 34, pp. 2934-2945.
-
(1993)
Polymer
, vol.34
, pp. 2934-2945
-
-
Musto, P.1
Karasz, F. E.2
MacKnight, W. J.3
-
26
-
-
84892028939
-
Durability of Gas-Diffusion and Microporous Layers
-
Buchi, F. N., Inaba, M., and Schmidt, T. J., eds., Springer, New York
-
Wood, D. L., III and Borup, R. L., 2009, "Durability of Gas-Diffusion and Microporous Layers," Polymer Electrolyte Fuel Cell Durability, Buchi, F. N., Inaba, M., and Schmidt, T. J., eds., Springer, New York.
-
(2009)
Polymer Electrolyte Fuel Cell Durability
-
-
Wood, D. L.1
Borup, R. L.2
|