Volumn 3, Issue 3, 1985, Pages 604-611

Residual Stress Characteristics of 13 Cr Cast Steel Weldments Prepared with Austenitic Weld Metal

Author keywords

13Cr cast steel; 3 D residual stress distribution; Both ends fixed bar specimen; Residual stress; Transient thermal stress

Indexed keywords


EID: 84998225275     PISSN: 02884771     EISSN: None     Source Type: Journal    
DOI: 10.2207/qjjws.3.604     Document Type: Article
Times cited : (8)

References (8)
  • 1
    • 84998291870 scopus 로고
    • 48-5 (1979), 322
    • (1979) , vol.48 , Issue.5 , pp. 322
  • 2
    • 84998484166 scopus 로고
    • 48-7 (1979), 518
    • (1979) , vol.48 , Issue.7 , pp. 518
  • 3
    • 84998303291 scopus 로고
    • 2-1 (1984), 83
    • (1984) , vol.2 , Issue.1 , pp. 83
  • 4
    • 84998303345 scopus 로고
    • 2-2 (1984), 150
    • (1984) , vol.2 , Issue.2 , pp. 150
  • 5
    • 84998499717 scopus 로고
    • 52-3 (1983), 314
    • (1983) , vol.52 , Issue.3 , pp. 314
  • 6
    • 84998329789 scopus 로고
    • (1985), 228
    • (1985) , pp. 228
  • 7
    • 84998219440 scopus 로고
    • 49-12 (1980), 845
    • (1980) , vol.49 , Issue.12 , pp. 845
  • 8
    • 84998499698 scopus 로고
    • 52-2 (1983), 110
    • (1983) , vol.52 , Issue.2 , pp. 110


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.