Volumn 26, Issue 2, 2009, Pages 385-396

A Laboratory Column Investigation for the Treatment of Cr(VI) with Zero-Valent Iron

Author keywords

chromium (VI); groundwater; permeable reactive barrier; zero valent iron

Indexed keywords


EID: 84995286908     PISSN: 10928758     EISSN: 15579018     Source Type: Journal    
DOI: 10.1089/ees.2007.0089     Document Type: Article
Times cited : (7)

References (49)
  • 1
    • 0036469556 scopus 로고    scopus 로고
    • Kinetics of nitrate, nitrite and Cr(VI) reduction by iron metal
    • Alowitz, M. J., and Scherer, M. M. (2002). Kinetics of nitrate, nitrite and Cr(VI) reduction by iron metal. Environ. Sci. Technol. 36, 299.
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 299
    • Alowitz, M.J.1    Scherer, M.M.2
  • 2
    • 0034307429 scopus 로고    scopus 로고
    • Immobilization of chromate from coal fly ash leachate using an attenuating barrier containing zero valent iron
    • Astrup, T., Stipp, S. L. S., and Christensen, T. H. (2000). Immobilization of chromate from coal fly ash leachate using an attenuating barrier containing zero valent iron. Environ. Sci. Technol. 34, 4163.
    • (2000) Environ. Sci. Technol. , vol.34 , pp. 4163
    • Astrup, T.1    Stipp, S.L.S.2    Christensen, T.H.3
  • 3
    • 0028181974 scopus 로고
    • Batch experiments characterizing the reduction of chromium(VI) using suboxic material from a mildly reducing sand and gravel aquifer
    • Anderson, L. D., Kent, D. B., and Davis, J. A. (1994). Batch experiments characterizing the reduction of chromium(VI) using suboxic material from a mildly reducing sand and gravel aquifer. Environ. Sci. Technol. 28, 178.
    • (1994) Environ. Sci. Technol. , vol.28 , pp. 178
    • Anderson, L.D.1    Kent, D.B.2    Davis, J.A.3
  • 4
    • 85018928998 scopus 로고    scopus 로고
    • Design, Construction, and Monitoring of the Permeable Reactive Barrier in Area 5 at Dover Air Force Base
    • Tyndall AFB, Florida. March 31
    • BATTELLE. (2000). Design, Construction, and Monitoring of the Permeable Reactive Barrier in Area 5 at Dover Air Force Base. Final Report Prepared for Air Force Research Laboratory, Tyndall AFB, Florida. March 31.
    • (2000) Final Report Prepared for Air Force Research Laboratory
    • BATTELLE1
  • 5
    • 0027430548 scopus 로고
    • X-ray absorption spectroscopy investigation of surface redox transformations of thallium and chromium on colloidal mineral oxides. Geochim. Cosmochim
    • Bidoglio, G., Gibson, P. N., O'Gorman, M. and Roberts, K. J. (1993). X-ray absorption spectroscopy investigation of surface redox transformations of thallium and chromium on colloidal mineral oxides. Geochim. Cosmochim. Acta 57, 2389.
    • (1993) Acta , vol.57 , pp. 2389
    • Bidoglio, G.1    Gibson, P.N.2    O'Gorman, M.3    Roberts, K.J.4
  • 6
    • 0031443113 scopus 로고    scopus 로고
    • In-situ remediation of Cr(VI) contaminated groundwater using permeable reactive barriers: Laboratory studies
    • Blowes, D. W., Ptacek, J. G. and Jambor, J. L. (1997). In-situ remediation of Cr(VI) contaminated groundwater using permeable reactive barriers: Laboratory studies. Environ. Sci. Technol. 31, 3348.
    • (1997) Environ. Sci. Technol. , vol.31 , pp. 3348
    • Blowes, D.W.1    Ptacek, J.G.2    Jambor, J.L.3
  • 7
    • 0032527837 scopus 로고    scopus 로고
    • Influence of organic ligands on chromium(VI) reduction by iron(II)
    • Buerge, I. J., and Hug, S. J. (1998). Influence of organic ligands on chromium(VI) reduction by iron(II). Environ. Sci. Technol. 32, 2092.
    • (1998) Environ. Sci. Technol. , vol.32 , pp. 2092
    • Buerge, I.J.1    Hug, S.J.2
  • 8
    • 0023821737 scopus 로고
    • Chromate removal from aqueous wastes by reduction with ferrous iron
    • Eary, L. E., and Rai, D. (1988). Chromate removal from aqueous wastes by reduction with ferrous iron. Environ. Sci. Technol. 22, 972.
    • (1988) Environ. Sci. Technol. , vol.22 , pp. 972
    • Eary, L.E.1    Rai, D.2
  • 9
    • 0000390524 scopus 로고
    • Kinetics of chromate reduction by ferrous ions derived from hematite and biotite at 25° C
    • Eary, L. E., and Rai, D. (1989). Kinetics of chromate reduction by ferrous ions derived from hematite and biotite at 25° C. Am. J. Sci. 289, 180.
    • (1989) Am. J. Sci. , vol.289 , pp. 180
    • Eary, L.E.1    Rai, D.2
  • 10
    • 0344897653 scopus 로고    scopus 로고
    • Effect of Fe0 quantity on the efficiency of integrated microbial-Feo treatment processes
    • Fernandez-Sanchez, J. M., Sawvel, E. J., and Alvarez, P. P. J. (2004). Effect of Fe0 quantity on the efficiency of integrated microbial-Feo treatment processes. Chemosphere 54, 823.
    • (2004) Chemosphere , vol.54 , pp. 823
    • Fernandez-Sanchez, J.M.1    Sawvel, E.J.2    Alvarez, P.P.J.3
  • 11
    • 0037114999 scopus 로고    scopus 로고
    • Formation of ferrihyrite and associated iron corrosion products in permeable reactive barriers of zero-valent iron
    • Furukawa, Y., Kim, J., Watkins, J., and Wilkin, R. T. (2002). Formation of ferrihyrite and associated iron corrosion products in permeable reactive barriers of zero-valent iron. Environ. Sci. Technol. 36, 5469.
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 5469
    • Furukawa, Y.1    Kim, J.2    Watkins, J.3    Wilkin, R.T.4
  • 12
    • 0036528211 scopus 로고    scopus 로고
    • Degradation of TCE, Cr(VI), sulfate and nitrate mixtures by granular iron in flow through columns under different microbial conditions
    • Gandhi, S., Oh, B., Schnoor, J. L., and Alvarez, P. J. J. (2002) Degradation of TCE, Cr(VI), sulfate and nitrate mixtures by granular iron in flow through columns under different microbial conditions. Water Res. 36, 1973.
    • (2002) Water Res. , vol.36 , pp. 1973
    • Gandhi, S.1    Oh, B.2    Schnoor, J.L.3    Alvarez, P.J.J.4
  • 14
    • 0028535136 scopus 로고
    • Enhanced degradation of halogenated aliphatics by zero-valent iron
    • Gillham, R. W., and O'Hannesin, S. F. (1994). Enhanced degradation of halogenated aliphatics by zero-valent iron. Ground Water, 32, 958.
    • (1994) Ground Water , vol.32 , pp. 958
    • Gillham, R.W.1    O'Hannesin, S.F.2
  • 15
    • 0019998559 scopus 로고
    • The kinetics of hexavalent chromium reduction by metallic iron
    • Gould, J. P. (1982). The kinetics of hexavalent chromium reduction by metallic iron. Water Resources Res. 16, 871.
    • (1982) Water Resources Res. , vol.16 , pp. 871
    • Gould, J.P.1
  • 16
    • 0032211286 scopus 로고    scopus 로고
    • Reductive precipitation of uranium(VI) by zero-valent iron
    • Gu, B., Liang, L., Dickey, M. J., Yin, X., and Dai, S. (1998). Reductive precipitation of uranium(VI) by zero-valent iron. Environ. Sci. Technol. 32, 3366.
    • (1998) Environ. Sci. Technol. , vol.32 , pp. 3366
    • Gu, B.1    Liang, L.2    Dickey, M.J.3    Yin, X.4    Dai, S.5
  • 17
    • 18344362135 scopus 로고    scopus 로고
    • Preparation and characterization of a new class of starch-stabilized bimetallic nanoparticles for degradation of chlorinated hydrocarbons in water
    • He, F., and Zhao, D. (2005). Preparation and characterization of a new class of starch-stabilized bimetallic nanoparticles for degradation of chlorinated hydrocarbons in water. Environ. Sci. Technol. 39, 3314.
    • (2005) Environ. Sci. Technol. , vol.39 , pp. 3314
    • He, F.1    Zhao, D.2
  • 18
    • 33645243131 scopus 로고    scopus 로고
    • PRB-4. Washington, D. C.: Interstate Technology & Regulatory Council, Permeable Reactive Barriers Team. www.itrcweb.org
    • Interstate Technology & Regulatory Council). (2005). Permeable Reactive Barriers: Lessons Learned/New Directions. PRB-4. Washington, D. C.: Interstate Technology & Regulatory Council, Permeable Reactive Barriers Team. www.itrcweb.org
    • (2005) Permeable Reactive Barriers: Lessons Learned/New Directions.
  • 19
    • 0142088788 scopus 로고    scopus 로고
    • Preferential flow path development and its influence on long term PRB performance: column study
    • Kamolpornwijit, W., Liang, L., West, O. R., Moline, G. R., and Sullivan, A. B. (2003). Preferential flow path development and its influence on long term PRB performance: column study. J. Contaminant Hydrol. 66, 161.
    • (2003) J. Contaminant Hydrol. , vol.66 , pp. 161
    • Kamolpornwijit, W.1    Liang, L.2    West, O.R.3    Moline, G.R.4    Sullivan, A.B.5
  • 20
    • 7444252227 scopus 로고    scopus 로고
    • Identification and quantification of mineral precipitation in a Fe0 fillings from a column study
    • Kamolpornwijit, W., Liang, L., Moline, G. R., Hart, T. R., and West, O. (2004). Identification and quantification of mineral precipitation in a Fe0 fillings from a column study. Environ. Sci. Technol. 38, 5757.
    • (2004) Environ. Sci. Technol. , vol.38 , pp. 5757
    • Kamolpornwijit, W.1    Liang, L.2    Moline, G.R.3    Hart, T.R.4    West, O.5
  • 21
    • 4944231549 scopus 로고    scopus 로고
    • Zero-valent iron removal rates of aqueous Cr(VI) measured under flowing conditions
    • Kaplan, D. I., and Gilmore, T. J. (2004). Zero-valent iron removal rates of aqueous Cr(VI) measured under flowing conditions. Water Air Soil Pollut. 155, 21.
    • (2004) Water Air Soil Pollut. , vol.155 , pp. 21
    • Kaplan, D.I.1    Gilmore, T.J.2
  • 22
    • 0034007527 scopus 로고    scopus 로고
    • Copper, chromium, and arsenic adsorption and equilibrium modeling in an iron-oxide-coated sand, background electrolyte system
    • Khaodhiar S., Azizian M. F., Osathaphan, K., and Nelson, P. O. (2000). Copper, chromium, and arsenic adsorption and equilibrium modeling in an iron-oxide-coated sand, background electrolyte system. Water Air Soil Pollut. 119, 105.
    • (2000) Water Air Soil Pollut. , vol.119 , pp. 105
    • Khaodhiar, S.1    Azizian, M.F.2    Osathaphan, K.3    Nelson, P.O.4
  • 24
    • 33947331071 scopus 로고    scopus 로고
    • Size effect in reactivity of copper nanoparticles to carbon tetrachloride degradation
    • Liou, Y. H., Lo, S. L., and Lin, C. S. (2007). Size effect in reactivity of copper nanoparticles to carbon tetrachloride degradation. Water Res. 41, 1705.
    • (2007) Water Res. , vol.41 , pp. 1705
    • Liou, Y.H.1    Lo, S.L.2    Lin, C.S.3
  • 25
    • 31744450592 scopus 로고    scopus 로고
    • Hardness and carbonate effects on the reactivity of zero-valent iron for Cr(VI) removal
    • Lo, I. M. C., Lam, C. S. C., and Lai, K. J. K. (2006). Hardness and carbonate effects on the reactivity of zero-valent iron for Cr(VI) removal. Water Res. 40, 595.
    • (2006) Water Res. , vol.40 , pp. 595
    • Lo, I.M.C.1    Lam, C.S.C.2    Lai, K.J.K.3
  • 26
    • 0032888413 scopus 로고    scopus 로고
    • Mineral precipitation and porosity losses in granular iron columns
    • Mackenzie, P. D., Horney, D. P., and Sivavec, T. M., (1999). Mineral precipitation and porosity losses in granular iron columns. J. Hazard. Mater. 68, 1.
    • (1999) J. Hazard. Mater. , vol.68 , pp. 1
    • Mackenzie, P.D.1    Horney, D.P.2    Sivavec, T.M.3
  • 27
    • 0035476788 scopus 로고    scopus 로고
    • Kinetics of soluble chromium removal from contaminated water by zerovalent iron media: Corrosion inhibition and passive oxide effects
    • Melitas, N., Chuffe-Moscoso, O., and Farrel, J. (2001). Kinetics of soluble chromium removal from contaminated water by zerovalent iron media: Corrosion inhibition and passive oxide effects. Environ. Sci. Technol. 35, 3948.
    • (2001) Environ. Sci. Technol. , vol.35 , pp. 3948
    • Melitas, N.1    Chuffe-Moscoso, O.2    Farrel, J.3
  • 28
    • 1842845753 scopus 로고    scopus 로고
    • Understanding chromate reduction with corroding iron media using tafel analysis and electrochemical impedance spectroscopy
    • Melitas, N., and Farrel, J. (2002). Understanding chromate reduction with corroding iron media using tafel analysis and electrochemical impedance spectroscopy. Environ. Sci. Technol. 36, 5476.
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 5476
    • Melitas, N.1    Farrel, J.2
  • 29
    • 0035863648 scopus 로고    scopus 로고
    • Uranium precipitation in a permeable reactive barrier by progressive irreversible dissolution of zero-valent iron
    • Morrison, S. J., Metzler, D. R., and Carpenter, C. E. (2001). Uranium precipitation in a permeable reactive barrier by progressive irreversible dissolution of zero-valent iron. Environ. Sci. Technol. 35, 385.
    • (2001) Environ. Sci. Technol. , vol.35 , pp. 385
    • Morrison, S.J.1    Metzler, D.R.2    Carpenter, C.E.3
  • 31
    • 0343157676 scopus 로고    scopus 로고
    • Direct XAFS evidence for heterogeneous redox at the aqueous chromium/magnetite interface. Colloids Surf. A Physiochem. Eng
    • Peterson, M. L., Brown, G. E., Jr., and Parks, G. A. (1996). Direct XAFS evidence for heterogeneous redox at the aqueous chromium/magnetite interface. Colloids Surf. A Physiochem. Eng. Aspects 107, 77.
    • (1996) Aspects , vol.107 , pp. 77
    • Peterson, M.L.1    Brown, G.E.2    Parks, G.A.3
  • 32
    • 0034659922 scopus 로고    scopus 로고
    • Remediation of Cr(VI) and Pb(II) aqueous solutions using supported, nanoscale zero-valent iron
    • Ponder, S. M., Garab, J. G., and Mallouk, T. E. (2000). Remediation of Cr(VI) and Pb(II) aqueous solutions using supported, nanoscale zero-valent iron. Environ. Sci. Technol. 34, 2564.
    • (2000) Environ. Sci. Technol. , vol.34 , pp. 2564
    • Ponder, S.M.1    Garab, J.G.2    Mallouk, T.E.3
  • 33
    • 0029412090 scopus 로고
    • Coupled iron corrosion and chromate reduction: Mechanisms for subsurface remediation
    • Powell, R. M., Puls, R. W., Hightower, S. K., and Sabatini, D. A. (1995). Coupled iron corrosion and chromate reduction: Mechanisms for subsurface remediation. Environ. Sci. Technol. 29, 1913.
    • (1995) Environ. Sci. Technol. , vol.29 , pp. 1913
    • Powell, R.M.1    Puls, R.W.2    Hightower, S.K.3    Sabatini, D.A.4
  • 34
    • 0028042674 scopus 로고
    • Transport and transformation of hexavalent chromium through soils and groundwater
    • Puls, R. W., Clark, D. A., Paul, C. J., and Vardy, J. (1994). Transport and transformation of hexavalent chromium through soils and groundwater. J. Soil Contam. 3, 203.
    • (1994) J. Soil Contam. , vol.3 , pp. 203
    • Puls, R.W.1    Clark, D.A.2    Paul, C.J.3    Vardy, J.4
  • 35
    • 0034477136 scopus 로고    scopus 로고
    • Characterization of corrosion products in the permeable reactive barriers
    • Roh, Y., Lee, S. Y., and Elless, M. P. (2000). Characterization of corrosion products in the permeable reactive barriers. Environ. Geol. 40, 184.
    • (2000) Environ. Geol. , vol.40 , pp. 184
    • Roh, Y.1    Lee, S.Y.2    Elless, M.P.3
  • 36
    • 0035388045 scopus 로고    scopus 로고
    • Mass transport effects on the kinetics of nitrobenzene reduction by iron metal
    • Scherer, M. M., Johnson, K. M., Westall, J. C., and Tratnyek, P. G. (2001). Mass transport effects on the kinetics of nitrobenzene reduction by iron metal. Environ. Sci. Technol. 35, 2104.
    • (2001) Environ. Sci. Technol. , vol.35 , pp. 2104
    • Scherer, M.M.1    Johnson, K.M.2    Westall, J.C.3    Tratnyek, P.G.4
  • 40
    • 0003747480 scopus 로고
    • EPA Groundwater Issue. U. S. Environmental Protection Agency, Office of Research and Development. EPA/540/5–94/505
    • U. S. Environmental Protection Agency. (1994). Natural Attenuation of Hexavalent Chromium in Groundwater and Soils. EPA Groundwater Issue. U. S. Environmental Protection Agency, Office of Research and Development. EPA/540/5–94/505.
    • (1994) Natural Attenuation of Hexavalent Chromium in Groundwater and Soils.
  • 42
    • 85018868455 scopus 로고    scopus 로고
    • An In Situ Permeable Reactive Barrier for the Treatment of Hexavalent Chromium and Trichloroethylene in Ground Water
    • Office of Research and Development. EPA/600/R-99/095a
    • U. S. Environmental Protection Agency. (1999). An In Situ Permeable Reactive Barrier for the Treatment of Hexavalent Chromium and Trichloroethylene in Ground Water: Volume 1: Design and Installation. Office of Research and Development. EPA/600/R-99/095a.
    • (1999) Design and Installation. , vol.1
  • 44
    • 0032599845 scopus 로고    scopus 로고
    • Performance evaluation of a permeable reactive barrier for remediation of dissolved chlorinated solvents in groundwater
    • Vogan, J. L., Focht, R. M., Clark, D. K., and Graham, S. L. (1999). Performance evaluation of a permeable reactive barrier for remediation of dissolved chlorinated solvents in groundwater. J. Hazard. Materials, 68, 97.
    • (1999) J. Hazard. Materials , vol.68 , pp. 97
    • Vogan, J.L.1    Focht, R.M.2    Clark, D.K.3    Graham, S.L.4
  • 45
    • 20744457064 scopus 로고    scopus 로고
    • Chromium-removal processes during ground-water remediation by a zero-valent iron permeable reactive barrier
    • Wilkin, R. T., Su, C., Ford, R. G., and Paul, C. J. (2005). Chromium-removal processes during ground-water remediation by a zero-valent iron permeable reactive barrier. Environ. Sci. Technol. 39, 4599.
    • (2005) Environ. Sci. Technol. , vol.39 , pp. 4599
    • Wilkin, R.T.1    Su, C.2    Ford, R.G.3    Paul, C.J.4
  • 46
    • 0033237832 scopus 로고    scopus 로고
    • Combined zero and first order kinetic model of the degradation of TCE and cis-DCE with commercial iron
    • Wüst, W. F., Köber, R., Schlicker, O., and Dahmke, A. (1999). Combined zero and first order kinetic model of the degradation of TCE and cis-DCE with commercial iron. Environ. Sci. Technol. 33, 4304.
    • (1999) Environ. Sci. Technol. , vol.33 , pp. 4304
    • Wüst, W.F.1    Köber, R.2    Schlicker, O.3    Dahmke, A.4
  • 47
    • 34247107217 scopus 로고    scopus 로고
    • Reduction immobilization of chromate in water and soil using stabilized iron nanoparticles
    • Xu, Y., and Zhao, D. (2007). Reduction immobilization of chromate in water and soil using stabilized iron nanoparticles. Water Res. 41, 2101.
    • (2007) Water Res. , vol.41 , pp. 2101
    • Xu, Y.1    Zhao, D.2
  • 48
    • 0023367537 scopus 로고
    • Chromate adsorption on amorphous iron oxyhydroxide in the presence of major groundwater ions
    • Zachara, J. M., Girvin, D. C., Schmidt, R. L., and Resch, C. T. (1987). Chromate adsorption on amorphous iron oxyhydroxide in the presence of major groundwater ions. Environ. Sci. Technol. 21, 589.
    • (1987) Environ. Sci. Technol. , vol.21 , pp. 589
    • Zachara, J.M.1    Girvin, D.C.2    Schmidt, R.L.3    Resch, C.T.4
  • 49
    • 15844400136 scopus 로고    scopus 로고
    • Effects of Gas Generation and Precipitates on Performance of Fe0 PRBs
    • Zhang, Y., and Gillham, R. W. (2005). Effects of Gas Generation and Precipitates on Performance of Fe0 PRBs. Ground Water 43, 113.
    • (2005) Ground Water , vol.43 , pp. 113
    • Zhang, Y.1    Gillham, R.W.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.