Volumn , Issue , 2015, Pages 335-346

Simultaneous Electrochemical Recovery of Rare Earth Elements and Iron from Magnet Scrap: A Theoretical Analysis

Author keywords

Electrochemical recycling; Electrorefining; NdFeB magnets; Neodymium; REEs

Indexed keywords

DISSOLUTION; ELECTROCHEMISTRY; ENERGY UTILIZATION; IRON SCRAP; MAGNETS; NEODYMIUM; RARE EARTH ELEMENTS; RARE EARTHS; RECOVERY; SCRAP METAL; SCRAP METAL REPROCESSING; SECONDARY RECOVERY; SOLUTIONS;

EID: 84960809554     PISSN: None     EISSN: None     Source Type: Book    
DOI: 10.1016/B978-0-12-802328-0.00022-X     Document Type: Chapter
Times cited : (16)

References (36)
  • 1
    • 85032598693 scopus 로고    scopus 로고
    • Magnetic Properties and Corrosion Resistance of Uncoated and Coated Rare-Earth Based Permanent Magnets (PhD thesis)
    • Ali, A., 2011. Magnetic Properties and Corrosion Resistance of Uncoated and Coated Rare-Earth Based Permanent Magnets (PhD thesis).
    • (2011)
    • Ali, A.1
  • 2
    • 0025867499 scopus 로고
    • An electrochemical investigation of dissolution from Nd-Fe-B magnets in acid solution under cathodic polarization
    • Bala S., Szymura H. An electrochemical investigation of dissolution from Nd-Fe-B magnets in acid solution under cathodic polarization. Corrosion Science 1991, 32(9):953-963.
    • (1991) Corrosion Science , vol.32 , Issue.9 , pp. 953-963
    • Bala, S.1    Szymura, H.2
  • 7
    • 0036568096 scopus 로고    scopus 로고
    • Grain growth effects on the corrosion behavior of nanocrystalline NdFeB magnets
    • El-Moneim A.A., Gebert A., Schneider F., Gutfleisch O., Schultz L. Grain growth effects on the corrosion behavior of nanocrystalline NdFeB magnets. Corrosion Science 2002, 44:1097-1112. 10.1016/S0010-938X(01)00123-8.
    • (2002) Corrosion Science , vol.44 , pp. 1097-1112
    • El-Moneim, A.A.1    Gebert, A.2    Schneider, F.3    Gutfleisch, O.4    Schultz, L.5
  • 8
    • 8344252799 scopus 로고    scopus 로고
    • Passivity and its breakdown of sintered NdFeB-based magnets in chloride containing solution
    • El-Moneim A.A. Passivity and its breakdown of sintered NdFeB-based magnets in chloride containing solution. Corrosion Science 2004, 46:2517-2532. 10.1016/j.corsci.2003.12.002.
    • (2004) Corrosion Science , vol.46 , pp. 2517-2532
    • El-Moneim, A.A.1
  • 10
    • 84957873625 scopus 로고    scopus 로고
    • Critical raw materials for the EU, report of the ad-hoc working group on defining critical raw materials
    • European Commission Critical raw materials for the EU, report of the ad-hoc working group on defining critical raw materials. Eucom 2010, 39(July):1-84. 10.1002/eji.200839120.IL-17-Producing.
    • (2010) Eucom , vol.39 , Issue.JULY , pp. 1-84
  • 11
    • 84960822467 scopus 로고
    • Recovering neodymium from iron-containing grinding swarf by sdding sodium hydroxide, grinding to crude oxide, digesting with acetic acid, evaporating to neodymium acetate crystals, removing ferric acetate, adding hydrofluoric acid, drying
    • Retrieved from
    • Greenberg, B., 1994. Recovering neodymium from iron-containing grinding swarf by sdding sodium hydroxide, grinding to crude oxide, digesting with acetic acid, evaporating to neodymium acetate crystals, removing ferric acetate, adding hydrofluoric acid, drying. Google Patents. Retrieved from: . http://www.google.com/patents/US5362459.
    • (1994) Google Patents
    • Greenberg, B.1
  • 12
    • 79951789569 scopus 로고    scopus 로고
    • Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient
    • Gutfleisch O., Willard M.a., Brück E., Chen C.H., Sankar S.G., Liu J.P. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient. Advanced Materials 2011, 23:821-842. 10.1002/adma.201002180.
    • (2011) Advanced Materials , vol.23 , pp. 821-842
    • Gutfleisch, O.1    Willard, M.2    Brück, E.3    Chen, C.H.4    Sankar, S.G.5    Liu, J.P.6
  • 13
    • 84914126694 scopus 로고    scopus 로고
    • RSC advances from NdFeB magnets towards the rare-earth oxides: a recycling process consuming only oxalic acid
    • Hoogerstraete T.V., Blanpain B., Gerven V. RSC advances from NdFeB magnets towards the rare-earth oxides: a recycling process consuming only oxalic acid. RSC Advances 2014, 4(1):64099-64111. 10.1039/C4RA13787F.
    • (2014) RSC Advances , vol.4 , Issue.1 , pp. 64099-64111
    • Hoogerstraete, T.V.1    Blanpain, B.2    Gerven, V.3
  • 14
    • 84885721496 scopus 로고    scopus 로고
    • John Wiley & Sons, Inc., Hoboken, NJ, USA., ch11, M. Schlesinger, M. Paunovic (Eds.), Fifth ed.
    • Izaki M. Electrodeposition of Iron and Iron Alloys, in Modern Electroplating 2010, John Wiley & Sons, Inc., Hoboken, NJ, USA., ch11. Fifth ed., 10.1002/9780470602638. M. Schlesinger, M. Paunovic (Eds.).
    • (2010) Electrodeposition of Iron and Iron Alloys, in Modern Electroplating
    • Izaki, M.1
  • 16
    • 0025493061 scopus 로고
    • Effect of oxygen, carbon, and nitrogen contents on the corrosion resistance of Nd-Fe-B magnets
    • Kim A.S., Camp F.E., Dulis E.J. Effect of oxygen, carbon, and nitrogen contents on the corrosion resistance of Nd-Fe-B magnets. IEEE Transactions on Magnetics 1990, 26(5):1936-1938. 10.1109/20.104576.
    • (1990) IEEE Transactions on Magnetics , vol.26 , Issue.5 , pp. 1936-1938
    • Kim, A.S.1    Camp, F.E.2    Dulis, E.J.3
  • 20
    • 79952537995 scopus 로고    scopus 로고
    • Corrosion properties of aluminium coatings deposited on sintered NdFeB by ion-beam-assisted deposition
    • Mao S., Yang H., Li J., Huang F., Song Z. Corrosion properties of aluminium coatings deposited on sintered NdFeB by ion-beam-assisted deposition. Applied Surface Science 2011, 257(13):5581-5585. 10.1016/j.apsusc.2011.01.049.
    • (2011) Applied Surface Science , vol.257 , Issue.13 , pp. 5581-5585
    • Mao, S.1    Yang, H.2    Li, J.3    Huang, F.4    Song, Z.5
  • 21
    • 79952898276 scopus 로고    scopus 로고
    • Corrosion behaviour of sintered NdFeB deposited with an aluminium coating
    • Mao S., Yang H., Song Z., Li J., Ying H., Sun K. Corrosion behaviour of sintered NdFeB deposited with an aluminium coating. Corrosion Science 2011, 53(5):1887-1894. 10.1016/j.corsci.2011.02.006.
    • (2011) Corrosion Science , vol.53 , Issue.5 , pp. 1887-1894
    • Mao, S.1    Yang, H.2    Song, Z.3    Li, J.4    Ying, H.5    Sun, K.6
  • 22
    • 0141686891 scopus 로고    scopus 로고
    • Anodic dissolution and selective corrosion of alloys
    • Marshakov I.K. Anodic dissolution and selective corrosion of alloys. Protection of Metals 2002, 38(2):118-123. 10.1023/A:1014908930959.
    • (2002) Protection of Metals , vol.38 , Issue.2 , pp. 118-123
    • Marshakov, I.K.1
  • 23
    • 50649110476 scopus 로고    scopus 로고
    • Extraction and recovery characteristics of Fe element from Nd-Fe-B sintered magnet powder scrap by carbonylation
    • Miura K., Itoh M., Machida K.-I. Extraction and recovery characteristics of Fe element from Nd-Fe-B sintered magnet powder scrap by carbonylation. Journal of Alloys and Compounds 2008, 466(1-2):228-232. 10.1016/j.jallcom.2007.11.013.
    • (2008) Journal of Alloys and Compounds , vol.466 , Issue.1-2 , pp. 228-232
    • Miura, K.1    Itoh, M.2    Machida, K.-I.3
  • 24
    • 0018308412 scopus 로고
    • Kinetics and mechanism of corrosion of iron in phosphoric acid
    • Muralidharan V., Raiagopalan K. Kinetics and mechanism of corrosion of iron in phosphoric acid. Corrosion Science 1978, 19(June):199-207.
    • (1978) Corrosion Science , vol.19 , Issue.JUNE , pp. 199-207
    • Muralidharan, V.1    Raiagopalan, K.2
  • 26
    • 0020878811 scopus 로고
    • Characteristic features of alloy polarization curves
    • Pickering H.W. Characteristic features of alloy polarization curves. Corrosion Science 1983, 23(April):1107-1120. 10.1016/0010-938X(83)90092-6.
    • (1983) Corrosion Science , vol.23 , pp. 1107-1120
    • Pickering, H.W.1
  • 28
    • 0021488794 scopus 로고
    • Permanent magnet materials based on the rare earth-iron-boron tetragonal compounds
    • Sagawa M., Fujimura S., Yamamoto H., Matsuura Y., Hiraga K. Permanent magnet materials based on the rare earth-iron-boron tetragonal compounds. IEEE Transactions on Magnetics 1984, 20(5):1584-1589. 10.1109/TMAG.1984.1063214.
    • (1984) IEEE Transactions on Magnetics , vol.20 , Issue.5 , pp. 1584-1589
    • Sagawa, M.1    Fujimura, S.2    Yamamoto, H.3    Matsuura, Y.4    Hiraga, K.5
  • 30
    • 0031148490 scopus 로고    scopus 로고
    • The electrochemical corrosion of pure magnesium in 1 N NaCl
    • Song G., Atrens a., Stjohn D., Nairn J., Li Y. The electrochemical corrosion of pure magnesium in 1 N NaCl. Corrosion Science 1997, 39(5):855-875. 10.1016/S0010-938X(96)00172-2.
    • (1997) Corrosion Science , vol.39 , Issue.5 , pp. 855-875
    • Song, G.1    Atrens, A.2    Stjohn, D.3    Nairn, J.4    Li, Y.5
  • 31
    • 55349086893 scopus 로고    scopus 로고
    • A comparative study on the corrosion behavior of NdFeB magnets in different electrolyte solutions
    • Song Y.W., Zhang H., Yang H.X., Song Z.L. A comparative study on the corrosion behavior of NdFeB magnets in different electrolyte solutions. Materials and Corrosion 2008, 59(10):794-801. 10.1002/maco.200804175.
    • (2008) Materials and Corrosion , vol.59 , Issue.10 , pp. 794-801
    • Song, Y.W.1    Zhang, H.2    Yang, H.X.3    Song, Z.L.4
  • 32
    • 74849095399 scopus 로고    scopus 로고
    • Corrosion, passivation and breakdown of passivity of neodymium
    • Sueptitz R., Uhlemann M., Gebert a., Schultz L. Corrosion, passivation and breakdown of passivity of neodymium. Corrosion Science 2010, 52(3):886-891. 10.1016/j.corsci.2009.11.008.
    • (2010) Corrosion Science , vol.52 , Issue.3 , pp. 886-891
    • Sueptitz, R.1    Uhlemann, M.2    Gebert, A.3    Schultz, L.4
  • 33
    • 0026239240 scopus 로고
    • Modification of the magnetic properties and corrosion resistance of Nd-Fe-B permanent magnets with addition of cobalt
    • Szymura S., Bala H., Pawłowska G., Rabinovich Y., Sergeev V., Pokrovskii D. Modification of the magnetic properties and corrosion resistance of Nd-Fe-B permanent magnets with addition of cobalt. Journal of the Less Common Metals 1991, 175:185-198. 10.1016/0022-5088(91)90003-M.
    • (1991) Journal of the Less Common Metals , vol.175 , pp. 185-198
    • Szymura, S.1    Bala, H.2    Pawłowska, G.3    Rabinovich, Y.4    Sergeev, V.5    Pokrovskii, D.6
  • 35
    • 9344220527 scopus 로고    scopus 로고
    • Effects of Dy and Nb on the magnetic properties and corrosion resistance of sintered NdFeB
    • Yu L.Q., Wen Y.H., Yan M. Effects of Dy and Nb on the magnetic properties and corrosion resistance of sintered NdFeB. Journal of Magnetism and Magnetic Materials 2004, 283:353-356. 10.1016/j.jmmm.2004.06.006.
    • (2004) Journal of Magnetism and Magnetic Materials , vol.283 , pp. 353-356
    • Yu, L.Q.1    Wen, Y.H.2    Yan, M.3
  • 36
    • 33745666511 scopus 로고    scopus 로고
    • Electrochemical corrosion behavior of Nd-Fe-B sintered magnets in different acid solutions
    • Zheng J., Jiang L., Chen Q. Electrochemical corrosion behavior of Nd-Fe-B sintered magnets in different acid solutions. Journal of Rare Earths 2006, 24:218-222. 10.1016/S1002-0721(06)60097-5.
    • (2006) Journal of Rare Earths , vol.24 , pp. 218-222
    • Zheng, J.1    Jiang, L.2    Chen, Q.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.