메뉴 건너뛰기




Volumn 80, Issue , 2015, Pages 91-101

Enhanced photocatalytic activity in anodized WO3-loaded TiO2 nanotubes

Author keywords

Anodizing; Nanotubes; Photocatalyst; WO3 TiO2

Indexed keywords

ANODIC OXIDATION; DEGRADATION; ELECTROLYTES; GRAFTING (CHEMICAL); NANOTUBES; OXIDE MINERALS; PHOTOCATALYSIS; PHOTOCATALYSTS; RATE CONSTANTS; TUNGSTEN COMPOUNDS; YARN;

EID: 84921636806     PISSN: 07496036     EISSN: 10963677     Source Type: Journal    
DOI: 10.1016/j.spmi.2014.12.008     Document Type: Article
Times cited : (29)

References (25)
  • 3
    • 84870227533 scopus 로고    scopus 로고
    • 2 nanotubes via wet impregnation and their water-splitting performance
    • 2 nanotubes via wet impregnation and their water-splitting performance Electrochim. Acta 87 2013 294 302
    • (2013) Electrochim. Acta , vol.87 , pp. 294-302
    • Lai, C.W.1    Sreekantan, S.2
  • 4
    • 77955569418 scopus 로고    scopus 로고
    • 2 nanotube powders derived by a rapid anodization process
    • 2 nanotube powders derived by a rapid anodization process J. Alloy. Compd. 505 2010 243 248
    • (2010) J. Alloy. Compd. , vol.505 , pp. 243-248
    • Liao, Y.1    Que, W.2
  • 6
    • 84885126278 scopus 로고    scopus 로고
    • Structure and photocatalysis activity of silver doped titanium oxide nanotubes array for degradation of pollutants
    • E.A. Al-Arfaj Structure and photocatalysis activity of silver doped titanium oxide nanotubes array for degradation of pollutants Superlattice Microst. 62 2013 285 291
    • (2013) Superlattice Microst. , vol.62 , pp. 285-291
    • Al-Arfaj, E.A.1
  • 8
    • 84863740360 scopus 로고    scopus 로고
    • Effect of anodization parameters on the structural morphology of titanium in fluoride containing electrolytes
    • K. Indiraa, S. Ningshen, U.K. Mudali, and N. Rajendrana Effect of anodization parameters on the structural morphology of titanium in fluoride containing electrolytes Mater. Charact. 71 2012 58 65
    • (2012) Mater. Charact. , vol.71 , pp. 58-65
    • Indiraa, K.1    Ningshen, S.2    Mudali, U.K.3    Rajendrana, N.4
  • 9
    • 80054756100 scopus 로고    scopus 로고
    • 2 nanotubes/nanorods with high visible light activity for the photodegradation of 2, 3-dichlorophenol
    • 2 nanotubes/nanorods with high visible light activity for the photodegradation of 2, 3-dichlorophenol Chem. Eng. J. 174 2011 539 545
    • (2011) Chem. Eng. J. , vol.174 , pp. 539-545
    • Yang, E.-I.1    Shi, J.-J.2    Liang, H.-C.3    Cheuk, W.-K.4
  • 11
    • 59249088034 scopus 로고    scopus 로고
    • 3/titanate nanotubes nanocomposite with enhanced photocatalytic properties
    • 3/titanate nanotubes nanocomposite with enhanced photocatalytic properties J. Alloy. Compd. 470 2009 486 491
    • (2009) J. Alloy. Compd. , vol.470 , pp. 486-491
    • Xiao, M.1    Wang, L.2    Huang, X.3    Wu, Y.4    Dang, Z.J.5
  • 13
    • 84864459220 scopus 로고    scopus 로고
    • 2 nanotubes for photocatalytic elimination of methylethylketone under UVA and solar light irradiation
    • 2 nanotubes for photocatalytic elimination of methylethylketone under UVA and solar light irradiation J. Photoch. Photobio. A: Chem. 245 2012 43 57
    • (2012) J. Photoch. Photobio. A: Chem. , vol.245 , pp. 43-57
    • Yamin, Y.1    Keller, N.2    Keller, V.3
  • 14
    • 84861624997 scopus 로고    scopus 로고
    • 3 nanotubular composite via single-step anodization and its application in photoelectrochemical hydrogen generation
    • 3 nanotubular composite via single-step anodization and its application in photoelectrochemical hydrogen generation Electrochem. Commun. 19 2012 131 134
    • (2012) Electrochem. Commun. , vol.19 , pp. 131-134
    • Smith, Y.R.1    Sarma, B.2    Mohanty, S.K.3    Misra, M.4
  • 16
    • 84862689015 scopus 로고    scopus 로고
    • 2 nanotube arrays prepared by anodization and their photocatalytic activity
    • 2 nanotube arrays prepared by anodization and their photocatalytic activity Ceram. Int. 38 2012 5791 5797
    • (2012) Ceram. Int. , vol.38 , pp. 5791-5797
    • Li, H.1    Cao, L.2    Liu, W.3    Su, G.4    Dong, B.5
  • 17
    • 0034244870 scopus 로고    scopus 로고
    • Measurement and calculation of optical band gap of chromium aluminum oxide films
    • E. Kim, Z.-T. Jiang, and K. No Measurement and calculation of optical band gap of chromium aluminum oxide films Jpn. J. Appl. Phys. 39 2000 4820 4825
    • (2000) Jpn. J. Appl. Phys. , vol.39 , pp. 4820-4825
    • Kim, E.1    Jiang, Z.-T.2    No, K.3
  • 18
    • 84899635888 scopus 로고    scopus 로고
    • 2 thin films by a modified sol-gel route and characterization of structural, optical and electrochromic properties
    • 2 thin films by a modified sol-gel route and characterization of structural, optical and electrochromic properties Adv. Mat. Lett. 5 2014 367 371
    • (2014) Adv. Mat. Lett. , vol.5 , pp. 367-371
    • Gokdemir, F.P.1    Yuzbasioglu, V.E.2    Keskin, B.3    Ozdemir, O.4    Kutlu, K.5
  • 19
    • 84874105842 scopus 로고    scopus 로고
    • 2 nanotube photoelectrodes using anodization and wet impregnation: Improved water-splitting hydrogen generation performance
    • 2 nanotube photoelectrodes using anodization and wet impregnation: Improved water-splitting hydrogen generation performance Int. J. Hydrogen Energ. 38 2013 2156 2166
    • (2013) Int. J. Hydrogen Energ. , vol.38 , pp. 2156-2166
    • Lai, C.W.1    Sreekantan, S.2
  • 24
    • 77957242876 scopus 로고    scopus 로고
    • x nano-structured porous catalysts grown by micro-arc oxidation method: Characterization and formation mechanism
    • x nano-structured porous catalysts grown by micro-arc oxidation method: characterization and formation mechanism Mater. Chem. Phys. 124 2010 203 207
    • (2010) Mater. Chem. Phys. , vol.124 , pp. 203-207
    • Bayati, M.R.1    Moshfegh, A.Z.2    Golestani-Fard, F.3    Molaei, R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.