1
-
-
0033750188
-
Silicon nitride and related materials
-
Riley F.L. Silicon nitride and related materials. J Am Ceram Soc 2000, 83:245-265.
-
(2000)
J Am Ceram Soc
, vol.83
, pp. 245-265
-
-
Riley, F.L.1
-
2
-
-
0029390450
-
Relationship between microstructure, toughening mechanisms, and fracture toughness of reinforced silicon nitride ceramics
-
Šajgalík P., Dusza J., Hoffmann M.J. Relationship between microstructure, toughening mechanisms, and fracture toughness of reinforced silicon nitride ceramics. J Am Ceram Soc 1995, 78:2619-2624.
-
(1995)
J Am Ceram Soc
, vol.78
, pp. 2619-2624
-
-
Šajgalík, P.1
Dusza, J.2
Hoffmann, M.J.3
-
5
-
-
0002681792
-
Ceramic-ceramic composite materials with improved friction and wear properties
-
Skopp A., Woydt M. Ceramic-ceramic composite materials with improved friction and wear properties. Tribol Int 1992, 61-70.
-
(1992)
Tribol Int
, pp. 61-70
-
-
Skopp, A.1
Woydt, M.2
-
9
-
-
41849141237
-
Enhanced mechanical properties of machinable Si3N4/BN composites by spark plasma sintering
-
Li Y.L., Li R.X., Zhang J.X. Enhanced mechanical properties of machinable Si3N4/BN composites by spark plasma sintering. Mater Sci Eng A 2008, 483-484:207-210.
-
(2008)
Mater Sci Eng A
, pp. 207-210
-
-
Li, Y.L.1
Li, R.X.2
Zhang, J.X.3
-
10
-
-
0030242049
-
Fracture behavior of multilayer silicon nitride/boron nitride ceramics
-
Liu H.Y., Hsu S.M. Fracture behavior of multilayer silicon nitride/boron nitride ceramics. J Am Ceram Soc 1996, 79:2452-2457.
-
(1996)
J Am Ceram Soc
, vol.79
, pp. 2452-2457
-
-
Liu, H.Y.1
Hsu, S.M.2
-
11
-
-
0036863613
-
Fabrication and microstructure of silicon nitride/boron nitride nanocomposites
-
Kusunose T., Sekino T., Choa Y.H., Niihara K. Fabrication and microstructure of silicon nitride/boron nitride nanocomposites. J Am Ceram Soc 2002, 85:2678-2688.
-
(2002)
J Am Ceram Soc
, vol.85
, pp. 2678-2688
-
-
Kusunose, T.1
Sekino, T.2
Choa, Y.H.3
Niihara, K.4
-
12
-
-
0037118057
-
Formation of tough interlocking microstructures in silicon nitride ceramics by dynamic ripening
-
Shen Z.J., Zhao Z., Peng H., Nygren M. Formation of tough interlocking microstructures in silicon nitride ceramics by dynamic ripening. Nature 2002, 417:266-268.
-
(2002)
Nature
, vol.417
, pp. 266-268
-
-
Shen, Z.J.1
Zhao, Z.2
Peng, H.3
Nygren, M.4
-
16
-
-
0035241967
-
4-hBN composites by water lubrication
-
4-hBN composites by water lubrication. Wear 2001, 247:223-230.
-
(2001)
Wear
, vol.247
, pp. 223-230
-
-
Saito, T.1
Hosoe, T.2
Honda, F.3
-
17
-
-
0029152508
-
Tribological behavior of silicon nitride materials under unlubricated sliding between 22°C and 1000°C
-
Skopp A., Woydt M., Habig K.H. Tribological behavior of silicon nitride materials under unlubricated sliding between 22°C and 1000°C. Wear 1995, 181-183:571-580.
-
(1995)
Wear
, pp. 571-580
-
-
Skopp, A.1
Woydt, M.2
Habig, K.H.3
-
18
-
-
0343550316
-
Tribofilm formation on boron carbide in sliding wear
-
Larsson P., Axen N., Hogmark S. Tribofilm formation on boron carbide in sliding wear. Wear 1999, 236:73-80.
-
(1999)
Wear
, vol.236
, pp. 73-80
-
-
Larsson, P.1
Axen, N.2
Hogmark, S.3
-
19
-
-
0022062149
-
Indentation fracture of WC-Co cermets
-
Shetty D.K., Wright I.G., Mincer P.N., Clauer A.H. Indentation fracture of WC-Co cermets. J Mat Sci 1985, 20:1873-1882.
-
(1985)
J Mat Sci
, vol.20
, pp. 1873-1882
-
-
Shetty, D.K.1
Wright, I.G.2
Mincer, P.N.3
Clauer, A.H.4
-
22
-
-
0032207131
-
Microstructural design of silicon nitride with improved fracture toughness. I. Effect of grain shape and size
-
Becher F.P., Sun Y.E., Plucknett P.K. Microstructural design of silicon nitride with improved fracture toughness. I. Effect of grain shape and size. J Am Ceram Soc 1998, 81:2821-2830.
-
(1998)
J Am Ceram Soc
, vol.81
, pp. 2821-2830
-
-
Becher, F.P.1
Sun, Y.E.2
Plucknett, P.K.3
-
23
-
-
0036497638
-
Microstructural designing of silicon nitride related to toughness
-
Peillon F.C., Thevenot F. Microstructural designing of silicon nitride related to toughness. J Eur Ceram Soc 2002, 22:271-278.
-
(2002)
J Eur Ceram Soc
, vol.22
, pp. 271-278
-
-
Peillon, F.C.1
Thevenot, F.2
-
24
-
-
0032207131
-
Microstructural design of silicon nitride with improved fracture toughness. I. Effects of grain shape and size
-
Becher P.F., Sun E.Y., Plucknett K.P., Alexander K.B., Hsueh Ch.H., Lin H.T., et al. Microstructural design of silicon nitride with improved fracture toughness. I. Effects of grain shape and size. J Am Ceram Soc 1998, 81:2821-2830.
-
(1998)
J Am Ceram Soc
, vol.81
, pp. 2821-2830
-
-
Becher, P.F.1
Sun, E.Y.2
Plucknett, K.P.3
Alexander, K.B.4
Hsueh, C.5
Lin, H.T.6
-
25
-
-
0042348636
-
Silicon nitride/boron nitride composite with enhanced fracture toughness
-
US Patent 5, 324, 694, 28 June 1994.
-
Petrak DR, Lee J. Silicon nitride/boron nitride composite with enhanced fracture toughness. US Patent 5, 324, 694, 28 June 1994.
-
-
-
Petrak, D.R.1
Lee, J.2
-
26
-
-
82155167650
-
Mechanical properties and electrical conductivity in a carbon nanotube reinforced silicon nitride composite
-
Kovalčíková A., Balázsi Cs Dusza J., Tapasztó O. Mechanical properties and electrical conductivity in a carbon nanotube reinforced silicon nitride composite. Ceram Int 2012, 38:527-533.
-
(2012)
Ceram Int
, vol.38
, pp. 527-533
-
-
Kovalčíková, A.1
Balázsi Cs Dusza, J.2
Tapasztó, O.3
-
29
-
-
77955555372
-
4-hBN ceramic materials sliding against stainless steel without lubrication
-
4-hBN ceramic materials sliding against stainless steel without lubrication. Wear 2010, 269:241-248.
-
(2010)
Wear
, vol.269
, pp. 241-248
-
-
Chen, W.1
Gao, Y.2
Chen, C.3
Xing, J.4
-
30
-
-
0029134318
-
Ceramic and ceramic composite materials with improved friction and wear properties
-
Skopp A., Woydt M. Ceramic and ceramic composite materials with improved friction and wear properties. Tribol Trans 1995, 38:233-242.
-
(1995)
Tribol Trans
, vol.38
, pp. 233-242
-
-
Skopp, A.1
Woydt, M.2
-
33
-
-
6344254423
-
Effect of rare-earth species on the wear properties of α-sialon and β-silicon nitride under tribochemical type conditions
-
Jones M.I., Hirao K., Hyuga H., Yamauchi Y. Effect of rare-earth species on the wear properties of α-sialon and β-silicon nitride under tribochemical type conditions. J Mater Res 2004, 19:2750-2758.
-
(2004)
J Mater Res
, vol.19
, pp. 2750-2758
-
-
Jones, M.I.1
Hirao, K.2
Hyuga, H.3
Yamauchi, Y.4
-
34
-
-
0035482049
-
Micro-and macro-tribological properties of SiC ceramics in sliding contact
-
Zum Gahr K.H., Blattner R., Hwang D.H., Pöhlmann K. Micro-and macro-tribological properties of SiC ceramics in sliding contact. Wear 2001, 250:299-310.
-
(2001)
Wear
, vol.250
, pp. 299-310
-
-
Zum Gahr, K.H.1
Blattner, R.2
Hwang, D.H.3
Pöhlmann, K.4
-
35
-
-
0029534389
-
Formation and self-lubricating mechanisms of boric acid on borided steel surfaces
-
Erdemir A., Bindal C. Formation and self-lubricating mechanisms of boric acid on borided steel surfaces. Surf Coat Technol 1995, 76-77:443-449.
-
(1995)
Surf Coat Technol
, pp. 443-449
-
-
Erdemir, A.1
Bindal, C.2
-
36
-
-
0002503934
-
Self-lubricating ceramic matrix composites
-
Marcel Dekker, New York, S. Jahanmir (Ed.)
-
Gangopadhyay A., Jahanmir S., Peterson M.B. Self-lubricating ceramic matrix composites. Friction and wear of ceramics 1994, 163-197. Marcel Dekker, New York. S. Jahanmir (Ed.).
-
(1994)
Friction and wear of ceramics
, pp. 163-197
-
-
Gangopadhyay, A.1
Jahanmir, S.2
Peterson, M.B.3
|