메뉴 건너뛰기




Volumn 49, Issue 16, 2014, Pages 5571-5578

Electrical conductivity of LSGM-YSZ composite materials synthesized via coprecipitation route

Author keywords

[No Author keywords available]

Indexed keywords

ACTIVATION ENERGY; COPRECIPITATION; RIETVELD ANALYSIS; SINTERING; YTTRIA STABILIZED ZIRCONIA; ZIRCONIA;

EID: 84903547478     PISSN: 00222461     EISSN: 15734803     Source Type: Journal    
DOI: 10.1007/s10853-014-8265-5     Document Type: Article
Times cited : (23)

References (44)
  • 1
    • 12044250695 scopus 로고
    • 3 perovskite type oxide as a new oxide ionic conductor
    • 10.1021/ja00088a016
    • 3 perovskite type oxide as a new oxide ionic conductor. J Am Chem Soc 116:3801-3803
    • (1994) J Am Chem Soc , vol.116 , pp. 3801-3803
    • Ishihara, T.1    Matsuda, H.2    Takita, Y.3
  • 3
    • 0030144646 scopus 로고    scopus 로고
    • Superior oxygen ion conductivity of lanthanum gallate doped with strontium and magnesium
    • 10.1149/1.1836692
    • Huang P, Petric A (1996) Superior oxygen ion conductivity of lanthanum gallate doped with strontium and magnesium. J Electrochem Soc 143:1644-1648
    • (1996) J Electrochem Soc , vol.143 , pp. 1644-1648
    • Huang, P.1    Petric, A.2
  • 8
    • 0015672153 scopus 로고
    • Conduction characteristics of the lithium iodide-aluminium oxide solid electrolytes
    • 10.1149/1.2403248
    • Liang CC (1973) Conduction characteristics of the lithium iodide-aluminium oxide solid electrolytes. J Electrochem Soc 120:1289-1292
    • (1973) J Electrochem Soc , vol.120 , pp. 1289-1292
    • Liang, C.C.1
  • 10
    • 0032022091 scopus 로고    scopus 로고
    • Solid oxide fuel cell with composite electrolyte consisting of samaria-doped ceria and yttria-stabilized zirconia
    • 10.1149/1.1838378
    • Mishima Y, Mitsuyasu H, Ohtaki M, Eguchi K (1998) Solid oxide fuel cell with composite electrolyte consisting of samaria-doped ceria and yttria-stabilized zirconia. J Electrochem Soc 145:1004-1007
    • (1998) J Electrochem Soc , vol.145 , pp. 1004-1007
    • Mishima, Y.1    Mitsuyasu, H.2    Ohtaki, M.3    Eguchi, K.4
  • 11
    • 0037096874 scopus 로고    scopus 로고
    • Preparation of YSZ/YDC and YSZ/GDC composite electrolytes by the tape casting and sol-gel dip-drawing coating method for low-temperature SOFC
    • 10.1023/A:1015451910081 10.1023/A:1015451910081
    • Jang WS, Hyun SH, Kim SG (2002) Preparation of YSZ/YDC and YSZ/GDC composite electrolytes by the tape casting and sol-gel dip-drawing coating method for low-temperature SOFC. J Mater Sci 37:2535-2541. doi: 10.1023/A:1015451910081
    • (2002) J Mater Sci , vol.37 , pp. 2535-2541
    • Jang, W.S.1    Hyun, S.H.2    Kim, S.G.3
  • 12
    • 33750366795 scopus 로고    scopus 로고
    • 1.9 composite materials for low-temperature solid oxide fuel cell cathodes
    • 10.1016/j.matlet.2006.03.075
    • 1.9 composite materials for low-temperature solid oxide fuel cell cathodes. Mater Lett 60:3642-3646
    • (2006) Mater Lett , vol.60 , pp. 3642-3646
    • Wei, B.1    Lü, Z.2    Huang, X.3    Li, S.4    Ai, G.5    Liu, Z.6    Su, W.7
  • 13
    • 34748853188 scopus 로고    scopus 로고
    • A brief review of the ionic conductivity enhancement for selected oxide electrolytes
    • 10.1016/j.jpowsour.2007.07.071
    • Hui S, Roller J, Yick S, Zhang X, Deces-Petit C, Xie Y, Maric R, Ghosh D (2007) A brief review of the ionic conductivity enhancement for selected oxide electrolytes. J Power Sources 172:493-502
    • (2007) J Power Sources , vol.172 , pp. 493-502
    • Hui, S.1    Roller, J.2    Yick, S.3    Zhang, X.4    Deces-Petit, C.5    Xie, Y.6    Maric, R.7    Ghosh, D.8
  • 14
    • 10044290860 scopus 로고    scopus 로고
    • Electrical conductivity and stability of CGO-YSZ solid solutions
    • 10.1016/j.ssi.2004.09.040
    • Zhou XD, Scarfino B, Anderson HU (2004) Electrical conductivity and stability of CGO-YSZ solid solutions. Solid State Ion 175:19-22
    • (2004) Solid State Ion , vol.175 , pp. 19-22
    • Zhou, X.D.1    Scarfino, B.2    Anderson, H.U.3
  • 16
    • 33846585961 scopus 로고    scopus 로고
    • Fabrication and characterization of SDC-LSGM composite electrolytes material in IT-SOFC
    • 10.1016/j.jallcom.2006.04.009
    • Xu D, Liu X, Wang D, Yi G, Gao Y, Zhang D, Su W (2007) Fabrication and characterization of SDC-LSGM composite electrolytes material in IT-SOFC. J Alloys Compd 429:292-295
    • (2007) J Alloys Compd , vol.429 , pp. 292-295
    • Xu, D.1    Liu, X.2    Wang, D.3    Yi, G.4    Gao, Y.5    Zhang, D.6    Su, W.7
  • 17
    • 74849137062 scopus 로고    scopus 로고
    • Electrical conductivity studies on the LSGM-CGO composite electrolytes
    • 10.1016/j.jallcom.2009.10.207
    • Jo SH, Muralidharan P, Kim DK (2010) Electrical conductivity studies on the LSGM-CGO composite electrolytes. J Alloys Compd 491:416-419
    • (2010) J Alloys Compd , vol.491 , pp. 416-419
    • Jo, S.H.1    Muralidharan, P.2    Kim, D.K.3
  • 18
    • 76549096543 scopus 로고    scopus 로고
    • Lanthanum gallate and ceria composite as electrolyte for solid oxide fuel cells
    • 10.1016/j.jallcom.2009.11.116
    • Li S, Li Z, Bergman B (2010) Lanthanum gallate and ceria composite as electrolyte for solid oxide fuel cells. J Alloys Compd 492:392-395
    • (2010) J Alloys Compd , vol.492 , pp. 392-395
    • Li, S.1    Li, Z.2    Bergman, B.3
  • 19
    • 84867582230 scopus 로고    scopus 로고
    • 2.85 composite electrolytes for intermediate-temperature solid oxide fuel cells
    • 10.1016/j.ssi.2012.03.005
    • 2.85 composite electrolytes for intermediate-temperature solid oxide fuel cells. Solid State Ion 225:81-84
    • (2012) Solid State Ion , vol.225 , pp. 81-84
    • Hao, G.1    Liu, X.2    Wang, H.3    Be, H.4    Pei, L.5    Su, W.6
  • 20
    • 69949089510 scopus 로고    scopus 로고
    • Microstructural studies on degradation of interface between LSM-YSZ cathode and YSZ electrolyte in SOFCs
    • 10.1016/j.ssi.2009.07.011
    • Liu YL, Hagen A, Barfod R, Chen M, Wang HJ, Poulsen FW, Hendriksen PV (2009) Microstructural studies on degradation of interface between LSM-YSZ cathode and YSZ electrolyte in SOFCs. Solid State Ion 180:1298-1304
    • (2009) Solid State Ion , vol.180 , pp. 1298-1304
    • Liu, Y.L.1    Hagen, A.2    Barfod, R.3    Chen, M.4    Wang, H.J.5    Poulsen, F.W.6    Hendriksen, P.V.7
  • 23
    • 0141674369 scopus 로고    scopus 로고
    • 3-y (x = 0:05; 0.1) single crystals
    • 10.1016/S0022-4596(03)00016-1
    • 3-y (x = 0:05; 0.1) single crystals. J Solid State Chem 172:396-441
    • (2003) J Solid State Chem , vol.172 , pp. 396-441
    • Vasylechko, L.1
  • 25
    • 84894540579 scopus 로고    scopus 로고
    • 3-δ electrolyte via ethylene glycol route and its characterizations for IT-SOFC
    • 10.1016/j.ceramint.2013.12.056
    • 3-δ electrolyte via ethylene glycol route and its characterizations for IT-SOFC. Ceram Int 40:7177-7184
    • (2014) Ceram Int , vol.40 , pp. 7177-7184
    • Raghvendra1    Singh, R.K.2    Singh, P.3
  • 27
    • 84945482342 scopus 로고
    • Bulk conductivity and defect chemistry of acceptor-doped strontium titanate in the quenched state
    • 10.1111/j.1151-2916.1991.tb07812.x
    • Waser R (1991) Bulk conductivity and defect chemistry of acceptor-doped strontium titanate in the quenched state. J Am Ceram Soc 74:1934-1940
    • (1991) J Am Ceram Soc , vol.74 , pp. 1934-1940
    • Waser, R.1
  • 28
    • 0023308715 scopus 로고
    • AC conduction in amorphous-chalcogenide and pnictide semiconductors
    • 10.1080/00018738700101971
    • Elliot SR (1987) AC conduction in amorphous-chalcogenide and pnictide semiconductors. Adv Phys 36:135-217
    • (1987) Adv Phys , vol.36 , pp. 135-217
    • Elliot, S.R.1
  • 29
    • 82455194964 scopus 로고    scopus 로고
    • 3 (x 0.100): Temperature and compositional- independent conductivity
    • 10.1103/PhysRevB.84.174306
    • 3 (x 0.100): temperature and compositional-independent conductivity. Phys Rev B 84:174306-174312
    • (2011) Phys Rev B , vol.84 , pp. 174306-174312
    • Singh, P.1    Raghvendra2    Parkash, O.3    Kumar, D.4
  • 30
    • 0017382315 scopus 로고
    • The 'universal' dielectric response
    • 10.1038/267673a0
    • Jonscher AK (1977) The 'universal' dielectric response. Nature 267:673-679
    • (1977) Nature , vol.267 , pp. 673-679
    • Jonscher, A.K.1
  • 32
    • 33746932703 scopus 로고
    • Anomalous conductivity prefactors in fast ion conductors
    • 10.1038/306456a0
    • Almond DP, West AR (1983) Anomalous conductivity prefactors in fast ion conductors. Nature 306:456-457
    • (1983) Nature , vol.306 , pp. 456-457
    • Almond, D.P.1    West, A.R.2
  • 33
    • 0020734862 scopus 로고
    • The determination of hopping rates and carrier concentrations in ionic conductors by a new analysis of ac conductivity
    • 10.1016/0167-2738(83)90079-6
    • Almond DP, Duncan GK, West AR (1983) The determination of hopping rates and carrier concentrations in ionic conductors by a new analysis of ac conductivity. Solid State Ion 8:159-164
    • (1983) Solid State Ion , vol.8 , pp. 159-164
    • Almond, D.P.1    Duncan, G.K.2    West, A.R.3
  • 34
    • 0020873645 scopus 로고
    • Mobile ion concentrations in solid electrolytes from an analysis of A.C. Conductivity
    • 10.1016/0167-2738(83)90247-3
    • Almond DP, West AR (1983) Mobile ion concentrations in solid electrolytes from an analysis of A.C. conductivity. Solid State Ion 9&10:277-282
    • (1983) Solid State Ion , vol.910 , pp. 277-282
    • Almond, D.P.1    West, A.R.2
  • 35
    • 0032655555 scopus 로고    scopus 로고
    • Ionic conductivity in glasses: Is the window effect statistically relevant?
    • 10.1016/S0022-3093(99)00017-4
    • Sidebottom DL (1999) Ionic conductivity in glasses: is the window effect statistically relevant? J Non Cryst Solids 244:223-231
    • (1999) J Non Cryst Solids , vol.244 , pp. 223-231
    • Sidebottom, D.L.1
  • 36
    • 84866487413 scopus 로고    scopus 로고
    • Dispersion in AC conductivity of fragile glass melts near glass transition temperature
    • 10.1016/j.ssi.2012.08.021
    • Singh P, Singh BP, Raghvendra (2012) Dispersion in AC conductivity of fragile glass melts near glass transition temperature. Solid State Ion 227:39-45
    • (2012) Solid State Ion , vol.227 , pp. 39-45
    • Singh, P.1    Singh, B.P.2    Raghvendra3
  • 37
    • 0023315712 scopus 로고
    • The activation entropy for transport in ionic conductors
    • 10.1016/0167-2738(87)90078-6
    • Almond DP, West AR (1987) The activation entropy for transport in ionic conductors. Solid State Ion 23:27-35
    • (1987) Solid State Ion , vol.23 , pp. 27-35
    • Almond, D.P.1    West, A.R.2
  • 38
    • 0022593350 scopus 로고
    • On the conductivity of polycrystalline materials
    • 10.1002/bbpc.19860900105
    • Maier J (1986) On the conductivity of polycrystalline materials. Ber Bunsenges Phys Chem 90:26-33
    • (1986) Ber Bunsenges Phys Chem , vol.90 , pp. 26-33
    • Maier, J.1
  • 39
    • 0034291323 scopus 로고    scopus 로고
    • Ionic conductor composites: Theory and materials
    • 10.1023/A:1009906101421
    • Knauth P (2000) Ionic conductor composites: theory and materials. J Electroceram 5:111-125
    • (2000) J Electroceram , vol.5 , pp. 111-125
    • Knauth, P.1
  • 40
    • 0001353206 scopus 로고
    • A theoretical model for composite electrolytes - I. Space charge layer as a cause for charge-carrier enhancement
    • 10.1016/0022-3697(95)00025-9
    • Jiang S, Wagner JB Jr (1995) A theoretical model for composite electrolytes - I. space charge layer as a cause for charge-carrier enhancement. J Phys Chem Solids 56:1101-1111
    • (1995) J Phys Chem Solids , vol.56 , pp. 1101-1111
    • Jiang, Jr.S.1    Wagner, J.B.2
  • 42
    • 0016544038 scopus 로고
    • Electrochemical studies on single crystalline CuCl solid electrolyte
    • 10.1149/1.2134396
    • Joshi AV, Wagner JRJB (1975) Electrochemical studies on single crystalline CuCl solid electrolyte. J Electrochem Soc 122:1071-1080
    • (1975) J Electrochem Soc , vol.122 , pp. 1071-1080
    • Joshi, A.V.1    Wagner, J.2
  • 43
    • 78649979761 scopus 로고    scopus 로고
    • Ionic conductivity in oxide heterostructures: The role of interfaces
    • 10.1088/1468-6996/11/5/054503
    • Fabbri E, Pergolesi D, Traversa E (2010) Ionic conductivity in oxide heterostructures: the role of interfaces. Sci Technol Adv Mater 11:054503-054512
    • (2010) Sci Technol Adv Mater , vol.11 , pp. 054503-054512
    • Fabbri, E.1    Pergolesi, D.2    Traversa, E.3
  • 44
    • 73549122941 scopus 로고    scopus 로고
    • Thermal expansion of SOFC materials
    • 10.1007/BF02375916
    • Tietz F (1999) Thermal expansion of SOFC materials. Ionics 5:129-139
    • (1999) Ionics , vol.5 , pp. 129-139
    • Tietz, F.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.