메뉴 건너뛰기




Volumn 34, Issue 12, 2014, Pages 2913-2924

Laser-supported joining of SiC-fiber/SiCN ceramic matrix composites fabricated by precursor infiltration

Author keywords

CMC; Glass ceramic filler; Laser joining; PIP; SiC fiber

Indexed keywords

CERAMIC MATRIX COMPOSITES; FILLERS; GLASS; JOINING; SECONDARY BATTERIES; SILICON; SILICON CARBIDE; SINTERING; THERMAL CONDUCTIVITY; WINDING;

EID: 84901634439     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2014.03.016     Document Type: Article
Times cited : (22)

References (42)
  • 1
    • 0003525853 scopus 로고    scopus 로고
    • National Academy of Science, Washington, Committee on Advanced Fibres for High-Temperature Ceramic Composites, C.o.E.a.T.S.
    • Committee on Advanced Fibres for High-Temperature Ceramic Composites, C.o.E.a.T.S. Ceramic fibres and coatings: advanced material for the twenty-first century 1998, National Academy of Science, Washington.
    • (1998) Ceramic fibres and coatings: advanced material for the twenty-first century
  • 2
    • 0036459350 scopus 로고    scopus 로고
    • Oxidation resistant non-oxide ceramic matrix composites
    • Klemm H., Bales A. Oxidation resistant non-oxide ceramic matrix composites. Ceram Eng Sci Proc 2002, 23(3):305-310.
    • (2002) Ceram Eng Sci Proc , vol.23 , Issue.3 , pp. 305-310
    • Klemm, H.1    Bales, A.2
  • 4
    • 84905668164 scopus 로고    scopus 로고
    • Composite materials for high temperature reactors: technology development roadmap
    • paper 148
    • Katoh Y., Snead L.L., Burchell T.D., Windes W.E. Composite materials for high temperature reactors: technology development roadmap. Proceedings of HTR 2010 2010, paper 148.
    • (2010) Proceedings of HTR 2010
    • Katoh, Y.1    Snead, L.L.2    Burchell, T.D.3    Windes, W.E.4
  • 7
    • 0032475143 scopus 로고    scopus 로고
    • Design requirements for SiC/SiC composites structural material in fusion power reactor blankets
    • Giancarli L., Bonal J.P., Caso A., Le Marois G., Morley N.B., Salavy J.F. Design requirements for SiC/SiC composites structural material in fusion power reactor blankets. Fus Eng Des 1998, 41:165-171.
    • (1998) Fus Eng Des , vol.41 , pp. 165-171
    • Giancarli, L.1    Bonal, J.P.2    Caso, A.3    Le Marois, G.4    Morley, N.B.5    Salavy, J.F.6
  • 8
    • 0033904611 scopus 로고    scopus 로고
    • Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications
    • Colombo P., Riccardi B., Donato A., Schubert C. Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications. J Nucl Mater 2000, 278:127-135.
    • (2000) J Nucl Mater , vol.278 , pp. 127-135
    • Colombo, P.1    Riccardi, B.2    Donato, A.3    Schubert, C.4
  • 9
    • 0036942657 scopus 로고    scopus 로고
    • Silicon carbide-based materials for joining silicon carbide composites for fusion energy applications
    • Lewinsohn C.A., Jones R.H., Colombo P., Riccardi B. Silicon carbide-based materials for joining silicon carbide composites for fusion energy applications. J Nucl Mater 2002, 307-311:1232-1236.
    • (2002) J Nucl Mater , pp. 1232-1236
    • Lewinsohn, C.A.1    Jones, R.H.2    Colombo, P.3    Riccardi, B.4
  • 10
    • 21844459503 scopus 로고    scopus 로고
    • Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites
    • Katoh Y., Kotani M., Kohyama A., Montorsi M., Salvo M., Ferraris M. Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites. J Nucl Mater 2000, 283-287:1262-1266.
    • (2000) J Nucl Mater , pp. 1262-1266
    • Katoh, Y.1    Kotani, M.2    Kohyama, A.3    Montorsi, M.4    Salvo, M.5    Ferraris, M.6
  • 12
    • 84862750082 scopus 로고    scopus 로고
    • Effects of neutron irradiation on glass-ceramics as pressure-less joining materials for SiC based components for nuclear applications
    • Ferraris M., Casalegno V., Rizzo S., Salvo M., Van Staveren T.O., Matejicek J. Effects of neutron irradiation on glass-ceramics as pressure-less joining materials for SiC based components for nuclear applications. J Nucl Mater 2012, 429:166-172.
    • (2012) J Nucl Mater , vol.429 , pp. 166-172
    • Ferraris, M.1    Casalegno, V.2    Rizzo, S.3    Salvo, M.4    Van Staveren, T.O.5    Matejicek, J.6
  • 13
    • 0036884673 scopus 로고    scopus 로고
    • Cordierite-mullite coating for SiC/SiC composites
    • Ferraris M., Salvo M., Smeacetto F. Cordierite-mullite coating for SiC/SiC composites. J Eur Ceram Soc 2002, 22:2332-2347.
    • (2002) J Eur Ceram Soc , vol.22 , pp. 2332-2347
    • Ferraris, M.1    Salvo, M.2    Smeacetto, F.3
  • 16
    • 0001000466 scopus 로고
    • Crystallization of yttria-alumina-silica-glasses
    • Arita I.H., Wilkingson D.S., Purdy G.R. Crystallization of yttria-alumina-silica-glasses. J Am Ceram Soc 1992, 75(12):3315-3320.
    • (1992) J Am Ceram Soc , vol.75 , Issue.12 , pp. 3315-3320
    • Arita, I.H.1    Wilkingson, D.S.2    Purdy, G.R.3
  • 18
    • 0037299702 scopus 로고    scopus 로고
    • Oxynitride glasses, their properties and crystallization - a review
    • Hampshire S. Oxynitride glasses, their properties and crystallization - a review. J Non-Cryst Solids 2003, 316:64-73.
    • (2003) J Non-Cryst Solids , vol.316 , pp. 64-73
    • Hampshire, S.1
  • 19
    • 64649100863 scopus 로고    scopus 로고
    • Recent advances and issues in development of silicon carbide composites for fusion applications
    • Nozawa T., Hinoki T., Hasegawa A., Kohyama A., Katoh Y., Snead L.L., et al. Recent advances and issues in development of silicon carbide composites for fusion applications. J Nucl Mater 2009, 386-388:622-627.
    • (2009) J Nucl Mater , pp. 622-627
    • Nozawa, T.1    Hinoki, T.2    Hasegawa, A.3    Kohyama, A.4    Katoh, Y.5    Snead, L.L.6
  • 21
    • 2942585034 scopus 로고    scopus 로고
    • Laser joining of silicon carbide - a new technology for ultra-high temperature resistant joint
    • Lippmann W., Knorr J., Wolf R., Rasper R., Exner H., Reinecke A.-M., et al. Laser joining of silicon carbide - a new technology for ultra-high temperature resistant joint. Nucl Eng Des 2004, 231:151-161.
    • (2004) Nucl Eng Des , vol.231 , pp. 151-161
    • Lippmann, W.1    Knorr, J.2    Wolf, R.3    Rasper, R.4    Exner, H.5    Reinecke, A.-M.6
  • 22
    • 84865638171 scopus 로고    scopus 로고
    • Electrically conductive ceramics and new joining technologies for applications in HTR engineering
    • Hille C., Lippmann W., Hurtado A. Electrically conductive ceramics and new joining technologies for applications in HTR engineering. Nucl Eng Des 2012, 251:222-229.
    • (2012) Nucl Eng Des , vol.251 , pp. 222-229
    • Hille, C.1    Lippmann, W.2    Hurtado, A.3
  • 23
    • 84883685283 scopus 로고    scopus 로고
    • High-temperature stability of laser-joined silicon carbide components
    • Herrmann M., Lippmann W., Hurtado A. High-temperature stability of laser-joined silicon carbide components. J Nucl Mater 2013, 443:458-464.
    • (2013) J Nucl Mater , vol.443 , pp. 458-464
    • Herrmann, M.1    Lippmann, W.2    Hurtado, A.3
  • 25
    • 84863869074 scopus 로고    scopus 로고
    • Mechanical and microstructural characterisation of SiC- and SiBNC-fibre reinforced CMCs manufactured via PIP method before and after exposure to air
    • Klatt E., Frass A., Frieß M., Koch D., Voggenreiter H. Mechanical and microstructural characterisation of SiC- and SiBNC-fibre reinforced CMCs manufactured via PIP method before and after exposure to air. J Eur Ceram Soc 2012, 32:3861-3874.
    • (2012) J Eur Ceram Soc , vol.32 , pp. 3861-3874
    • Klatt, E.1    Frass, A.2    Frieß, M.3    Koch, D.4    Voggenreiter, H.5
  • 26
    • 0030385839 scopus 로고    scopus 로고
    • Processing and performance of SiC/Blackglas™ CFCCs using filament winding
    • Nejhad M.N.G., Chandramouli M.V. Processing and performance of SiC/Blackglas™ CFCCs using filament winding. Ceram Eng Sci Proc 1996, 17(4):449-458.
    • (1996) Ceram Eng Sci Proc , vol.17 , Issue.4 , pp. 449-458
    • Nejhad, M.N.G.1    Chandramouli, M.V.2
  • 27
    • 0035707276 scopus 로고    scopus 로고
    • Processing and performance of continuous fiber ceramic composites by preceramic polymer pyrolysis: I - Filament winding
    • Nejhad M.N.G., Chandramouli M.V., Yousefpour A. Processing and performance of continuous fiber ceramic composites by preceramic polymer pyrolysis: I - Filament winding. J Compos Mater 2001, 35(24):2207-2237.
    • (2001) J Compos Mater , vol.35 , Issue.24 , pp. 2207-2237
    • Nejhad, M.N.G.1    Chandramouli, M.V.2    Yousefpour, A.3
  • 28
    • 0035476106 scopus 로고    scopus 로고
    • Processing and performance of Nicalon/Blackglas and Nextel/Blackglas using cure-on-the-fly filament winding and preceramic polymer pyrolysis with inactive fillers
    • Yousefpour A., Ghasemi Nejhad M.N. Processing and performance of Nicalon/Blackglas and Nextel/Blackglas using cure-on-the-fly filament winding and preceramic polymer pyrolysis with inactive fillers. Compos Sci Technol 2001, 61(13):1813-1820.
    • (2001) Compos Sci Technol , vol.61 , Issue.13 , pp. 1813-1820
    • Yousefpour, A.1    Ghasemi Nejhad, M.N.2
  • 29
    • 84901613361 scopus 로고    scopus 로고
    • KiON® Corporation. TB2: KiON® Ceraset® Polyureasilazane and KiON® Ceraset® Polysilazane 20. Pensylvania: KiON® Corporation.
    • KiON® Corporation. TB2: KiON® Ceraset® Polyureasilazane and KiON® Ceraset® Polysilazane 20. Pensylvania: KiON® Corporation.
  • 31
    • 77953110972 scopus 로고    scopus 로고
    • Silicon nitride for high-temperature applications
    • Klemm H. Silicon nitride for high-temperature applications. J Am Ceram Soc 2010, 93(1501):1522.
    • (2010) J Am Ceram Soc , vol.93 , Issue.1501 , pp. 1522
    • Klemm, H.1
  • 34
    • 84901593273 scopus 로고    scopus 로고
    • Verband der keramischen Industrie, Selb, Informationszentrum technische Keramik
    • Informationszentrum technische Keramik Brevier Technische Keramik 2012, Verband der keramischen Industrie, Selb.
    • (2012) Brevier Technische Keramik
  • 35
    • 0036863082 scopus 로고    scopus 로고
    • Thermo-mechanical properties and microstructure of silicon carbide composites fabricated by nano-infiltrated transient eutectoid process
    • Katoh Y., Dong S.M., Kohyama A. Thermo-mechanical properties and microstructure of silicon carbide composites fabricated by nano-infiltrated transient eutectoid process. Fus Eng Des 2002, 61/62:723-731.
    • (2002) Fus Eng Des , pp. 723-731
    • Katoh, Y.1    Dong, S.M.2    Kohyama, A.3
  • 36
    • 84901598161 scopus 로고    scopus 로고
    • CeramTec: material table. [19.04.13].
    • CeramTec: material table. [19.04.13]. http://www.ceramtec.com/.
  • 37
    • 32544443062 scopus 로고    scopus 로고
    • Property tailorability for advanced CVI silicon carbide for fusion
    • Katoh Y., Nozawa T., Snead L.L., Hinoki T., Kohyama A. Property tailorability for advanced CVI silicon carbide for fusion. Fus Eng Des 2006, 81:937-944.
    • (2006) Fus Eng Des , vol.81 , pp. 937-944
    • Katoh, Y.1    Nozawa, T.2    Snead, L.L.3    Hinoki, T.4    Kohyama, A.5
  • 39
    • 0001225009 scopus 로고    scopus 로고
    • SiC particle reinforced oxynitride glass: processing and mechanical properties
    • Baron B., Chartier T., Rouxel T., Verdier P., Laurent Y. SiC particle reinforced oxynitride glass: processing and mechanical properties. J Eur Ceram Soc 1997, 17:773-780.
    • (1997) J Eur Ceram Soc , vol.17 , pp. 773-780
    • Baron, B.1    Chartier, T.2    Rouxel, T.3    Verdier, P.4    Laurent, Y.5
  • 40
    • 43449106185 scopus 로고    scopus 로고
    • Effect of SiC particles on the laser sintering of Al-7Si-0.3Mg alloy
    • Simchi A., Godlinski D. Effect of SiC particles on the laser sintering of Al-7Si-0.3Mg alloy. Scripta Mater 2008, 59:199-200.
    • (2008) Scripta Mater , vol.59 , pp. 199-200
    • Simchi, A.1    Godlinski, D.2
  • 41
    • 18144429937 scopus 로고
    • Gaskorrosion nichtoxidischer Werkstoffe
    • Deutscher Wirtschaftsdienst, Köln, [Kapitel 5.4.1.1], J. Kriegesmann (Ed.)
    • Nickel K.G., Quirmbach P. Gaskorrosion nichtoxidischer Werkstoffe. Technische Keramische Werkstoffe. - Erg. -Lieferung 6 1991, 1-76. Deutscher Wirtschaftsdienst, Köln, [Kapitel 5.4.1.1]. J. Kriegesmann (Ed.).
    • (1991) Technische Keramische Werkstoffe. - Erg. -Lieferung 6 , pp. 1-76
    • Nickel, K.G.1    Quirmbach, P.2
  • 42
    • 0027282886 scopus 로고
    • Corrosion of silicon-based ceramics in combustion environments
    • Jacobson N. Corrosion of silicon-based ceramics in combustion environments. J Am Ceram Soc 1993, 76(1):3-28.
    • (1993) J Am Ceram Soc , vol.76 , Issue.1 , pp. 3-28
    • Jacobson, N.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.