메뉴 건너뛰기




Volumn 4, Issue 4, 2013, Pages 341-356

Dissolution of UK high-level waste glass under simulated hyperalkaline conditions of a colocated geological disposal facility

Author keywords

[No Author keywords available]

Indexed keywords

CALCIUM SILICATE; DISSOLUTION; GLASS; SILICON; THERMOANALYSIS; WASTE DISPOSAL;

EID: 84897049896     PISSN: 20411286     EISSN: 20411294     Source Type: Journal    
DOI: 10.1111/ijag.12042     Document Type: Article
Times cited : (45)

References (28)
  • 1
    • 84897093282 scopus 로고    scopus 로고
    • Geological Disposal: Steps Towards Implementation. Nuclear Decommissioning Authority report, NDA/RWMD/013
    • Geological Disposal: Steps Towards Implementation. Nuclear Decommissioning Authority report, NDA/RWMD/013, 2010.
    • (2010)
  • 2
    • 84897075362 scopus 로고    scopus 로고
    • Development of the Nirex Reference Vault Backfill; Report on Current Status in 1994. United Kingdom Nirex Ltd. Report number S/97/014
    • Development of the Nirex Reference Vault Backfill; Report on Current Status in 1994. United Kingdom Nirex Ltd. Report number S/97/014, 1997.
    • (1997)
  • 3
    • 84897106173 scopus 로고    scopus 로고
    • Geological Disposal: Generic Environmental Safety Case Main Report. Nuclear Decommissioning Authority report, NDA/RWMD/021
    • Geological Disposal: Generic Environmental Safety Case Main Report. Nuclear Decommissioning Authority report, NDA/RWMD/021, 2010.
    • (2010)
  • 4
    • 0033688227 scopus 로고    scopus 로고
    • Single-Pass Flow-Through Experiments on a Simulated Waste Glass in Alkaline Media at 40 °C: I. Experiments Conducted at Variable Solution Flow Rates to Glass Surface Area Ratio
    • P. K. Abraitis, B. P. McGrail, D. P. Trivedi, F. R. Livens, and D. J. Vaughan, "Single-Pass Flow-Through Experiments on a Simulated Waste Glass in Alkaline Media at 40 °C: I. Experiments Conducted at Variable Solution Flow Rates to Glass Surface Area Ratio, " J. Nucl. Mat., 280 196-205 (2000).
    • (2000) J. Nucl. Mat. , vol.280 , pp. 196-205
    • Abraitis, P.K.1    McGrail, B.P.2    Trivedi, D.P.3    Livens, F.R.4    Vaughan, D.J.5
  • 5
    • 0035336859 scopus 로고    scopus 로고
    • SON 68 Nuclear Glass Alteration Kinetics Between pH 7 and pH 11.5
    • S. Gin and J. P. Mestre, "SON 68 Nuclear Glass Alteration Kinetics Between pH 7 and pH 11.5, " J. Nucl. Mat., 295 83-96 (2001).
    • (2001) J. Nucl. Mat. , vol.295 , pp. 83-96
    • Gin, S.1    Mestre, J.P.2
  • 6
    • 50249120698 scopus 로고    scopus 로고
    • An Experimental Study of the Dissolution Rates of Stimulated Aluminoborosilicate Waste Glasses as a Function of pH and Temperature Under Dilute Conditions
    • E. M. Pierce, W. E. A. Rodriguez, L. J. Calligan, W. J. Shaw, and B. P. McGrail, "An Experimental Study of the Dissolution Rates of Stimulated Aluminoborosilicate Waste Glasses as a Function of pH and Temperature Under Dilute Conditions, " Appl. Geochem., 23 2559-2573 (2008).
    • (2008) Appl. Geochem. , vol.23 , pp. 2559-2573
    • Pierce, E.M.1    Rodriguez, W.E.A.2    Calligan, L.J.3    Shaw, W.J.4    McGrail, B.P.5
  • 7
    • 0011983696 scopus 로고
    • Glass Alteration in the Presence of Mortar: Effect of the Cement Grade
    • Z. Andriambololona, N. Godon, and E. Vernaz, "Glass Alteration in the Presence of Mortar: Effect of the Cement Grade, " Proc. Mat. Sci. Symp., 257 151-158 (1992).
    • (1992) Proc. Mat. Sci. Symp. , vol.257 , pp. 151-158
    • Andriambololona, Z.1    Godon, N.2    Vernaz, E.3
  • 8
    • 79959724138 scopus 로고    scopus 로고
    • Glass-Water Interphase Reactivity with Calcium Rich Solutions
    • T. Chave, P. Frugier, S. Gin, and A. Ayral, "Glass-Water Interphase Reactivity with Calcium Rich Solutions, " Geochim. Cosmochim. Acta, 75 4125-4139 (2011).
    • (2011) Geochim. Cosmochim. Acta , vol.75 , pp. 4125-4139
    • Chave, T.1    Frugier, P.2    Gin, S.3    Ayral, A.4
  • 10
    • 84884342593 scopus 로고    scopus 로고
    • Formation of Alteration Products During Dissolution of Vitrified ILW in a High-pH Calcium-Rich Solution
    • C. A. Utton, R. J. Hand, N. C. Hyatt, S. W. Swanton, and S. J. Williams, "Formation of Alteration Products During Dissolution of Vitrified ILW in a High-pH Calcium-Rich Solution, " J. Nucl. Mat., 442 33-45 (2013).
    • (2013) J. Nucl. Mat. , vol.442 , pp. 33-45
    • Utton, C.A.1    Hand, R.J.2    Hyatt, N.C.3    Swanton, S.W.4    Williams, S.J.5
  • 11
    • 84881380476 scopus 로고    scopus 로고
    • Antagonist Effects of Calcium on Borosilicate Glass Alteration
    • S. Mercardo-Depierre, F. Angell, F. Frizon, and S. Gin, "Antagonist Effects of Calcium on Borosilicate Glass Alteration, " J. Nucl. Mat., 441 402-410 (2013).
    • (2013) J. Nucl. Mat. , vol.441 , pp. 402-410
    • Mercardo-Depierre, S.1    Angell, F.2    Frizon, F.3    Gin, S.4
  • 12
    • 84875702293 scopus 로고    scopus 로고
    • Chemical Durability of Vitrified Wasteforms: Effects of pH and Solution Composition
    • C. A. Utton, S. W. Swanton, J. Schofield, R. J. Hand, A. Clacher, and N. C. Hyatt, "Chemical Durability of Vitrified Wasteforms: Effects of pH and Solution Composition, " Min. Mag., 76 2919-2930 (2012).
    • (2012) Min. Mag. , vol.76 , pp. 2919-2930
    • Utton, C.A.1    Swanton, S.W.2    Schofield, J.3    Hand, R.J.4    Clacher, A.5    Hyatt, N.C.6
  • 13
    • 33745206894 scopus 로고    scopus 로고
    • Long-term Corrosion of Two Nuclear Waste Reference Glasses (MW and SON68): A Kinetic and Mineral Alteration Study
    • E. Curti, L. Crovisier, J. L. Morvan, and A. M. Karpoff, "Long-term Corrosion of Two Nuclear Waste Reference Glasses (MW and SON68): A Kinetic and Mineral Alteration Study, " Appl. Geochem., 21 1152-1168 (2006).
    • (2006) Appl. Geochem. , vol.21 , pp. 1152-1168
    • Curti, E.1    Crovisier, L.2    Morvan, J.L.3    Karpoff, A.M.4
  • 14
    • 74549158359 scopus 로고    scopus 로고
    • ASTM Standard Test Methods for Determining Chemical Durability of Nuclear, Hazardous, and Mixed Waste Glasses and Muliphase Glass Ceramics: The Product Consistency Test (PCT)
    • doi: 10.1520/C1285-02R08.
    • ASTM Standard Test Methods for Determining Chemical Durability of Nuclear, Hazardous, and Mixed Waste Glasses and Muliphase Glass Ceramics: The Product Consistency Test (PCT). ASTM International(2008). doi: 10.1520/C1285-02R08.
    • (2008) ASTM International
  • 15
    • 84949741580 scopus 로고    scopus 로고
    • Standard Test Method for Static Leaching of Monolithic Waste Forms for the Disposal of Radioactive Waste
    • ASTM C 1220-98
    • ASTM C 1220-98, Standard Test Method for Static Leaching of Monolithic Waste Forms for the Disposal of Radioactive Waste. ASTM International (2004).
    • (2004) ASTM International
  • 16
    • 84897061984 scopus 로고
    • User's Guide to PHREEQC - A Computer Program for Speciation, Reaction-Path, Advective Transport, and Inverse Geochemical Calculations," US. Geological Survey Water-Resources Investigations Report -, 143 ().
    • D. L. Parkhurst, "User's Guide to PHREEQC - A Computer Program for Speciation, Reaction-Path, Advective Transport, and Inverse Geochemical Calculations, " US. Geological Survey Water-Resources Investigations Report 95-4227, 143 (1995).
    • (1995) , pp. 95-4227
    • Parkhurst, D.L.1
  • 18
    • 52349100249 scopus 로고    scopus 로고
    • SON68 Nuclear Glass Dissolution Kinetics: Current State of Knowledge and Basis of the New GRAAL Model
    • P. Frugier et al., "SON68 Nuclear Glass Dissolution Kinetics: Current State of Knowledge and Basis of the New GRAAL Model, " J. Nucl. Mat, 380 8-21 (2008).
    • (2008) J. Nucl. Mat , vol.380 , pp. 8-21
    • Frugier, P.1
  • 19
    • 33644799493 scopus 로고    scopus 로고
    • Characterisation of Alteration Phases on HLW Glasses After 15 years of PCT Leaching
    • I. S. Muller, S. Ribet, I. L. Pegg, S. Gin, and P. Frugier, "Characterisation of Alteration Phases on HLW Glasses After 15 years of PCT Leaching, " Proc. Am. Ceram. Soc., 176 191 (2005).
    • (2005) Proc. Am. Ceram. Soc. , vol.176 , pp. 191
    • Muller, I.S.1    Ribet, S.2    Pegg, I.L.3    Gin, S.4    Frugier, P.5
  • 20
    • 0021168302 scopus 로고
    • Leach Testing of Waste Glasses Under Near-Saturation Conditions
    • B. Grambow and D. M. Strachan, "Leach Testing of Waste Glasses Under Near-Saturation Conditions, " Mat. Res. Soc. Syrup. Proc., 26 623-634 (1984).
    • (1984) Mat. Res. Soc. Syrup. Proc. , vol.26 , pp. 623-634
    • Grambow, B.1    Strachan, D.M.2
  • 22
    • 0022766744 scopus 로고
    • Aqueous Solubility Relationships for Two Types of Calcium Silicate Hydrate
    • H. M. Jennings, "Aqueous Solubility Relationships for Two Types of Calcium Silicate Hydrate, " J. Am. Ceram. Soc., 69 614-618 (1986).
    • (1986) J. Am. Ceram. Soc. , vol.69 , pp. 614-618
    • Jennings, H.M.1
  • 23
    • 0035783187 scopus 로고    scopus 로고
    • Protective Effect of the Alteration Gel: A Key Mechanism in the Long-Term Behaviour of Nuclear Waste Glass
    • S. Gin, "Protective Effect of the Alteration Gel: A Key Mechanism in the Long-Term Behaviour of Nuclear Waste Glass, " Proc. Mat. Res. Soc. Symp, 633 207-215 (2001).
    • (2001) Proc. Mat. Res. Soc. Symp , vol.633 , pp. 207-215
    • Gin, S.1
  • 24
    • 56749169173 scopus 로고    scopus 로고
    • Insight into Silicate-Glass Corrosion Mechanisms
    • C. Cailleteau et al., "Insight into Silicate-Glass Corrosion Mechanisms, " Nat. Mater., 7 978-983 (2008).
    • (2008) Nat. Mater. , vol.7 , pp. 978-983
    • Cailleteau, C.1
  • 25
    • 0026613660 scopus 로고
    • Evolution of Pore Water Chemistry During Degradation of Cement in a Radioactive Waste Repository Environment
    • U. R. Berner, "Evolution of Pore Water Chemistry During Degradation of Cement in a Radioactive Waste Repository Environment, " Waste Manag., 12 201-219 (1992).
    • (1992) Waste Manag. , vol.12 , pp. 201-219
    • Berner, U.R.1
  • 26
    • 78649654331 scopus 로고    scopus 로고
    • Crystallisation During Processing of Nuclear Waste Glass
    • P. Hrma, "Crystallisation During Processing of Nuclear Waste Glass", J. Non-Cryst. Solids, 356 3019-3025 (2010).
    • (2010) J. Non-Cryst. Solids , vol.356 , pp. 3019-3025
    • Hrma, P.1
  • 27
    • 84897064511 scopus 로고    scopus 로고
    • Sorption of Radionuclides to Specific Mineral Phases Present in Repository Cements", AES Technology Report, AES-D&R-0395 ().
    • S. Aggarwal, M. J. Angus, and J. Ketchen, "Sorption of Radionuclides to Specific Mineral Phases Present in Repository Cements", AES Technology Report, AES-D&R-0395 (2000).
    • (2000)
    • Aggarwal, S.1    Angus, M.J.2    Ketchen, J.3
  • 28
    • 84871937317 scopus 로고    scopus 로고
    • Np(V/VI) Redox Chemistry in Cementitious Systems: XAFS Investigations on the Speciation Under Anoxic and Oxidising Conditions
    • X. Gaona, E. Wieland, J. Tits, A. C. Sheinost, and R. Dahn, "Np(V/VI) Redox Chemistry in Cementitious Systems: XAFS Investigations on the Speciation Under Anoxic and Oxidising Conditions, " Appl. Geochem., 28 109-118 (2013).
    • (2013) Appl. Geochem. , vol.28 , pp. 109-118
    • Gaona, X.1    Wieland, E.2    Tits, J.3    Sheinost, A.C.4    Dahn, R.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.