Volumn 68, Issue 10, 2013, Pages 2178-2185

Visible light-degradation of azo dye methyl orange using TiO 2/β-FeOOH as a heterogeneous photo-Fenton-like catalyst

Author keywords

Heterogeneous catalyst; Methyl orange; Photo Fenton; TiO2 FeOOH; Visible light degradation

Indexed keywords

HETEROGENEOUS CATALYST; METHYL ORANGE; PHOTO-FENTON; TIO; VISIBLE LIGHT;

EID: 84892530687     PISSN: 02731223     EISSN: None     Source Type: Journal    
DOI: 10.2166/wst.2013.475     Document Type: Article
Times cited : (66)

References (39)
  • 2
    • 0344439805 scopus 로고    scopus 로고
    • Reduction of aromatic nitrocompounds with hydrazine hydrate in the presence of an iron hydroxide catalyst II. Activity, X-ray diffraction and Mossbauer study of the iron oxide hydroxide catalyst
    • Benz, M., van der Kraan, A. M. & Prins, R. 1998 Reduction of aromatic nitrocompounds with hydrazine hydrate in the presence of an iron hydroxide catalyst II. Activity, X-ray diffraction and Mossbauer study of the iron oxide hydroxide catalyst. Applied Catalysis A: General 172, 149-157.
    • (1998) Applied Catalysis A: General , vol.172 , pp. 149-157
    • Benz, M.1    Van Der Kraan, A.M.2    Prins, R.3
  • 3
    • 0037061103 scopus 로고    scopus 로고
    • Occurrence and prevention of photodissolution at the phase junction of magnetite and titanium dioxide
    • Beydoun, D., Amal, R., Low, G. & McEvoy, S. 2002 Occurrence and prevention of photodissolution at the phase junction of magnetite and titanium dioxide. Journal of Molecular Catalysis A: Chemical 180, 193-200.
    • (2002) Journal of Molecular Catalysis A: Chemical , vol.180 , pp. 193-200
    • Beydoun, D.1    Amal, R.2    Low, G.3    McEvoy, S.4
  • 4
    • 24644524154 scopus 로고    scopus 로고
    • Solar photocatalytic degradation of azo-dyes by photo-Fenton process
    • Chacon, J. M., Leal, M. T., Sanchez, M. & Bandala, E. R. 2006 Solar photocatalytic degradation of azo-dyes by photo-Fenton process. Dyes and Pigments 69 (3), 144-150.
    • (2006) Dyes and Pigments , vol.69 , Issue.3 , pp. 144-150
    • Chacon, J.M.1    Leal, M.T.2    Sanchez, M.3    Bandala, E.R.4
  • 5
    • 79952984275 scopus 로고    scopus 로고
    • Effects of experimental conditions on one-dimensional single-crystal nanostructure of β-FeOOH
    • Cheng, Z. W. & Zhao, D. N. 2011 Effects of experimental conditions on one-dimensional single-crystal nanostructure of β-FeOOH. Materials Chemistry and Physics 127, 220-226.
    • (2011) Materials Chemistry and Physics , vol.127 , pp. 220-226
    • Cheng, Z.W.1    Zhao, D.N.2
  • 6
    • 34250315801 scopus 로고    scopus 로고
    • Low cost removal of reactive dyes using wheat bran
    • Cicek, F., Ozer, D. & Ozer, A. 2007 Low cost removal of reactive dyes using wheat bran. Journal of Hazardous Materials 146, 408-416.
    • (2007) Journal of Hazardous Materials , vol.146 , pp. 408-416
    • Cicek, F.1    Ozer, D.2    Ozer, A.3
  • 7
    • 80054874056 scopus 로고    scopus 로고
    • Preparation and catalytic activity of Fe alginate gel beads for oxidative degradation of azo dyes under visible light irradiation
    • Dong, Y. C., Dong, W. J., Cao, Y. N., Han, Z. B. & Ding, Z. H. 2011 Preparation and catalytic activity of Fe alginate gel beads for oxidative degradation of azo dyes under visible light irradiation. Catalysis Today 175 (1), 346-355.
    • (2011) Catalysis Today , vol.175 , Issue.1 , pp. 346-355
    • Dong, Y.C.1    Dong, W.J.2    Cao, Y.N.3    Han, Z.B.4    Ding, Z.H.5
  • 9
    • 84155188939 scopus 로고    scopus 로고
    • Photocatalytic degradation of azo dye by novel Bi-based photocatalyst Bi4TaO8I under visible-light irradiation
    • Fan, J., Hu, X. Y., Xie, Z. G., Zhang, K. L. & Wang, J. J. 2012 Photocatalytic degradation of azo dye by novel Bi-based photocatalyst Bi4TaO8I under visible-light irradiation. Chemical Engineering Journal 179,44-51.
    • (2012) Chemical Engineering Journal , vol.179 , pp. 44-51
    • Fan, J.1    Hu, X.Y.2    Xie, Z.G.3    Zhang, K.L.4    Wang, J.J.5
  • 11
    • 84863831300 scopus 로고    scopus 로고
    • 2/CdS 'spindle-like' composite with high photodegradation and antibacterial capability under visible light irradiation
    • 2/CdS 'spindle-like' composite with high photodegradation and antibacterial capability under visible light irradiation. Journal of Hazardous Materials 229-230, 209-216.
    • (2012) Journal of Hazardous Materials , vol.229-230 , pp. 209-216
    • Gao, P.1    Liu, J.C.2    Zhang, T.3    Sun, D.D.4    Ng, W.5
  • 15
    • 57549101421 scopus 로고    scopus 로고
    • Direct hydro-alcohol thermal synthesis of special core-shell structured Fe-doped titania microspheres with extended visible light response and enhanced photoactivity
    • Li, J. X., Xu, J. H., Dai, W. L., Li, H. X. & Fan, K. N. 2009 Direct hydro-alcohol thermal synthesis of special core-shell structured Fe-doped titania microspheres with extended visible light response and enhanced photoactivity. Applied Catalysis B: Environmental 85, 162-170.
    • (2009) Applied Catalysis B: Environmental , vol.85 , pp. 162-170
    • Li, J.X.1    Xu, J.H.2    Dai, W.L.3    Li, H.X.4    Fan, K.N.5
  • 16
    • 84856335462 scopus 로고    scopus 로고
    • Photocatalytic degradation of 2, 4-dichlorophenol using nanoscale Fe/TiO2
    • Liu, L. F., Chen, F., Yang, F. L., Chen, Y. S. & Crittenden, J. 2012 Photocatalytic degradation of 2, 4-dichlorophenol using nanoscale Fe/TiO2. Chemical Engineering Journal 182-182, 189-195.
    • (2012) Chemical Engineering Journal , vol.182 , Issue.182 , pp. 189-195
    • Liu, L.F.1    Chen, F.2    Yang, F.L.3    Chen, Y.S.4    Crittenden, J.5
  • 17
    • 78649317673 scopus 로고    scopus 로고
    • Temperature dependence of magnetic property and photocatalytic activity of Fe3O4/hydroxyapatite nanoparticles
    • Liu, Y. C., Zhong, H., Li, L. F. & Zhang, C. J. 2010 Temperature dependence of magnetic property and photocatalytic activity of Fe3O4/hydroxyapatite nanoparticles. Materials Research Bulletin 45, 2036-2039.
    • (2010) Materials Research Bulletin , vol.45 , pp. 2036-2039
    • Liu, Y.C.1    Zhong, H.2    Li, L.F.3    Zhang, C.J.4
  • 18
    • 30744473946 scopus 로고    scopus 로고
    • Decolorization of the azo dye reactive black 5 by Fenton and photo-Fenton oxidation
    • Marco, S. L. & Jose, A. P. 2006 Decolorization of the azo dye reactive black 5 by Fenton and photo-Fenton oxidation. Dyes and Pigments 71, 236-244.
    • (2006) Dyes and Pigments , vol.71 , pp. 236-244
    • Marco, S.L.1    Jose, A.P.2
  • 19
    • 84862676033 scopus 로고    scopus 로고
    • Facile synthesis of visible light responsive V2O5/N, S-TiO2 composite photocatalyst: Enhanced hydrogen production and phenol degradation
    • Martha, S., Das, D. P., Biswal, N. & Parida, K. M. 2012 Facile synthesis of visible light responsive V2O5/N, S-TiO2 composite photocatalyst: enhanced hydrogen production and phenol degradation. Journal of Materials Chemistry 22, 10695-10703.
    • (2012) Journal of Materials Chemistry , vol.22 , pp. 10695-10703
    • Martha, S.1    Das, D.P.2    Biswal, N.3    Parida, K.M.4
  • 20
    • 0347124746 scopus 로고    scopus 로고
    • Adsorption of three azo reactive dyes by metal hydroxide sludge: Effect of temperature, pH, and electrolytes
    • Netpradit, S., Thiravetyan, P. & Towprayoon, S. 2004 Adsorption of three azo reactive dyes by metal hydroxide sludge: effect of temperature, pH, and electrolytes. Journal of Colloid and Interface Science 270, 255-261.
    • (2004) Journal of Colloid and Interface Science , vol.270 , pp. 255-261
    • Netpradit, S.1    Thiravetyan, P.2    Towprayoon, S.3
  • 21
    • 0022597708 scopus 로고
    • The degradation of dye-stuffs. Part II. Behaviour of dyestuffs in aerobic biodegradation tests
    • Pagga, U. & Drown, D. 1986 The degradation of dye-stuffs. Part II. behaviour of dyestuffs in aerobic biodegradation tests. Chemosphere 15, 479-491.
    • (1986) Chemosphere , vol.15 , pp. 479-491
    • Pagga, U.1    Drown, D.2
  • 22
    • 0023593981 scopus 로고
    • Studies of β-FeOOH. Chemical composition, microstructure and other characteristics of some synthetic akaganeite samples
    • Parida, K. M. 1987 Studies of β-FeOOH. Chemical composition, microstructure and other characteristics of some synthetic akaganeite samples. Journal of Materials Science Letters 6, 1476-1478.
    • (1987) Journal of Materials Science Letters , vol.6 , pp. 1476-1478
    • Parida, K.M.1
  • 23
    • 0023995066 scopus 로고
    • Studies on β-FeOOH part 2 physico-chemical characteristics of thermally treated akaganeite (β-FeOOH)
    • Parida, K. M. 1988 Studies on β-FeOOH part 2 physico-chemical characteristics of thermally treated akaganeite (β-FeOOH). Journal of Materials Science 23, 1201 -1205.
    • (1988) Journal of Materials Science , vol.23 , pp. 1201-1205
    • Parida, K.M.1
  • 29
    • 36049026944 scopus 로고    scopus 로고
    • Photocatalytic degradation of azo dye metanil yellow: Optimization and kinetic modeling using a chemometric approach
    • Sleiman, M., Vildozo, D., Ferronato, C. & Chovelon, J. M. 2007 Photocatalytic degradation of azo dye metanil yellow: optimization and kinetic modeling using a chemometric approach. Applied Catalysis B: Environmental 77,1-11.
    • (2007) Applied Catalysis B: Environmental , vol.77 , pp. 1-11
    • Sleiman, M.1    Vildozo, D.2    Ferronato, C.3    Chovelon, J.M.4
  • 31
    • 79952988938 scopus 로고    scopus 로고
    • Goethite Hierarchical Nanostructures: Glucose-assisted Synthesis, chemical conversion into hematite with excellent photocatalytic properties
    • Tong, G. X., Guan, J. G. & Zhang, Q. J. 2011 Goethite hierarchical nanostructures: glucose-assisted synthesis, chemical conversion into hematite with excellent photocatalytic properties. Materials Chemistry and Physics 127, 371-378.
    • (2011) Materials Chemistry and Physics , vol.127 , pp. 371-378
    • Tong, G.X.1    Guan, J.G.2    Zhang, Q.J.3
  • 32
    • 33745203051 scopus 로고    scopus 로고
    • Synthesis of mesoporous titania and the photocatalytic activity for decomposition of methyl orange
    • Wang, Z. H., Jiang, T. S., Du, Y. M., Chen, K. M. & Yin, H. B. 2006 Synthesis of mesoporous titania and the photocatalytic activity for decomposition of methyl orange. Materials Letters 60, 2493-2496.
    • (2006) Materials Letters , vol.60 , pp. 2493-2496
    • Wang, Z.H.1    Jiang, T.S.2    Du, Y.M.3    Chen, K.M.4    Yin, H.B.5
  • 35
    • 84866514556 scopus 로고    scopus 로고
    • Photo-Fenton-like degradation of azo dye methyl orange using synthetic ammonium and hydronium jarosite
    • Xu, Z. H., Liang, J. R. & Zhou, L. X. 2013 Photo-Fenton-like degradation of azo dye methyl orange using synthetic ammonium and hydronium jarosite. Journal of Alloys and Compounds 546, 112-118.
    • (2013) Journal of Alloys and Compounds , vol.546 , pp. 112-118
    • Xu, Z.H.1    Liang, J.R.2    Zhou, L.X.3
  • 37
    • 4344679282 scopus 로고    scopus 로고
    • Surfactant mediated nanoparticle assembly of catalytic mesoporous crystalline iron oxide materials
    • Yuan, Z. Y., Ren, T. Z. & Su, B. L. 2004 Surfactant mediated nanoparticle assembly of catalytic mesoporous crystalline iron oxide materials. Catalysis Today 93-95, 743-750.
    • (2004) Catalysis Today , vol.93-95 , pp. 743-750
    • Yuan, Z.Y.1    Ren, T.Z.2    Su, B.L.3
  • 38
    • 77952741953 scopus 로고    scopus 로고
    • Elimination of estrogen and its estrogenicity by heterogeneous photo-Fenton catalyst β-FeOOH/resin
    • Zhao, Y. P., Hu, J. Y. & Chen, H. B. 2010 Elimination of estrogen and its estrogenicity by heterogeneous photo-Fenton catalyst β-FeOOH/resin. Journal of Photochemistry and Photobiology A: Chemistry 212,94-100.
    • (2010) Journal of Photochemistry and Photobiology A: Chemistry , vol.212 , pp. 94-100
    • Zhao, Y.P.1    Hu, J.Y.2    Chen, H.B.3
  • 39
    • 84875755975 scopus 로고    scopus 로고
    • A comparative study about the effects of isomorphous substitution of transition metals (Ti, Cr, Mn, Co and Ni) on the UV/Fenton catalytic activity of magnetite
    • Zhong, Y. H., Liang, X. L., Tan, W., Zhong, Y., He, H. P., Zhu, J. X., Yuan, P. & Jiang, Z. 2013 A comparative study about the effects of isomorphous substitution of transition metals (Ti, Cr, Mn, Co and Ni) on the UV/Fenton catalytic activity of magnetite. Journal of Molecular Catalysis A: Chemical 372,29-34.
    • (2013) Journal of Molecular Catalysis A: Chemical , vol.372 , pp. 29-34
    • Zhong, Y.H.1    Liang, X.L.2    Tan, W.3    Zhong, Y.4    He, H.P.5    Zhu, J.X.6    Yuan, P.7    Jiang, Z.8


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.