Volumn 23, Issue , 2009, Pages 1492-1495

Cytotoxicity and Cell Adhesion of PLLA/keratin Composite Fibrous Membranes

Author keywords

Cell adhesion; Cytotoxicity; PLLA; Tissue engineering; Wool keratin

Indexed keywords

CELL ADHESION; CELL ENGINEERING; CELLS; COMPOSITE MEMBRANES; CYTOTOXICITY; KERATIN; TISSUE ENGINEERING; WOOL; YARN;

EID: 84891952195     PISSN: 16800737     EISSN: None     Source Type: Conference Proceeding    
DOI: 10.1007/978-3-540-92841-6_369     Document Type: Conference Paper
Times cited : (4)

References (27)
  • 1
    • 33745004453 scopus 로고    scopus 로고
    • Fiber diameter and texture of electrospun PEOT/PBT scaffolds influence human mesenchymal stem cell proliferation and morphology, and the release of incorporated compounds
    • Moroni L, Licht R, de Boer J et al. (2006) Fiber diameter and texture of electrospun PEOT/PBT scaffolds influence human mesenchymal stem cell proliferation and morphology, and the release of incorporated compounds. Biomaterials 27: 4911-4922.
    • (2006) Biomaterials , vol.27 , pp. 4911-4922
    • Moroni, L.1    Licht, R.2    de Boer, J.3
  • 3
    • 15244353095 scopus 로고    scopus 로고
    • Multilineage differentiation of human mesenchymal stem cells in a three-dimentional nanofibrous scaffold
    • Li WJ, Tuli R, Huang XX et al. (2005) Multilineage differentiation of human mesenchymal stem cells in a three-dimentional nanofibrous scaffold. Biomaterials 26: 5158-5166.
    • (2005) Biomaterials , vol.26 , pp. 5158-5166
    • Li, W.J.1    Tuli, R.2    Huang, X.X.3
  • 4
    • 33745931055 scopus 로고    scopus 로고
    • Electrospun Bombyx mori gland silk
    • Putthanarat S, Eby RK, Kataphinan W et al. (2006) Electrospun Bombyx mori gland silk. Polymer 47: 5630-5632.
    • (2006) Polymer , vol.47 , pp. 5630-5632
    • Putthanarat, S.1    Eby, R.K.2    Kataphinan, W.3
  • 5
    • 0026071229 scopus 로고
    • Degradation of and tissue reaction to biodegradable poly (L-lactide) for use as internal fixation of fractures: A study in rats
    • Bos RRM, Rozema FR, Boering G et al. (1991) Degradation of and tissue reaction to biodegradable poly (L-lactide) for use as internal fixation of fractures: a study in rats. Biomaterials 12: 32-36.
    • (1991) Biomaterials , vol.12 , pp. 32-36
    • Bos, R.R.M.1    Rozema, F.R.2    Boering, G.3
  • 6
    • 0031127883 scopus 로고    scopus 로고
    • In vitro and in vivo degradation of films of chitin and its deacetylated derivatives
    • Tomihata K, Ikada Y. (1997) In vitro and in vivo degradation of films of chitin and its deacetylated derivatives. Biomaterials 18: 567-575.
    • (1997) Biomaterials , vol.18 , pp. 567-575
    • Tomihata, K.1    Ikada, Y.2
  • 7
    • 11144281219 scopus 로고    scopus 로고
    • Electrospun nano- to microfiber fabrics made of biodegradable copolyesters: Structural characteristics, mechanical properties and cell adhesion potential
    • Kwon IK, Kidoaki S, Matsuda T. (2005) Electrospun nano- to microfiber fabrics made of biodegradable copolyesters: structural characteristics, mechanical properties and cell adhesion potential. Biomaterials 26: 3929-3939.
    • (2005) Biomaterials , vol.26 , pp. 3929-3939
    • Kwon, I.K.1    Kidoaki, S.2    Matsuda, T.3
  • 8
    • 0041880043 scopus 로고    scopus 로고
    • Regeneration of Bombyx mori silk by electrospinning. Part 1. Processing parameters and geometric properties
    • Sukigara S, Gandhi M, Ayutsede J et al. (2003) Regeneration of Bombyx mori silk by electrospinning. Part 1. Processing parameters and geometric properties. Polymer 44: 5721-5727.
    • (2003) Polymer , vol.44 , pp. 5721-5727
    • Sukigara, S.1    Gandhi, M.2    Ayutsede, J.3
  • 9
    • 33645989162 scopus 로고    scopus 로고
    • Electrospun three-dimensional hyaluronic acid nanofibrous scaffolds
    • Ji Y, Ghosh K, Shu XZ et al. (2006) Electrospun three-dimensional hyaluronic acid nanofibrous scaffolds. Biomaterials 27: 3782-3792.
    • (2006) Biomaterials , vol.27 , pp. 3782-3792
    • Ji, Y.1    Ghosh, K.2    Shu, X.Z.3
  • 10
    • 0030232761 scopus 로고    scopus 로고
    • Nanometre diameter fibres of polymer, produced by electrospinning
    • Reneker DH, Chun I. (1996) Nanometre diameter fibres of polymer, produced by electrospinning. Nanotechnology 7: 216-223.
    • (1996) Nanotechnology , vol.7 , pp. 216-223
    • Reneker, D.H.1    Chun, I.2
  • 11
    • 33749552865 scopus 로고    scopus 로고
    • Continuing differentiation of human mesenchymal stem cells and induced chondrogenic and osteogenic lineages in electrospun PLGA nanofiber scaffold
    • Xin XJ, Hussain M, Mao JJ (2007). Continuing differentiation of human mesenchymal stem cells and induced chondrogenic and osteogenic lineages in electrospun PLGA nanofiber scaffold. Biomaterials 28: 316-325.
    • (2007) Biomaterials , vol.28 , pp. 316-325
    • Xin, X.J.1    Hussain, M.2    Mao, J.J.3
  • 12
    • 33646483947 scopus 로고    scopus 로고
    • Electrospinning of chitin nanofibers: Degradation behavior and cellular response to normal human keratinocytes and fibroblasts
    • Noh HK, Lee SW, Kim JM. (2006) Electrospinning of chitin nanofibers: Degradation behavior and cellular response to normal human keratinocytes and fibroblasts. Biomaterials 27: 3934-3944.
    • (2006) Biomaterials , vol.27 , pp. 3934-3944
    • Noh, H.K.1    Lee, S.W.2    Kim, J.M.3
  • 13
    • 1642272096 scopus 로고    scopus 로고
    • An in vitro assessment of the antibacterial properties and cytotoxicity of nanoparticulate silver bone cement
    • Alt V, Bechert T, Steinrucke P. (2004) An in vitro assessment of the antibacterial properties and cytotoxicity of nanoparticulate silver bone cement. Biomaterials 25:4383-4391.
    • (2004) Biomaterials , vol.25 , pp. 4383-4391
    • Alt, V.1    Bechert, T.2    Steinrucke, P.3
  • 14
    • 33744778068 scopus 로고    scopus 로고
    • In vitro culture of human dermal fibroblasts on electrospun polycaprolactone collagen nanofibrous membrane
    • Venugopal JR, Zhang YZ, Ramakrishna S. (2006) In vitro culture of human dermal fibroblasts on electrospun polycaprolactone collagen nanofibrous membrane. Artificial Organs 30: 440-446.
    • (2006) Artificial Organs , vol.30 , pp. 440-446
    • Venugopal, J.R.1    Zhang, Y.Z.2    Ramakrishna, S.3
  • 15
    • 31544476834 scopus 로고    scopus 로고
    • Carbon nanotube reinforced bombyx mori silk nanofibers by the electrospinning process
    • Ayutsede J, Gandhi M, Sukigara S. (2006) Carbon nanotube reinforced bombyx mori silk nanofibers by the electrospinning process. Biomacromolecules 7: 208-214.
    • (2006) Biomacromolecules , vol.7 , pp. 208-214
    • Ayutsede, J.1    Gandhi, M.2    Sukigara, S.3
  • 16
    • 20444380699 scopus 로고    scopus 로고
    • Electrospun protein fibers as matrices for tissue engineering
    • Li MY, Mondrinos MJ, Gandhi MR et al. (2005) Electrospun protein fibers as matrices for tissue engineering. Biomaterials 26: 5999-6008.
    • (2005) Biomaterials , vol.26 , pp. 5999-6008
    • Li, M.Y.1    Mondrinos, M.J.2    Gandhi, M.R.3
  • 18
    • 73149103724 scopus 로고    scopus 로고
    • Morphology and adhesion of mesenchymal stem cells on PLLA, apatite and apatite/collagen surfaces
    • Chen Y, Cho MR, Mak AFT et al. (2008) Morphology and adhesion of mesenchymal stem cells on PLLA, apatite and apatite/collagen surfaces. J Mater Sci: Mater Med 19: 2563-2567.
    • (2008) J Mater Sci: Mater Med , vol.19 , pp. 2563-2567
    • Chen, Y.1    Cho, M.R.2    Mak, A.F.T.3
  • 19
    • 0037074717 scopus 로고    scopus 로고
    • Fabrication of wool keratin sponge scaffolds for long-term cell cultivation
    • Tachibana A, Furuta Y, Takeshima H et al. (2002) Fabrication of wool keratin sponge scaffolds for long-term cell cultivation. Journal of Biotechnology 93:165-170.
    • (2002) Journal of Biotechnology , vol.93 , pp. 165-170
    • Tachibana, A.1    Furuta, Y.2    Takeshima, H.3
  • 20
    • 3242678876 scopus 로고    scopus 로고
    • Rapid fabrication of keratin-hydroxyapatite hybrid sponges toward osteoblast cultivation and differentiation
    • Tachibana A, Kaneko S, Tanabe T et al. (2005) Rapid fabrication of keratin-hydroxyapatite hybrid sponges toward osteoblast cultivation and differentiation. Biomaterials 26: 297-302.
    • (2005) Biomaterials , vol.26 , pp. 297-302
    • Tachibana, A.1    Kaneko, S.2    Tanabe, T.3
  • 21
    • 1642389170 scopus 로고    scopus 로고
    • Novel approach to fabricate keratin sponge scaffolds with controlled pore size and porosity
    • Katoh K, Tanabe T, Yamauchi K. (2004) Novel approach to fabricate keratin sponge scaffolds with controlled pore size and porosity. Biomaterials 25: 4255-4262.
    • (2004) Biomaterials , vol.25 , pp. 4255-4262
    • Katoh, K.1    Tanabe, T.2    Yamauchi, K.3
  • 22
    • 33646040441 scopus 로고    scopus 로고
    • Nanofibrous poly (acrylonitrile-comaleic acid) membranes functionalized with gelatin and chitosan for lipase immobilization
    • Ye P, Xu ZK, Wu J et al. (2006) Nanofibrous poly (acrylonitrile-comaleic acid) membranes functionalized with gelatin and chitosan for lipase immobilization, Biomaterials 27: 4169-4176.
    • (2006) Biomaterials , vol.27 , pp. 4169-4176
    • Ye, P.1    Xu, Z.K.2    Wu, J.3
  • 23
    • 33646353199 scopus 로고    scopus 로고
    • The effect of surface area on the degradation rate of nano-fibrous poly (L-lactic acid) foams
    • Chen VJ, Ma PX. (2006) The effect of surface area on the degradation rate of nano-fibrous poly (L-lactic acid) foams. Biomaterials 27: 3708-3715.
    • (2006) Biomaterials , vol.27 , pp. 3708-3715
    • Chen, V.J.1    Ma, P.X.2
  • 27
    • 56349159538 scopus 로고    scopus 로고
    • Antibacterial and non toxic nano silver PLLA composites for tissue engineering
    • Hong Kong. 28 July-31 July, Advanced Materials Research
    • Li L, Li Y, Li JS et al. (2008) Antibacterial and non toxic nano silver PLLA composites for tissue engineering. International conference on Multi-functional Materials and Structures, Hong Kong. 28 July-31 July, 2008. Advanced Materials Research 47-50: 849-852.
    • (2008) International Conference On Multi-functional Materials and Structures , vol.47-50 , pp. 849-852
    • Li, L.1    Li, Y.2    Li, J.S.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.