메뉴 건너뛰기




Volumn 241, Issue , 2014, Pages 200-206

Catalytic activity of regenerated catalyst after the oxidation of 1,2-dichloroethane and trichloroethylene

Author keywords

Catalytic oxidation; Chlorinated VOC; Deactivation; H zeolites; Regeneration

Indexed keywords

1 ,2-DICHLOROETHANES; CATALYST SURFACES; CHLORINATED VOCS; CHLORINATED VOLATILE ORGANIC COMPOUND (CLVOCS); DEACTIVATION; H-ZEOLITES; REGENERATION; REGENERATION TREATMENT;

EID: 84891801499     PISSN: 13858947     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.cej.2013.12.008     Document Type: Article
Times cited : (43)

References (36)
  • 3
    • 78650308337 scopus 로고    scopus 로고
    • Environmental catalyst. Solid catalyst for the oxidation of volatile organic compounds
    • Wiley-VCH, G. Ertl, H. Knözinger, F. Schüth, J. Weitkamp (Eds.)
    • Spivey J.J. Environmental catalyst. Solid catalyst for the oxidation of volatile organic compounds. Handbook of Heterogeneous Catalyst 2008, 2394-2411. Wiley-VCH. G. Ertl, H. Knözinger, F. Schüth, J. Weitkamp (Eds.).
    • (2008) Handbook of Heterogeneous Catalyst , pp. 2394-2411
    • Spivey, J.J.1
  • 4
    • 60649109466 scopus 로고    scopus 로고
    • Simplified design methods of reverse flow catalytic combustors for the treatment of lean hydrocarbon-air mixtures
    • Marín P., Ordóñez S., Díez F.V. Simplified design methods of reverse flow catalytic combustors for the treatment of lean hydrocarbon-air mixtures. Chem. Eng. Process: Process Intensif. 2009, 48:229-238.
    • (2009) Chem. Eng. Process: Process Intensif. , vol.48 , pp. 229-238
    • Marín, P.1    Ordóñez, S.2    Díez, F.V.3
  • 5
    • 0344366676 scopus 로고    scopus 로고
    • Is it economically feasible to use heterogeneous catalysts for VOC control in regenerative oxidizersα
    • Matros Y.S., Bunimovich G.A., Patterson S.E., Meyer S.F. Is it economically feasible to use heterogeneous catalysts for VOC control in regenerative oxidizersα. Catal. Today 1996, 27:307-313.
    • (1996) Catal. Today , vol.27 , pp. 307-313
    • Matros, Y.S.1    Bunimovich, G.A.2    Patterson, S.E.3    Meyer, S.F.4
  • 6
    • 84985831487 scopus 로고
    • Economic effects of catalyst deactivation during VOC oxidation
    • Agarwal S.K., Spivey J.J. Economic effects of catalyst deactivation during VOC oxidation. Environ. Prog. 1993, 12:182.
    • (1993) Environ. Prog. , vol.12 , pp. 182
    • Agarwal, S.K.1    Spivey, J.J.2
  • 7
    • 0026626826 scopus 로고
    • Literature review: deactivation of catalysts in the oxidation of volatile organic compounds
    • Spivey J.J., Butt J.B. Literature review: deactivation of catalysts in the oxidation of volatile organic compounds. Catal. Today 1992, 11:465-500.
    • (1992) Catal. Today , vol.11 , pp. 465-500
    • Spivey, J.J.1    Butt, J.B.2
  • 12
    • 0041411493 scopus 로고    scopus 로고
    • Pt catalysts supported on H-type zeolites for the catalytic combustion of chlorobenzene
    • Scirè S., Minicò S., Crisafulli C. Pt catalysts supported on H-type zeolites for the catalytic combustion of chlorobenzene. Appl. Catal. B: Environ. 2003, 45:117-125.
    • (2003) Appl. Catal. B: Environ. , vol.45 , pp. 117-125
    • Scirè, S.1    Minicò, S.2    Crisafulli, C.3
  • 14
    • 79956034920 scopus 로고    scopus 로고
    • Deactivation and Regeneration of Solid Catalysts
    • Imperial College Press, London, M. Guisnet, F.R. Ribeiro (Eds.)
    • Guisnet M., Ribeiro F.R. Deactivation and Regeneration of Solid Catalysts. Deactivation and Regeneration of Zeolite Catalysts 2011, 3-18. Imperial College Press, London. M. Guisnet, F.R. Ribeiro (Eds.).
    • (2011) Deactivation and Regeneration of Zeolite Catalysts , pp. 3-18
    • Guisnet, M.1    Ribeiro, F.R.2
  • 15
    • 79956034920 scopus 로고    scopus 로고
    • Regeneration of Coked Zeolite Catalyst
    • Imperial College Press, London, M. Guillemot, F.R. Ribeiro (Eds.)
    • Guisnet M. Regeneration of Coked Zeolite Catalyst. Deactivation and Regeneration of Zeolite Catalyst 2011, 217-232. Imperial College Press, London. M. Guillemot, F.R. Ribeiro (Eds.).
    • (2011) Deactivation and Regeneration of Zeolite Catalyst , pp. 217-232
    • Guisnet, M.1
  • 16
    • 0035971280 scopus 로고    scopus 로고
    • The regeneration or disposal of deactivated heterogeneous catalysts
    • Trimm D.L. The regeneration or disposal of deactivated heterogeneous catalysts. Appl. Catal. A: Gen. 2001, 212:153-160.
    • (2001) Appl. Catal. A: Gen. , vol.212 , pp. 153-160
    • Trimm, D.L.1
  • 17
    • 66849119230 scopus 로고    scopus 로고
    • 3 for enhanced production of hydrogen without formation of methane
    • 3 for enhanced production of hydrogen without formation of methane. Fuel 2009, 88:1572-1579.
    • (2009) Fuel , vol.88 , pp. 1572-1579
    • Wang, J.1    Jiang, M.2    Yao, Y.3    Zhang, Y.4    Cao, J.5
  • 18
    • 78650756402 scopus 로고    scopus 로고
    • 2 atmosphere and its kinetics since 1948: a brief review
    • 2 atmosphere and its kinetics since 1948: a brief review. Energy 2011, 36:12-40.
    • (2011) Energy , vol.36 , pp. 12-40
    • Irfan, M.F.1    Usman, M.R.2    Kusakabe, K.3
  • 19
    • 79952440065 scopus 로고    scopus 로고
    • Coke steam reforming in FCC regenerator: a new mastery over high coking feeds
    • Corma A., Sauvanaud L., Doskocil E., Yaluris G. Coke steam reforming in FCC regenerator: a new mastery over high coking feeds. J. Catal. 2011, 279:183-195.
    • (2011) J. Catal. , vol.279 , pp. 183-195
    • Corma, A.1    Sauvanaud, L.2    Doskocil, E.3    Yaluris, G.4
  • 20
    • 0026711363 scopus 로고
    • Deactivation of metal exchanged zeolite catalysts during exposure to chlorinated hydrocarbons under oxidizing conditions
    • Chatterjee S., Greene H.L., Joon Park Y. Deactivation of metal exchanged zeolite catalysts during exposure to chlorinated hydrocarbons under oxidizing conditions. Catal. Today 1992, 11:569-596.
    • (1992) Catal. Today , vol.11 , pp. 569-596
    • Chatterjee, S.1    Greene, H.L.2    Joon Park, Y.3
  • 21
    • 0034590822 scopus 로고    scopus 로고
    • Deep catalytic oxidation of chlorinated VOC mixtures from groundwater stripping emissions
    • Studies in Surface Science and Catalysis, Elsevier
    • A. Aranzabal, J.A. González-Marcos, R. López-Fonseca, M.A. Gutiérrez-Ortiz, J.R. González-Velasco, Deep catalytic oxidation of chlorinated VOC mixtures from groundwater stripping emissions, in: Studies in Surface Science and Catalysis, Elsevier, 2000, pp. 1229-1234.
    • (2000) , pp. 1229-1234
    • Aranzabal, A.1    González-Marcos, J.A.2    López-Fonseca, R.3    Gutiérrez-Ortiz, M.A.4    González-Velasco, J.R.5
  • 22
    • 0001317294 scopus 로고
    • Catalytic destruction of halogenated volatile organic compounds. Mechanisms of platinum catalyst systems
    • Windawi H., Wyatt M. Catalytic destruction of halogenated volatile organic compounds. Mechanisms of platinum catalyst systems. Platinum Met. Rev. 1993, 37:186-193.
    • (1993) Platinum Met. Rev. , vol.37 , pp. 186-193
    • Windawi, H.1    Wyatt, M.2
  • 23
    • 0344334105 scopus 로고    scopus 로고
    • Catalytic oxidation of volatile organic compounds 1. Oxidation of xylene over a 0.2wt.% Pd/HFAU(17) catalyst
    • Guisnet M., Dégé P., Magnoux P. Catalytic oxidation of volatile organic compounds 1. Oxidation of xylene over a 0.2wt.% Pd/HFAU(17) catalyst. Appl. Catal. B: Environ. 1999, 20:1-13.
    • (1999) Appl. Catal. B: Environ. , vol.20 , pp. 1-13
    • Guisnet, M.1    Dégé, P.2    Magnoux, P.3
  • 24
    • 0037014345 scopus 로고    scopus 로고
    • Studies on the catalytic dechlorination and abatement of chlorided VOC: the cases of 2-chloropropane, 1,2-dichloropropane and trichloroethylene
    • Finocchio E., Pistarino C., Dellepiane S., Serra B., Braggio S., Baldi M., Busca G. Studies on the catalytic dechlorination and abatement of chlorided VOC: the cases of 2-chloropropane, 1,2-dichloropropane and trichloroethylene. Catal. Today 2002, 75:263-267.
    • (2002) Catal. Today , vol.75 , pp. 263-267
    • Finocchio, E.1    Pistarino, C.2    Dellepiane, S.3    Serra, B.4    Braggio, S.5    Baldi, M.6    Busca, G.7
  • 26
    • 67649814723 scopus 로고    scopus 로고
    • Removal of hazardous chlorinated VOCs over Mn-Cu mixed oxide based catalyst
    • Vu V.H., Belkouch J., Ould-Dris A., Taouk B. Removal of hazardous chlorinated VOCs over Mn-Cu mixed oxide based catalyst. J. Hazard. Mater. 2009, 169:758-765.
    • (2009) J. Hazard. Mater. , vol.169 , pp. 758-765
    • Vu, V.H.1    Belkouch, J.2    Ould-Dris, A.3    Taouk, B.4
  • 27
    • 44649111836 scopus 로고    scopus 로고
    • Low-temperature catalytic combustion of trichloroethylene over cerium oxide and catalyst deactivation
    • Dai Q., Wang X., Lu G. Low-temperature catalytic combustion of trichloroethylene over cerium oxide and catalyst deactivation. Appl. Catal. B: Environ. 2008, 81:192-202.
    • (2008) Appl. Catal. B: Environ. , vol.81 , pp. 192-202
    • Dai, Q.1    Wang, X.2    Lu, G.3
  • 28
    • 3242734715 scopus 로고    scopus 로고
    • Hydrodechlorination over Pd-Pt/Al2O3 catalysts: a comparative study of chlorine removal from dichlorodifluoromethane, carbon tetrachloride and 1,2-dichloroethane
    • Legawiec-Jarzyna M., Śrebowata A., Juszczyk W., Karpiński Z. Hydrodechlorination over Pd-Pt/Al2O3 catalysts: a comparative study of chlorine removal from dichlorodifluoromethane, carbon tetrachloride and 1,2-dichloroethane. Appl. Catal. A: Gen. 2004, 271:61-68.
    • (2004) Appl. Catal. A: Gen. , vol.271 , pp. 61-68
    • Legawiec-Jarzyna, M.1    Śrebowata, A.2    Juszczyk, W.3    Karpiński, Z.4
  • 29
    • 34447097714 scopus 로고    scopus 로고
    • Mode of zeolite catalysts deactivation during chlorinated VOCs oxidation
    • Guillemot M., Mijoin J., Mignard S., Magnoux P. Mode of zeolite catalysts deactivation during chlorinated VOCs oxidation. Appl. Catal. A: Gen. 2007, 327:211-217.
    • (2007) Appl. Catal. A: Gen. , vol.327 , pp. 211-217
    • Guillemot, M.1    Mijoin, J.2    Mignard, S.3    Magnoux, P.4
  • 31
    • 58449136010 scopus 로고    scopus 로고
    • 3 catalyst: effects of chlorine ions and water on catalytic activity
    • 3 catalyst: effects of chlorine ions and water on catalytic activity. Chin. J. Catal. 2008, 29:1221-1225.
    • (2008) Chin. J. Catal. , vol.29 , pp. 1221-1225
    • Gao, D.1    Wang, S.2    Zhang, C.3    Yuan, Z.4    Wang, S.5
  • 32
    • 0034144638 scopus 로고    scopus 로고
    • Oxidation and reduction effects of propane-oxygen on Pd-chlorine/alumina catalysts
    • Schmal M., Aranda D.A.G., Noronha F.B., Guimaraes A.L., Monteiro R.S. Oxidation and reduction effects of propane-oxygen on Pd-chlorine/alumina catalysts. Catal. Lett. 2000, 64:163-169.
    • (2000) Catal. Lett. , vol.64 , pp. 163-169
    • Schmal, M.1    Aranda, D.A.G.2    Noronha, F.B.3    Guimaraes, A.L.4    Monteiro, R.S.5
  • 33
    • 0001134360 scopus 로고    scopus 로고
    • Surface acidic properties of alumina-supported niobia prepared by chemical vapour deposition and hydrolysis of niobium pentachloride
    • da Silva C.L.T., Camorim V.L.L., Zotin J.L., Duarte Pereira M.L.R., Faro A.d.C. Surface acidic properties of alumina-supported niobia prepared by chemical vapour deposition and hydrolysis of niobium pentachloride. Catal. Today 2000, 57:209-217.
    • (2000) Catal. Today , vol.57 , pp. 209-217
    • da Silva, C.L.T.1    Camorim, V.L.L.2    Zotin, J.L.3    Duarte Pereira, M.L.R.4    Faro, A.5
  • 34
    • 84871280614 scopus 로고    scopus 로고
    • Characterization of Aged Zeolite Catalyst
    • Imperial College Press, London, M. Guisnet, F.R. Ribeiro (Eds.)
    • Guisnet M. Characterization of Aged Zeolite Catalyst. Deactivation and Regeneration of Zeolite Catalysts 2011, 83-98. Imperial College Press, London. M. Guisnet, F.R. Ribeiro (Eds.).
    • (2011) Deactivation and Regeneration of Zeolite Catalysts , pp. 83-98
    • Guisnet, M.1
  • 35
    • 75249105081 scopus 로고    scopus 로고
    • Infrared Spectroscopy for the Characterization of Surface Acidity and Basicity
    • Wiley-VCH, Weinheim, G. Ertl, H. Knözinger, F. Schüth, J. Weitkamp (Eds.)
    • Knözinger H. Infrared Spectroscopy for the Characterization of Surface Acidity and Basicity. Handbook of Heterogeneous Catalysis 2008, 1135-1163. Wiley-VCH, Weinheim. G. Ertl, H. Knözinger, F. Schüth, J. Weitkamp (Eds.).
    • (2008) Handbook of Heterogeneous Catalysis , pp. 1135-1163
    • Knözinger, H.1
  • 36
    • 0001570958 scopus 로고    scopus 로고
    • Interaction of Pyridine with Acidic (H-ZSM5, H-β, H-MORD Zeolites) and Superacidic (H-Nafion Membrane) Systems: An IR Investigation
    • Buzzoni R., Bordiga S., Ricchiardi G., Lamberti C., Zecchina A., Bellussi G. Interaction of Pyridine with Acidic (H-ZSM5, H-β, H-MORD Zeolites) and Superacidic (H-Nafion Membrane) Systems: An IR Investigation. Langmuir 1996, 12:930-940.
    • (1996) Langmuir , vol.12 , pp. 930-940
    • Buzzoni, R.1    Bordiga, S.2    Ricchiardi, G.3    Lamberti, C.4    Zecchina, A.5    Bellussi, G.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.