Volumn 35, Issue 3, 2014, Pages 347-354

Catalytic oxidation of low-concentration CO at ambient temperature over supported PdCu catalysts

Author keywords

Ambient temperature; CO oxidation; Deactivation; Low concentration; Pd Cu catalyst

Indexed keywords

CATALYST DEACTIVATION; DISPERSIONS; MOISTURE; TEMPERATURE;

EID: 84891009335     PISSN: 09593330     EISSN: 1479487X     Source Type: Journal    
DOI: 10.1080/09593330.2013.828092     Document Type: Article
Times cited : (21)

References (41)
  • 2
    • 70349545565 scopus 로고    scopus 로고
    • 4 at moderate temperature for CO oxidation at-80°C
    • doi: 10.1016/j.jcat.2009.08.003
    • 4 at moderate temperature for CO oxidation at -80°C. J Catal. 2009; 267: 121-128. doi: 10.1016/j.jcat.2009.08.003
    • (2009) J Catal , vol.267 , pp. 121-128
    • Yu, Y.1    Takei, T.2    Ohashi, H.3    He, H.4    Zhang, X.5    Haruta, M.6
  • 3
    • 0009983459 scopus 로고
    • The mechanism of CO oxidation over Cu(110): Effect of CO gas energy
    • doi: 10.1007/BF00769083
    • Domagala ME, Campbell CT. The mechanism of CO oxidation over Cu(110): effect of CO gas energy. Catal Lett. 1991; 9: 65-70. doi: 10.1007/BF00769083
    • (1991) Catal Lett , vol.9 , pp. 65-70
    • Domagala, M.E.1    Campbell, C.T.2
  • 6
    • 0038660642 scopus 로고    scopus 로고
    • The removal of carbon monoxide by iron oxide nanoparticles
    • doi: 10.1016/S0926-3373(02)00297-7
    • Li P, Miser DE, Rabiei S, Yadav RT, Hajaligol MR. The removal of carbon monoxide by iron oxide nanoparticles. Appl Catal B: Environ. 2003; 43: 151-162. doi: 10.1016/S0926-3373(02)00297-7
    • (2003) Appl Catal B: Environ , vol.43 , pp. 151-162
    • Li, P.1    Miser, D.E.2    Rabiei, S.3    Yadav, R.T.4    Hajaligol, M.R.5
  • 7
    • 84857033527 scopus 로고    scopus 로고
    • Low temperature CO oxidation over Fe-Co mixed oxide nanocatalysts
    • doi: 10.1016/j.cej.2012.01.017
    • Ravandi AB, Rezaei M. Low temperature CO oxidation over Fe-Co mixed oxide nanocatalysts. Chem Eng J. 2012; 184: 141-146. doi: 10.1016/j.cej.2012.01.017
    • (2012) Chem Eng J , vol.184 , pp. 141-146
    • Ravandi, A.B.1    Rezaei, M.2
  • 8
    • 0041914646 scopus 로고    scopus 로고
    • The preparation and activity of copper zinc oxide catalysts for ambient temperature carbon monoxide oxidation
    • doi: 10.1016/S0920-5861(03)00264-5
    • Taylor SH, Hutchings GJ, Mirzaei AA. The preparation and activity of copper zinc oxide catalysts for ambient temperature carbon monoxide oxidation. Catal Today. 2003; 84: 113-119. doi: 10.1016/S0920-5861(03)00264-5
    • (2003) Catal Today , vol.84 , pp. 113-119
    • Taylor, S.H.1    Hutchings, G.J.2    Mirzaei, A.A.3
  • 9
    • 65649094164 scopus 로고    scopus 로고
    • Copper manganese oxide catalysts for ambient temperature carbon monoxide oxidation: Effect of calcinations on activity
    • doi: 10.1016/j.molcata.2008.10.027
    • Jones C, Cole KJ, Taylor SH, Crudace MJ, Hutchings GJ. Copper manganese oxide catalysts for ambient temperature carbon monoxide oxidation: effect of calcinations on activity. J Mol Catal A: Chem. 2009; 305: 121-124. doi: 10.1016/j.molcata.2008.10.027
    • (2009) J Mol Catal A: Chem , vol.305 , pp. 121-124
    • Jones, C.1    Cole, K.J.2    Taylor, S.H.3    Crudace, M.J.4    Hutchings, G.J.5
  • 11
    • 0009746572 scopus 로고
    • Gold catalysts prepared by coprecipitation for low-temperature oxidation of hydrogen and of carbon monoxide
    • doi: 10.1016/0021-9517(89)90034-1
    • Haruta M, Yamada N, Kobayashi T, Iijima S. Gold catalysts prepared by coprecipitation for low-temperature oxidation of hydrogen and of carbon monoxide. J Catal. 1989; 115: 301-309. doi: 10.1016/0021-9517(89)90034-1
    • (1989) J Catal , vol.115 , pp. 301-309
    • Haruta, M.1    Yamada, N.2    Kobayashi, T.3    Iijima, S.4
  • 12
    • 78049396118 scopus 로고    scopus 로고
    • 3 catalyst for low temperature CO oxidation
    • doi: 10.1039/c0cc02776f
    • 3 catalyst for low temperature CO oxidation. Chem Commun. 2010; 46: 8433-8435. doi: 10.1039/c0cc02776f
    • (2010) Chem Commun , vol.46 , pp. 8433-8435
    • Shen, Y.1    Lu, G.2    Guo, Y.3    Wang, Y.4
  • 13
    • 47249151833 scopus 로고    scopus 로고
    • 2 catalysts prepared via oxalate coprecipitation
    • doi: 10.1007/s10562-008-9485-6
    • 2 catalysts prepared via oxalate coprecipitation. Catal Lett. 2008; 124: 74-79. doi: 10.1007/s10562-008-9485-6
    • (2008) Catal Lett , vol.124 , pp. 74-79
    • Frey, K.1    Yablokov, V.2    Melaet, G.3    Guczi, L.4    Kruse, N.5
  • 14
    • 77955561313 scopus 로고    scopus 로고
    • x support for oxygen supply during reactions
    • doi: 10.1016/j.jcat.2010.05.022
    • x support for oxygen supply during reactions. J Catal. 2010; 274: 1-10. doi: 10.1016/j.jcat.2010.05.022
    • (2010) J Catal , vol.274 , pp. 1-10
    • Liu, L.1    Zhou, F.2    Wang, L.3    Qi, X.4    Shi, F.5    Deng, Y.6
  • 16
    • 0003161296 scopus 로고    scopus 로고
    • Process development for low temperature CO oxidation in the presence of water and halogen compounds
    • doi: 10.1016/S0920-5861(99)00168-6
    • Lee JS, Park ED, Song BJ. Process development for low temperature CO oxidation in the presence of water and halogen compounds. Catal Today. 1999; 54: 57-64. doi: 10.1016/S0920-5861(99)00168-6
    • (1999) Catal Today , vol.54 , pp. 57-64
    • Lee, J.S.1    Park, E.D.2    Song, B.J.3
  • 18
    • 39349111856 scopus 로고    scopus 로고
    • Low temperature CO oxidation over supported Pt catalysts prepared by colloid-deposition method
    • doi: 10.1016/j.catcom.2007.10.016
    • Li S, Liu G, Lian H, Jia M, Zhao G, Jiang D, Zhang W. Low temperature CO oxidation over supported Pt catalysts prepared by colloid-deposition method. Catal Commun. 2008; 9: 1045-1049. doi: 10.1016/j.catcom.2007.10.016
    • (2008) Catal Commun , vol.9 , pp. 1045-1049
    • Li, S.1    Liu, G.2    Lian, H.3    Jia, M.4    Zhao, G.5    Jiang, D.6    Zhang, W.7
  • 19
    • 0000065345 scopus 로고
    • 2 dispersed on alumina or carbon
    • doi: 10.1016/0021-9517(91)90179-8
    • 2 dispersed on alumina or carbon. J Catal. 1994; 127: 465-488. doi: 10.1016/0021-9517(91)90179-8
    • (1994) J Catal , vol.127 , pp. 465-488
    • Choi, K.I.1    Vannice, M.A.2
  • 20
    • 0002879901 scopus 로고    scopus 로고
    • Effect of surface treatment of the support on CO oxidation over carbon-supported Wacker-Type catalysts
    • doi: 10.1006/jcat.2000.2879
    • Park ED, Lee JS. Effect of surface treatment of the support on CO oxidation over carbon-supported Wacker-Type catalysts. J Catal. 2000; 193: 5-15. doi: 10.1006/jcat.2000.2879
    • (2000) J Catal , vol.193 , pp. 5-15
    • Park, E.D.1    Lee, J.S.2
  • 21
    • 0001286759 scopus 로고
    • 3 or carbon
    • doi: 10.1016/0021-9517(91)90180-C
    • 3 or carbon. J Catal. 1991; 127: 489-511. doi: 10.1016/0021-9517(91) 90180-C
    • (1991) J Catal , vol.127 , pp. 489-511
    • Choi, K.I.1    Vannice, M.A.2
  • 22
    • 0028751378 scopus 로고
    • 2 catalysts for carbon monoxide oxidation 1. Effect of catalyst composition and reaction conditions
    • doi: 10.1016/0926-3373(94)00029-8
    • 2 catalysts for carbon monoxide oxidation 1. Effect of catalyst composition and reaction conditions. Appl Catal B: Environ. 1994; 5: 103-115. doi: 10.1016/0926-3373(94)00029-8
    • (1994) Appl Catal B: Environ , vol.5 , pp. 103-115
    • Kim, K.D.1    Nam, I.S.2    Chung, J.S.3    Lee, J.S.4    Ryu, S.G.5    Yang, Y.S.6
  • 26
    • 84875159704 scopus 로고    scopus 로고
    • On the synergetic catalytic effect in heterogeneous nanocomposite catalysts
    • Shi J. On the synergetic catalytic effect in heterogeneous nanocomposite catalysts. Catal Rev. 2013; 113: 2139-2181.
    • (2013) Catal Rev , vol.113 , pp. 2139-2181
    • Shi, J.1
  • 27
    • 0035972386 scopus 로고    scopus 로고
    • The influence of the support on the activity and selectivity of Pd in CO hydrogenation
    • doi: 10.1016/S0926-860X(01)00465-3
    • Shen W, Okumura M, Matsumura Y, Haruta M. The influence of the support on the activity and selectivity of Pd in CO hydrogenation. Appl Catal A: Gen. 2001; 213: 225-232. doi: 10.1016/S0926-860X(01)00465-3
    • (2001) Appl Catal A: Gen , vol.213 , pp. 225-232
    • Shen, W.1    Okumura, M.2    Matsumura, Y.3    Haruta, M.4
  • 28
    • 84948487488 scopus 로고
    • Hydrogen spillover
    • doi: 10.1080/01614947408071861
    • Sermon PA, Bond GC. Hydrogen spillover. Catal Rev. 1974; 8: 211-239. doi: 10.1080/01614947408071861
    • (1974) Catal Rev , vol.8 , pp. 211-239
    • Sermon, P.A.1    Bond, G.C.2
  • 29
    • 0030567888 scopus 로고    scopus 로고
    • Alloy formation and stability in PdCu bimetallic catalysts
    • doi: 10.1021/jp9608133
    • Garcia MF, Anderson JA, Haller GL. Alloy formation and stability in PdCu bimetallic catalysts. J Phys Chem. 1996; 100: 16247-16254. doi: 10.1021/jp9608133
    • (1996) J Phys Chem , vol.100 , pp. 16247-16254
    • Garcia, M.F.1    Anderson, J.A.2    Haller, G.L.3
  • 30
    • 0035147988 scopus 로고    scopus 로고
    • XPS and TPR examination of γ-alumina-supported Pd-Cu catalysts
    • doi: 10.1016/S0926-860X(00)00589-5
    • Batista J, Pintar A, Mandrino D, Jenko M, Martin V. XPS and TPR examination of γ-alumina-supported Pd-Cu catalysts. Appl Catal A: Gen. 2001; 206: 113-124. doi: 10.1016/S0926-860X(00)00589-5
    • (2001) Appl Catal A: Gen , vol.206 , pp. 113-124
    • Batista, J.1    Pintar, A.2    Mandrino, D.3    Jenko, M.4    Martin, V.5
  • 31
    • 0000304687 scopus 로고    scopus 로고
    • Effects of copper phase on CO oxidation over supported Wacker-Type catalysts
    • doi: 10.1006/jcat.1998.2263
    • Park ED, Lee JS. Effects of copper phase on CO oxidation over supported Wacker-Type catalysts. J Catal. 1998; 180: 123-131. doi: 10.1006/jcat.1998.2263
    • (1998) J Catal , vol.180 , pp. 123-131
    • Park, E.D.1    Lee, J.S.2
  • 32
    • 84858286826 scopus 로고    scopus 로고
    • x on CO oxidation over supported Wacker-Type catalysts
    • doi: 10.1016/j.fuel.2011.12.005
    • x on CO oxidation over supported Wacker-Type catalysts. Fuel. 2012; 96: 440-445. doi: 10.1016/j.fuel.2011.12.005
    • (2012) Fuel , vol.96 , pp. 440-445
    • Wang, L.1    Feng, Y.2    Zhang, Y.3    Lou, Y.4    Lu, G.5    Guo, Y.6
  • 33
    • 0000633618 scopus 로고    scopus 로고
    • Infrared study of oxygen adsorption and activation on cerium-zirconium mixed oxides
    • doi: 10.1006/jcat.2000.3023
    • Descorme C, Madier Y, Duprez D. Infrared study of oxygen adsorption and activation on cerium-zirconium mixed oxides. J Catal. 2000; 196: 167-173. doi: 10.1006/jcat.2000.3023
    • (2000) J Catal , vol.196 , pp. 167-173
    • Descorme, C.1    Madier, Y.2    Duprez, D.3
  • 34
    • 3242748329 scopus 로고    scopus 로고
    • Recent advances in automobile exhaust catalysts
    • doi: 10.1016/j.cattod.2004.04.048
    • Matsumoto S. Recent advances in automobile exhaust catalysts. Catal Today. 2004; 90: 183-190. doi: 10.1016/j.cattod.2004.04.048
    • (2004) Catal Today , vol.90 , pp. 183-190
    • Matsumoto, S.1
  • 35
    • 0035742004 scopus 로고    scopus 로고
    • Reaction kinetics on heterogeneous model catalysts: The CO oxidation on alumina-supported Pd particles
    • doi: 10.1006/jcat.2001.3374
    • Hoffmann J, Mesusel I, Hartmann J, Libuda J, Freund HJ. Reaction kinetics on heterogeneous model catalysts: the CO oxidation on alumina-supported Pd particles. J Catal. 2001; 204: 378-392. doi: 10.1006/jcat.2001.3374
    • (2001) J Catal , vol.204 , pp. 378-392
    • Hoffmann, J.1    Mesusel, I.2    Hartmann, J.3    Libuda, J.4    Freund, H.J.5
  • 37
    • 58649111959 scopus 로고    scopus 로고
    • Preparation of highly effective ferric hydroxide supported noble metal catalysts for CO oxidations: From gold to palladium
    • doi: 10.1016/j.jcat.2008.11.012
    • Qiao B, Liu L, Zhang J, Deng Y. Preparation of highly effective ferric hydroxide supported noble metal catalysts for CO oxidations: from gold to palladium. J Catal. 2009; 261: 241-244. doi: 10.1016/j.jcat.2008.11.012
    • (2009) J Catal , vol.261 , pp. 241-244
    • Qiao, B.1    Liu, L.2    Zhang, J.3    Deng, Y.4
  • 39
    • 78650169340 scopus 로고    scopus 로고
    • Oxygen-enhanced water gas shift on ceria-supported PdCu and PtCu bimetallic catalysts
    • doi: 10.1016/j.jcat.2010.10.014
    • Kugai J, Miller JT, Guo N, Song C. Oxygen-enhanced water gas shift on ceria-supported PdCu and PtCu bimetallic catalysts. J Catal. 2011; 277: 46-43. doi: 10.1016/j.jcat.2010.10.014
    • (2011) J Catal , vol.277 , pp. 46-43
    • Kugai, J.1    Miller, J.T.2    Guo, N.3    Song, C.4
  • 40
    • 79959381321 scopus 로고    scopus 로고
    • Recent advances in catalytic hydrogenation of carbon dioxide
    • doi: 10.1039/c1cs15008a
    • Wang W, Wang S, Ma X, Gong J. Recent advances in catalytic hydrogenation of carbon dioxide. Chem Soc Rev. 2011; 40: 3703-3727. doi: 10.1039/c1cs15008a
    • (2011) Chem Soc Rev , vol.40 , pp. 3703-3727
    • Wang, W.1    Wang, S.2    Ma, X.3    Gong, J.4
  • 41
    • 84862773085 scopus 로고    scopus 로고
    • Oxidation of formaldehyde over Pd/Beta catalyst
    • doi: 10.1016/j.cej.2012.04.028
    • Park SJ, Bae I, Nam IS, Cho BK, Jung SM, Lee JH. Oxidation of formaldehyde over Pd/Beta catalyst. Chem Eng J. 2012; 195-196: 392-402. doi: 10.1016/j.cej.2012.04.028
    • (2012) Chem Eng J , vol.195-196 , pp. 392-402
    • Park, S.J.1    Bae, I.2    Nam, I.S.3    Cho, B.K.4    Jung, S.M.5    Lee, J.H.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.