Enhancement of the compressive strength of highly porous Al 2O3 foam through crack healing and improvement of the surface condition by dip-coating
|
Author keywords
Alumina; Compressive strength; Dip coating; Porous ceramics
|
Indexed keywords
DIFFERENT PARTICLE SIZES;
DIP COATING;
DIP-COATING PROCESS;
HIGH-TEMPERATURE FILTRATION;
LIGHTWEIGHT MATERIALS;
POROUS CERAMICS;
STRUCTURAL COMPONENT;
SURFACE CONDITIONS;
ALUMINA;
ALUMINUM;
CERAMIC MATERIALS;
COATINGS;
COMPRESSIVE STRENGTH;
CRACKS;
INDUSTRIAL APPLICATIONS;
INTERFACES (MATERIALS);
PARTICLE SIZE;
POROSITY;
SINTERING;
SURFACES;
ALUMINUM COATINGS;
|
EID: 84889096008
PISSN: 02728842
EISSN: None
Source Type: Journal
DOI: 10.1016/j.ceramint.2013.09.057 Document Type: Article |