메뉴 건너뛰기




Volumn 580, Issue SUPPL1, 2013, Pages

Degradation mechanisms of high-energy bipolar nickel metal hydride battery with AB5 and A2B7 alloys

Author keywords

Electrochemical reactions; Failure mode; Hydrogen absorbing materials; Metal hydride electrode

Indexed keywords

CAPACITY DEGRADATION; DEGRADATION MECHANISM; ELECTROCHEMICAL REACTIONS; HYDROGEN ABSORBING MATERIAL; METAL HYDRIDE ALLOYS; METAL HYDRIDE ELECTRODES; NICKEL/METAL HYDRIDE BATTERY; X-RAY ENERGY DISPERSIVE SPECTROSCOPY;

EID: 84886719544     PISSN: 09258388     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jallcom.2013.03.014     Document Type: Article
Times cited : (35)