Volumn 33, Issue , 2013, Pages 381-386

Corrosion failure analysis of galvanized steel pipes in a water irrigation system

Author keywords

Acid corrosion; Creek water; Galvanized steel pipes; Impingement; Irrigation system

Indexed keywords

ACID CORROSION; CHEMICAL AND PHYSICAL ANALYSIS; CORROSION FAILURE ANALYSIS; GALVANIZED STEEL PIPES; IMPINGEMENT; IRRIGATION SYSTEMS; MANUFACTURING DEFECTS; MICRO-STRUCTURAL CHARACTERIZATION;

EID: 84882581448     PISSN: 13506307     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.engfailanal.2013.06.024     Document Type: Article
Times cited : (20)

References (18)
  • 1
    • 84882642443 scopus 로고    scopus 로고
    • CITRUSBR, Brazilian Association of Citrus Exporters, Orange [Online]. <>. [accessed 14.05.13].
    • CITRUSBR, Brazilian Association of Citrus Exporters, Orange [Online]. <>. [accessed 14.05.13]. http://www.citrusbr.com/en/citrusbr/subjects/citrus.asp.
  • 2
    • 84882565663 scopus 로고    scopus 로고
    • EMBRAPA, Brazilian Agricultural Research Corporation, Clima. <>. [accessed 14. 05. 13].
    • EMBRAPA, Brazilian Agricultural Research Corporation, Clima. <>. [accessed 14. 05. 13]. http://sistemasdeproducao.cnptia.embrapa.br/FontesHTML/Citros/CitrosBahia_2ed/clima.htm.
  • 3
    • 0034478822 scopus 로고    scopus 로고
    • The metallurgy of zinc-coated steel
    • Marder A.R. The metallurgy of zinc-coated steel. Prog. Mater. Sci. 2000, 45:191-271.
    • (2000) Prog. Mater. Sci. , vol.45 , pp. 191-271
    • Marder, A.R.1
  • 6
    • 84882635742 scopus 로고    scopus 로고
    • Zinc
    • John Wiley & Sons Inc., New Jersey, R. Winston Revie (Ed.)
    • Zhang X.G. Zinc. Uhlig's corrosion handbook 2011, 879-892. John Wiley & Sons Inc., New Jersey. 3rd ed. R. Winston Revie (Ed.).
    • (2011) Uhlig's corrosion handbook , pp. 879-892
    • Zhang, X.G.1
  • 7
    • 84882667408 scopus 로고    scopus 로고
    • AGA, American Galvanizers Association, In Water. <>. [accessed 14.05.13].
    • AGA, American Galvanizers Association, In Water. <>. [accessed 14.05.13]. http://www.galvanizeit.org/about-hot-dip-galvanizing/how-long-does-hdg-last/in-water.
  • 10
    • 33645963105 scopus 로고    scopus 로고
    • Erosion corrosion of pump impeller of cyclic cooling water system
    • Ariely S., Khentov A. Erosion corrosion of pump impeller of cyclic cooling water system. Eng Fail Anal 2006, 13:925-932.
    • (2006) Eng Fail Anal , vol.13 , pp. 925-932
    • Ariely, S.1    Khentov, A.2
  • 12
    • 0033370366 scopus 로고    scopus 로고
    • Control of the growth of zinc-iron phases in the hot-dip galvanizing process
    • Culcasi J.D., Seré P.R., Elsner C.I., Di Sarli A.R. Control of the growth of zinc-iron phases in the hot-dip galvanizing process. Surf Coat Tech 1999, 122:21-23.
    • (1999) Surf Coat Tech , vol.122 , pp. 21-23
    • Culcasi, J.D.1    Seré, P.R.2    Elsner, C.I.3    Di Sarli, A.R.4
  • 13
    • 56949098389 scopus 로고    scopus 로고
    • Corrosion mechanism of hot-dip galvanised reinforcement bar in cracked concrete
    • Sistonen E., Cwirzen A., Puttonen J. Corrosion mechanism of hot-dip galvanised reinforcement bar in cracked concrete. Corros Sci 2008, 50:3416-3428.
    • (2008) Corros Sci , vol.50 , pp. 3416-3428
    • Sistonen, E.1    Cwirzen, A.2    Puttonen, J.3
  • 14
    • 33344457003 scopus 로고    scopus 로고
    • Corrosion behaviour in concrete of three differently galvanized steel bars
    • Bellezze T., Malavolta M., Quaranta A., Ruffini N., Roventi G. Corrosion behaviour in concrete of three differently galvanized steel bars. Cem Concr Comp 2006, 28:246-255.
    • (2006) Cem Concr Comp , vol.28 , pp. 246-255
    • Bellezze, T.1    Malavolta, M.2    Quaranta, A.3    Ruffini, N.4    Roventi, G.5
  • 16
    • 84882655407 scopus 로고
    • Metals handbook, Corrosion, 9th ed, ASTM, INTERNATIONAL
    • Metals handbook, vol. 13, Corrosion, 9th ed, ASTM, INTERNATIONAL, 1987.
    • (1987) , vol.13
  • 17
    • 11144249127 scopus 로고    scopus 로고
    • Total hardness of surface waters in São Paulo State (Brazil)
    • Aragão M.A., Buratini S.V., Bertoletti E. Total hardness of surface waters in São Paulo State (Brazil). Acta Limnol Bras 2003, 15:15-18.
    • (2003) Acta Limnol Bras , vol.15 , pp. 15-18
    • Aragão, M.A.1    Buratini, S.V.2    Bertoletti, E.3
  • 18
    • 84882690794 scopus 로고    scopus 로고
    • USGS, U.S. Geological Survey, Water Hardness and Alkalinity. <>. [accessed 14.05.13].
    • USGS, U.S. Geological Survey, Water Hardness and Alkalinity. <>. [accessed 14.05.13]. http://water.usgs.gov/owq/hardness-alkalinity.html#hardness.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.