Volumn 55, Issue , 2013, Pages 407-420

HDPE/Cu-nanofiber nanocomposites with enhanced mechanical and UV stability properties

Author keywords

A. Nano structures; B. Environmental degradation; B. Mechanical properties; D. Surface analysis

Indexed keywords

ACOUSTIC MICROSCOPY; FINE DISPERSIONS; FTIR MEASUREMENTS; FTIR SPECTROSCOPY; MACROMOLECULAR CHAIN; OXYGEN DIFFUSION; SEM MICROGRAPHS; YOUNG'S MODULUS;

EID: 84881137801     PISSN: 13598368     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.compositesb.2013.07.002     Document Type: Article
Times cited : (45)

References (61)
  • 1
    • 74249084994 scopus 로고    scopus 로고
    • Nanocomposites in food packaging
    • A. Arora, and G.W. Padua Nanocomposites in food packaging J Food Sci 75 2010 R43 R49
    • (2010) J Food Sci , vol.75
    • Arora, A.1    Padua, G.W.2
  • 2
    • 84863688891 scopus 로고    scopus 로고
    • Polyethylene and biodegradable mulches for agricultural applications: A review
    • in press (doi 10.1007/s13593-011-0068-3)
    • Kasirajan S, Ngouajio M. Polyethylene and biodegradable mulches for agricultural applications: a review. Agron Sustain Dev; in press (doi 10.1007/s13593-011-0068-3).
    • Agron Sustain Dev
    • Kasirajan, S.1    Ngouajio, M.2
  • 3
    • 59849114686 scopus 로고    scopus 로고
    • Thermal degradation mechanism of HDPE nanocomposites containing fumed silica nanoparticles
    • K. Chrissafis, K.M. Paraskevopoulos, E. Pavlidou, and D. Bikiaris Thermal degradation mechanism of HDPE nanocomposites containing fumed silica nanoparticles Thermochim Acta 485 1-2 2009 65 71
    • (2009) Thermochim Acta , vol.485 , Issue.12 , pp. 65-71
    • Chrissafis, K.1    Paraskevopoulos, K.M.2    Pavlidou, E.3    Bikiaris, D.4
  • 4
    • 0037068109 scopus 로고    scopus 로고
    • Influence of clay exfoliation on the physical properties of montmorillonite/polyethylene composites
    • T.G. Gopakumar, J.A. Lee, M. Kontopoulou, and J.S. Parent Influence of clay exfoliation on the physical properties of montmorillonite/polyethylene composites Polymer 43 20 2002 5483 5491
    • (2002) Polymer , vol.43 , Issue.20 , pp. 5483-5491
    • Gopakumar, T.G.1    Lee, J.A.2    Kontopoulou, M.3    Parent, J.S.4
  • 5
    • 69949158893 scopus 로고    scopus 로고
    • Wear behavior of carbon nanotube/high density polyethylene composites
    • B.B. Johnson, M.H. Santare, J.E. Novotny, and S.G. Advani Wear behavior of carbon nanotube/high density polyethylene composites Mech Mater 41 10 2009 1108 1115
    • (2009) Mech Mater , vol.41 , Issue.10 , pp. 1108-1115
    • Johnson, B.B.1    Santare, M.H.2    Novotny, J.E.3    Advani, S.G.4
  • 6
    • 0348230367 scopus 로고    scopus 로고
    • Processing and properties of MWNT/HDPE composites
    • Y. Zou, Y. Feng, L. Wang, and X. Liu Processing and properties of MWNT/HDPE composites Carbon 42 2 2004 271 277
    • (2004) Carbon , vol.42 , Issue.2 , pp. 271-277
    • Zou, Y.1    Feng, Y.2    Wang, L.3    Liu, X.4
  • 7
    • 0142126763 scopus 로고    scopus 로고
    • Melt processing and mechanical property characterization of multi-walled carbon nanotube/high density polyethylene (MWNT/HDPE) composite films
    • W. Tang, M.H. Santare, and S.G. Advani Melt processing and mechanical property characterization of multi-walled carbon nanotube/high density polyethylene (MWNT/HDPE) composite films Carbon 41 14 2003 2779 2785
    • (2003) Carbon , vol.41 , Issue.14 , pp. 2779-2785
    • Tang, W.1    Santare, M.H.2    Advani, S.G.3
  • 8
    • 68749088421 scopus 로고    scopus 로고
    • Comparative study of the effect of different nanoparticles on the mechanical properties, permeability, and thermal degradation mechanism of HDPE
    • K. Chrissafis, K.M. Paraskevopoulos, I. Tsiaoussis, and D. Bikiaris Comparative study of the effect of different nanoparticles on the mechanical properties, permeability, and thermal degradation mechanism of HDPE J Appl Polym Sci 114 3 2009 1606 1618
    • (2009) J Appl Polym Sci , vol.114 , Issue.3 , pp. 1606-1618
    • Chrissafis, K.1    Paraskevopoulos, K.M.2    Tsiaoussis, I.3    Bikiaris, D.4
  • 9
    • 0029394462 scopus 로고
    • Photooxidative degradation of polyethylene containing flame retardants by monochromatic light
    • A. Torikai, K. Chigita, F. Okisaki, and M. Nageta Photooxidative degradation of polyethylene containing flame retardants by monochromatic light J Appl Polym Sci 58 1995 685 690
    • (1995) J Appl Polym Sci , vol.58 , pp. 685-690
    • Torikai, A.1    Chigita, K.2    Okisaki, F.3    Nageta, M.4
  • 10
    • 0033075093 scopus 로고    scopus 로고
    • Mineral filler influence on the photo-oxidation of high density polyethylene: I. Accelerated UV chamber exposure test
    • A. Valadez-Gonzalez, M. Cervantes-Uc J, and L. Veleva Mineral filler influence on the photo-oxidation of high density polyethylene: I. Accelerated UV chamber exposure test Polym Degrad Stabil 63 2 1999 253 260
    • (1999) Polym Degrad Stabil , vol.63 , Issue.2 , pp. 253-260
    • Valadez-Gonzalez, A.1    Cervantes-Uc, J.M.2    Veleva, L.3
  • 11
    • 1542790701 scopus 로고    scopus 로고
    • Mineral filler influence on the photo-oxidation mechanism degradation of high density polyethylene Part II: Natural exposure test
    • A. Valadez-Gonzalez, and L. Veleva Mineral filler influence on the photo-oxidation mechanism degradation of high density polyethylene Part II: Natural exposure test Polym Degrad Stabil 83 1 2004 139 148
    • (2004) Polym Degrad Stabil , vol.83 , Issue.1 , pp. 139-148
    • Valadez-Gonzalez, A.1    Veleva, L.2
  • 13
    • 14544306415 scopus 로고    scopus 로고
    • Effects of inorganic fillers on the natural photo-oxidation of high-density polyethylene
    • DOI 10.1016/j.polymdegradstab.2004.11.011, PII S0141391004003921
    • R. Yang, J. Yu, Y. Liu, and K. Wang Effects of inorganic fillers on the natural photooxidation of high-density polyethylene Polym Degrad Stabil 88 2 2005 333 340 (Pubitemid 40304759)
    • (2005) Polymer Degradation and Stability , vol.88 , Issue.2 , pp. 333-340
    • Yang, R.1    Yu, J.2    Liu, Y.3    Wang, K.4
  • 14
    • 33947611334 scopus 로고    scopus 로고
    • Solid-phase photocatalytic degradation of polyethylene plastic under UV and solar light irradiation
    • DOI 10.1016/j.molcata.2006.12.012, PII S1381116906014270
    • X. Zhao, Z. Li, Y. Chen, L. Shi, and Y. Zhu Solid-phase photocatalytic degradation of polyethylene plastic under UV and solar light irradiation J Mol Catal A Chem 268 1-2 2007 101 106 (Pubitemid 46484451)
    • (2007) Journal of Molecular Catalysis A: Chemical , vol.268 , Issue.1-2 , pp. 101-106
    • Zhao, X.U.1    Li, Z.2    Chen, Y.3    Shi, L.4    Zhu, Y.5
  • 18
    • 0029848731 scopus 로고    scopus 로고
    • Copper toxicity towards Saccharomyces cerevisiae: Dependence on plasma membrane fatty acid composition
    • S.V. Avery, N.G. Howlett, and S. Radice Copper toxicity towards Saccharomyces cerevisiae: dependence on plasma membrane fatty acid composition Appl Environ Microbiol 62 1996 3960
    • (1996) Appl Environ Microbiol , vol.62 , pp. 3960
    • Avery, S.V.1    Howlett, N.G.2    Radice, S.3
  • 19
    • 0030249657 scopus 로고    scopus 로고
    • An electron spin resonance study and antimicrobial activity of copper(II)-phenanthroline complexes
    • M.A. Zoruddu, S. Zanetti, R. Pogni, and R. Basosi An electron spin resonance study and antimicrobial activity of copper(II)-phenanthroline complexes J Inorg Biochem 63 4 1996 291
    • (1996) J Inorg Biochem , vol.63 , Issue.4 , pp. 291
    • Zoruddu, M.A.1    Zanetti, S.2    Pogni, R.3    Basosi, R.4
  • 20
    • 0035971321 scopus 로고    scopus 로고
    • Synthesis, characterization, antifungal properties and X-ray crystal structures of five- and six-coordinate copper(II) complexes of the 6-methyl-2-formylpyridine4N-dimethylthiosemicarbazone
    • M.A. Ali, A.H. Mirza, A.M.S. Hossain, and M. Nazimuddin Synthesis, characterization, antifungal properties and X-ray crystal structures of five- and six-coordinate copper(II) complexes of the 6-methyl-2-formylpyridine4N- dimethylthiosemicarbazone Polyhedron 20 9-10 2001 1045
    • (2001) Polyhedron , vol.20 , Issue.910 , pp. 1045
    • Ali, M.A.1    Mirza, A.H.2    Hossain, A.M.S.3    Nazimuddin, M.4
  • 21
    • 0037051776 scopus 로고    scopus 로고
    • Synthesis, characterization and biological activity of two new polymeric copper(II) complexes with α-ketoglutaric acid thiosemicarbazone
    • M. Belicchi Ferrari, F. Bisceglie, G. Gasparri Fava, G. Pelosi, R. Tarasconi Albertini, and S. Pinelli Synthesis, characterization and biological activity of two new polymeric copper(II) complexes with α-ketoglutaric acid thiosemicarbazone J Inorg Biochem 89 1-2 2002 36
    • (2002) J Inorg Biochem , vol.89 , Issue.12 , pp. 36
    • Belicchi Ferrari, M.1    Bisceglie, F.2    Gasparri Fava, G.3    Pelosi, G.4    Tarasconi Albertini, R.5    Pinelli, S.6
  • 22
    • 78650923992 scopus 로고    scopus 로고
    • Synthesis of copper-polystyrene nanocomposite particles using water in supercritical carbon dioxide medium and its antimicrobial activity
    • I.R. Kamrupi, and S.K. Dolui Synthesis of copper-polystyrene nanocomposite particles using water in supercritical carbon dioxide medium and its antimicrobial activity J Appl Polym Sci 120 2011 1027 1033
    • (2011) J Appl Polym Sci , vol.120 , pp. 1027-1033
    • Kamrupi, I.R.1    Dolui, S.K.2
  • 23
    • 0000296287 scopus 로고    scopus 로고
    • Characterization and Antimicrobial Activities of Some New Coordination Polymers
    • H.B. Pancholi, and M.M. Patel Characterization and antimicrobial activities of some new coordination polymers J Polym Mater 13 1996 261 267 (Pubitemid 126429559)
    • (1996) Journal of Polymer Materials , vol.13 , Issue.4 , pp. 261-267
    • Pancholi, H.B.1    Patel, M.M.2
  • 24
    • 84871773337 scopus 로고    scopus 로고
    • HDPE/Cu-nanofiber nanocomposites with enhanced antibacterial and oxygen barrier properties appropriate for food packaging applications
    • D.N. Bikiaris, and K.S. Triantafyllidis HDPE/Cu-nanofiber nanocomposites with enhanced antibacterial and oxygen barrier properties appropriate for food packaging applications Mater Lett 93 2013 1 4
    • (2013) Mater Lett , vol.93 , pp. 1-4
    • Bikiaris, D.N.1    Triantafyllidis, K.S.2
  • 25
    • 56349088266 scopus 로고    scopus 로고
    • Synthesis of ultralong copper nanowires by reduction of copper-amine complexes
    • Y.S. Cho, and Y.D. Huh Synthesis of ultralong copper nanowires by reduction of copper-amine complexes Mater Lett 63 2 2009 227 229
    • (2009) Mater Lett , vol.63 , Issue.2 , pp. 227-229
    • Cho, Y.S.1    Huh, Y.D.2
  • 26
    • 84881133514 scopus 로고    scopus 로고
    • Acoustic microscopy for really time and non-destructive analysis of tablet coating thickness
    • G. Karagiannis, D. Alexiadis, A. Damtsios, I. Koutri, and D. Bikiaris Acoustic microscopy for really time and non-destructive analysis of tablet coating thickness Int J Pharm 438 1-2 2012 33 44
    • (2012) Int J Pharm , vol.438 , Issue.12 , pp. 33-44
    • Karagiannis, G.1    Alexiadis, D.2    Damtsios, A.3    Koutri, I.4    Bikiaris, D.5
  • 27
    • 78149284788 scopus 로고    scopus 로고
    • Microstructure and properties of polypropylene/carbon nanotube nanocomposites
    • D. Bikiaris Microstructure and properties of polypropylene/carbon nanotube nanocomposites Materials 3 4 2010 2884 2946
    • (2010) Materials , vol.3 , Issue.4 , pp. 2884-2946
    • Bikiaris, D.1
  • 29
    • 77956443841 scopus 로고    scopus 로고
    • Oxidized multiwalled carbon nanotubes as effective reinforcement and thermal stability agents of poly(lactic acid) ligaments
    • K. Chrissafis, K.M. Paraskevopoulos, A. Jannakoudakis, T. Beslikas, and D. Bikiaris Oxidized multiwalled carbon nanotubes as effective reinforcement and thermal stability agents of poly(lactic acid) ligaments J Appl Polym Sci 118 5 2010 2712 2721
    • (2010) J Appl Polym Sci , vol.118 , Issue.5 , pp. 2712-2721
    • Chrissafis, K.1    Paraskevopoulos, K.M.2    Jannakoudakis, A.3    Beslikas, T.4    Bikiaris, D.5
  • 31
    • 79952607250 scopus 로고    scopus 로고
    • Micromechanism of surface and sub-surface deformation behavior of high density polyethylene containing dispersion of nanoparticles: An electron microscopy study and indenter-substrate interaction
    • P.K.C. Venkatasurya, Q. Yuan, and R.D.K. Misra Micromechanism of surface and sub-surface deformation behavior of high density polyethylene containing dispersion of nanoparticles: an electron microscopy study and indenter-substrate interaction Mech Mater 43 2011 254 268
    • (2011) Mech Mater , vol.43 , pp. 254-268
    • Venkatasurya, P.K.C.1    Yuan, Q.2    Misra, R.D.K.3
  • 32
    • 33644780820 scopus 로고    scopus 로고
    • On significant retention of impact strength in clay-reinforced high-density polyethylene (HDPE) nanocomposites
    • M. Tanniru, Q. Yuan, and R.D.K. Misra On significant retention of impact strength in clay-reinforced high-density polyethylene (HDPE) nanocomposites Polymer 47 6 2006 2133
    • (2006) Polymer , vol.47 , Issue.6 , pp. 2133
    • Tanniru, M.1    Yuan, Q.2    Misra, R.D.K.3
  • 33
    • 35649013194 scopus 로고    scopus 로고
    • Rheological investigation of the influence of molecular structure on natural and accelerated UV degradation of linear low density polyethylene
    • I.A. Husein Rheological investigation of the influence of molecular structure on natural and accelerated UV degradation of linear low density polyethylene Polym Degrad Stabil 92 11 2007 2026 2032
    • (2007) Polym Degrad Stabil , vol.92 , Issue.11 , pp. 2026-2032
    • Husein, I.A.1
  • 34
    • 67650266276 scopus 로고    scopus 로고
    • Effect of extrusion and photo-oxidation on polyethylene/clay nanocomposites
    • N.T. Dintcheva, S. Al-Malaika, and F.P. LaMantia Effect of extrusion and photo-oxidation on polyethylene/clay nanocomposites Polym Degrad Stabil 94 9 2009 1571 1588
    • (2009) Polym Degrad Stabil , vol.94 , Issue.9 , pp. 1571-1588
    • Dintcheva, N.T.1    Al-Malaika, S.2    Lamantia, F.P.3
  • 36
    • 52049101385 scopus 로고    scopus 로고
    • Photochemical stabilization of linear low-density polyethylene/clay nanocomposites: Towards durable nanocomposites
    • S. Morlat-Therias, E. Fanton, J.-L. Gardette, N.Tz. Dintcheva, F.P. La Mantia, and V. Malatesta Photochemical stabilization of linear low-density polyethylene/clay nanocomposites: towards durable nanocomposites Polym Degrad Stabil 93 10 2008 1776 1780
    • (2008) Polym Degrad Stabil , vol.93 , Issue.10 , pp. 1776-1780
    • Morlat-Therias, S.1    Fanton, E.2    Gardette, J.-L.3    Dintcheva, N.Tz.4    La Mantia, F.P.5    Malatesta, V.6
  • 38
    • 58149161541 scopus 로고    scopus 로고
    • Photo-oxidation behaviour of polyethylene/multi-wall carbon nanotube composite films
    • N.T. Dintcheva, F.P. La Mantia, and V. Malatesta Photo-oxidation behaviour of polyethylene/multi-wall carbon nanotube composite films Polym Degrad Stabil 94 2 2009 162 170
    • (2009) Polym Degrad Stabil , vol.94 , Issue.2 , pp. 162-170
    • Dintcheva, N.T.1    La Mantia, F.P.2    Malatesta, V.3
  • 39
    • 48549095053 scopus 로고    scopus 로고
    • Wood plastic composites weathering: Visual appearance and chemical changes
    • J.S. Fabiyi, A.G. McDonald, M.P. Wolcott, and P.R. Griffiths Wood plastic composites weathering: visual appearance and chemical changes Polym Degrad Stabil 93 8 2008 1405 1414
    • (2008) Polym Degrad Stabil , vol.93 , Issue.8 , pp. 1405-1414
    • Fabiyi, J.S.1    McDonald, A.G.2    Wolcott, M.P.3    Griffiths, P.R.4
  • 42
    • 26844458285 scopus 로고    scopus 로고
    • Degradation and stabilisation of poly(ethylene-stat-vinyl acetate): 1 - Spectroscopic and rheological examination of thermal and thermo-oxidative degradation mechanisms
    • DOI 10.1016/j.polymdegradstab.2005.04.034, PII S0141391005002065
    • M.R. Vazquez, C.M. Liauw, N.S. Allen, M. Edge, and E. Fontan Degradation and stabilisation of poly(ethylene-stat-vinyl acetate): 1 - spectroscopic and rheological examination of thermal and thermo-oxidative degradation mechanisms Polym Degrad Stabil 91 1 2006 154 164 (Pubitemid 41455153)
    • (2006) Polymer Degradation and Stability , vol.91 , Issue.1 , pp. 154-164
    • Rodriguez-Vazquez, M.1    Liauw, C.M.2    Allen, N.S.3    Edge, M.4    Fontan, E.5
  • 43
    • 65649105049 scopus 로고    scopus 로고
    • Investigating the role of metal oxidation state on the degradation behaviour of LDPE
    • P.K. Roy, P. Surekha, R. Raman, and C. Rajagopal Investigating the role of metal oxidation state on the degradation behaviour of LDPE Polym Degrad Stabil 94 7 2009 1033 1039
    • (2009) Polym Degrad Stabil , vol.94 , Issue.7 , pp. 1033-1039
    • Roy, P.K.1    Surekha, P.2    Raman, R.3    Rajagopal, C.4
  • 44
    • 61849130102 scopus 로고    scopus 로고
    • The role of organoclay and matrix type in photo-oxidation of polyolefin/clay nanocomposite films
    • L. Botta, N.T. Dintcheva, and F.P. La Mantia The role of organoclay and matrix type in photo-oxidation of polyolefin/clay nanocomposite films Polym Degrad Stabil 94 4 2009 712 718
    • (2009) Polym Degrad Stabil , vol.94 , Issue.4 , pp. 712-718
    • Botta, L.1    Dintcheva, N.T.2    La Mantia, F.P.3
  • 47
    • 0031108510 scopus 로고    scopus 로고
    • Effect of EAA and starch on the thermooxidative degradation of LDPE
    • PII S0141391096001930
    • D. Bikiaris, J. Prinos, and C. Panayiotou Effect of EAA and starch on the thermooxidative degradation of LDPE Polym Degrad Stabil 56 1 1997 1 9 (Pubitemid 127412147)
    • (1997) Polymer Degradation and Stability , vol.56 , Issue.1 , pp. 1-9
    • Bikiaris, D.1    Prinos, J.2    Panayiotou, C.3
  • 48
    • 0035400749 scopus 로고    scopus 로고
    • Artificial aging of high-density polyethylene by ultraviolet irradiation
    • DOI 10.1016/S0014-3057(00)00251-2, PII S0014305700002512
    • F. Carrasco, P. Pagès, S. Pascual, and X. Colom Artificial aging of high-density polyethylene by ultraviolet irradiation Eur Polym J 37 7 2001 1457 1464 (Pubitemid 32491677)
    • (2001) European Polymer Journal , vol.37 , Issue.7 , pp. 1457-1464
    • Carrasco, F.1    Pages, P.2    Pascual, S.3    Colom, X.4
  • 49
    • 0028484218 scopus 로고
    • Photodegradation of polyethylene films formulated with a titanium-based photosensitizer and titanium dioxide pigment
    • J.L. Angulo-Sanchez, H. Ortega-Ortiz, and S. Sanchez-Valdes Photodegradation of polyethylene films formulated with a titanium-based photosensitizer and titanium dioxide pigment J Appl Polym Sci 53 7 1994 847 856
    • (1994) J Appl Polym Sci , vol.53 , Issue.7 , pp. 847-856
    • Angulo-Sanchez, J.L.1    Ortega-Ortiz, H.2    Sanchez-Valdes, S.3
  • 52
    • 0008653886 scopus 로고    scopus 로고
    • Natural and Controlled Photo Aging of LDPE: Changes in Structural, Molecular and Surface Characteristics
    • J. Khan, and S.J. Hamid Natural and controlled photo aging of LDPE: changes in structural, molecular and surface characteristics J Polym Mater 15 1998 177 184 (Pubitemid 128461169)
    • (1998) Journal of Polymer Materials , vol.15 , Issue.2 , pp. 177-184
    • Khan, J.H.1    Hamid, S.H.2
  • 53
    • 27744539697 scopus 로고    scopus 로고
    • Processability and properties of re-graded, photo-oxidized post-consumer greenhouse films
    • DOI 10.1002/mame.200500180
    • F.P. La Mantia, and N.T. Dintcheva Processability and properties of re-graded photo-oxidized post-consumer greenhouse films Macromol Mater Eng 290 10 2005 970 975 (Pubitemid 41584138)
    • (2005) Macromolecular Materials and Engineering , vol.290 , Issue.10 , pp. 970-975
    • La Mantia, F.P.1    Dintcheva, N.T.2
  • 55
    • 34147141349 scopus 로고    scopus 로고
    • On striking variation in impact toughness of polyethylene-clay and polypropylene-clay nanocomposite systems: The effect of clay-polymer interaction
    • DOI 10.1016/j.msea.2006.12.069, PII S0921509306027183
    • C. Deshmane, Q. Yuan, R.S. Perkins, and R.D.K. Misra On striking variation in impact toughness of polyethylene-clay and polypropylene-clay nanocomposite systems: the effect of clay-polymer interaction Mater Sci Eng A 458 2007 150 157 (Pubitemid 46555036)
    • (2007) Materials Science and Engineering A , vol.458 , Issue.1-2 , pp. 150-157
    • Deshmane, C.1    Yuan, Q.2    Perkins, R.S.3    Misra, R.D.K.4
  • 56
    • 42749097035 scopus 로고    scopus 로고
    • Nanoscale near-surface deformation in polymer nanocomposites
    • Q. Yuan, N. Ramisetti, and R.D.K. Misra Nanoscale near-surface deformation in polymer nanocomposites Acta Mater 56 2008 2089 2100
    • (2008) Acta Mater , vol.56 , pp. 2089-2100
    • Yuan, Q.1    Ramisetti, N.2    Misra, R.D.K.3
  • 57
    • 41049115906 scopus 로고    scopus 로고
    • Structure and morphology of HDPE-g-MA/organoclay nanocomposites: Effects of the preparation procedures
    • S. Filippi, C. Marazzato, P. Magagnini, A. Famulari, P. Arosio, and S.V. Meille Structure and morphology of HDPE-g-MA/organoclay nanocomposites: effects of the preparation procedures Eur Polym J 44 4 2008 987 1002
    • (2008) Eur Polym J , vol.44 , Issue.4 , pp. 987-1002
    • Filippi, S.1    Marazzato, C.2    Magagnini, P.3    Famulari, A.4    Arosio, P.5    Meille, S.V.6
  • 58
    • 47249119739 scopus 로고    scopus 로고
    • Nanoparticle effects on the crystallization of polyethylene at elevated pressures
    • Q. Yuan, R. Gudavalli, and R.D.K. Misra Nanoparticle effects on the crystallization of polyethylene at elevated pressures Mater Sci Eng A492 2008 434 442
    • (2008) Mater Sci Eng , vol.492 A , pp. 434-442
    • Yuan, Q.1    Gudavalli, R.2    Misra, R.D.K.3
  • 60
    • 84863728775 scopus 로고    scopus 로고
    • The effect of oxygen on the irradiation process of ethylene-butene copolymer
    • M.D. Failla, A. Brandolin, C. Sarmoria, and E.M. Vallés The effect of oxygen on the irradiation process of ethylene-butene copolymer Polym Degrad Stabil 97 8 2012 1485 1494
    • (2012) Polym Degrad Stabil , vol.97 , Issue.8 , pp. 1485-1494
    • Failla, M.D.1    Brandolin, A.2    Sarmoria, C.3    Vallés, E.M.4
  • 61
    • 0037233216 scopus 로고    scopus 로고
    • Degradation profile of polyethylene after artificial accelerated weathering
    • J.V. Gulmine, P.R. Janissek, H.M. Heise, and L. Akcelrud Degradation profile of polyethylene after artificial accelerated weathering Polym Degrad Stabil 79 3 2003 385 397
    • (2003) Polym Degrad Stabil , vol.79 , Issue.3 , pp. 385-397
    • Gulmine, J.V.1    Janissek, P.R.2    Heise, H.M.3    Akcelrud, L.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.